Lyondellbasell Polybatch 60186u Almond Concentrate Based In Lldpe

LyondellBasell POLYBATCH™ 60186U Almond Concentrate Based in LLDPE

    • Product Name: LyondellBasell POLYBATCH™ 60186U Almond Concentrate Based in LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 917553
    Product Name LyondellBasell POLYBATCH 60186U Almond Concentrate Based in LLDPE
    Manufacturer LyondellBasell
    Product Type Color concentrate / masterbatch
    Carrier Resin LLDPE
    Color Almond
    Form Pellets
    Density Approximately 1.1 g/cm3
    Melt Flow Rate Approximately 20 g/10 min at 190 C/2.16 kg
    Letdown Ratio Typically 2-4%
    Processing Temperature 180-260 C
    Moisture Content <= 0.2%
    Compatibility Polyolefins
    Packaging 25 kg bags
    Shelf Life 24 months
    Storage Conditions Dry, below 30 C

    As an accredited LyondellBasell POLYBATCH™ 60186U Almond Concentrate Based in LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg polyethylene bags, palletized, with 1,000 kg per pallet for LyondellBasell POLYBATCH™ 60186U Almond Concentrate Based in LLDPE.
    Container Loading (20′ FCL) POLYBATCH™ 60186U in 20' FCL: 20 pallets, 40 x 25 kg bags each, 20,000 kg net, shrink-wrapped, secured for shipment.
    Shipping LyondellBasell POLYBATCH™ 60186U Almond Concentrate Based in LLDPE is shipped as a non-hazardous solid in bags/boxes on pallets. Not regulated by DOT/IMDG/IATA. No UN number, hazard class, or packing group. Protect from moisture and excessive heat. Use normal PPE and keep containers closed.
    Storage Store LyondellBasell POLYBATCH™ 60186U Almond Concentrate in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed when not in use to prevent moisture and contamination. Use original packaging; avoid excessive temperatures. Follow local regulations and supplier guidance. Shelf life may be reduced by prolonged exposure to heat or moisture.
    Shelf Life Typical shelf life is 12 months from date of manufacture when stored in original, unopened packaging in a cool, dry environment.
    Application of LyondellBasell POLYBATCH™ 60186U Almond Concentrate Based in LLDPE

    On three-layer blown film lines running opaque almond-toned LLDPE/LDPE packaging, POLYBATCH 60186U is dosed into the core or skin layer through a gravimetric feeder at 2.0–5.0 wt% based on total polymer throughput. The LLDPE carrier requires melt temperatures between 175°C and 210°C; sustained die temperatures above 220°C may shift the almond tone toward yellow due to thermal oxidation of the organic pigments. Extrusion lines with 30:1 L/D barrier screws and mixing sections produce the most uniform dispersion; field lines with 60/80/100 mesh screen packs record pressure drop increases of 5–15 bar over clear LLDPE, and screen changes are typically scheduled when total head pressure exceeds 350 bar. The blown film die gap is maintained at 1.8–2.5 mm, the blow-up ratio at 2.5:1–3.5:1, and the frost line height at 250–450 mm above the die face. Compliance for food-contact film must be confirmed against Regulation (EU) No 10/2011, including the overall migration limit of 10 mg/dm² under food simulants A, B, and D1, and against FDA 21 CFR 177.1520 for olefin polymers; industrial non-food liners fall under EC 1907/2006 and 2011/65/EU heavy-metal restrictions. Finished food-contact status requires supplier migration documentation and testing on the final film structure. Terminal product types include gusseted freezer pouches, taped-bottom carrier bags, industrial bin liners, and opaque agricultural film sleeves where the almond colour masks product staining.

    What Limits the Addition Ratio in Injection Moulded Polyethylene Housewares?

    In thin-wall injection moulding of polyethylene housewares, a 2.0–4.0 wt% addition of POLYBATCH 60186U is metered through a reciprocating-screw plasticating unit with 18:1–22:1 L/D and compression ratio 2.5:1–3.0:1. Barrel temperatures are profiled from 180°C at the hopper to 220°C at the nozzle, with melt temperatures of 200–230°C. Injection pressures of 70–110 MPa and hold pressures of 40–70 MPa pack sections of 1.5–3.0 mm; gates below 1.0 mm can produce visible flow lines because pigment dispersion breaks along shear gradients. Mould temperature is held at 15–35°C, and cooling time increases by 5–10% compared with natural LLDPE due to pigment nucleation effects. Consumer goods compliance is assessed under EC 1907/2006; if the finished article is a toy, EN 71-3 migration limits for barium, cadmium, lead, and chromium apply, and food-contact containers require finished-article validation under Regulation (EU) No 10/2011. Terminal product types include almond-coloured storage crates, caps and overcaps, thin-wall food containers validated for food contact, and opaque toy housings.

