Lyondellbasell Polyaxis Cp813 31 General Purpose Polyethylene

LyondellBasell POLYAXIS® CP813-31 General-Purpose Polyethylene

    • Product Name: LyondellBasell POLYAXIS® CP813-31 General-Purpose Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 442589
    Density 0.957 g/cm³
    Melt Index 8.0 g/10 min
    Tensile Strength At Yield 29 MPa
    Elongation At Break 600%
    Flexural Modulus 1400 MPa
    Hardness Shore D 66
    Vicat Softening Point 127°C
    Heat Deflection Temperature At 0 46 Mpa 78°C
    Melting Point 134°C
    Brittleness Temperature -70°C

    As an accredited LyondellBasell POLYAXIS® CP813-31 General-Purpose Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell POLYAXIS® CP813-31 is supplied in 25 kg bags, available on stretch-wrapped pallets for safe handling and storage.
    Container Loading (20′ FCL) 20′ FCL: LyondellBasell POLYAXIS® CP813-31 General-Purpose Polyethylene loaded in 25 kg bags, palletized or floor-loaded, secured within container weight limits.
    Shipping POLYAXIS® CP813-31 is shipped as solid polyethylene pellets in moisture-barrier bags, octabins, bulk bags, or bulk trucks/railcars. It is generally not classified as dangerous goods for transport. Keep dry, clean, and away from heat; handle according to the SDS and local regulations.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and strong oxidizers. Keep containers sealed and labeled; protect from moisture, dust, and contamination. Polyethylene resin should be stored indoors on pallets, off the ground, to prevent water absorption and bag deterioration. Use first-in, first-out stock rotation. Avoid prolonged high temperatures and UV exposure. Follow manufacturer SDS and local regulations.
    Shelf Life Shelf life is typically 24 months from date of manufacture when stored in original packaging under recommended cool, dry conditions.
    Application of LyondellBasell POLYAXIS® CP813-31 General-Purpose Polyethylene

    In potable water storage, rotomolded high-density polyethylene tanks built from CP813-31 carry a measurable advantage over two-piece injection molded assemblies: the biaxial rotational molding process produces a seamless, low-weld-line shell with wall thickness maintained between 4.5 mm and 6.5 mm on vertical sidewalls. The powder is dry-blended with 2.0 wt% titanium dioxide white masterbatch and 0.25 wt% hindered amine light stabilizer before charging the mold. A four-arm independent carousel machine with a 2.4 m swing is used. Primary-axis rotation is set to 6 rpm. Secondary-axis rotation is held at 1.5 rpm. Oven air temperature is maintained at 280 °C to 300 °C. Peak internal air temperature reaches 190 °C to 205 °C. Cooling is performed with forced air and water mist until the mold surface drops below 80 °C. The finished tank is conditioned for 24 h at 23 °C before dimensional inspection. This process produces portable RV freshwater tanks, marine potable water tanks, and stationary rainwater collection vessels. The grade must comply with FDA 21 CFR 177.1520(c) for olefin polymer extractives and NSF/ANSI 61 for drinking water contact. ASTM D1998-21 governs vertical cylindrical polyethylene tanks for above-ground service. Density should be verified per ISO 1183-1:2019. Environmental stress-crack resistance should be measured per ASTM D1693-15b, condition B, with an F50 value above 1000 h in 10% Igepal CO-630 at 50 °C. Limitations apply: continuous exposure to chlorinated water above 60 °C accelerates oxidative chain scission. Sodium hypochlorite solutions above 5 ppm free chlorine at elevated temperature can initiate slow crack growth in stressed corners. Published data for long-term chlorine resistance in this specific rotomolding configuration is limited. Processors should conduct immersion testing per ASTM D543-21 before specifying the resin for high-residual chlorine service.

    Which Processing Window Limits Pinholing in Agricultural Sprayer Tanks?

