Lyondellbasell Npp11 0218 Linear Low Density Polyethylene

LyondellBasell NPP11-0218 Linear Low Density Polyethylene

    • Product Name: LyondellBasell NPP11-0218 Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 814339
    Density 0.918 g/cm3
    Melt Index 1.0 g/10 min (190°C/2.16 kg)
    Comonomer Type Butene-1
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 22.1 MPa
    Elongation At Break 800%
    Flexural Modulus 276 MPa
    Vicat Softening Temperature 95°C
    Melting Temperature 122°C
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 300 g
    Elmendorf Tear Strength Td 500 g
    Haze 12%
    Gloss 75%
    Coefficient Of Friction 0.2

    As an accredited LyondellBasell NPP11-0218 Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell NPP11-0218 Linear Low Density Polyethylene is supplied in 25 kg polyethylene-lined bags on pallets, or in bulk.
    Container Loading (20′ FCL) LyondellBasell NPP11-0218 Linear Low Density Polyethylene loaded in 20′ FCL; 25 kg bags, palletized, shrink-wrapped, secured for ocean transport.
    Shipping LyondellBasell NPP11-0218 Linear Low Density Polyethylene is supplied as non-hazardous thermoplastic pellets. Typically shipped in 25 kg polyethylene bags, jumbo bags, or bulk trucks/railcars. Keep dry; avoid heat, sunlight, and contamination. Store in a cool, dry, well-ventilated area. No special hazardous transport classification is required; standard industrial handling applies.
    Storage Store LyondellBasell NPP11-0218 Linear Low Density Polyethylene in a cool, dry, well-ventilated warehouse. Keep original bags closed, palletized, and off the floor. Protect from direct sunlight, heat, ignition sources, moisture, and contamination. Avoid excessive stacking and rough handling to prevent bag damage and dust. Use first-in, first-out inventory. Follow the supplier’s SDS and local regulations.
    Shelf Life Typically 24 months from date of manufacture when stored cool, dry, and in unopened original packaging away from direct sunlight.
    Application of LyondellBasell NPP11-0218 Linear Low Density Polyethylene

    Production-scale thin-wall food packaging lines processing LyondellBasell NPP11-0218 linear low-density polyethylene—nominal melt flow rate 11 g/10 min under ISO 1133-1:2022 at 190°C/2.16 kg, nominal density 0.918 g/cm³—typically configure hydraulic or servo-hydraulic injection molding machines with clamp force between 800 kN and 1,600 kN and screw L/D ratios of 20:1 to 24:1. The melt temperature corridor is held at 190°C–230°C, with the nozzle zone generally set 5°C–10°C below the metering zone to reduce stringing. Tool temperatures between 10°C and 40°C are employed to stabilize solidification and maintain cycle times below 9 s on multi-cavity tools. For direct food-contact lids and tubs, the finished formulation may use NPP11-0218 as a neat resin at 100 wt%, but multi-cavity tools with wall sections below 0.8 mm frequently incorporate 15–30 wt% of a fractional-melt LDPE to extend flow length and reduce gate blush; the actual ratio is determined by spiral-flow length measurement and short-shot mapping against the tool’s pressure-volume-temperature characteristics. Food-contact compliance is established through FDA 21 CFR 177.1520, with overall migration testing under EU Regulation (EU) No 10/2011 using EN 1186-1 and an overall migration limit of 10 mg/dm². The downstream production process is high-productivity injection molding; terminal articles are thin-wall dairy tubs, overcap lids, and delicatessen containers.

    What Happens When NPP11-0218 Is Introduced into Recycled Polypropylene Compounds?

    Addition of NPP11-0218 to post-consumer recycled polypropylene at 20–35 wt% modifies the low-temperature failure mode of the compound from brittle fracture to ductile yielding, but the actual transition depends on the rPP contamination level and the dispersion domain size achieved in compounding. The compounding operation uses a co-rotating twin-screw extruder with L/D 40:1, a barrel profile from 170°C to 210°C, vacuum degassing at barrel 9, and strand pelletization. Domain size control is critical: when LLDPE domains exceed 2.0 µm, impact resistance measured under ISO 180/A at -20°C becomes inconsistent across production lots; below 0.5 µm, the stiffening contribution of the polypropylene matrix is retained. At 35 wt% addition, flexural modulus under ISO 178 generally falls below 900 MPa, which excludes the material from rigid appliance housing specifications requiring ≥1,000 MPa. Compliance is evaluated under REACH Regulation (EC) No 1907/2006 for recycled feedstock and under IEC 60695-2-11 for end-product glow-wire performance in electrical-enclosure applications. The downstream process is melt compounding followed by injection molding; terminal product types include appliance back panels, internal brackets, and non-enclosure automotive interior components.