    Rotational Moulding Powder Dry-Flow, Bubble Collapse and Almond-Coloured Part Uniformity

    During the heating phase of biaxial rotational moulding, POLYBATCH 60186U is blended with LLDPE or LLDPE/HDPE micro-powder at 0.8–2.5 wt% before the dry-flow step. Oven temperatures are set at 260–290°C, with peak internal air temperature maintained at 180–200°C; the biaxial rotation ratio is typically 4:1 major-to-minor axis. The masterbatch is drum-tumbled or high-shear blended with polyethylene powder of 35–60 mesh for 10–20 min to prevent agglomeration. Cycle residence times below 18 min can trap air bubbles at the inner wall, and peak internal air temperatures above 205°C may darken the almond tone. Tanks and containers moulded for potable water contact require FDA 21 CFR 177.1520 and finished-tank dimensional and environmental stress-crack evaluation under ASTM D1998; toy applications require EN 71-3 migration testing on the final part. Terminal products include agricultural water tanks, insulated coolers, playground cladding, and material-handling totes. Pre-drying is not normally required at ambient relative humidity below 60%; masterbatch stored in humid conditions should be dried at 70°C for 2–4 h before blending.

    Downstream processTypical addition ratioThermal envelopeCritical control pointStandard designations
    Three-layer blown film2.0–5.0 wt%175–210°CDie temperatures above 220°C may shift almond toneRegulation (EU) No 10/2011, FDA 21 CFR 177.1520
    Injection moulded housewares2.0–4.0 wt%200–230°CGates below 1.0 mm produce visible flow linesEC 1907/2006, EN 71-3
    Rotational moulding0.8–2.5 wt%260–290°C ovenPeak internal air temperature above 205°C darkens colourASTM D1998, FDA 21 CFR 177.1520
    Extrusion coating3.0–6.0 wt%285–320°CHold time above 320°C shifts tone toward brownFDA 21 CFR 176.170, Regulation (EU) No 10/2011
    Cast film4.0–6.0 wt%230–260°CPre-screen melt pressure above 300 bar triggers screen changeEC 1907/2006, 2011/65/EU

    Paperboard extrusion coating lines running almond-tinted LLDPE/LDPE blends use a 3.0–6.0 wt% addition of POLYBATCH 60186U in the coating resin. The concentrate is dry-tumbled with LDPE coating resin before the extruder hopper because short residence-time coating extruders with 24:1–30:1 L/D require pre-distribution to avoid streaking. Melt temperatures at the die are maintained at 285–320°C, the die gap is set at 0.5–1.0 mm, and coating weight is controlled at 15–40 g/m². Chill roll temperature is held at 15–25°C, and in-line corona treatment at 38–42 dyn/cm is applied for lamination or printing. Extended hold time above 320°C may shift the almond tone toward brown; therefore processing campaigns are limited to 4–6 h before purging. Food-contact paperboard cups and cartons are assessed under FDA 21 CFR 176.170 and the plastic layer under Regulation (EU) No 10/2011; non-food service trays and freezer cartons fall under EC 1907/2006 and 2011/65/EU. Terminal product types include hot-beverage cup outer wraps, frozen-food cartons, foodservice outer sleeves, and barrier paperboard sleeves.

    When Almond Concentrate Enters Cast Film Edge Trim Reprocessing

    Because cast film edge trim reclaim raises residence time, almond-coloured LLDPE cast film lines run POLYBATCH 60186U at 4.0–6.0 wt% to compensate for opacity loss in films of 20–80 µm. Melt temperatures are set at 230–260°C, the chill roll is held at 15–25°C, and the air gap is maintained at 5–15 cm. Edge trim containing the concentrate is reclaimed through a fluff feed system and reintroduced at 10–30 wt% of total throughput; the almond pigment is heat-sensitive, so the reclaim stream must not exceed 260°C or more than 3 residence-time cycles. A screen changer with 100–120 mesh filtration removes gel particles and pigment agglomerates from the trim stream; screen changes are triggered when pre-screen melt pressure exceeds 300 bar. Compliance for printed overwrap and protective masking films defaults to EC 1907/2006 and 2011/65/EU; food-contact interleaving films require validation under Regulation (EU) No 10/2011. Terminal product types include printed overwrap film, hygiene packaging backsheets, protective masking films, and interleaving films where almond colour prevents product show-through.