    The first processing variable governing pinhole suppression in agricultural chemical containment is not oven residence time alone but the interaction between peak internal air temperature and mold stall time during the melt-coalescence stage. For CP813-31, a cast aluminum mold charged with 2.0 wt% carbon black masterbatch and 0.2 wt% phenolic antioxidant produces a full-thickness melt film when the peak internal air temperature reaches 200 °C. Mold stall time across the primary axis of 3 min to 4 min is standard on a closed-loop shuttle machine. Premature demolding before the internal air temperature drops below 90 °C induces sink marks at threaded inserts and boss attachments. The finished part is a one-piece agricultural sprayer tank with a capacity range of 200 L to 10,000 L. Wall thickness at the corners is specified at 5.0 mm minimum. The resin must be evaluated for chemical resistance against diluted mineral acids, alkali cleaners, and aqueous urea-ammonium nitrate mixtures. ASTM D543-21 provides the immersion test framework. Transport packaging for hazardous liquids must meet UN 1H1 drum drop and leakproofness protocols. ESCR values per ASTM D1693-15b condition B should exceed 1000 h. Oxidative induction time should be established per ISO 11357-6:2018 at 200 °C. The operational boundary is defined by swelling and permeation: aromatic solvents, methylene chloride, and concentrated nitric acid are not recommended. Published field data for long-term containment of organophosphate emulsion concentrates in HDPE rotomolded tanks shows acceptable service when wall thickness exceeds 5.5 mm and internal surfaces are not flame-treated.

    Test or regulatory areaReferenceRepresentative value or condition
    Potable water contactFDA 21 CFR 177.1520(c), NSF/ANSI 61Extractables per standard method
    DensityISO 1183-1:20190.940–0.945 g/cm³
    Melt flow rateISO 1133-1:20222.5–3.5 g/10 min at 190 °C/2.16 kg
    Environmental stress-crack resistanceASTM D1693-15bCondition B, F50 > 1000 h
    Tensile yield strengthASTM D638-1420–23 MPa
    Flexural modulusASTM D790-17800–1000 MPa
    Notched Izod impact at low temperatureASTM D256-10e1-20 °C
    Oxidative induction timeISO 11357-6:2018200 °C
    UV weatheringASTM D4329-21, Cycle A2000 h
    Flammability classificationIEC 60695-11-10:2013UL 94 HB

    Cold-storage logistics boxes and multi-trip aquaculture containers are rotomolded in double-wall construction with CP813-31 outer skins and polyurethane foam insulation injected between the walls. The process begins with charging the outer mold with 1.8 wt% carbon black masterbatch and 0.3 wt% hindered amine light stabilizer. The inner wall is formed in a second mold cycle using the same powder blend. The two shells are joined by hot-plate welding at 190 °C to 210 °C. Cavity injection of polyurethane foam at 0.25 MPa fills the annular space. The finished containers are used as insulated fish totes, meat lugs, and cold-chain distribution boxes. Low-temperature impact resistance is the critical acceptance parameter. Notched Izod impact strength should be verified per ASTM D256-10e1 at -20 °C. Puncture resistance is measured per ISO 6603-2:2000 at 23 °C and -20 °C. Flexural modulus is determined per ASTM D790-17. A ductile-to-brittle transition can occur below -25 °C in unmodified HDPE; therefore, this material is generally limited to cold-chain applications with sustained product temperatures not below -20 °C. In continuous-use freezer handling at -30 °C, impact-modified grades are recommended. The seamless rotomolded corners eliminate sharp stress concentrations. The absence of molded-in weld lines improves drop performance. Drop testing should follow ASTM D5276-19.

    Marine Flotation Billets and Dockside Impact Ductility at Sub-Zero Exposure

    For marine flotation service, CP813-31 is processed as a sealed outer shell later filled with expanded polystyrene foam. The shell wall thickness is held at 5.0 mm to 7.0 mm to resist boat impact and ice abrasion. Molds are fabricated from steel plate with an internal release angle of 3°. The resin is processed without filler. Carbon black loading at 2.5 wt% provides ultraviolet screening. Peak internal air temperature is set at 210 °C. Cooling is extended to 30 min with forced air before demolding. The finished shells are filled with 32 kg/m³ expanded polystyrene foam and sealed with a rotomolded cap. End products include floating dock segments, mooring buoys, and platform float assemblies. Water absorption of the foam should be tested per ASTM D2842-19. The shell material must retain impact ductility at -20 °C; ASTM D256-10e1 notched Izod values above 50 J/m in the rotomolded plane are typical for this density class, but CP813-31 certificates should be consulted. The outer shell is tested for hydrostatic leakage after cap welding. Published data for long-term saltwater aging of HDPE dock floats is available from marine polymer service studies. Limitations include swelling upon prolonged contact with diesel sheen and loss of impact strength after 5 years of continuous unsheltered UV exposure without adequate carbon black loading. The design must include vent holes for freeze-thaw cycles. Otherwise, entrapped water in the foam cavity can expand at -10 °C and split the shell.

