| HS Code | 289956 |
| Product Name | LyondellBasell POLYBATCH™ Beige 60199 Concentrate Based In LLDPE |
| Brand | LyondellBasell |
| Product Code | 60199 |
| Product Type | Color concentrate masterbatch |
| Carrier Resin | LLDPE |
| Color | Beige |
| Physical Form | Pellets |
| Density | 1.10–1.20 g/cm³ (typical) |
| Melt Flow Rate | 20 g/10 min (190°C/2.16 kg, typical) |
| Moisture Content | <0.10% (typical) |
| Pigment Content | 50% (typical) |
| Recommended Let Down Ratio | 2–5% |
| Processing Temperature | 180–230°C |
| Processing Methods | Blown film, cast film, injection molding, blow molding |
| Compatibility | Polyethylene resins (LLDPE, LDPE, HDPE) |
| Heat Stability | Up to 260°C (typical) |
| Light Fastness | 7 (Blue Wool scale, typical) |
| Storage Conditions | Dry, below 30°C, away from direct sunlight |
| Packaging | 25 kg bags |
| Shelf Life | 24 months |
As an accredited LyondellBasell POLYBATCH™ Beige 60199 Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell POLYBATCH™ Beige 60199 Concentrate is packaged in 25 kg polyethylene-lined bags, 40 bags per pallet. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): LyondellBasell POLYBATCH™ Beige 60199 LLDPE-based concentrate, palletized bags, loaded and secured in a 20-foot full container. |
| Shipping | LyondellBasell POLYBATCH™ Beige 60199 Concentrate Based in LLDPE ships as a non-hazardous, non-regulated solid plastic color concentrate. Typically packaged in moisture-resistant 25 kg bags or octabins. No DOT/IMDG/IATA hazard class, UN number, packing group, or placards required. Store cool, dry, away from heat. |
| Storage | Store LyondellBasell POLYBATCH™ Beige 60199 Concentrate Based In LLDPE in a cool, dry, well-ventilated area. Keep containers tightly closed and use original packaging. Protect from direct sunlight, heat, moisture, and contamination. Keep away from ignition sources, incompatible oxidizers, food, drink, and animal feed. Avoid excessive stacking or damage. Follow the SDS and local regulations. Ensure containers remain labeled. |
| Shelf Life | Shelf life is typically 12 months when stored unopened in original packaging, cool and dry, away from sunlight and moisture. |
Melt temperature control in high-output blown film lines is the first boundary condition when POLYBATCH™ Beige 60199 is let down into LLDPE-rich formulations for opaque packaging webs. On a 250 mm annular die fed by a 30:1 L/D grooved-feed single-screw extruder, the carrier resin in the concentrate lowers the effective melt viscosity at the die lip; die pressure typically fluctuates by ±1.5 bar when the hopper loader delivers masterbatch at an unstable ratio. The recommended letdown for 50–70 µm film is 3–6 wt%, with 4 wt% as the reference starting point for opacity targets above 0.97 contrast ratio measured per ASTM D2805. Regulatory compliance in food-adjacent packaging requires confirmation that the letdown film meets FDA 21 CFR 177.1520(c) for olefin polymers used in contact with food, and Commission Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² under the intended time-temperature condition. The production process for opaque liners and outer bags is blown film coextrusion with an outer layer containing the beige concentrate, a core layer of uncoloured LLDPE/LDPE blend, and an inner layer formulated for seal initiation at 85–95°C. Bubble stability is maintained at a blow-up ratio of 2.5:1–3.2:1; frost-line height is held at 600–800 mm above the die to preserve gauge uniformity, which is measured inline with a capacitance thickness scanner at a tolerance of ±4%. Terminal finished goods produced within this envelope include cereal liners, frozen food pouches, bakery bag overwrap, and high-opacity protective furniture wrap.
