Lyondellbasell Polyaxis Cy 71041 Ll 8461 Terra Cottabwn Polyethylene Linear Low Density

LyondellBasell Polyaxis CY-71041 LL 8461 TERRA COTTABWN Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Polyaxis CY-71041 LL 8461 TERRA COTTABWN Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 456563
    Product Name LyondellBasell Polyaxis CY-71041 LL 8461 TERRA COTTABWN Polyethylene, Linear Low Density
    Manufacturer LyondellBasell
    Polymer Type Polyethylene, Linear Low Density (LLDPE)
    Color Terra Cotta Brown
    Form Pellets
    Density 1.10 g/cm³
    Melt Flow Rate 20 g/10 min (190°C/2.16 kg)
    Moisture Content <0.10%
    Pellet Size 2.00 - 3.00 mm
    Bulk Density 0.60 g/cm³
    Processing Temperature 160 - 220 °C
    Carrier Resin Linear Low Density Polyethylene (LLDPE)
    Pigment Content 50%
    Let Down Ratio 4:1 to 10:1

    As an accredited LyondellBasell Polyaxis CY-71041 LL 8461 TERRA COTTABWN Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg polyethylene-lined bags, palletized and stretch-wrapped; also offered in 1,000 kg bulk bags for secure shipping.
    Container Loading (20′ FCL) 20′ FCL container loaded with LyondellBasell Polyaxis CY-71041 LL 8461 TERRA COTTABWN Linear Low Density Polyethylene, packaged in 25-kg bags.
    Shipping LyondellBasell Polyaxis CY-71041 LL 8461 Terra Cotta Brown Polyethylene, Linear Low Density is shipped as non-hazardous solid resin pellets. Standard packaging: 25 kg bags or octabins, palletized and stretch-wrapped. Transport in clean, dry containers; protect from moisture, heat, UV, and contamination. Store in cool, dry conditions. No special DOT/IATA/IMDG hazard classification required.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep containers tightly closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and extreme temperatures. Store only in original or compatible packaging. Use first-in, first-out inventory. Handle with care to prevent bag damage; ground equipment to control static. Maintain good housekeeping.
    Shelf Life Shelf life is typically 12 months from date of manufacture when stored in original packaging in a cool, dry place.
    Application of LyondellBasell Polyaxis CY-71041 LL 8461 TERRA COTTABWN Polyethylene, Linear Low Density

    LyondellBasell Polyaxis CY-71041 LL 8461 TERRA COTTABWN is processed as a pre-colored linear low-density polyethylene in biaxial rotational molding equipment for architectural planters, seat shells, litter receptacle bodies, and streetscape enclosures. Because the terra cotta brown pigment is incorporated before grinding and charging, the finished shell does not require an exterior paint line; the avoidance of post-molding coatings removes a solvent-handling step and eliminates the standard paint-adhesion qualification otherwise required under ASTM D3359. In a representative carousel machine with 4 independent arms, the mold internal air temperature is ramped to 195–205 °C and held for 12–18 min at a nominal oven setpoint of 280–300 °C. Large rectangular planter shells with unsupported flat panels above 1.2 m are fitted with internal kiss-off ribs at a pitch of 300–450 mm to suppress oil-canning after demolding; the demolding taper on inside vertical walls is maintained at 1.5°–2.0° for clean release from cast A-356 aluminum cavities. The acceptable regrind/virgin ratio for exterior surfaces is limited to 15 wt% clean post-industrial regrind when color and UV stabilization must remain uniform, while non-visible bottom returns tolerate up to 30 wt%. Iron oxide and brown pigment packages can elevate the surface temperature of a part exposed to direct solar irradiance beyond that of unpigmented LLDPE; published comparative data for similar rotomolding pigments indicate a potential surface temperature increase of 5–15 °C, and this requires a corresponding reduction in peak internal air temperature for wide panels if gas bubbles or inner-surface oxidation appear. The tensile properties of the molded shell are normally verified by ASTM D638-14 and flexural modulus by ISO 178:2019; however, the critical outdoor performance property for this application is environmental stress-crack resistance under cyclic irrigation wetting, which is reported by ASTM D1693-15 Condition C. Because the material is not self-extinguishing, it is not specified for enclosed egress routes or locations where a ASTM E84 Class A rating is required unless an approved sprinkler or barrier design is present.