    When Rotomolded HDPE Replaces Welded Steel in Off-Highway Hydraulic Reservoirs

    Hydraulic reservoirs for compact excavators and agricultural tractors can be rotomolded from CP813-31 when the service temperature does not exceed 60 °C and the fluid is mineral oil-based. The mold is a fabricated steel shell with internal baffles formed as raised ribs. The charge contains 2.0 wt% carbon black masterbatch and no migratory plasticizer. Peak internal air temperature is held at 195 °C to 205 °C to avoid thermal degradation of the antioxidant package. Post-mold machining inserts brass NPT fittings and fluid level gauge openings. A flat sealing face is machined on the top opening to accept a nitrile gasket. The tank wall is 6.0 mm to 8.0 mm thick. The absence of welded seams removes a source of particulate contamination. The HDPE tank also reduces interior condensation compared with steel in cyclical temperature environments. The tank must be pressure-tested per the system specification; rotomolded HDPE hydraulic reservoirs are typically limited to 0.3 barg internal pressure and 0.1 barg vacuum. Burst testing is conducted hydrostatically to 0.6 MPa. The resin must resist mineral oil swell. Immersion testing per ASTM D543-21 in ISO VG 46 hydraulic oil should show mass increase below 0.5% after 168 h at 60 °C. Limitations include poor compatibility with phosphate ester fluids and ethylene glycol mixtures above 70 °C. The tank should not be powder-coated or exposed to continuous service above 70 °C. Published data for long-term dynamic fatigue in rotomolded hydraulic reservoirs is limited. Processors should instrument a pilot build with strain gauges at baffle transitions.

    Because the enclosure is formed without weld lines, outdoor electrical junction enclosures and telecommunications pedestals are rotomolded from CP813-31 where the application requires one-piece construction, resistance to soil acids, and low water ingress. A standard mold uses a steel shell with a hinged lid and integrally molded cover latch. The powder is dry-blended with 2.5 wt% carbon black masterbatch and 0.5 wt% processing aid before charging. Oven air temperature is 270 °C to 290 °C with a total cycle time of 45 min to 60 min. Wall thickness is specified at 4.0 mm minimum. The completed enclosure is drilled with a template for cable glands. The material is tested for flammability according to IEC 60695-11-10:2013. HDPE typically achieves a UL 94 HB classification; CP813-31 must be evaluated for a finished-part thickness of 1.5 mm to 3.0 mm. Weathering performance is assessed per ASTM D4329-21, Cycle A, for 2000 h. Color change and chalking are recorded; carbon black-filled HDPE should retain at least 80% of initial elongation after exposure. The absence of weld lines at the hinge boss reduces crack initiation under repeated lid cycling. The design must account for thermal expansion; HDPE expands approximately 1.3 × 10⁻⁴ K⁻¹ in linear coefficient. Mounting inserts should be brass or stainless steel. Limitations include a maximum continuous service temperature of 65 °C for sealed equipment compartments. Solvent-based cable jointing compounds containing methyl ethyl ketone are incompatible.

