Lyondellbasell Polybatch Blue 40395u Concentrate Based In Lldpe

LyondellBasell POLYBATCH™ Blue 40395U Concentrate Based In LLDPE

    • Product Name: LyondellBasell POLYBATCH™ Blue 40395U Concentrate Based In LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 477384
    Productname LyondellBasell POLYBATCH™ Blue 40395U Concentrate Based In LLDPE
    Producttype Color concentrate
    Carrierresin LLDPE
    Color Blue
    Form Pellets
    Density 1.05 g/cm³
    Meltflowrate 20 g/10 min at 190°C/2.16 kg
    Recommendedletdownratio 2-5%
    Processingmethods Injection molding, blow molding, film extrusion
    Compatiblepolymers Polyethylene and polypropylene
    Pigmentcontent 40%
    Moisturecontent <0.1%
    Processingtemperature 180-230°C
    Heatstability Up to 260°C
    Shelflife 24 months
    Storageconditions Dry, below 30°C
    Packaging 25 kg bags

    As an accredited LyondellBasell POLYBATCH™ Blue 40395U Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing The product is supplied in 25 kg bags, palletized as 40 bags per pallet (1,000 kg net weight).
    Container Loading (20′ FCL) Container Loading (20′ FCL): LyondellBasell POLYBATCH™ Blue 40395U Concentrate Based in LLDPE, palletized, securely stowed in dry container, ambient.
    Shipping LyondellBasell POLYBATCH™ Blue 40395U Concentrate Based In LLDPE is typically shipped as a non-hazardous, solid plastic color concentrate in 25 kg bags or bulk bags on pallets. It is not regulated by DOT, IMDG, or IATA; no UN number, hazard class, or packing group applies. Keep dry, avoid excessive heat, and use standard freight.
    Storage For LyondellBasell POLYBATCH™ Blue 40395U Concentrate Based in LLDPE, store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed and palletized off the floor to prevent moisture pickup and contamination. Segregate from strong oxidizers and incompatible materials. Avoid prolonged storage above ambient temperatures; protect from physical damage. Maintain good housekeeping. Follow manufacturer’s SDS.
    Shelf Life Typically 24 months from date of manufacture when stored unopened in original packaging, cool/dry, and away from direct sunlight.
    Application of LyondellBasell POLYBATCH™ Blue 40395U Concentrate Based In LLDPE

    The material under evaluation is a pelletised blue colour concentrate supplied in an LLDPE carrier resin. The carrier is selected for viscosity compatibility with polyethylene homopolymer and ethylene-α-olefin copolymer matrices across blown film, injection moulding, rotational moulding, extrusion blow moulding, pipe extrusion, and extrusion coating. Because the carrier is non-polar, the concentrate should not be combined with PET, polyamide, polycarbonate, or rigid PVC matrices; incompatible polar matrices produce visible delamination, pigment migration, and loss of mechanical integrity at the interface. The following scenarios are restricted to real downstream polyethylene conversion routes for which LLDPE-carrier colour concentrates are established industrial input materials. Each scenario records the applicable regulatory instrument, the formulation addition ratio, the downstream production process, and the terminal finished product type. Published data for this specific LyondellBasell grade configuration is limited outside the manufacturer’s controlled technical data sheet; therefore, all letdown ratios and processing windows must be confirmed on the converter’s own equipment and final article certification.

    Regulatory / test referenceScopeVerification boundary
    EU Regulation 10/2011Plastic materials and articles intended for food contactOverall migration and specific migration limits on final article per Annex I
    FDA 21 CFR 177.1520Olefin polymers in food-contact articlesMatrix conformance under intended food-type conditions
    FDA 21 CFR 178.3290Colorants for polymers in food-contact useColorant composition and end-use concentration limits
    REACH Regulation (EC) No 1907/2006SVHC and Annex XVII restrictionsSubstance registration and restricted metal screening
    RoHS Directive 2011/65/EUHazardous substances in electrical/electronic equipment and associated packagingCadmium, lead, mercury, chromium VI, PBB/PBDE limits
    CONEGUS state packaging heavy-metal restrictionsSum of lead, cadmium, mercury, hexavalent chromium ≤ 100 ppm
    ISO 1133-1:2022Melt flow rate of thermoplasticsCarrier and letdown compound viscosity comparison
    ASTM D638-14 / ISO 527-2Tensile properties of plasticsMechanical retention after colour concentrate addition