Operational experience on three-layer lines shows that colour streaks appear when melt temperature falls below 190°C because the beige pigment phase cannot be fully dispersed into the LLDPE matrix; this is addressed by raising the rear zone temperature to 195–205°C and using a screen pack of 60/80/120 mesh to generate shear. A die gap of 1.8–2.2 mm is preferred; narrower gaps increase shear heating and can shift the beige hue by ΔE < 1.0 if the residence time exceeds 5 min at 210°C, but lot-specific pigment thermal stability data should be checked against the certificate of analysis. Pre-drying is normally unnecessary at ambient relative humidity below 60%; however, when sacks have been stored in unheated warehouses or exposed to concrete-floor condensation, a desiccant dryer at 70–75°C for 2 h prevents surface moisture from generating micro-bubbles. Published data for this specific LLDPE-based beige concentrate in all possible layer ratios is limited, so a pilot run of 300 kg is the standard method to verify film torque load, die pressure stability, and final visual haze.
On single-layer cast film lines running 20–40 µm webs, the quench-sided surface of a beige-pigmented LLDPE layer is the primary optical sink. The concentrate is let down at 2–5 wt%, with the lower end used for label facestock that will accept surface printing and the upper end specified where total opacity must exceed 0.95 contrast ratio per ASTM D2805. The downstream process is cast film extrusion through a 1000 mm coat hanger die with a 75 mm 30:1 L/D single-screw extruder, followed by a polished chill roll at 18–25°C and an air-knife assist. Surface roughness generated by quench roll temperature below 18°C lowers 60° gloss measured per ISO 2813 from a typical 60–85 GU to below 45 GU, which creates an undesired matte finish in opaque label stock. Regulatory compliance for hygiene packaging and non-food printed film depends on the final article and is typically limited to REACH Regulation (EC) No 1907/2006 Annex XVII and EC No 1935/2004 if food contact is declared; no heavy-metal pigments are used when the grade is certified against Directive 94/62/EC packaging essential requirements. Terminal products from this process include printed label facestock for tissue bundles, opaque packaging pouches, hygiene product overwrap, and direct mail film.
Production data from cast film lines at 150–250 m/min indicate that edge neck-in and draw resonance become the limiting factors when addition exceeds 5 wt%, because the carrier LLDPE increases the elastic character of the melt curtain. The web is drawn over a chill roll at a haul-off rate that produces a draw ratio of 8:1–15:1; maintaining a melt temperature of 220–240°C at the die exit reduces transverse gauge variation to ±3%. At high letdown, the higher pigment loading can produce visible pinstripe lines if the die gap is set below 0.4 mm; a gap of 0.5–0.7 mm is preferred. Static charge accumulation on the rewound roll is measured by ASTM D2578 and should remain below 38 mN/m surface tension after corona treatment for adhesive lamination or printing. No pre-drying is required at normal controlled plant humidity, but condensation on the resin conveying line during humid months above 70% RH has been observed to create gloss variation on the chill-roll side.
Extrusion coating of woven polypropylene sacks with pigmented LLDPE requires a balance between coating weight and adhesion; the beige concentrate is let down at 4–8 wt% in an LDPE/LLDPE coating blend applied at 15–25 g/m². The limiting parameter is not colour development but adhesion to corona-treated woven PP, measured by ASTM D1876 T-peel; adhesion values below 1.5 N/15 mm are associated with line stops and adhesion failure at crease lines. In a typical coating line, a 90–114 mm 32:1 L/D extruder feeds a 2.2–2.8 m slot die at 290–320°C, with an air gap of 180–250 mm and a chill roll temperature of 12–18°C. The woven substrate is pre-treated inline to 38–44 mN/m per ASTM D2578. Compliance for industrial packaging sacks for cement, fertilizer, and dry bulk is anchored to REACH Regulation (EC) No 1907/2006 and, where specified, EN 15593:2008 packaging hygiene for food-grade transport; food-contact use would additionally require migration assessment under EU No 10/2011. Terminal finished goods are laminated polypropylene woven sacks for seed, animal feed, construction powders, and industrial salt.