    Part Thickness Stability in Rotomolded Playground Panels After UV Weathering

    Playground and recreational panels molded from CP813-31 are installed in public play structures where impact and solar exposure occur simultaneously. The rotomolding powder is let down with 2.0 wt% carbon black masterbatch, 0.3 wt% hindered amine light stabilizer, and 0.2 wt% antioxidant. Mold construction is cast aluminum with a polished cavity surface. Peak internal air temperature is limited to 200 °C to avoid gloss variation. Primary-axis rotation at 5 rpm and secondary-axis rotation at 1.2 rpm produce a uniform wall of 5.0 mm to 8.0 mm on curved play panels. The finished parts must meet ASTM F1487-21 for public playground equipment performance. Projections, entrapment gaps, and head-form impact zones are controlled by the mold design. Material properties should be verified: tensile yield strength per ASTM D638-14 should be in the vicinity of 20 MPa; flexural modulus per ASTM D790-17 should exceed 800 MPa. UV weathering resistance is tested per ASTM D4329-21 for 2000 h. Impact strength at 23 °C is determined by ASTM D256-10e1. Playground equipment must also comply with EN 1176-1:2017 for European installations. The material is not flame-retardant; open flame sources must be excluded by design. The lower service temperature limit without impact modification is approximately -20 °C. High-stress areas around metal inserts should be radiused at 3.0 mm minimum to prevent crack initiation. Published data for long-term gloss retention of carbon black HDPE playground panels after 10 years is available from outdoor weathering studies.

    Free Quote

    Competitive LyondellBasell POLYAXIS® CP813-31 General-Purpose Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell POLYAXIS® CP813-31 is a general-purpose polyethylene powder supplied for rotational molding of hollow, thin-walled parts. The grade belongs to the Polyaxis powder portfolio and carries a general-purpose classification rather than a high-ESCR or UV-stabilized designation. Processors specify this class of material when the molded article requires balanced processability, moderate stiffness, and standard low-temperature impact performance without a specialized stabilizer package. The model designation CP813-31 is the primary grade identifier for ordering and lot traceability. Because release properties vary by production campaign, the current supplier technical bulletin and certificate of analysis should be consulted for exact nominal values for density, melt flow index, and additive content. Published data for this specific configuration is limited in this document, and process characterization must therefore be performed on the lot intended for production.

    The product is used in non-pressure storage tanks, agricultural containers, playground components, equipment covers, and general industrial housings. Typical wall thickness in such parts ranges from 3 mm to 25 mm; industrial designs most often fall between 5 mm and 12 mm. The resin is not automatically qualified for sustained internal pressure above atmospheric unless the finished tank or vessel is tested under ASTM D1998 or ISO 16101. Continuous outdoor exposure, contact with aggressive hydrocarbons, or hot chlorinated water service should trigger substitution or validation against a UV-stabilized or high-ESCR grade.

    In rotational molding, CP813-31 is processed as a dry powder charged into a cold or warm mold, then sintered and consolidated under biaxial rotation. The general-purpose classification implies that processing behavior is designed for a broad range of simple shapes rather than extreme service environments. The absence of a high-intensity stabilizer system can reduce additive interference during pigment dry blending, but it also sets a boundary for outdoor weathering and high-temperature oxidative stability.

    What Distinguishes CP813-31 from High-ESCR and UV-Stabilized Polyaxis Powders?

    Differentiation is primarily molecular and additive-based. A general-purpose rotomolding polyethylene balances melt flow index, density, stiffness, and impact. High-ESCR grades shift molecular weight and comonomer distribution toward longer chains and higher tie-molecule density. Under ASTM D1693, Condition A or B, high-ESCR grades can show an order-of-magnitude advantage over a general-purpose grade at similar density. The exact CP813-31 ESCR value must be taken from the supplier’s release documentation. A processor cannot infer ESCR from density or melt flow index alone.

    UV-stabilized grades incorporate hindered amine light stabilizers and UV absorbers. A general-purpose grade may have only process stabilizers and a nominal antioxidant package. This difference becomes critical when parts are subjected to ASTM D2565 or ISO 4892-2 weathering cycles. CP813-31 should be considered unproven for multi-year outdoor exposure unless the final article is tested in the intended color. Carbon black or pigmented dry blends may alter weathering resistance independently of the base resin.

    Melt flow index also separates application grades. Rotational molding materials are lower in flow than many injection-molding grades, but high enough for particle coalescence at low shear. The supplier’s melt flow index value for CP813-31, measured by ASTM D1238 at 190 °C/2.16 kg, should be checked because shifts of 0.5 g/10 min can alter oven dwell time and bubble release. High-flow injection-molding polyethylene should not be substituted without evaluating powder particle size, dry flow, and sintering behavior.