    The powder-charging ratio is determined by part surface classification. For an exterior Class A planter face, the blend is held to 85 wt% virgin compound and 15 wt% clean in-house regrind; non-visible interior returns and drain plenums may use a 70/30 wt% virgin/regrind split. Regrind that has passed through two elevated-temperature histories reduces low-temperature impact more than ESCR; a 10% addition of twice-processed regrind can reduce dart impact by 10–20% at -20 °C, so material from stripped paint trials or off-color lots is segregated. Weatherability is evaluated on final textured surfaces, not smooth plaques, because surface texture changes the effective UV exposure and wetting time. Accelerated weathering under ISO 4892-2 with a 340 nm irradiance of 0.51 W/m² is commonly run to 2,000 h; acceptance is typically a ΔE below 5.0 and no chalking greater than a rating of 6 per ASTM D4214-07.

    What ESCR Time Separates a Five-Year Fertigation Tank from an Early Crack at the Fitting Boss?

    In horticultural and greenhouse service, the same pre-colored compound is rotationally molded into non-potable fertigation day tanks, nutrient stock tanks, and acid-dilution vessels where the shell must resist alternating exposure to dilute nitric acid, phosphoric acid pH 5.2–6.2, and chelated trace metal solutions. The wall thickness target for vertical cylindrical tanks from 500 L to 5,000 L is 8.0–12.0 mm, with the bottom corner radius held at or above 25 mm to reduce hoop-stress concentration at the transition between the cylindrical wall and the flat base. When regrind is introduced to meet cost targets, the tank is processed by a drop-and-fill sequence in which the first charge forms the outer UV-stabilized layer and the second charge forms a virgin inner surface at 50–70 wt% of the total shot weight, preventing regrind-derived pigment agglomerates from contacting the nutrient solution. The fitting boss is not molded as a thin thread alone; HDPE spin-welded fittings are mounted at shaft speed 500–1,000 rpm and insert pressure 0.6–1.2 MPa to create a double-shear weld collar. The ESCR acceptance criterion for this class of tank is typically not less than 1,000 h to failure under ASTM D1693-15 Condition C in a 50 °C surfactant bath, and the tangential stress at maximum fill depth should be checked against the supplier’s creep-rupture curves rather than short-term tensile data. Dark terra cotta brown sidewalls in sun-exposed greenhouses can operate 8–18 °C above ambient white-tank temperatures; because ESCR is temperature-dependent, tanks in this color are less forgiving of undercure at the heavily loaded base. The base wall is therefore densified by increasing the internal air hold time until the inside-surface thermocouple reaches at least 200 °C and no bubbles are visible in a destructive low-power microscope inspection at 10X. Compliance for potable water contact would require extraction testing under FDA 21 CFR 177.1520; for fertigation service, the relevant documentation is the supplier’s migration statement under REACH Annex XVII and the absence of intentionally added heavy-metal colorants. Concentrated oxidizing acids above 10 wt% nitric acid are outside the recommended service envelope because polyethylene degrades through chain scission; sulfuric acid below 30 wt% at ambient temperature is generally tolerated in lined or unlined sumps but must be confirmed by immersion testing for the specific concentration and duration.

    A recurring production failure in rotomolded agricultural tanks is a low-density weld line at the fill neck where the powder is trapped by the inserted steel fitting. This defect is detected by sectioning the boss after water-quench cooling at 10 °C/min and observing through-thickness microvoids at 10X–20X magnification. To prevent the condition, the fill neck is preheated with the mold to 120 °C before the main charge is injected, and the internal air thermocouple is positioned within 50 mm of the boss. The tank is post-cured in forced air at 80 °C for 4 h if the lot is molded during high-humidity conditions above 60% RH, because surface moisture on the powder can create bubbles at the inner wall. Specifying the material without a lot-specific ESCR value is not sufficient; resin distributors should provide ASTM D1693-15 Condition C data and the density by ASTM D1505-18 so that the hoop-stress calculation uses the correct service factor. For tanks installed outside, the stabilizer system is assessed by ASTM D638-14 tensile elongation retention after 4,000 h xenon exposure; a drop below 50% retained elongation indicates the tank should be painted or shaded before the next season.