    Blown Film Extrusion: Melt Temperature and Frost-Line Control Boundaries

    On blown-film lines equipped with single-screw extruders of 25:1–30:1 L/D, low-shear barrier screws, and air-ring cooling, the concentrate is let down at 2.0–4.0 wt% into LLDPE or LDPE film resin. The LLDPE carrier is compatible with hexene- and octene-copolymer film grades, which limits melt pool disruption in the metering section of the screw. Typical settings are melt temperatures of 190–215 °C, die lip gaps of 1.6–2.0 mm, and blow-up ratios between 2.0:1 and 2.5:1. At film gauges below 25 µm, frost-line height should be kept below 25 cm; faster quench reduces pigment agglomeration but also lowers bubble stability, particularly when line speed exceeds 120 m/min. Colour speck formation is a production-scale failure mode when the screen pack is omitted or when the extruder barrel temperature profile is below 180 °C in the compression zone.

    In high-output operations with die diameters above 450 mm, die lip build-up has been observed when throughput exceeds 450 kg/h and the concentrate is added above 3.5 wt% without purge intervals. Batch-to-batch pellet bulk density variation greater than ±5% is associated with gravimetric feeder oscillations and screw surging. Regulatory compliance for flexible packaging follows EU Regulation 10/2011 where food contact is intended; the final film must also comply with FDA 21 CFR 177.1520 for the olefin polymer matrix and FDA 21 CFR 178.3290 for the colorant component. Heavy-metal restrictions are screened under the CONEG model legislation and EU Directive 94/62/EC. Terminal finished products are collation shrink film, industrial liners, and coloured agricultural overlay films.

    Polyethylene injection moulding plants running cold-runner tools with clamp forces from 1,200 to 8,000 kN dose the concentrate gravimetrically at 2.0–3.5 wt% into HDPE or MDPE. Melt temperature at the nozzle is held between 200 and 235 °C, mould surface temperature between 15 and 40 °C, and back pressure between 8 and 15 bar; the LLDPE carrier has a minor viscosity-reducing effect relative to HDPE, so back pressure is used to control striation in thick-walled parts. Short-shot weight variation above ±0.5% produces gate streaks and opacity drift in multicavity tools. Melt flow rate of the letdown compound should be verified according to ISO 1133-1:2022. Compliance for food-contact rigid packaging is assessed under EU Regulation 10/2011 and FDA 21 CFR 178.3290; heavy-metal packaging limits are screened under CONEG and RoHS Directive 2011/65/EU where relevant. Terminal parts are industrial crates, pails, screw caps, and thin-wall houseware containers used for colour-coded segregation and light shielding.

    How Does Rotational Moulding Oven Residence Time Affect Blue Concentrate Dispersion?

    In dry-blend rotational moulding, the concentrate is pulverized with 35-mesh PE powder or metered as micro-pellets at 2.0–5.0 wt%. The principal technical risk is not melt temperature alone but peak internal air temperature, because blue pigments can alter the heat absorption of the mould skin. Peak internal air temperature is therefore controlled at 200–230 °C for LLDPE-based moulding powders, with oven set temperatures of 260–300 °C and residence times of 12–18 min for wall sections between 3 and 10 mm. Insufficient cook produces unmelts at vent ports and poor surface gloss around the parting line; over-cook produces oxidation-related colour drift and reduces impact strength, as measured by ASTM D638-14 and ASTM D256 on cut specimens.