    Polyethylene density controls crystallinity and stiffness. A shift from 0.938 g/cm³ to 0.945 g/cm³ in rotomolding powders raises flexural modulus by approximately 150 MPa to 250 MPa while reducing ESCR and impact. A change of 0.002 g/cm³ can therefore affect part stiffness and stress-crack behavior. For this reason, density is not a secondary specification. Rotomolding powders in this class often fall between 0.938 g/cm³ and 0.945 g/cm³, but the exact CP813-31 nominal density must be obtained from the current datasheet.

    Mechanical properties for general-purpose rotomolding polyethylene at 23 °C commonly fall between 15 MPa and 22 MPa tensile yield strength, with elongation at break often exceeding 300%. Flexural modulus commonly falls between 600 MPa and 1,100 MPa. These are class-typical ranges, not grade-specific values. CP813-31 lot-specific values must be confirmed by ASTM D638 and ASTM D790 testing on rotomolded panels, since mechanical properties depend strongly on thermal cycle and cooling rate.

    Specimen preparation affects test interpretation. Mechanical testing should use rotomolded panels or flat sections cut from production parts, not injection-molded or compression-molded plaques. Tensile specimens in ASTM D638 Type IV format are generally used at 50 mm/min. Low-temperature impact is often measured by notched Izod per ASTM D256 or Charpy per ISO 179 at -20 °C or -40 °C. Drop-weight or instrumented puncture tests such as ISO 6603-2 or ASTM D3763 often better represent service for rotomolded parts than notched specimens.

    Rotational molding polyethylene is a low-shear process. Capillary viscosity at 190 °C may be on the order of 10³ Pa·s to 10⁴ Pa·s at shear rates below 10 s⁻¹. Melt flow index is a relative flow indicator, not a direct measure of powder coalescence. Air bubble removal depends on particle size, surface tension, zero-shear viscosity, and oven residence time. This is why a rotomolding powder with acceptable ASTM D1238 flow can still produce porosity if the internal air temperature is not brought high enough for long enough.

    If Peak Internal Air Temperature Falls Below 190 °C or Exceeds 220 °C, Part Quality Is Thermally Limited

    Rotational molding of CP813-31 is governed by the relationship between oven setpoint, internal mold air temperature, and wall thickness. On production shuttle and carousel machines, oven setpoints between 280 °C and 320 °C are typical for polyethylene in this density range. The internal air temperature should normally reach 190 °C to 210 °C for complete sintering. If the peak internal air temperature remains below 190 °C, particle fusion may be incomplete and the part can show pinholes, low weld-line strength, and reduced tensile elongation. If the internal air temperature exceeds 220 °C, oxidative degradation and bubble formation can occur, especially in thick sections where residual heat slows cooling.

    Optimum residence time depends on wall thickness. A 6 mm wall may require a total oven cycle of 18 min to 25 min in many industrial machines, while a 12 mm wall may require 30 min to 40 min. These are equipment-dependent starting ranges and must be adjusted by mold mass, oven efficiency, and ambient conditions. Production-scale experience shows that powder lot changes can shift the internal air temperature ramp by a few degrees at fixed oven settings. Operators should compare time–temperature curves from a through-mold thermocouple rather than relying on oven timer alone.

    Cooling rate after oven removal is equally important. Air cooling followed by water mist is used to control crystallinity and warpage. Rapid water quench increases toughness but may introduce distortion. Slow air cooling increases stiffness but may reduce low-temperature impact. The cooling sequence should be recorded and repeated because rotomolded polyethylene properties are strongly influenced by thermal history, not solely by resin selection. Mold surfaces should be prepared with a semi-permanent release agent appropriate for polyolefins. Vent tubes with an inside diameter of 6 mm to 12 mm prevent pressure excursions and blowback during heating and cooling.