At coating weights below 18 g/m², the addition of 8 wt% beige concentrate can reduce draw-down stability because the pigment fraction increases melt curtain tension, causing edge tear at line speeds above 250 m/min. Operators report that dropping the melt temperature to 275°C improves adhesion but raises backpressure by 10–15%, which can trip extruder motor alarms if the screw speed exceeds 120 rpm. Pre-drying is not required when the masterbatch is stored in sealed containers; however, moisture absorption above 0.05% by weight can create pinholing in the coating layer. A 2-zone screw with a mixing section of 4–6 L/D is recommended to disperse the concentrate without excessive shear. Colour consistency on the coated fabric is controlled against a CIELAB tolerance of ΔE < 1.2 using ISO 11664-4; batch-to-batch variation from the concentrate supplier should be less than ΔE < 0.8 for stable brand printing.
| Sector | Addition ratio | Machine configuration | Critical process control | Terminal product |
|---|---|---|---|---|
| Blown film | 3–6 wt% | 30:1 L/D grooved-feed, 250 mm die | Melt 193–210°C, BUR 2.5:1–3.2:1 | Cereal liners, freezer pouches, protective wrap |
| Cast film | 2–5 wt% | 75 mm 30:1 L/D, 1000 mm coat hanger | Chill roll 18–25°C, draw ratio 8:1–15:1 | Label facestock, hygiene overwrap, mailer film |
| Extrusion coating | 4–8 wt% | 90–114 mm 32:1 L/D, 2.2–2.8 m die | Air gap 180–250 mm, melt 290–320°C | Laminated woven PP sacks |
| Blow moulding | 2–4 wt% | 80 mm 24:1 L/D, shuttle press | Melt 175–195°C, blow pressure 0.6–0.8 MPa | Opaque PE bottles |
| Injection moulding | 2–4 wt% | 150–350 t clamp, 20:1–25:1 L/D | Melt 195–220°C, injection velocity 150–250 mm/s | Thin-wall containers, trays, closures |
| Sheet / thermoforming | 3–6 wt% | 90 mm 33:1 L/D, three-roll stack | Roll stack 70–85°C, sheet surface 150–180°C | Dunnage trays, totes, nursery trays |
When the concentrate is specified for monolayer blow moulding of opaque polyethylene bottles, the LLDPE carrier in 60199 shifts the parison swell window relative to a conventional HDPE-based masterbatch. The recommended addition rate is 2–4 wt% in an HDPE/LLDPE blend or in LLDPE-rich bottles with wall thickness from 0.7–1.5 mm; at 4 wt%, the final bottle opacity is sufficient to hide light-sensitive liquid contents. Compliance for home care and personal care packaging requires conformity to FDA 21 CFR 177.1520(c) for olefin polymers, EU No 10/2011 where sold into the European market, and USP <661.1> for plastic containers used in pharmaceutical and cosmetic applications if a drug-product filing is involved. The downstream process is continuous shuttle or reciprocating screw blow moulding, with an 80 mm 24:1 L/D extruder operating at 175–195°C, blow pressure of 0.6–0.8 MPa, and mould temperature of 12–20°C. The parison programmer reduces wall-thickness variance to ±0.15 mm, which prevents beige hue shifts in the pinch-off area. Terminal finished product types include opaque HDPE/LLDPE bottles for liquid soap, hand sanitiser, household cleaners, and agrochemical concentrates.
Field experience on shuttle presses shows that when the LLDPE carrier fraction in the final blend exceeds 8 wt%, parison sag increases and the operator must advance the programmer set points by 5–10% to return the bottle waist thickness to target. This becomes especially visible in beige bottles because wall-thickness variation changes the perceived colour depth; a thickness difference of 0.2 mm can produce a CIELAB ΔE of 1.0–1.5 when measured through the sidewall. Pre-drying is only required if the concentrate has been exposed to ambient humidity above 60% RH for more than 24 h; then a desiccant dryer at 70°C for 2 h is sufficient. Processors should avoid letting the melt residence time exceed 4 min at 190°C because total volatile byproducts can cause gate blush or pinholing at the pinch seam. Published data for this specific commercial colour formulation in all blow moulded formats is limited, so a production trial of 500 bottles is recommended to validate sidewall colour, drop performance per ASTM D2463, and environmental stress crack resistance per ASTM D2561.