    Free Quote

    Competitive LyondellBasell POLYBATCH™ 60186U Almond Concentrate Based in LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    For dry blending and gravimetric dosing on linear low-density polyethylene extrusion lines, LyondellBasell POLYBATCH™ 60186U Almond Concentrate Based in LLDPE is introduced as a pelletised colour concentrate whose carrier resin is a linear low-density polyethylene. The product designation identifies an almond-shade pigmentation system dispersed in an LLDPE vehicle, delivered in free-flowing pellets. Because the carrier is polymer from the same family as the intended diluent resin, the density mismatch at the pellet surface is smaller than that encountered with ethylene-vinyl acetate or hydrocarbon wax carriers. Test designations relevant to lot acceptance include ISO 1133-1:2022 for melt mass-flow rate at 190 °C and 2.16 kg, ISO 1183-1:2019 for density, ISO 3451-1:2019 for ash content, and ISO 2811-1:2011 for liquid pigment dispersion density where applicable. The certificate of analysis for each batch should be consulted for the exact carrier melt flow index, pigment loading, and volatile content; generic LLDPE data cannot substitute for those lot-specific values.

    Physical form is pelletised, with pellet geometry, bulk density, and pellet-to-pellet weight variation reported on the product data sheet. For dosing accuracy, the concentrate should be free-flowing and free of pellet clusters. Bulk density is typically measured by ISO 60:1977; moisture content can be measured by ISO 15512:2019. In a gravimetric dosing system, pellet bulk density differences above 10% from the base resin can produce feed factor error. The concentrate supplier may report melt flow index of the carrier tested at 190 °C/2.16 kg with ISO 1133-1:2022.

    The concentrate is intended for polyolefin conversion processes, particularly blown film, cast film, sheet extrusion, and injection moulding where the base resin is LLDPE, LDPE, or a compatible polyethylene blend. It is not designed for polyamide, polyethylene terephthalate, polycarbonate, or other condensation polymers, because the olefinic carrier is immiscible with those matrices and may produce delamination or surface blemishes. In LLDPE blown film, initial addition rates are commonly screened between 2 wt% and 5 wt%, with the exact level governed by film thickness, pigment strength, and target opacity. At addition levels below 2 wt%, colour streaks can appear if screw mixing is short; at addition levels above 6 wt%, the dilution of the base resin can alter tensile yield stress, dart drop, and Elmendorf tear performance. Evaluations should be based on ASTM D1709-22, ASTM D1922-23, and ASTM D882-22.

    Which processing routes are most sensitive to carrier-rheology mismatch?

    Cast film lines with narrow die gaps and high melt temperatures expose the LLDPE carrier to elevated shear stress. When the concentrate is added at the feed throat, the screw must generate sufficient dispersive mixing before the melt reaches the die. If the carrier melt flow index is significantly higher than the base resin, the lower-viscosity carrier can coat the screw and produce melt-pressure fluctuations. On a cast line running LLDPE with a melt temperature of 240 °C to 260 °C, the recommended practice is to evaluate the concentrate at a let-down ratio that does not introduce viscosity dilution beyond the line’s pressure control band. Colour uniformity is assessed on cast film by spectrophotometric reflectance using a d/8 sphere geometry under ISO 11664-4:2008 and by transmitted haze measurement per ASTM D1003-21.

    Blown film towers are less sensitive to small viscosity differences but are sensitive to pellet segregation in the hopper. If the concentrate pellets differ in bulk density from the base pellets, stratification can occur during hopper drawdown. Use of a feeder mounted close to the main throat, or a static mixing element in the melt stream, reduces colour fluctuation. On single-screw blown film extruders with L/D ratios of 24:1 to 30:1, the colourant is generally dispersed adequately at melt temperatures below 220 °C; however, thick films above 100 µm may require higher pigment addition or longer mixing sections. The effect on bubble stability should be recorded, because an LLDPE carrier can increase the overall low-viscosity component in the melt and affect frost-line height.