    Mould release and pigmentation interact when the concentrate is added above 4.0 wt% in cast aluminium tools; the lower melt viscosity of the carrier may thin the inner wall near the sprue, so reduced peak internal air temperature and increased oven residence time are used. Published data for this specific concentrate in rotational moulding configurations is limited; industrial practice requires validation of the final moulded article for food-contact or water-contact use. Compliance for water-contact tanks is carried out under NSF/ANSI/CAN 61; food-contact articles are governed by FDA 21 CFR 177.1520 and EU Regulation 10/2011. The concentrate falls under REACH Regulation (EC) No 1907/2006 for SVHC and Annex XVII screening. Terminal finished products are intermediate bulk containers, agricultural spray tanks, and recreational goods requiring colour-coded segregation.

    Extrusion blow moulding of high-density polyethylene bottles imposes a narrower processing envelope because parison sag and die swell shift with even small changes in carrier viscosity. The concentrate is added at 2.0–4.0 wt% through a gravimetric feeder above the extruder throat and mixed in a 24:1–32:1 L/D single-screw extruder with barrier mixing sections. Melt temperatures are maintained at 185–210 °C; accumulator-head tooling relies on parison programming to compensate for wall thinning below 0.6 mm in handle pinch-off zones. At letdowns above 4.0 wt%, parison length instability and neck-in variation are observed, because carrier-rich regions reduce melt strength at the die exit. Compliance for bottle-grade articles follows EU Regulation 10/2011 where food contact is intended and FDA 21 CFR 178.3290 for the colorant component; hazardous-liquid packaging is subject to 49 CFR and the IMDG Code when the packaging is certified for transport. Terminal articles are blue industrial jerry cans, chemical bottles, and personal care bottles with light-shielding requirements.

    When the Concentrate Is Let Down Into Pipe Extrusion for Pressure-Rated PE Water Lines

    Addition is normally limited to 2.0–4.0 wt% in a natural PE100 or PE80 matrix when the concentrate is used in pipe extrusion for pressure-rated PE water lines to avoid disturbing long-term hydrostatic strength. Single-screw extruders with 33:1 L/D, grooved feed sections, and spiral mandrel dies are operated at 205–230 °C; vacuum sizing is maintained at −0.2 to −0.8 bar and haul-off speed is synchronized to wall thickness. The critical control point is pigment dispersion after the melt filter; screen packs of 60/80/100 mesh upstream of the die are used to prevent visible specks in the pipe wall. Filter pressure rise above 8–10 MPa signals agglomeration or incompatible carrier gels and requires a feed zone temperature reduction or concentrate letdown adjustment.

    Compliance for pressure-rated PE piping systems is evaluated under ISO 4427 and EN 12201-1; potable-water acceptance in North America is based on NSF/ANSI/CAN 61 and NSF/ANSI 372. The concentrate is additionally screened against REACH Annex XVII and RoHS Directive 2011/65/EU. Published data for this specific blue grade in pressure-rated pipe applications is limited; final compound hydrostatic testing must follow ISO 9080 or ASTM D1598 on the finished pipe. Terminal forms are blue solid-wall water distribution pipe, striped utility conduit, and cable ducting where colour-coded identification is mandatory.

    Cast film and extrusion coating of polyethylene onto paperboard demands a low-viscosity carrier to maintain stable web tension at line speeds above 150 m/min. The concentrate is metered at 2.0–5.0 wt% into LDPE coating grades through gravimetric dosing and processed in a single-screw extruder with 30:1 L/D, a screen changer, and a flat die with 0.5–0.7 mm lip gap. Melt temperature at the die is 285–320 °C; air gap is kept below 150 mm to limit draw resonance, and chill roll temperature is controlled at 15–25 °C. Die-deposit streak formation is a known failure mode after line stoppages and reheating, so purge cycles of 20–30 min with neat LDPE are used before restart. Compliance for food-contact paperboard constructions is evaluated under FDA 21 CFR 176.170 and, where applicable, FDA 21 CFR 176.180; the plastic layer is simultaneously assessed under EU Regulation 10/2011. Heavy-metal packaging limits are screened under CONEG and EU Directive 94/62/EC. Terminal products are blue-tinted liquid packaging board, industrial laminating film, and overwrap where the coloured layer provides light shielding and product identification.

