Lyondellbasell Polybatch Birch 60171u 4 Concentrate Based In Lldpe

LyondellBasell POLYBATCH™ Birch 60171U/4 Concentrate Based in LLDPE

    • Product Name: LyondellBasell POLYBATCH™ Birch 60171U/4 Concentrate Based in LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 935378
    Product Name LyondellBasell POLYBATCH™ Birch 60171U/4 Concentrate Based in LLDPE
    Manufacturer LyondellBasell
    Brand POLYBATCH™
    Product Code 60171U/4
    Product Type Color Concentrate
    Carrier Resin LLDPE
    Color Birch
    Form Pellets
    Compatibility Polyolefins
    Processing Methods Extrusion, Injection Molding, Blow Molding
    Recommended Let Down Ratio 4%
    Additive UV Stabilizer
    Moisture Content <0.1%
    Storage Conditions Dry, below 30°C
    Shelf Life 24 months
    Packaging 25 kg bags

    As an accredited LyondellBasell POLYBATCH™ Birch 60171U/4 Concentrate Based in LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell POLYBATCH™ Birch 60171U/4 Concentrate Based in LLDPE is supplied in 25 kg polyethylene bags, palletized and shrink-wrapped.
    Container Loading (20′ FCL) 20′ FCL container loaded with LyondellBasell POLYBATCH™ Birch 60171U/4 Concentrate Based in LLDPE, palletized, shrink-wrapped, and secured for transport.
    Shipping LyondellBasell POLYBATCH™ Birch 60171U/4 Concentrate, based in LLDPE, is typically shipped as a non-hazardous solid in moisture-resistant bags or boxes on pallets. Keep dry, avoid heat, moisture, and direct sunlight. Not regulated for transport; follow local rules and the SDS.
    Storage Storage: Store LyondellBasell POLYBATCH™ Birch 60171U/4 Concentrate Based in LLDPE in original, tightly sealed packaging in a cool, dry, well-ventilated area. Protect from direct sunlight, heat, moisture, and contamination. Keep away from ignition sources. Avoid excessive stacking or crushing. Do not store outdoors or near oxidizing agents. Close containers after partial use. Maintain stock rotation and use within recommended shelf life.
    Shelf Life Typically 24 months from manufacture when stored unopened in original packaging, dry, below 30°C, and protected from direct sunlight.
    Application of LyondellBasell POLYBATCH™ Birch 60171U/4 Concentrate Based in LLDPE

    In LLDPE-based wood-plastic composite capstock and solid profile extrusion, 2–5 wt% of LyondellBasell POLYBATCH™ Birch 60171U/4 Concentrate Based in LLDPE is metered into a counter-rotating twin-screw compounding line producing high-density polyethylene/wood flour composite profiles. The concentrate is used where a birch-toned surface layer must be maintained across multiple manufacturing shifts, and the carrier resin is selected because its melt rheology matches the PE/wood flour matrix rather than the wood fraction. Gravimetric dosing is held to ±0.3 wt% because wood flour lot-to-lot chroma variation, particularly with ash levels between 0.8% and 2.2%, becomes visible in the extrudate when the colour concentrate drops below 3 wt%. Wood flour is pre-dried to ≤1.0% moisture content before side feeding, while the melt temperature at the die is kept between 155 °C and 180 °C to avoid thermal darkening of the wood fraction. The compounding line is typically a 28:1–36:1 L/D counter-rotating twin-screw extruder with vacuum venting at 0.06–0.09 MPa absolute to strip residual water and volatile wood extractives; die head pressure is maintained between 6 MPa and 14 MPa depending on profile wall stock. Calibration blocks and spray tanks are held at 15–25 °C to set surface gloss and prevent post-die colour drift. Regulatory documentation for the composite product references EN 15534-1:2014+A1:2017 for wood-plastic composites used in non-load-bearing applications and ASTM D7032-17 for decking and railing performance; the colourant addition is also screened against REACH Annex XVII restrictions on heavy metals and PAHs where the finished profile is placed on the EU market. Terminal product types include decking boards, railing sleeves, fascia profiles, and tongue-and-groove cladding.