In thin-wall moulding, the dominant failure mode is flow-line hue shift across flat surfaces. The beige concentrate is let down at 2–4 wt% for articles with nominal wall thickness below 1.8 mm, using a 150–350 metric ton hydraulic or electric injection moulding machine with a 20:1–25:1 L/D general-purpose screw. Melt temperature is held between 195°C and 220°C, and mould temperature is maintained at 15–35°C; a cold runner with valve gate or sequential edge gating is preferred to avoid jetting. Colour uniformity is evaluated by CIELAB ΔE per ISO 11664-4, with an acceptance limit of ΔE < 1.0 across five measurement points on the visible surface. Compliance for housewares, storage boxes, and closures is generally limited to REACH Regulation (EC) No 1907/2006 Annex XVII and CONEG heavy-metal limits; food-contact applications require FDA 21 CFR 177.1520(c) and EU No 10/2011 migration testing. Terminal finished product types are thin-wall storage containers, lids, food storage boxes, and light-shielding medical packaging trays.
At wall thickness below 1.2 mm, the melt front temperature gradient creates visible colour variation if the filling speed is below 120 mm/s; production trials show that raising injection velocity to 150–250 mm/s and using a heated sprue bushing at 60–80°C reduces the flow-line defect. Injection pressures of 90–120 MPa are typical, and holding pressure is set at 55–70% of peak injection pressure to minimise gate blush. Beige concentrates containing inorganic pigments can accelerate screw and check-ring wear; after 500 t of processed material, the screw clearance should be inspected and maintained below 0.25 mm to prevent colour drift caused by melt leakage. Pre-drying is normally unnecessary at plant conditions below 60% RH; if moisture-induced splay is observed, a hopper dryer at 70–75°C for 2 h is used. Published data for this exact grade in sub-1.2 mm walls is limited, so validation is required against ISO 178 flexural modulus and ASTM D256 Izod impact to confirm that the final mechanical properties meet the specification.
Reusable dunnage trays made from coloured LLDPE sheet tolerate a narrower thermoforming window than uncoloured sheet because the beige pigment phase alters the sheet surface emissivity and reheating response. The concentrate is added at 3–6 wt% in a monolayer LLDPE or LDPE/LLDPE blend, extruded as sheet through a 90 mm 33:1 L/D extruder with a polished three-roll stack set at 70–85°C. Sheet thickness is typically 1.5–4.0 mm; for thermoforming, the sheet surface temperature must reach 150–180°C before forming, with a sag compensation program on the oven because pigmented LLDPE absorbs infrared energy unevenly. Compliance for industrial dunnage and automotive returnable packaging is normally based on REACH Regulation (EC) No 1907/2006 and, where required, RoHS Directive 2011/65/EU for electrical and electronic equipment transport accessories; food-contact cutlery trays would require EU No 10/2011 migration testing. Terminal products are reusable pallet-top trays, internal transport totes, vehicle floor-protection liners, and heavy-duty agricultural nursery trays.
Thermoforming operators record that sheet with 5 wt% beige concentrate requires 5–10°C higher oven setpoint than uncoloured sheet to avoid low-temperature cracking at corners, while overheating above 180°C produces webbing and produces a caramel-like hue shift in the beige. The failure mode on high-density forming tools is vacuum-pin marking, which is controlled by tool temperature above 40°C and a plug assist speed of 200–400 mm/s. Mechanical properties after colouring are verified by ASTM D638 tensile yield, ISO 8256 tensile impact, and ASTM D2240 Shore D hardness; the LLDPE carrier should not move the tensile yield outside the specified ±10% of the uncoloured control. Pre-drying is only necessary when sheet edge trimmings are re-extruded at a regrind rate above 20%; then a desiccant dryer at 65–75°C for 3 h minimises hydrolysis of any additive package. Published data for this specific beige concentration in thermoformed tray structures is limited, so plant validation on 20 sheets is recommended before production.
Competitive LyondellBasell POLYBATCH™ Beige 60199 Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell POLYBATCH™ Beige 60199 Concentrate Based In LLDPE is a pelletised beige colour concentrate in which the carrier phase is linear low-density polyethylene. The designation identifies a colour-and-carrier system rather than a finished compound. Incoming lots are commonly evaluated for melt mass-flow rate under ISO 1133-1:2022 at 190 °C/2.16 kg, density under ISO 1183-1:2019, and moisture content under ISO 15512:2019. Published data for this specific configuration is limited; the supplier’s certificate of analysis remains the controlling document for lot-specific values.