    Standard/RegulationScopeTest method or clauseLimit/requirement
    FDA 21 CFR 177.1520United States food-contact olefin polymersExtraction testing under 21 CFR 177.1520(b)Compliance with specified total extractables and end-use limitations
    EU Regulation (EU) No 10/2011European Union plastic food-contact materialsEN 1186-1 overall migration10 mg/dm²
    REACH Regulation (EC) No 1907/2006European Economic Area chemical safetySVHC screening under Article 33≤0.1 wt% per SVHC in article
    IEC 60695-2-11Fire hazard testing for electrical productsGlow-wire end-product test550–850°C depending application category

    Extrusion Lamination Sealant Layers and Neck-In Control

    On tandem extrusion lamination lines, NPP11-0218 is introduced into the sealant layer at 15–40 wt% with a high-pressure LDPE to balance hot-tack strength and seal initiation temperature in multi-layer flexible packaging. The blend is processed through a single-screw extruder with barrier screw design, L/D 30:1, die gap 0.5–0.8 mm, and melt temperature at the die lip of 280°C–310°C. Because LLDPE exhibits higher extensional viscosity than LDPE, the neck-in is controlled by reducing the air gap to 150 mm–250 mm and maintaining draw ratio below 10:1; failure to restrict draw ratio on high-speed lines produces edge-bead thickness variation greater than ±5%. Compliance for direct food-contact flexible packaging requires FDA 21 CFR 177.1520 or EU Regulation (EU) No 10/2011, with overall migration testing under EN 1186-1 and a limit of 10 mg/dm². The downstream process is extrusion coating and lamination onto aluminum foil, oriented polyester, or paperboard. Terminal products include retort lidding film, sachet stock, and snack packaging laminates.

    When NPP11-0218 functions as a carrier resin in additive or color concentrates, the formulation addition ratio is generally 55–70 wt% carrier to 20–35 wt% pigment or filler and 5–10 wt% processing aid/dispersant, depending on pigment oil absorption and letdown ratio target. The compounding operation uses a co-rotating twin-screw extruder with 32:1–48:1 L/D, side feeding at barrel 5 or 6, and screw temperature profile from 160°C in the feed throat to 200°C at the die plate, with melt temperature kept below 220°C to avoid thermal degradation of organic pigments and hindered amine light stabilizers. Dispersion quality is evaluated by pressure filtration test according to EN 13900-5 or by film optical inspection after letdown at 4 wt% masterbatch in a LLDPE/LDPE blown film matrix. Compliance is governed by REACH Regulation (EC) No 1907/2006 for substance registration and, where the masterbatch is intended for food-contact packaging, by FDA 21 CFR 177.1520 for the olefin polymer fraction and colorant restrictions under FDA 21 CFR 178.3297. Terminal product types are color masterbatches, antioxidant masterbatches, and slip/antiblock concentrates.

    When High-Speed Cast Stretch Film Lines Reach Draw Resonance Limits

    High-speed cast stretch film lines typically process NPP11-0218 as a modifier in LDPE-based formulations at 10–25 wt% to improve puncture resistance and machine-direction tear behavior without raising the total melt viscosity beyond the die pressure limits of the cast line. The downstream process uses a slot die with coat-hanger manifold, die gap 0.6–1.0 mm, chill roll temperatures 15°C–30°C, and line speeds from 200 m/min to 600 m/min. Draw resonance and edge weave are controlled by maintaining melt temperature at 240°C–270°C and by adjusting the air gap between die exit and chill roll to 20–40 mm; below 20 mm the film may freeze too rapidly and develop surface haze, while above 40 mm neck-in becomes progressively worse. Mechanical performance is tested under ASTM D882 for tensile and ASTM D5748 for puncture resistance. Compliance for industrial non-food stretch wrap falls under REACH Regulation (EC) No 1907/2006; food-wrap variants require EU Regulation (EU) No 10/2011 or FDA 21 CFR 177.1520. Terminal products include pallet stretch film, silage wrap, and protective surface films.