    Free Quote

    Competitive LyondellBasell POLYBATCH™ Blue 40395U Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell POLYBATCH™ Blue 40395U is a color concentrate supplied in a linear low-density polyethylene carrier resin. The product belongs to the POLYBATCH™ masterbatch range and is intended for let-down into polyethylene film, sheet, and moulding grades where the carrier can reduce viscosity mismatch, assist pigment wetting, and limit stiffness changes in the diluted compound. Because the carrier is LLDPE, the concentrate is not an all-purpose colour system; it is selected primarily when the converter is running linear low-density polyethylene, metallocene LLDPE, or compatible polyethylene blends. The trade name identifies a blue shade and a carrier technology, but it does not by itself disclose pigment loading, exact melt flow index, or colour coordinates. Those values are lot-specific and must be obtained from the certificate of analysis and the supplier’s product data sheet. Published data for this specific configuration is limited; the ranges discussed in this document are representative of industrial practice for LLDPE-based blue colour concentrates and are not substitute specifications. If the product has been reformulated or supplied from a different production site, the controlling data are those printed on the lot-specific CoA.

    What melt-processing boundaries affect let-down behaviour in LLDPE film lines?

    In a conventional LLDPE blown-film line using a single-screw extruder with L/D ratio between 24:1 and 30:1 and a barrier-screw mixing section, the concentrate is normally added at the main feed throat through a gravimetric feeder. Let-down ratios for saturated blue tones in film typically fall between 2 wt% and 5 wt% of the total feed. Lower addition levels may produce weak tint strength and poor hiding, while higher levels can reduce bubble stability, increase die-lip deposit formation, and carry more carrier resin into the film structure than the target resin grade allows. Melt temperature should remain within the supply-chain-approved window for the LLDPE carrier and final film resin; many LLDPE film operations set barrel and die temperatures between 190 °C and 230 °C. Copper phthalocyanine blue pigments can tolerate short excursions above 300 °C, but the complete masterbatch may contain waxes, processing aids, or stabilizers that degrade at lower temperatures. Therefore, residence time above 240 °C should be minimised and not exceed supplier guidance; in the absence of supplier guidance, a maximum of 10 minutes is used as a conservative plant-control limit for organic blue concentrates. Pre-drying is not normally required for LLDPE-based colour concentrates because the carrier is hydrophobic. If storage at relative humidity above 60% has produced surface condensation, drying at 70 °C to 80 °C for 2 h to 4 h is common for polyolefin masterbatches. Static charge can cause concentrate pellets to segregate from natural pellets in volumetric feeders; the use of grounded hopper equipment or anti-static feed tubes reduces this risk.

    Representative test methods for lot verification of LLDPE-based colour concentrates
    PropertyStandardTypical condition
    Melt mass-flow rateISO 1133-1:2022190 °C, 2.16 kg
    DensityISO 1183-1:2019Immersion or gas pycnometer
    Ignition residueISO 3451-1:2019Controlled muffle furnace
    Colour differenceISO 11664-4:2019D65/10° CIELAB
    Pigment dispersionISO 18553:2002Pressed film or moulded plaque inspection

    These methods are not approval tests for finished articles; they establish a common measurement language between converter, compounder, and resin supplier.

    Dispersion Quality, Pressure Drop and Screen Pack Selection

    Screen pack selection and pressure drop are the first observational tools for concentrate dispersion. In a film line fitted with a screen changer, typical LLDPE screen packs are 60/80/60 or 80/100/80 mesh. Changing from a 60/80/60 to an 80/100/80 pack can raise head pressure by 10 bar to 35 bar under constant screw speed and output. If the pressure drop rises more than 1.5 bar/h to 2 bar/h after a clean screen change, the operator should suspect pigment agglomeration, gel formation, or an incompatible additive interaction. Raising barrel temperature to force the pressure down is not a substitute for identifying the cause; additional thermal energy can oxidise the LLDPE carrier and shift the blue shade toward a greener or duller hue. For a 50 µm thick film, undispersed pigment particles larger than 30 µm are visible as specks. Dispersion quality is assessed according to ISO 18553:2002 by pressing a thin plaque or film and examining undispersed pigment agglomerates under magnification. On production-scale lines, batch-to-batch variation in concentrate pellet geometry can alter feeding consistency and require feeder recalibration. The concentrate is most reliably evaluated at the let-down ratio planned for production; laboratory trials at 1 wt% and 5 wt% should bracket the expected shade to expose non-linear colour development. When highly opaque blue layers are required, let-down ratios above 6 wt% may exceed the distribution capability of a smooth-bore single-screw extruder; a melt pump or twin-screw compounding line is then required to achieve uniform colour.