For polyolefin processors, the principal function of Beige 60199 is to deliver a controlled beige shade at a defined let-down ratio without requiring bulk pigment handling. The LLDPE carrier reduces viscosity mismatch with polyethylene-based dilution resins, which is particularly relevant in blown film and cast film operations where film thickness may be 20 μm to 120 μm. The concentrate should be pre-blended with the base resin by tumble mixing or gravimetric dosing; direct feeding without blending may cause local colour deviations.
Storage practice for colour concentrates based in LLDPE should prevent exposure to direct sunlight and high relative humidity. Pellets should be kept in closed containers at ambient temperatures below 35 °C; prolonged storage above 45 °C may cause pellet agglomeration and surface tack. A first-in-first-out consumption policy should be applied because pigment particles may settle or migrate within the carrier under prolonged static load.
Melt temperature in the barrel and die should be maintained within 190 °C to 230 °C for LLDPE-rich systems using Beige 60199. Temperatures above 240 °C can accelerate oxidative yellowing of the beige shade and may produce gel particles in the film; temperatures below 180 °C may reduce dispersive shear and allow pigment agglomerates to pass through the filtration system. On single-screw extruders with 30:1 to 40:1 L/D, the barrel profile should be flat or reverse after the feed throat. A rising melt-pressure trend of more than 15 % over the initial operating point generally indicates screen-pack loading or pigment filtration.
Deviations of more than ±5 °C in the metering zone may shift the beige colour coordinates because the carrier’s oxidative behaviour and pigment wetting are temperature sensitive. At the die, the temperature should likewise be held within ±5 °C of the target; larger fluctuations can appear as oscillating colour depth in the film. The use of a slip additive or antiblock masterbatch alongside Beige 60199 should be verified by a small-scale trial because additive packages can influence colour development at the die lip.
Pre-drying is required for storage environments exceeding 60 % relative humidity; drying at 60 °C for 2 h to 4 h in a desiccant dryer is typical for colour concentrates when surface moisture is detected. Moisture content measured by Karl Fischer titration should remain below 0.05 % for film applications; higher moisture may cause surface streaks and splay in injection moulding or blow moulding. This value is a typical incoming quality threshold for colour concentrates and is not a guaranteed property of Beige 60199 unless stated by the supplier.
One production-scale failure mode observed in LLDPE colour concentrates is feed-section slip, where pellets with smooth surfaces and low surface energy are not conveyed uniformly by the screw. A grooved feed section with forced cooling can restore feed stability without raising the melt temperature. When Beige 60199 is added at 5 wt%, screw speed should be selected to maintain a fill ratio that avoids excessive residence time in the feed zone.
Processing of LLDPE-based colour concentrates at high shear may cause frictional heat generation. On a twin-screw extruder with 44:1 L/D, the temperature profile along zones is typically set from 170 °C at the feed to 210 °C at the die; if the die pressure exceeds 250 bar, screen-pack blockage or insufficient melt pump temperature should be suspected. Such pressure levels are general for LLDPE colour concentrate extrusion and should be adjusted to the line.
Melt filtration may be used to remove residual pigment agglomerates. A screen pack consisting of a breaker plate, 60 mesh, and 120 mesh screens is often installed for film-grade masterbatches; however, for thin films below 40 μm, finer filtration at 150 mesh may be required to prevent visible particles. Published data for this specific configuration is limited.
Purge behaviour matters in multi-product lines. LLDPE-based colour concentrates often require a higher melt-temperature purge compound than EVA-based systems because residual beige colour may remain in stagnant zones at the screw root if the purge lacks sufficient viscosity. A commercial LLDPE purge compound should be run at 200 °C to 210 °C after the product run, followed by an unfilled LLDPE purge until the colour disappears from the die lip. If colour streaks persist, a purging compound with mild abrasive action should be used.
Thermal degradation products from prolonged residence time in barrel dead spots can cause brown specks. A residence time test using a tracer pellet can help identify dead zones; if dead zones are present, screw design modification may be required rather than increasing purge time.