    Thermal oxidative stability can be screened by differential scanning calorimetry oxidation induction time under ASTM D3895 or ISO 11357-6. A general-purpose PE without a heavy stabilizer package may show a shorter oxidation induction time than a UV-stabilized or long-term heat-stabilized alternative. This does not disqualify CP813-31 from general indoor applications, but it defines a processing ceiling and storage boundary. Overheating in the oven or extended hold at peak temperature should be avoided because polyolefin oxidation is autocatalytic and cannot be reversed by cooling.

    Selection of CP813-31 over an injection-molding polyethylene is also driven by the need for controlled particle size distribution and dry flow. A general-purpose rotomolding powder is typically controlled to a top size below 500 µm. Bulk density by ASTM D1895 Method A commonly falls between 0.38 g/cm³ and 0.45 g/cm³ for powders in this class. A change in bulk density of 0.02 g/cm³ can alter charge weight by approximately 5% at constant volume, which affects wall thickness control. The certificate of analysis should provide sieve distribution and bulk density, and incoming lots should be checked if the molding line uses volumetric charging.

    Dry flow can be assessed by ASTM D1895 methods and by funnel-flow time. Moisture, compaction, or excessive fines can increase flow time and cause incomplete fill of deep mold cavities. Rotational molding powder with excessive fines may also dust during charging, creating a housekeeping issue and a potential respiratory irritant. General-purpose powders are expected to be free-flowing and non-dusting when handled under normal plant conditions. If the powder does not flow consistently, the root cause is usually moisture pickup, compaction, or contamination rather than resin molecular properties.

    Powder Handling, Moisture Control, and Regrind Addition

    Ambient storage in original multilayer bags or containers at temperatures below 40 °C is recommended. Polyethylene powders are relatively insensitive to moisture, but surface moisture can reduce dry flow and create steam bubbles during molding. If bags are exposed to high humidity or condensation, pre-drying at 80 °C for 2 h to 4 h in a desiccant or hot-air powder dryer may be required. Drying temperatures approaching the softening point must be avoided because particle agglomeration can occur and the powder may lose its free-flowing character.

    Processors should minimize regrind addition to CP813-31. General-purpose rotomolding powders tolerate up to 20 wt% clean, melt-stage regrind of the same material in many non-specialty applications, but higher regrind fractions may reduce impact strength and increase melt flow index due to chain scission. The exact regrind retention for CP813-31 should be validated by ASTM D1238 melt flow index and ASTM D638 tensile elongation tests on molded panels. Regrind from multiple sources should not be introduced without segregation by melt index and color.

    Table 1 lists the test methods most commonly referenced for grade release and application qualification. The presence of a method in the table does not by itself establish compliance for a specific CP813-31 lot; verification must be made against the final article and its intended use.

    Property or requirement Test method Typical role in CP813-31 evaluation
    Melt flow index ASTM D1238 / ISO 1133-1:2022, 190 °C/2.16 kg Sintering and particle coalescence
    Density ASTM D1505 Stiffness and ESCR balance
    Environmental stress crack resistance ASTM D1693, Condition A/B Chemical contact resistance
    Tensile yield and elongation ASTM D638 Short-term mechanical property
    Flexural modulus ASTM D790 Part stiffness comparison
    Vicat softening temperature ASTM D1525 Heat softening behavior
    Deflection temperature under load ASTM D648 Dimensional stability under heat
    Oxidation induction time ASTM D3895 / ISO 11357-6 Thermal oxidative stability
    Weathering resistance ASTM D2565 / ISO 4892-2 Outdoor stabilizer screening
    Food-contact olefin polymer FDA 21 CFR 177.1520 Regulatory verification if required
    EU food-contact plastic Regulation (EU) 10/2011 Migration limit compliance if required
    Bulk density and dry flow ASTM D1895 Charge weight control and mold fill

    For food-contact and potable-water applications, polyolefin resin compliance is typically evaluated under FDA 21 CFR 177.1520 and Regulation (EU) 10/2011. Users must verify that the lot supplied for the application carries the appropriate conformity letter, because resin-level compliance does not automatically cover migration limits for the finished article in all food simulants. For industrial articles sold in the European Union, REACH registration duties are generally placed on the resin manufacturer or importer, while RoHS restrictions are article-level obligations when electrical or electronic equipment is placed on the market.

    Top