    How Does Pelletized LLDPE Carrier Pigment Distribute Across a 35-Mesh Rotational Molding Powder Bed?

    Dry blending 1–2.5 wt% of the pelletized concentrate with 35-mesh polyethylene powder can be used in rotational molding only where a two-stage pre-compounding step or a high-intensity mixer has reduced the colour pellet below 600 µm; direct drum tumbling followed by mould charging is likely to produce localised tint streaks on interior surfaces of parts with wall thicknesses below 4 mm. Published data for this specific 60171U/4 pellet in rotomoulding applications is limited, so a pre-milled batch trial on a 200 kg powder line is required to establish minimum pre-blend residence time for the available ribbon blender or high-intensity mixer. The biaxial rotational molding cycle is run at oven set-point 265–315 °C and peak internal air temperature 175–210 °C, with a 3:1 or 4:1 rotation speed ratio on carousel machines; forced air cooling to 70 °C before water mist is applied reduces warpage and improves colour uniformity at sharp radii. Compliance documents for beige parts in public furniture and storage include EN 71-3:2019+A1:2021 heavy metal migration where children’s contact is foreseeable, ASTM D1998-21 for upright polyethylene tanks, and EU Regulation 10/2011 where the rotomoulded article is intended for repeated food contact as a container insert. Terminal products are outdoor sofas, coolers, planter liners, chemical dosing tanks, and equipment housings.

    In high-cavitation closure molding, the beige concentrate in LLDPE carrier is dosed at 2–3.5 wt% into a 12–18 g/10 min melt index LLDPE or HDPE base resin using a gravimetric hopper loader on a 250–350 metric ton hydraulic toggle injection machine. The screw L/D is typically 20:1 to 24:1, plasticizing back pressure is set at 0.5–1.5 MPa hydraulic, and barrel zones are profiled from 190 °C in the feed zone to 220–240 °C at the nozzle; hold pressure between 35 MPa and 55 MPa keeps 0.8–1.2 mm-thick lid panels free of sink marks. Valve-gated hot runner tips are maintained at 1.5–2.5 mm diameter, and total melt residence time below 5 min prevents pigment degradation visible as colour shift at the gate vestige. Compliance requirements cited for closures include FDA 21 CFR 177.1520 for olefin polymers, EU Regulation 10/2011 with an overall migration limit of 10 mg/dm², and 21 CFR 178.3297 for colorants used in polymers; non-food closures are validated against REACH Annex XVII and, for electronics-adjacent dispensing fitments, RoHS Directive 2011/65/EU as amended by (EU) 2015/863. Terminal parts include tamper-evident beverage caps, nutraceutical lids, dispensing spouts, and overcaps for cosmetic jars.

    When Institutional Waste Segregation Film Requires Controlled Opacity Under CONEG and EU Packaging Limits

    Blown film lines running 70–120 µm industrial liners require 4–6 wt% loading to achieve sufficiently low light transmission for colour-coded waste segregation; at 2 wt% the tint is visually rejected under high-frequency fluorescent inspection, while above 6 wt% dispersed pigment can act as a stress concentrator and depress Elmendorf tear strength. The film is extruded through a 250–400 mm spiral mandrel die with a 1.8–2.4 mm die gap, at a blow-up ratio of 2.5:1 to 3.2:1 and melt temperature 180–215 °C; frost line height is maintained within ±100 mm of the calibration value to control dart impact anisotropy. The single-screw extruder is specified at 30:1–36:1 L/D with a barrier screw and mixing pins, because the concentrate must be fully homogenized before the melt enters the annular die and any feed surge becomes visible as brown streaking in the film bubble. The colourant package is tested against the heavy-metal concentration limits of EU Packaging and Packaging Waste Directive 94/62/EC, which sets 100 mg/kg total for lead, cadmium, mercury, and chromium VI, and against North American CONEG limits of 100 ppm per metal. Terminal products are beige/tan waste segregation bags, infectious linen disposal bags, pharmaceutical waste liners, and temporary construction barrier film.