    Snap-Fit Closure Geometries Shift the Required HDPE Addition Level

    The injection molded closure segment uses NPP11-0218 at 70–85 wt% with high-density polyethylene at 15–30 wt% to provide a balance of hinge flexural fatigue resistance and environmental stress-crack resistance in fatty-food contact. The formulation is processed on high-cavitation stack molds with hot runner systems, melt temperature 200°C–240°C, holding pressure 50–70 bar hydraulic, and cooling time 3–6 s. Dimensional stability is checked by measuring cap ovality and top-load force after conditioning at 23°C and 50% RH for 48 h; melt flow rate of the blend is measured under ISO 1133-1:2022 at 190°C/2.16 kg. Environmental stress-crack resistance is tested under ASTM D1693 condition B; published data for this specific blend configuration is limited, so lot-to-lot verification is required for applications exposed to oleic acid or other fatty test media. Compliance for food-contact closures requires FDA 21 CFR 177.1520 or EU Regulation (EU) No 10/2011, and the terminal product types include snap-fit closures, beverage overcaps, and dispensing caps.

    Free Quote

    Competitive LyondellBasell NPP11-0218 Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell NPP11-0218 Linear Low Density Polyethylene is a butene-comonomer LLDPE supplied as pellets with a nominal density of 0.918 g/cm³ under ISO 1183-1:2019 and a melt mass-flow rate of 2.0 g/10 min under ISO 1133-1:2022 at 190 °C and 2.16 kg load. The grade is stabilized for conventional extrusion and film conversion, but the published technical bulletin does not itemize the complete additive package. The density below 0.920 g/cm³ classifies the material as a linear low-density polyethylene with short-chain branching produced by 1-butene; this composition lowers the crystalline fraction and modulus relative to HDPE and shifts the melting range below that of polypropylene. Because the molecular weight distribution is broader than that of a single-site metallocene LLDPE of equivalent density, the product shows a different balance of shear thinning, bubble stability, seal initiation, and optical clarity.

    The product’s most commonly referenced distinction from other LLDPE offerings is the pairing of 2.0 g/10 min flow with 0.918 g/cm³ density. This combination supports downgauging in blown film while retaining sufficient bubble integrity. However, product-specific lot release tolerances for this grade are typically maintained within ±0.002 g/cm³ on density and ±0.3 g/10 min on melt flow rate. Published data for this specific configuration is limited; conversion trials are required when the application depends on tight seal-initiation or tear-resistance limits.

    What Limits the Processing Window on High-Speed Blown Film Lines?

    On a 65 mm grooved-feed extruder with 30:1 L/D and a barrier screw, the resin is typically processed with a barrel profile of 170 °C to 210 °C, die temperature 210 °C, and a die gap of 1.8 mm to 2.2 mm. When the blow-up ratio is held between 2.2:1 and 2.8:1, a stable bubble is obtainable for film gauges between 25 µm and 60 µm without internal bubble cooling. Production-scale observations show that melt pressure before the screen changer rises by 10 bar to 15 bar per 100 h of continuous operation once edge-trim regrind exceeds 20 wt%; the increase is attributed to gel accumulation on a 60/80/100 mesh screen pack. The practical melt-temperature ceiling is 235 °C. Above this value, oxidative gel formation accelerates and film odor increases; below 175 °C, screw torque limits may be reached on machines without high-torque gearboxes.

    Pre-drying is not mandatory when storage relative humidity remains below 60%. If surface moisture exceeds 0.05%, hopper drying at 60 °C for 4 h returns melt pressure and film appearance to baseline. When melt fracture appears at gauge below 20 µm, the standard remedy is to increase die lip temperature to 215 °C or to introduce a polymer processing-aid masterbatch at 300 ppm to 500 ppm active fluoropolymer. Bubble instability at frost-line heights above 700 mm can be reduced by raising the die gap to 2.2 mm and lowering the blow-up ratio to 2.0:1, but this adjustment generally reduces transverse-direction tear resistance.

    Property Values and Test Methodology

    Representative values for a 0.918 g/cm³/2.0 g/10 min butene LLDPE are tabulated below for 25 µm blown film. They are not lot-release limits unless the supplier’s certificate of analysis states otherwise.

    Property Test method Nominal value Unit
    Density ISO 1183-1:2019 0.918 g/cm³
    Melt mass-flow rate ISO 1133-1:2022 2.0 g/10 min
    Tensile stress at yield, MD/TD ISO 527-3 10/9 MPa
    Tensile strain at break, MD/TD ISO 527-3 600/750 %
    Elmendorf tear resistance, MD/TD ISO 6383-2 45/70 g
    Dart drop impact, F50 ISO 7765-1 90 g
    Vicat softening temperature ISO 306/A50 96 °C
    Haze ASTM D1003 12 %
    Gloss at 60° ASTM D2457 70 dimensionless

    Film property balance is anisotropic. Machine-direction tear resistance is lower than transverse-direction tear resistance because molecular orientation along the machine direction increases fibrillation tendency. When frost-line height is increased from 400 mm to 700 mm, transverse-direction tear and dart drop impact typically improve while machine-direction tear decreases; the effect is more pronounced below 30 µm gauge. Lot-to-lot variation in comonomer incorporation can shift the density by ±0.002 g/cm³, which is within specification but can alter seal initiation temperature by 2 °C to 3 °C.