Beige colour development is quantified using CIE L*, a*, and b* coordinates from a spectrophotometer with D65 illumination and 10° observer geometry, following ISO 11664-4:2008. The total colour difference ΔE*ab is calculated according to ASTM D2244-23. For beige masterbatch used in polyolefin film, a common interlot tolerance is ΔE*ab ≤ 1.0 against a reference plaque; however, the grade-specific tolerance should be extracted from the supplier’s quality documentation. Pigment dispersion quality can be evaluated by filter pressure value according to EN 13900-5:2005 using a screen pack of 14 μm aperture.
Spectrophotometric measurements should be taken on compression-moulded plaques or blown film specimens with controlled thickness, typically 2 mm for plaques and 50 μm for film. Differences in surface roughness between plaque and film alter specular reflection and can shift the measured colour coordinates. Therefore, colour tolerances should be defined on the same substrate geometry used for production.
Colour strength is often expressed relative to a standard at the recommended let-down ratio. When the let-down ratio is reduced below 2 wt%, there is a risk of insufficient hiding power and visible streak formation; when it exceeds 5 wt%, the additional carrier may alter film seal initiation temperature and tensile properties in the machine direction. A practical evaluation should compare mechanical properties according to ISO 527-3:2018 for film and ISO 1133-1:2022 for melt flow before finalising the formulation.
The opacity and undertone of beige masterbatches are partially controlled by titanium dioxide content. Higher loadings of titanium dioxide may increase density and create a more opaque beige, but can also raise die pressure. The pigment class may include iron oxides, titanium dioxide, and organic colourants; therefore, a laboratory twin-screw extrusion should be used to compare filter pressure value before scaling to production. Published data for this specific configuration is limited.
Amine-functional additives can shift beige hue due to surface interaction with pigment treatments. If the additive package contains high-amine components, compatibility testing is required before production because colour coordinates may drift in the machine direction. A screening trial should compare ΔE*ab and filter pressure value after 30 min of continuous extrusion.
Incoming quality control should include a colour development test at the intended let-down ratio using a two-roll mill or a single-screw extruder with a flat film die. The test specimen should be compared against a retained reference standard; if ΔE*ab exceeds 0.8 in the incoming QC environment, the lot should be quarantined for review. This threshold is a common screening limit for colour concentrates and should not replace supplier-specific certification.
In applications where a universal concentrate with EVA or ethylene-acrylate carrier has been used previously, substituting Beige 60199 changes the rheological and sealing behaviour of the melt. The LLDPE carrier reduces the likelihood of carrier-induced melt fracture at high line speeds and improves compatibility with the LLDPE dilution resin. However, the processing window is narrower than that of a wax-based universal concentrate because LLDPE requires sufficient melt temperature to homogenise the pigment. A direct substitution without reprofiling the screw temperature settings from the universal-grade profile may produce colour streaks or dimensional variability.
Comparative evaluation should include blow-up ratio consistency in blown film and neck-in performance in cast film. Wax-based universal concentrates can lower melt viscosity and permit lower barrel temperatures, but they may contribute to seal-area contamination and odour in the finished film. Beige 60199 is not a universal concentrate and should not be let down in polar polymers such as polyamide, PET, or polycarbonate without compatibility testing; carrier incompatibility can appear as delamination or island formation.
Compared with polypropylene-based concentrates, the LLDPE carrier in Beige 60199 has a lower melting temperature and may allow processing at lower melt temperatures in polyethylene systems. However, for polypropylene fibre or moulding applications, an LLDPE carrier will behave as a contaminant in the polypropylene matrix and may reduce stiffness; a polypropylene-based concentrate should be used in polypropylene-dominant systems.
Compared with colour concentrates based in high-density polyethylene, Beige 60199 provides greater compatibility with LLDPE and LDPE film resins but may have slightly lower thermal stability at the top of the processing window. In coextruded films, the LLDPE carrier prevents viscosity mismatch with skin layers made of metallocene LLDPE and reduces interfacial instabilities.