    Parison Programming and Die Swell Variation with a 3% Beige Concentrate in Extrusion Blow Molding

    Extrusion blow molding of 0.8–1.5 mm-thick opaque HDPE/LLDPE bottles uses 2–4 wt% of the LLDPE-based concentrate, with the most significant process impact observed as a 4–7% increase in parison die swell compared with unpigmented resin at the same screw speed. The continuous shuttle or rotary wheel line is operated with a 24:1–30:1 L/D extruder, barrel temperatures from 170 °C to 200 °C, and head tooling adjusted so that parison weight variation across 16 cavities remains below ±1.5%; blow pressure is set at 0.6–1.0 MPa and mould coolant is held at 8–15 °C to prevent bottlenecks on high-output lines. Parison programmers are recalibrated after colour concentrate addition because the changed melt elasticity alters hang time and wall thickness distribution at pinch-off and shoulder regions. Regulatory compliance for chemical and personal-care containers includes UN 3H1 certification for dangerous goods packagings, FDA 21 CFR 177.1520 where the final article contacts food, and EU Regulation 10/2011 for consumer packaging; the colourant must not contribute more than 100 mg/kg total heavy metals under 94/62/EC. Terminal products are 250 mL–5 L opaque cosmetic bottles, household chemical containers, jerrican preforms, and pharmaceutical canisters.

    Polyethylene foam sheet and profile extrusion for wood-look underlay and protective padding is another production route in which the beige concentrate is dosed at 2–4 wt% into an LDPE/LLDPE foamable compound containing 1.5–3.0 phr azodicarbonamide blowing agent. The tandem foam extrusion line uses a first extruder to plasticate at 105–115 °C and a second cooling extruder to bring the melt to 95–100 °C before the annular or flat die; gauge reduction and cell integrity depend on controlling die pressure above 6 MPa to prevent premature foaming. Published data for this specific concentrate in foam extrusion is limited, so cell nucleation must be validated on-line because the added pigment can alter nucleation density and increase open-cell content when processing temperatures drift more than ±3 °C from the baseline. The coloured foam is evaluated according to ASTM D3575-20 for compression set and tensile properties, while the heavy-metal profile of the colour concentrate is verified against RoHS Directive 2011/65/EU where the final foam article is incorporated into electrical and electronic equipment, and against REACH Annex XVII for all articles placed on the European market. Terminal products include expansion joint filler strips, anti-vibration underlay for floating floors, protective corner pads, and case inserts.

    Free Quote

    Competitive LyondellBasell POLYBATCH™ Birch 60171U/4 Concentrate Based in LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell POLYBATCH™ Birch 60171U/4 is supplied as a colour concentrate carried in linear low-density polyethylene. The grade belongs to the POLYBATCH masterbatch range and is intended for let-down in polyethylene-based extrusion and moulding processes rather than for direct use as a compounded finished material. Grade-specific compositional data, including pigment loading, ash content, and organic carrier content, are to be taken from the manufacturer’s certificate of analysis because published data for this specific configuration is limited. The alphanumeric suffix is consistent with a supplier-specific product code rather than a public specification; processors should verify the exact let-down ratio and pigment system against the current batch documentation. Incoming inspection on a production floor commonly records melt mass-flow rate, density, moisture content, and filter pressure build-up before the concentrate is released to film or injection moulding lines. Typical LLDPE-carrier concentrates of this class may show a melt mass-flow rate between 5 g/10 min and 25 g/10 min when determined at 190 °C under 2.16 kg, but the exact value for this product requires confirmation. The LLDPE carrier provides a viscosity bridge between pigment agglomerates and the base polyethylene melt, which is particularly relevant when the concentrate is diluted into LLDPE, LDPE, or HDPE-rich formulations.

    What Primary Specifications Apply to the LLDPE Carrier Phase?