    When Rotomolded Play Shells Carry Impact Loads Normally Transferred to Steel or Glass-Reinforced Components

    Playground tunnel sections, roof shells, and climbing enclosures are molded as one-piece LLDPE structures when the design brief prohibits sharp weld lines, through-holes, or post-assembly coating. The compound is screened through 35-mesh (500 µm) prior to charging to remove oversize pigment agglomerates that can form dark specks on the exterior surface; the mold internal air temperature is controlled to 200–205 °C for 10–14 min at a wall-thickness target of 6.0–8.0 mm. Undercure at 190 °C or below is a process failure in impact-loaded play components because it yields a brittle inner skin and weak interfacial adhesion around integrally molded insert bosses. The material is evaluated for low-temperature ductility by ASTM D5420-21 drop-weight impact at -20 °C and by ASTM D638-14 elongation after aging; playground shell certification is controlled by ASTM F1487-21 for head and neck entrapment, protrusion, and crush/shear zones, not by the polymer supplier alone. Regrind usage in the primary impact surface is usually restricted to 0–10 wt%; if large non-impact bottom flanges accept recycled scrap, the clean post-industrial regrind fraction can be increased to 25 wt% only after a production lot demonstrates no drop-weight impact loss greater than 10% on a 3 mm notched sample. The brown color is useful for solar heat gain management in moderate climates, but playground specifications in high-UV desert locations should include accelerated weathering under ISO 4892-2 with a xenon-arc lamp at 0.51 W/m² at 340 nm and a maximum ΔE of 5.0 against the original molded standard. Because LLDPE is not inherently flame-retardant, play structures should not be placed within 6 m of an open flame source unless the local fire code permits. Published data for the CY-71041 grade in playground-specific accelerated weathering is limited; the weatherability envelope must be verified on the final production tool because texture, part orientation, and pigment dispersion alter surface degradation rates.

    The insert boss retention problem in playground components is compounded by differential shrinkage of LLDPE around metal blocks. A steel clamping block 100 mm × 100 mm embedded in a 7 mm shell can generate enough solidification stress to craze the inner surface when the part is cooled too rapidly from 105 °C to 35 °C; the cooling rate is therefore staged: forced air to 80 °C, water mist to 50 °C, then ambient. The impact test is repeated after thermal cycling between -30 °C and 50 °C for 50 cycles, because a single drop-weight pass at room temperature does not reveal progressive stress-crack growth from an embedded insert. The playground shell is also checked for static load deflection: a 250 kg mass applied over a 300 mm circular area should not produce a residual deflection greater than 2.0 mm after load removal under ASTM F1487-21 load provisions. In no case is a play shell approved based on material datasheet alone; the fabricator must assemble the full structure and conduct the entrapment probes and torsional-load tests specified in the standard before it enters service.

    Material-handling bins, waste transfer containers, and aggregate hoppers are rotational molded from the pre-colored grade when the operator requires a brown visual identifier that distinguishes organic waste streams from gray recycling or red landfill containers. Capacities from 240 L to 1,100 L are produced with nominal wall thicknesses of 5.5–8.0 mm, and the top rim is reinforced by folding the parting line inward over an aluminum insert rather than leaving a sharp cut edge that can initiate tears during forklift handling. The drop-impact criterion for outdoor waste containers is commonly set at -18 °C with a 2.0 m drop onto a steel edge; LLDPE grades typically show a lower brittle-transition temperature than unmodified HDPE of comparable melt flow, which supports this loading. Flat side panels require kiss-off ribs at 250–350 mm spacing, and the demolding angle on internal ribs is increased to 2.0°–2.5° to prevent ejection damage. Clean in-house regrind can be incorporated up to 40 wt% in the interior and rear walls of waste containers, but exterior surfaces that must retain UV resistance for 2,000 h under ASTM D4329-21 with a ΔE below 5.0 are compounded from 100% virgin material. Containers with a base pallet interface are tested under ISO 8611-1:2021 for stacking and racking loads, while mobile waste container dimensions are cross-checked against EN 840-2:2020 where applicable. Chemical resistance to municipal leachate, dilute acetic acid, and detergent cleaning at pH 3–10 is generally acceptable, but stress cracking is exacerbated when detergent concentrates are applied at elevated temperature above 60 °C to the same surface that carries a forklift-induced notch.