    In multilayer blown film structures, the concentrate is introduced into a skin layer rather than the core. The let-down calculation must use skin-layer throughput as the denominator. If the skin layer is 20 wt% of total structure and the target overall blue addition is 1 wt% of total output, the required skin-layer dosage is 5 wt% of the skin-layer feed. Failure to recalculate on layer throughput is a common cause of shade drift during start-up. LLDPE carriers are compatible with metallocene-catalysed LLDPE in most practical ratios, but a secondary viscosity mismatch can still appear when the skin layer is a very low-viscosity mLLDPE and the concentrate carrier is a conventional LLDPE. In such cases, a higher-melt-flow carrier grade should be discussed with the supplier. Optical haze and dart impact are influenced by the carrier and pigment. When the concentrate is added at levels above 3 wt% in films below 40 µm, dart impact should be tested according to ASTM D1709 and tensile properties according to ASTM D882 to confirm that the final structure meets specification. The LLDPE carrier generally contributes less stiffness than an HDPE carrier, but the pigment hardness and loading are stronger factors in gel and speck formation.

    If the final film is evaluated for haze, clarity, or gloss, the concentrate can alter the optical result even when the blue shade is visually acceptable. In LLDPE film, the addition of a particulate pigment concentrate increases surface roughness and forward scattering. Haze is measured according to ASTM D1003; gloss is measured according to ASTM D2457. The LLDPE carrier may crystallise at a different rate than the base resin and change the film surface texture. At a let-down ratio below 2 wt%, the haze effect is usually small, but above 4 wt% the change can be measurable. When a blue overprint film is required, the converter should specify a concentrated colour system with the lowest possible carrier inclusion and should validate the effect on haze and 45° gloss. In addition, the blue shade can mask yellowing from antioxidant packages; a formulation with low antioxidant loading may pass initial colour tests but fail after oven ageing. Oven ageing at 60 °C to 80 °C for 7 d to 14 d is commonly used to screen for post-ageing shade drift.

    If the concentrate is used in injection moulding or sheet extrusion, what differs?

    Injection moulding of LLDPE-based concentrates into polyethylene caps, closures, crates, or thin-wall containers uses shorter residence times and higher injection shear than blown film. The same carrier compatibility principle applies, but the let-down ratio is usually lower: 1 wt% to 4 wt% is common for saturated colours in opaque moulded parts. Melt temperature in LLDPE injection grades can be set between 220 °C and 260 °C, but the exact upper limit for Blue 40395U depends on the pigment and additive package. Because injection screws often operate with a compression ratio between 2.5:1 and 3.5:1 and a non-return valve, the concentrate should be metered with a positive-displacement or gravimetric feeder; inconsistent pellet geometry or static charging can cause short shots in machines with tight shot-size control. The carrier resin can affect mould shrinkage and warpage. LLDPE carriers are usually lower in modulus than high-density polyethylene carriers, so they introduce less stiffness change in the diluted part. When the final article is tested under ISO 527-2:2012 for tensile properties, the effect of 2 wt% to 4 wt% concentrate on modulus should be quantified, especially if the part is load-bearing. Injection pressures of 60 MPa to 100 MPa are typical for LLDPE thin-wall parts; high pigment loading in the masterbatch does not necessarily change injection pressure if let-down is low, but it can change viscosity at the gate. Published data for this specific configuration is limited; performance must be confirmed on the actual tool and press.

    Compared with LDPE, HDPE, polypropylene, or universal carrier masterbatches, the LLDPE carrier in Blue 40395U influences both rheology and end-use properties. The following matrix summarises the main industrial distinctions that govern carrier selection.