    The carrier phase should be characterised before the concentrate is committed to production. Melt mass-flow rate is determined according to ISO 1133-1:2022 using a 2.16 kg load at 190 °C; this value governs how the concentrate divides into the base resin at the hopper throat or side feeder. Density is measured by ISO 1183-1:2019, and ash content by ISO 3451-1:2019 at 600 °C or 850 °C, depending on the pigment class, gives an indirect measure of inorganic loading. Volatile content is typically checked by ISO 15512:2019 or an equivalent Karl Fischer method because moisture above 0.10 wt% can create surface defects in film and splay in injection moulding. Filter pressure value, measured on a laboratory single-screw extruder with a 25 µm screen pack, is a production-relevant rheological indicator. A pressure rise above 0.5 MPa is often treated as a batch rejection criterion for thin-gauge film, although the limit is site-specific. These methods do not replace the supplier data sheet; they provide a standard incoming inspection framework for LLDPE-carrier colour concentrates.

    On production lines with grooved-feed extruders and barrier screws, LLDPE-based concentrates require sufficient downstream dispersive mixing to prevent colour streaks. Screws with an L/D 30:1 or greater, a Maddock or equivalent dispersive mixing section, and a screen pack of 60/80/100 mesh are common in blown film operations processing this class of masterbatch. Barrel temperatures are frequently set between 180 °C and 220 °C depending on the host polyethylene, but the concentrate should not be processed above 240 °C unless heat-stable pigment chemistry is confirmed in writing. Residence time should be kept below 5 min during start-up interruptions to limit thermal decomposition. Pre-drying is not normally required when packaging is intact and ambient relative humidity is below 60%; if sacks are opened in humid environments, drying at 60 °C for 2 h to 4 h may be applied. Production-scale behaviour includes occasional melt-pressure rise caused by pigment agglomerates accumulating on breaker plates; this is reduced by increasing back pressure or using a more open screen pack if film quality tolerates it.

    Comparative Differences from Polypropylene-Carrier and Wax-Based Concentrates

    The LLDPE carrier differentiates this product from polypropylene-carrier masterbatches and from low-viscosity wax-based systems. A polypropylene carrier is often preferred for polypropylene extrusion and injection moulding, but it can create compatibility limitations in polyethylene film because the carrier may not fully disperse or may form visible gel-like domains. An LLDPE carrier is more compatible with polyethylene hosts and contributes to melt continuity under high-shear dispersion. Compared with a wax-based concentrate, the LLDPE carrier has higher melt viscosity and greater mechanical coupling to the base resin. This can increase extruder torque but reduces the tendency toward plate-out and migration in blown film. Unlike a fully compounded single-pigment compound, the POLYBATCH grade functions as a let-down masterbatch, so the final pigment concentration is controlled by addition ratio rather than by a fixed compound formulation. A 4% addition rate therefore means 40 kg of concentrate per 1,000 kg of base resin. That creates flexibility in colour inventory but introduces feeder accuracy and mix homogeneity requirements that do not exist in a precompounded pellet.

    For blown film operations, the difference between this LLDPE carrier and a wax carrier is most visible in bubble stability and film optics. Wax carriers can reduce melt viscosity and may allow lower extrusion temperatures, but they may also increase surface haze or reduce tensile properties if overdosed. An LLDPE carrier tends to preserve film toughness and is less likely to exude to the die lip during long extrusion runs. In cast film, the carrier’s melt index relative to the base resin is a critical variable. If the carrier melt mass-flow rate is significantly higher than the base LLDPE, the diluted system may show lower apparent viscosity and modified draw resonance behaviour. Conversely, if the carrier is more viscous, line speed may be limited by increased melt pressure or torque. These operational contrasts are not cosmetic; they influence gauge uniformity, film blocking, and colour distribution in the finished web.

    When a Let-Down Ratio of 4% Is Used in Blown Film

    When the concentrate is used at a nominal let-down ratio of 4% by mass in blown film, the effect on bubble stability is governed by the melt index difference between carrier and base resin. If the carrier melt mass-flow rate is significantly higher than the base LLDPE, the diluted system may show reduced apparent viscosity and an altered frost-line height. Processor adjustments include raising the frost line, increasing cooling air, and lowering the metering-zone barrel temperature. If the carrier is more viscous, bubble tension increases and bubble stability can deteriorate in films below 25 µm. The masterbatch should be fed through a calibrated gravimetric or volumetric feeder and preferably pre-blended with base resin pellets before entering the hopper to avoid segregation. Colour streaks in film are commonly caused by insufficient mixing in short screws or by electrostatic build-up on pellets. Dispersion evaluation is performed by examining film samples under transmitted light or using microscopy at 100× magnification to identify pigment agglomerates larger than 10 µm. Mechanical properties of the diluted film should be verified by ISO 527-1:2019 and ASTM D638-14, while film tear resistance may be assessed by ASTM D1922.