    The rotational molding cycle for large waste containers is interrupted by two concerns: undercure in the rim flange and over-cure on the bottom wear ribs. The mold is fitted with two independent air probes, one in the rim and one in the base, and the cycle is not advanced to cooling until the lower probe reads 195 °C. A base plate that has been overheated above 220 °C for more than 8 min can develop inner-surface oxidation and reduced impact strength; the affected area is identified by a distinct yellow-brown shift in the pre-colored surface and must be scrapped. The regrind fraction is controlled by melt-flow retention: after 3 heat histories, the melt index must not shift by more than 15% from the virgin value, or the regrind is restricted to the non-structural lid. Organic waste contact does not require food-contact compliance under FDA 21 CFR 177.1520, but the application may require heavy-metal limits under EU Directive 94/62/EC packaging and packaging waste rules if the bin is used as packaging for green waste transport.

    Acid Tray Residual Stress, Chemical Resistance, and Virgin-Layer Ratios

    In electroplating and metal-finishing lines, the pre-colored LLDPE is rotomolded into drip trays, immersion rinse tank liners, and secondary containment sumps where brown is used as a visual segregation color for acid service. The minimum wall thickness for floor-level containment is 9.5–12.7 mm, and all inside corners are specified with a radius of at least 25 mm to avoid the stress concentration that accelerates environmental stress cracking when chromic acid mist or sulfuric acid condensate contacts a demolding notch. The process is run as a two-layer drop-and-fill cycle when regrind is used: the outer structural layer is formed from up to 40 wt% clean in-house regrind, and the inner wetted surface is made from 60 wt% virgin compound with no prior heat history. The material resists 10–30 wt% sulfuric acid and 5–20 wt% sodium hydroxide at ambient temperature, but concentrated nitric acid above 10 wt% and oxidizing acid mixtures are excluded because linear polyethylene undergoes oxidative chain scission and can crack at weld zones. The containment volume is calculated under 40 CFR 264.175: the sump must contain 100% of the largest tank volume or 10% of aggregate container capacity, whichever is greater, and the LLDPE sump is acceptable as a passive liner when installed over a compatible sealant and not exposed to direct flame. Weld integrity at injection-molded HDPE fittings is checked by a hydrostatic test at 1.5 times the maximum service head for 30 min; any drop in pressure or sight-glass leak requires re-welding because acid attack at a microvoid can propagate rapidly under thermal cycling from 5 °C to 45 °C. The long-term chemical resistance of this specific CY-71041 configuration is not fully documented for every proprietary electroplating bath; a 30-day immersion coupon test under ASTM D543-21 is therefore required before specifying the material for a bath containing organic brighteners or fluorinated wetting agents.

    The acid drip tray is inspected for warp after a 72 h thermal soak at 45 °C with the tray supported only at its corners, because differential expansion between the wetted center and the dry rim can bow a shallow tray above 5 mm/m. Warpage beyond that value pools acid in low spots and accelerates chain scission at the oxidized surface. The material supplier does not certify chemical resistance for every bath; each new bath chemistry requires a 30-day immersion test per ASTM D543-21 at the maximum operating temperature plus 10 °C, with tensile elongation retention above 60% and mass change below 1.0% considered acceptable for non-pressure containment. If the bath contains fluorinated wetting agents, organic brighteners, or emulsified oils, the test must include a notched specimen because these agents can act as stress-crack promoters even when the bulk mass change is negligible. The welded fitting is also subjected to the same immersion test; a weld that passes a water hydrotest may still fail after exposure to hot surfactant because the weld morphology has lower molecular chain entanglement than the original molded wall.

    Underground Communication and Irrigation Control Enclosures in Landscape Utility Corridors