    In injection moulding, the colour concentrate is usually metered at the feed throat with a separate gravimetric feeder. The short plastication residence time in a reciprocating screw may not fully disperse large pigment agglomerates if the let-down ratio is high. Machines with screw diameters above 60 mm and L/D ratios below 20:1 are particularly vulnerable to shot-to-shot colour variation. The use of a mixing nozzle or a barrier screw improves homogenisation. Processors should measure colour consistency on moulded plaques conditioned at 23 °C and 50% relative humidity according to ISO 291:2008 before spectrophotometric comparison.

    In colour metrology, the almond designation is not a single CIELAB coordinate but a target region defined by the end application. Spectrophotometric measurements under D65/10° geometry are reported as CIELAB L*, a*, b* and compared to an agreed standard. The colour difference metric should be specified as CIE ΔE*ab or CIEDE2000; a ΔE₀₀ value below 1.0 is a common in-plant acceptance criterion, but not a product guarantee. For film products, luminous transmittance and haze are measured according to ASTM D1003-21. Sample conditioning should follow ISO 291:2008 or the customer’s documented method. Appearance under a light booth alone is not considered an adequate acceptance test because metamerism can occur when the pigment package is viewed under different illuminants without spectral data.

    Batch-to-batch variance in pigment strength is controlled by the producer through colour strength testing, but downstream users should measure the colour difference after every lot change because pellet size and bulk density can vary. The melt flow index of the carrier is not a fixed property across all lots; a variation of ±2 g/10 min may be acceptable for some applications but may alter the pressure profile on a high-shear cast line. Users should request the supplier’s lot-specific tolerances and compare them against their process capability data.

    The almond colorant does not necessarily contain an ultraviolet stabiliser package; therefore, weatherability must be evaluated in the final formulation. Accelerated weathering of pigmented polyethylene films is evaluated using ASTM G154-23 with UVA-340 lamps, but such tests only approximate service life. In packaging films exposed to retail display light, stabiliser packages are specified separately from the colour concentrate.

    A co-rotating twin-screw extruder used for masterbatch manufacture typically employs L/D ratios of 40:1 to 48:1 and segmented screw elements. Dispersion is achieved through kneading blocks and gear elements. The downstream converter does not need to repeat that level of shear; however, if the converter uses a low-shear single-screw extruder with a barrier screw, the colour concentrate may require a longer transition section. Screw designs with L/D below 20:1 may show visible pigment agglomerates in film, particularly at high let-down ratios. Use of a melt pump can stabilise pressure and reduce surging.

    When an LLDPE-based masterbatch replaces an EVA- or wax-dispersed colourant

    The principal difference is the carrier polymer. LLDPE carriers have a density in the range 0.918 g/cm³ to 0.935 g/cm³, measured by ISO 1183-1:2019, whereas EVA carriers can range from 0.93 g/cm³ to 0.95 g/cm³ depending on vinyl acetate content. The melt viscosity of an LLDPE carrier is generally lower than that of a high-molecular-weight film resin but higher than low-molecular-weight wax carriers. In thin-gauge film, wax-dispersed colorants can reduce film clarity and contribute to die-lip build-up because the low-viscosity wax phase separates at high stock temperatures. The LLDPE carrier in POLYBATCH™ 60186U remains within the polyolefin melt phase, so the tendency for screw coating and plate-out is lower under normal polyethylene processing conditions. This does not eliminate die-lip deposition; accumulation may still occur from pigment agglomerates or process stabiliser interaction, particularly when the line operates above 260 °C without purging.

    The mechanical penalty of dilution is also smaller when a polyethylene carrier is used in polyethylene film. Because the carrier contributes to the film’s semicrystalline network, replacement of a wax carrier by LLDPE can preserve a greater fraction of the film’s tensile energy to break. In practice, the comparative effect is measured by ASTM D882-22 for tensile properties and ASTM D1709-22 for dart impact. When comparing different concentrates, the test should use the same base resin, the same let-down ratio, and the same film thickness; otherwise apparent differences may be caused by the substrate rather than the colourant package. For injection moulding, an LLDPE carrier has a lower heat deflection burden than a high-melting pigment carrier, but it may reduce the moulding’s flexural modulus if the let-down ratio is high. Flexural modulus is evaluated according to ISO 178:2019; impact resistance is evaluated according to ISO 180:2019 or ISO 179-1:2010.