    For injection moulding applications, let-down at 2% to 4% is usually sufficient for colour development in parts with wall sections between 1.5 mm and 3.0 mm. Screw recovery time can increase if the concentrate is denser than the base resin or if inorganic pigments raise apparent melt viscosity. Back pressure between 0.5 MPa and 1.5 MPa and a screw speed adjusted to maintain a homogeneous melt help prevent colour striations. Short-shot or colour-gradient defects in thin-wall parts can occur when the concentrate is added directly to the press throat without tumble blending. Mould deposits on polished core surfaces have been observed in operations where the concentrate is over-dosed above the supplier-designated let-down ratio; this is generally reversible by reducing dosage and using a purging compound. No specific clause under FDA 21 CFR 177.1520 should be assumed for this product unless the supplier provides written food-contact documentation for the complete formulation.

    Addressing Batch-to-Batch Consistency and Production-Scale Verification

    Incoming batch verification should compare melt mass-flow rate, ash content, and CIELAB colour coordinates against the approved reference. A standard practice on production lines is to retain a sealed reference sample from the initial approved batch and to test each incoming lot by injection moulding or cast film sampling. Colour difference ΔE*ab should be evaluated according to ISO 11664-4:2019 or an equivalent CIELAB procedure. Values below 1.0 are generally acceptable for non-critical applications, while critical packaging colours may require ΔE*ab below 0.5. Density by ISO 1183-1:2019 can detect carrier substitution or significant pigment loading deviations. Ash content by ISO 3451-1:2019 confirms inorganic pigment level but does not identify organic pigments. Production-scale experience shows that batch-to-batch variation in LLDPE carrier melt index is a more frequent source of processing drift than pigment strength variation; a shift in carrier melt mass-flow rate of 3 g/10 min to 5 g/10 min can alter feeder behaviour and mixing in single-screw extruders. The certificate of analysis should therefore be checked for the carrier melt mass-flow rate range and not only for colour values.

    Test parameterStandard or regulationApplication
    Melt mass-flow rateISO 1133-1:2022Carrier flow characterisation at 190 °C and 2.16 kg
    DensityISO 1183-1:2019Carrier and filler detection
    Ash contentISO 3451-1:2019Inorganic loading estimation
    Moisture/volatile contentISO 15512:2019Drying decision
    Tensile evaluation of diluted filmISO 527-1:2019 / ASTM D638-14Mechanical integrity of diluted compound
    Colour differenceISO 11664-4:2019ΔE*ab against retained standard
    RoHS restricted substancesDirective 2011/65/EURaw material compliance for electrical and electronic component applications

    Before warehouse release for food-contact packaging, the processor should obtain written confirmation that the specific grade meets the relevant food-contact legislation. The presence of an LLDPE carrier alone is not sufficient because colour pigments and processing aids can be subject to different restrictions. Under REACH Regulation (EC) No 1907/2006, each substance must be registered or exempted, and Safety Data Sheet sections should list any pigment components that carry hazard classifications. Operational boundaries include storage in a sealed container at 10 °C to 30 °C and avoidance of direct sunlight, because thermal cycling can increase moisture absorption and condensation in the package. The product should not be pre-blended with resins containing high levels of acid-functional additives unless compatibility testing has been performed, as acidic residues can affect pigment dispersion and colour development. When the concentrate is introduced through a side feeder, the feeder should be calibrated to maintain a constant let-down ratio; a feeder deviation of ±0.5% may produce visible colour drift in thin film. These boundaries are established practices for LLDPE-based colour concentrates and must be confirmed against the current supplier data sheet for Polybatch Birch 60171U/4.