    Processing-aid masterbatch addition at 300 ppm to 500 ppm active fluoropolymer is compatible with the base resin and can reduce sharkskin at high shear rates, but the converter should not combine the processing aid with high levels of zinc stearate in the feedstock because the metal soap can reduce the effectiveness of the fluoropolymer coating on the die lip. The base antioxidant system is designed for standard film extrusion; repeated recycling above 5 passes can deplete the stabilizer and increase the gel count measured by ISO 18553.

    Comparison with other polyethylene families is dominated by comonomer type and molecular architecture. In a standard 25 µm film, a butene-based Ziegler-Natta LLDPE of this density typically exhibits lower dart drop impact and lower hot-tack strength than an octene-based LLDPE at equivalent density. The difference is usually attributed to the shorter 1-butene branch and the resulting lower concentration of long tie molecules. Below -10 °C, impact performance of the butene grade declines more rapidly than that of an octene or hexene grade; for cold-chain packaging, a C6/C8 resin is preferred unless downgauging or cost constraints control the formulation.

    When compared with LDPE, the product has a narrower molecular weight distribution and no measurable long-chain branching fraction by standard dynamic rheological methods. Consequently, converters blend 20 wt% to 30 wt% LDPE into the formulation to increase melt strength and raise bubble stability on high-stalk lines; the same blend reduces optics and dart impact. Against metallocene LLDPE, the product may exhibit haze values 3 to 5 percentage points higher and dart impact values 15% to 25% lower at 25 µm, but extrusion pressure is lower and die lip build-up is often less severe. Published data for this specific configuration is limited; comparative values should be generated on converter lines.

    Resin system Comonomer Typical density Typical MFR Relative dart impact in 25 µm film Optical haze range
    NPP11-0218 1-butene 0.918 g/cm³ 2.0 g/10 min reference 10–15%
    Hexene/octene LLDPE 1-hexene/1-octene 0.918–0.920 g/cm³ 0.5–2.0 g/10 min 20–35% higher 7–12%
    LDPE none 0.916–0.924 g/cm³ 0.2–2.0 g/10 min 20–40% lower 4–8%
    mLLDPE 1-hexene/1-octene 0.912–0.918 g/cm³ 0.8–2.0 g/10 min 30–50% higher 5–10%

    When Food-Contact and Regulatory Boundaries Constrain Formulation

    Food-contact compliance for NPP11-0218 must be established through the supplier’s product-specific declaration and not inferred from the grade class. Polyethylene resins manufactured from authorized monomers may comply with FDA 21 CFR 177.1520(c) for olefin polymers in contact with food, provided the finished article meets extraction limits under the intended condition of use. For the European market, migration testing must follow EU 10/2011 and its amendments, with the final film structure evaluated rather than the base resin alone. Converters should require the certificate of composition, lot-specific traceability, and a statement of REACH registration before use in direct food packaging. The product is not automatically suitable for medical device or pharmaceutical packaging; USP Class VI and ISO 10993 assessment are outside the standard film-grade documentation and must be commissioned separately. Heavy-metal and brominated flame-retardant restrictions under EU RoHS Directive 2011/65/EU are generally satisfied by the base polyolefin, but printed or laminated structures require separate assessment of inks, adhesives, and coatings.

    For industrial liners and heavy-duty sacks, conversion on blown film lines with die diameters of 200 mm to 300 mm and output rates between 180 kg/h and 240 kg/h is typical. At film gauges of 50 µm to 80 µm, puncture resistance should be evaluated by ISO 7765-1 dart drop or a puncture probe method before use in dry bulk packaging; the base resin contributes toughness but does not provide puncture specifications on its own. Exposure to strong oxidizing agents or high-shear compounding with acidic flame-retardant systems is not recommended because such conditions accelerate chain scission and reduce melt stability. If the film is subjected to repeated flexing below -20 °C, an impact-modified or octene-based LLDPE is preferable. The operating boundary for regrind content remains 20 wt%; exceeding this fraction without prior film property testing can produce visible gel defects in the finished web. For agricultural film requiring multi-season outdoor exposure, the base resin must be compounded with a UV stabilizer masterbatch evaluated under EN 13206 or equivalent accelerated weathering protocols.

    Top