    Compared with an HDPE-carrier masterbatch, the LLDPE vehicle in POLYBATCH™ 60186U has a lower crystallinity and a lower melt temperature, which can reduce the heat input needed to soften the carrier during extrusion. This can be beneficial for LLDPE film lines but can also lower the concentrate’s resistance to blocking during storage in warm environments. The pellets should not be stored above 40 °C to avoid blocking. Compared with a universal carrier based on EVA, the LLDPE carrier introduces no vinyl acetate comonomer, which eliminates the distinctive acetic-acid odour that can be generated when EVA is overheated. It also avoids the polar vinyl acetate groups that can promote moisture uptake and interfacial tension against nonpolar polyethylene.

    Regulatory compliance and migration testing obligations for polyolefin colour concentrates

    Compliance statements for a coloured final article cannot be assigned solely by the masterbatch composition. The concentrate is a component of the final plastic; therefore, its suitability for food contact, toys, or electrical equipment must be assessed in the final formulation and wall thickness. The following checklist identifies the standards most often referenced during raw material qualification.

    Regulatory checklist for polyethylene-based colour concentrate in finished articles
    Standard or regulation Scope / test method Assessment requirement
    EU Regulation 10/2011 Plastic materials in contact with food; overall migration limit 10 mg/dm² or 60 mg/kg Test on final article with intended food simulant; not automatically satisfied by the concentrate
    FDA 21 CFR 177.1520 Olefin polymers for food contact use LLDPE carrier may qualify under the regulation; colourants must additionally comply with 21 CFR 178.3297 and any applicable conditions of use
    FDA 21 CFR 178.3297 Colorants for polymers Pigment package must be acceptable for the intended use; purity and use limitations apply
    REACH Regulation (EC) No 1907/2006 Registration, evaluation, authorisation and restriction of chemicals Substances of very high concern must be below applicable thresholds; Article 33 communication obligations may apply
    RoHS Directive 2011/65/EU Restriction of hazardous substances in electrical and electronic equipment; Annex II maximum concentration values Lead, mercury, hexavalent chromium, PBB and PBDE each limited to 0.1 wt%; cadmium limited to 0.01 wt% in homogeneous material
    Packaging and Packaging Waste Directive 94/62/EC Sum of lead, cadmium, mercury and hexavalent chromium in packaging Combined concentration not to exceed 100 mg/kg in the packaging material

    The above table is not a declaration of conformity for POLYBATCH™ 60186U; it identifies the test obligations that the downstream converter must close. If a food-contact claim is required, migration testing should be performed on the final article with the intended food simulant and time–temperature conditions. If the concentrate is used in coloured packaging for children’s toys, EN 71-3:2019+A1:2021 may also apply for migration of certain elements.

    Storage before processing influences colour consistency and feed accuracy. The concentrate should be kept in closed containers away from direct sunlight and moisture. If pellets have been exposed to relative humidity above 60% for more than 24 h, pre-drying at 70 °C to 80 °C for 2 h to 4 h is recommended before extrusion. Drying should use a desiccant dryer or a hopper dryer with dew point below -20 °C. Over-drying above 85 °C can soften the LLDPE pellet surface and cause agglomeration in the dryer. The processing melt temperature should remain below 260 °C unless the line has been validated for higher thermal load; above that temperature, the LLDPE carrier can begin to undergo chain scission, which changes both viscosity and colour hold. Purge with a polyolefin purging compound after the run to reduce residual pigment carryover into subsequent natural or light-colour campaigns.

    Because published product-specific thermal degradation data for POLYBATCH™ 60186U is limited, the temperature boundary stated here is based on generic LLDPE thermal stability and must be verified against the lot-specific certificate of analysis. No product-specific shelf life is assigned without storage condition data from the supplier.

    In high-closure force injection moulding of large-surface-area parts, the concentrate may influence warpage if it adds a low-density fraction to a high-density base resin. When the base resin is HDPE, the use of an LLDPE carrier at high let-down ratio can reduce density, flexural modulus, and heat deflection temperature. Conversely, when the base resin is LLDPE, the effect is lower. The converter should evaluate warpage and shrinkage with ISO 294-4:2018 for thermoplastics injection moulding shrinkage. Any comparative statement that POLYBATCH™ 60186U is “better” than another product is meaningful only when the comparison is performed on the same machine, with the same let-down ratio, and with identical downstream thermal history.