    Comparative carrier-resin attributes in polyolefin masterbatch selection
    Carrier systemTypical interaction with LLDPE film or mouldingPrimary technical restriction
    LLDPE carrierLow melt-viscosity mismatch in LLDPE; low stiffness penalty; low-temperature toughness retentionNarrower compatibility window in PP; may require higher let-down for HDPE rigidity
    LDPE carrierBroad polyolefin compatibility; bubble stability in some film linesMay dilute toughness and reduce heat-seal strength in LLDPE-rich structures
    HDPE carrierHigher stiffness contribution; suitable for HDPE caps and cratesCan increase modulus and reduce clarity in LLDPE film
    PP carrierCorrect carrier for polypropylene fibre and mouldingPhase incompatibility risk in polyethylene; delamination and poor impact
    Universal or ethylene-copolymer carrierUseful across PE and PP in short runs; reduces inventoryMay introduce copolymer residues, higher odour, or organoleptic shifts in sensitive packaging

    Colourimetric verification in final articles should follow the same geometry and illuminant as the brand reference. CIE L*a*b* values are measured with D65/10° per ISO 11664-4:2019. A lot-to-lot ΔE*ab tolerance of 0.5 to 1.0 is common for film packaging, but the acceptable limit depends on the brand owner. In thin-gauge films, the same pigment loading produces greater apparent shade variation if the film thickness changes by more than ±5%. Therefore, thickness control is part of colour control. Blue shades are sensitive to yellowing of the carrier resin; if the carrier oxidises, the measured b* value shifts toward yellow and the shade appears greener. Processors should track Δa* and Δb* separately, not only total ΔE*ab, because colour drift direction matters for corrective action. Spectrophotometric measurements of pellet-form masterbatch are not representative of the final shade; verification must be performed on let-down plaques, bottles, or films. If the product is used in a multi-pass regrind stream, colorant concentration can build up if the same shade is returned into the product. A regrind addition maximum of 20 wt% to 30 wt% is common for LLDPE film, but the actual allowable level for Blue 40395U must be validated for the article and application.

    Regulatory compliance is not a single property of the concentrate; it is a function of the complete formulation and final article. In the European Union, plastic food-contact materials are evaluated under Regulation (EU) No 10/2011 and its amendments. In the United States, colourants for polymers in food-contact applications are commonly assessed against 21 CFR 178.3290 and the applicable conditions of use. The LLDPE carrier may comply with generic polyolefin requirements, but the pigment and additives must also be authorised for the specific food type, temperature, and contact duration. A written compliance statement for Blue 40395U should be requested before use in food packaging or medical packaging. Heavy metal limits for packaging under EU Directive 94/62/EC set the sum of lead, cadmium, mercury and chromium(VI) below 100 ppm by mass. RoHS Directive 2011/65/EU restricts lead, cadmium, mercury, hexavalent chromium, and certain brominated flame retardants in electrical and electronic equipment; coloured plastic components must not exceed the maximum concentration values. The supplier should confirm that the product is not formulated with substances on the REACH Candidate List above the applicable concentration threshold. These regulatory standards do not replace migration testing; specific migration testing according to the intended use may be necessary.

    Storage and handling boundaries are part of concentrate performance. The product should be kept in closed original packaging below 35 °C and protected from direct sunlight. Polyethylene carrier pellets can absorb odours from strong-smelling chemicals; storage near aromatic solvents, flavour compounds, or diesel exhaust should be avoided. The supplier’s recommended re-test date should be followed because long storage can change pellet flow properties and static charge. If the concentrate is exposed to high humidity and visible surface moisture, the drying conditions previously noted should be applied before processing. Incompatibilities can arise when the concentrate is combined with amine-based additives, certain silanes, or highly acidic coupling agents; such interactions can cause colour shifts, gel formation, or corrosive volatiles. The final conversion line must be cleaned between product changes when switching from a blue concentrate to a white or clear product; purging with a high-viscosity LLDPE or a commercial purging compound is required to remove residual pigment from screw roots, screen packs, and die lips.