During blown film extrusion, extensional viscosity of the LLDPE carrier influences bubble stability. A carrier with insufficient extensional hardening may reduce bubble integrity at blow-up ratios above 2.5:1. Beige 60199 should be evaluated in the intended film structure because inorganic pigments used in beige shades may nucleate crystallisation and alter the film’s crystalline orientation. This can produce a slight increase in dart-drop impact variability; published data for this specific configuration is limited.
Regulatory status for concentrates depends on the final article, migration testing, and the dilution resin. A compliance checklist for Beige 60199 should include the following screening requirements: EU 10/2011 for plastic food-contact materials, US FDA 21 CFR 170–199 for indirect food additives, and Regulation (EC) 1907/2006 for REACH registration. Heavy-metal limits are often screened against EU Directive 94/62/EC for packaging and EN 71-3 for the migration of certain elements, but these are not substitutes for end-use compliance.
| Screening dimension | Standard or method | Application note |
|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | Used at 190 °C/2.16 kg to confirm carrier lot consistency. |
| Density | ISO 1183-1:2019 | Accept only if within the supplier-controlled range. |
| Moisture content | ISO 15512:2019 | Pre-dry if surface moisture is detected. |
| Pigment dispersion | EN 13900-5:2005 | Filter pressure value on 14 μm screen pack. |
| Colour coordinates | ISO 11664-4:2008, ASTM D2244-23 | ΔE*ab against retained reference plaque. |
| Food-contact end use | EU 10/2011, FDA 21 CFR 170–199 | Not automatically compliant; final article must be assessed. |
| Hazardous substances | Regulation (EC) 1907/2006 | REACH conformity to be confirmed by supplier documentation. |
Food-contact status under FDA is defined by the intended use and conditions of use. A concentrate itself is not listed as a food-contact substance; rather, the pigments and additives must be covered by an applicable regulation or a Food Contact Notification. Formulators should obtain a letter of conformity from the supplier for the specific polymer matrix and use conditions.
The end-use evaluation must address specific migration limits for primary aromatic amines if organic pigments are used, heavy metals, and overall migration. Directive 94/62/EC requires the sum of lead, cadmium, mercury, and chromium(VI) not to exceed 100 mg/kg in packaging; this is a packaging material limit, not a product-specific guarantee. For toys and childcare articles, EN 71-3 migration limits may apply depending on the final article.
Suppliers must declare SVHC content above 0.1 % weight per article according to Regulation (EC) 1907/2006 Article 33. A documented absence of SVHCs in the concentrate does not substitute for the final article assessment because the base resin and processing aids may introduce regulated substances.
For gravimetric dosing systems, the narrow particle size distribution of pelletised concentrate reduces bridging in feed hoppers compared with powder pigments. The dosing unit should be calibrated for bulk density of the concentrate, and a minimum hopper residence time should be maintained to prevent segregation when Beige 60199 is blended with pelletised LLDPE. If a single-screw extruder is used with a barrier screw, the concentrate should be introduced with the base resin at the feed throat; side feeding is not required because the carrier does not require staged addition.
The apparent viscosity of the concentrate at let-down is influenced by the carrier’s melt flow rate. If the concentrate has a lower melt flow rate than the base resin, local viscosity peaks may occur in the metering zone. On blown film lines equipped with internal bubble cooling, the melt temperature should be monitored at the die lip rather than the barrel to account for shear heating. Published data for this specific configuration is limited.
Scale-up trials should begin at the midpoint of the recommended let-down ratio and hold melt temperature constant while varying screw speed. The resulting samples should be tested for tensile elongation according to ISO 527-3:2018 and dart impact according to ISO 7765-1:1988 if the concentrate is used in film. Documenting these tests on production-scale equipment ensures that pigment dispersion and carrier dilution do not produce localised mechanical property gradients.
For applications requiring beige colour retention under exterior exposure, accelerated weathering is evaluated in accordance with ISO 4892-2:2013 or ASTM G155-13. Such testing should be selected only when the final article is intended for outdoor service because indoor beige packaging applications do not require xenon-arc exposure. Light fastness depends on the final let-down ratio; higher dilution reduces pigment content and may shift the weatherability profile. Published data for this specific configuration is limited.