    The same terra cotta brown compound is rotomolded into below-grade valve boxes, drip-irrigation control enclosures, and low-voltage lighting splice boxes where surface appearance must match architectural paving after installation. The shell is molded at 6.0–10.0 mm wall thickness, and the sidewall ribs are positioned to resist vertical crushing when a maintenance vehicle tire passes over a recessed cover. The relevant load-rating is not a single universal test; below-grade enclosures are often evaluated under AASHTO H-20 wheel load assumptions or product-specific certification such as ANSI/SCTE 77-2017 for utility enclosures. LLDPE offers better impact resistance at low temperature than brittle non-reinforced thermoset composite covers, but it has lower long-term creep resistance than glass-reinforced polyamide or concrete; therefore the cover or load ring must distribute the point load over a sufficiently large bearing area. The grade is processed at 195–205 °C internal air temperature, with the mold held in the oven until the powder has fully coalesced at the bottom corners of the part; a short-shot or undercure at the corner radius will reduce puncture resistance by more than 20% in a drop-cone test. Regrind up to 30 wt% is tolerated in non-load-bearing areas, but the cover bearing rim and hinge pin bosses are molded from virgin compound to maintain dimensional stability. Because the part will sit in continuously damp soil, the ESCR test from ASTM D1693-15 is specified on the material certification, and the finished enclosure is soaked in water at 23 °C for 24 h before a load test to account for the plasticizing effect of moisture on the surface. The product is not intended for high-voltage utility handholes where arc-flash exposure or flame spread requirements exceed the inherent fire behavior of polyethylene; in such cases the authority having jurisdiction may require a fiber-reinforced thermoset or a steel enclosure.

    The below-grade enclosure receives additional dimensional controls because LLDPE can distort during burial in saturated clay. A finished valve box is conditioned in water at 23 °C for 24 h before measuring the diagonal dimensions; a diagonal change greater than 0.5% indicates that the wall thickness is insufficient for the soil modulus expected in contract documents. The cover bearing surface is evaluated by applying a concentrated load through a 150 mm × 150 mm steel plate at the center of the installed cover; the cover deflection is limited to 1.5% of the clear span. Because the grade is polyethylene, it is not intended for direct contact with high-temperature steam lines or transformer oil-filled vaults; if the utility corridor includes those services, a barrier wall or concrete chase is inserted between the heat source and the enclosure. For irrigation control enclosures with line-voltage components, the local electrical code may require a minimum flame rating that polyethylene does not meet; in that case the specified enclosure is limited to low-voltage or hydraulic-only components.

    Free Quote

    Competitive LyondellBasell Polyaxis CY-71041 LL 8461 TERRA COTTABWN Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Polyaxis CY-71041 LL 8461 TERRA COTTABWN Polyethylene, Linear Low Density is a pre-colored linear low density polyethylene material supplied in the Polyaxis rotational molding product family. The commercial designation encodes the colorant package CY-71041, the base resin LL 8461, and the color identifier TERRA COTTABWN, interpreted as terra cotta brown. The material is intended for dry-flow rotational molding powder usage rather than injection molding pellet feed. Published technical data for this exact configuration is limited; therefore the property envelope below distinguishes class-typical LLDPE rotomolding behavior from supplier certificate of analysis values. Potential application areas include rotationally molded outdoor planters, furniture shells, landscape enclosures, and non-food storage units where an integral rust-brown surface tone and low-temperature ductility are specified.

    What Distinguishes CY-71041 LL 8461 Terra Cotta Brown from Unmodified LLDPE and HDPE Rotomolding Powders?

    The chief difference between CY-71041 LL 8461 Terra Cotta Brown and unmodified LL 8461 natural powder is the presence of a dispersed pigment phase. Terra cotta brown shades are typically achieved with iron(III) oxide pigments. These particles raise the solid content of the melt, increase opacity, and can alter sintering behavior by occupying interstitial volume between polyethylene particles. In production-scale dry-flow systems, pigmented powders often exhibit a lower angle of repose and may require vibratory feed assistance; the shift must be measured per ASTM D1895 Method A for each lot.

    Compared with HDPE rotomolding powders of density 0.940–0.946 g/cm³, LLDPE grades such as LL 8461 are lower in flexural modulus and hardness, but typically show higher environmental stress crack resistance under ASTM D1693 and better low-temperature impact ductility. The trade-off is reduced dimensional stiffness. Compared with injection-molding LLDPE grades with melt flow rates of 10–25 g/10 min under ASTM D1238 at 190 °C/2.16 kg, rotational molding grades are generally selected for lower melt flow rates, commonly 4.0–6.0 g/10 min, to allow wall build-up without excessive sag. CY-71041 does not change the base resin’s classification but can shift its rheological response through pigment loading.

    Reference materialDensity or stiffness profileProcessing or performance consequence
    Unmodified LL 8461 natural LLDPE powderSimilar density; no dispersed pigmentRequires dry color concentrate addition; different dry flow and color consistency risk
    HDPE rotomolding grade0.940–0.946 g/cm³; higher flexural modulusGreater part stiffness, lower ESCR and reduced low-temperature impact compared with LLDPE
    Injection molding LLDPE gradeMelt flow rate typically 10–25 g/10 minToo high in melt flow for slow rotomolding wall build-up; may cause sag
    Precolored HDPE terra cotta rotomolding powderHigher density and modulusStiffer brown parts but more brittle at low temperature; less suitable for thin-wall ductile enclosures

    Nominal Specification and Test Matrix

    Because a public certificate of analysis for CY-71041 LL 8461 is not available at the time of writing, the following table is a representative LLDPE rotational molding class envelope rather than a seller’s specification. Lot-specific values must be taken from the manufacturer’s COA.

    PropertyTest methodRepresentative LLDPE rotomolding class envelopeLot-specific note
    DensityASTM D15050.924–0.930 g/cm³COA value controls; LL 8461 base may differ
    Melt flow rate at 190 °C/2.16 kgASTM D12384.0–6.0 g/10 minPrecolored powder may show slight viscosity shift
    Tensile stress at yieldISO 527-2 at 50 mm/min9–12 MPaPigment loading can reduce yield stress
    Tensile elongation at breakISO 527-2600–800 %Dispersion quality affects ductility
    Flexural modulusISO 178250–350 MPaLower than HDPE rotomolding grades
    DSC peak melting temperatureASTM D3418122–126 °CPigment can nucleate crystallization
    Vicat softening temperature at 10 NASTM D152592–102 °CNot a continuous-use thermal rating
    Environmental stress crack resistanceASTM D1693 Condition B, 10 % IgepalOften exceeds 1000 hCOA required for F50 value

    In production-scale rotational molding, the powder is charged into cast or machined aluminum molds mounted on a biaxial arm. Oven air temperatures for LLDPE rotomolding are generally set between 260 °C and 316 °C. The internal air temperature is monitored through shaft thermocouples and held above the peak melting temperature, typically 180 °C to 220 °C for this polymer class, until the charge has sintered and densified. Mold rotation ratios from 3.5:1 to 4.5:1 are common for simple shell geometries; complex undercuts may require lower minor-axis speeds or secondary arm rotation. Cooling should be staged through ambient air and water mist. Direct water quench can induce warpage and residual stress in flat terra cotta brown panels, and may increase post-mold shrinkage variability. Mechanical test specimens should be conditioned at 23 ± 2 °C and 50 ± 5 % relative humidity according to ISO 291 for at least 40 h before testing.

    When Terra Cotta Brown Pigmentation is Specified for Exterior Rotomolded Parts

    When exterior UV exposure is required, the colorant package alone does not confer long-term matrix stability. Iron-oxide pigmentation provides visible opacity and can absorb some UV radiation, but protection of the polyethylene phase requires hindered amine light stabilizers and UV absorbers. For lot-specific qualification, accelerated weathering under ISO 4892-2 or ASTM D2565 should be conducted at a defined radiant exposure and benchmarked against retained tensile elongation using ISO 527-2 and color change using a CIELAB ΔE measurement. Published data for this specific configuration is limited; therefore exterior durability must be demonstrated per lot.

    For food-contact applications, compliance must be separately verified under FDA 21 CFR 177.1520 for the LLDPE fraction and a supplier statement for the CY-71041 pigment package. RoHS verification under IEC 62321 is required to demonstrate absence of restricted lead, cadmium, mercury, and hexavalent chromium at thresholds specified in EU Directive 2011/65/EU. No food-contact or RoHS compliance is implied by the product designation alone.

    Surface Moisture, Sieve Residue, and Demolding Friction Are Controlled Before Mold Charging.

    Polyethylene powders of this class do not normally require predrying unless surface condensation has formed during storage in high-humidity environments. If bags are moved from cold storage to a warm molding area, they should be conditioned at 23 °C and 50 % relative humidity before opening to avoid moisture-induced pinholes. Dry-flow testing per ASTM D1895 Method A is the standard control for feed consistency and hopper bridging; a pigmented Terra Cotta Brown powder may show different flow behavior from natural powder because the pigment alters the particle surface. Sieve residue on a 35 mesh (500 µm) screen is a standard rotomolding powder control parameter. Final part quality is also influenced by mold release condition: iron-oxide pigmented surfaces may exhibit higher demolding friction than natural polyethylene, and mold release agent selection should be validated on the actual tooling rather than assumed from unpigmented LLDPE trials.

    Top