| HS Code | 135251 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Density | 0.919 g/cm3 |
| Melt Index | 1.0 g/10 min |
| Antiblock | Yes |
| Slip | No |
| Tensile Strength At Yield Md | 10.3 MPa |
| Tensile Strength At Yield Td | 10.3 MPa |
| Tensile Strength At Break Md | 24.1 MPa |
| Tensile Strength At Break Td | 22.1 MPa |
| Elongation At Break Md | 500% |
| Elongation At Break Td | 700% |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 200 g/mil |
| Elmendorf Tear Strength Td | 350 g/mil |
| Haze | 12% |
| Gloss | 55% |
| Vicat Softening Point | 94 °C |
| Melting Point | 122 °C |
| Low Temperature Brittleness | -70 °C |
As an accredited LyondellBasell NPP11-0119 Linear Low Density Polyethylene with Antiblock factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell NPP11-0119 Linear Low Density Polyethylene with Antiblock is supplied in 25 kg polyethylene-lined bags, palletized and stretch-wrapped. |
| Container Loading (20′ FCL) | 20′ FCL container loading: LyondellBasell NPP11-0119 Linear Low Density Polyethylene with Antiblock, 25 kg bags, palletized, shrink-wrapped, secured for transport. |
| Shipping | LyondellBasell NPP11-0119 LLDPE with antiblock ships as non-hazardous polyethylene resin in 25 kg bags, 1000 kg super sacks, or bulk trucks/railcars. Store cool and dry, away from ignition sources, moisture, and direct sunlight. No special transport placards required; avoid bag punctures and pellet release. |
| Storage | Store LyondellBasell NPP11-0119 Linear Low Density Polyethylene with Antiblock in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and flames. Keep original bags or containers closed, palletized, and off the floor to prevent moisture and contamination. Avoid prolonged UV exposure and excessive stacking. Use first-in, first-out inventory. Maintain good housekeeping; material is combustible as dust or pellets. |
| Shelf Life | Shelf life is typically 12 months from manufacture when stored in original packaging in a cool, dry area, away from direct sunlight. |
A three-layer heavy-duty sack line running LyondellBasell NPP11-0119 Linear Low Density Polyethylene with Antiblock in the outer skins at 70–80 wt% and a low-melt-index LDPE core at 20–30 wt% is operated with a 100 mm grooved-feed extruder, L/D 30:1, and a 250 mm spiral mandrel die having 1.6 mm die gap. The bubble is maintained at a blow-up ratio of 2.5:1 to 3.0:1, frost line height at 8–10 die diameters, and die-lip melt temperature between 195 °C and 215 °C. Compliance under FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011 requires an overall migration limit not exceeding 10 mg/dm² when converted film is evaluated with assigned food simulants; for non-food chemical liners, REACH Regulation (EC) No 1907/2006 SVHC screening applies to tonnage placed on the EU market. Terminal products include 25 kg chemical sacking, 50 kg resin shipping sacks, and flat-tube liners for FIBCs at thicknesses between 80 µm and 150 µm. The pre-dispersed antiblock in the skin layers reduces reel blocking after corona treatment, while the absence of slip at the core interface preserves heat-seal strength measured by ASTM F88/F88M-21. On lines exceeding 120 kg/h, bubble instability becomes the limiting defect when the outer skin reaches 225 °C; reducing die gap to 1.2 mm and raising air-ring pressure restores stability but typically lowers dart impact from 120 g to 90 g under ASTM D1709-16e1, Method A.
| Requirement | Applicable standard | Measured parameter and limit |
|---|---|---|
| EU food-contact plastics | Regulation (EU) No 10/2011 | Overall migration 10 mg/dm² |
| US food-contact olefin polymers | FDA 21 CFR 177.1520(c) | Polyethylene resin specification and condition of use |
| Paper and paperboard component | FDA 21 CFR 176.170(c) | Components for aqueous and fatty food contact |
| Melt flow rate | ASTM D1238-20 / ISO 1133-1:2022 | 190 °C / 2.16 kg |
| Dart impact | ASTM D1709-16e1 | F50, g/mil or g |
| Coefficient of friction | ASTM D1894-14 | Film-to-film kinetic COF |
| Heat-seal strength | ASTM F88/F88M-21 | N/15 mm after specified dwell |
| Silage film performance | EN 13207 | Tensile and tear after weathering |
In 23 µm machine stretch film produced on a high-speed cast line, NPP11-0119 is typically incorporated at 75–85 wt% in the core layer, with a tackified LLDPE or metallocene skin occupying 10–15 wt%. The pre-dispersed antiblock creates a lower room-temperature coefficient of friction when tested according to ASTM D1894-14; film-to-film kinetic COF is normally specified between 0.35 and 0.55 for reliable machine unwinding. Secondary antiblock masterbatch addition above 0.5 wt% generates surface micro-roughness sufficient to suppress cling force below 250 g/cm in ASTM D4649-20 evaluations, which causes film-roll telescoping on pallet wrappers running above 30 rpm. The cast process uses a 0.9 mm flat-die gap, melt temperature of 245–260 °C, and a matte-finish chill roll held at 18–24 °C; line speed for 23 µm film is limited to 450–600 m/min by web flutter and edge-bead formation. Terminal products are machine rolls of 500 mm width and 1500 m roll length for high-speed wrappers, plus hand-wrap cores of 250 mm width. Mechanical conformance is checked under ISO 527-3 for machine-direction tensile elongation; film at 200% pre-stretch must retain at least 10 MPa MD tensile strength. For retail export packaging, EN 15343 may be referenced for recycled-content traceability when post-industrial reclaim is introduced.
Silage cover film made with NPP11-0119 at 80 wt%, blended with 20 wt% low-melt-index LDPE for improved film toughness, is extruded through a 140 mm blown-film die at a 2.8:1 blow-up ratio and 20–25 °C air-ring air temperature. Terminal products include 130–180 µm black-and-white coextruded silage covers and 40 µm bale wrap, supplied in 50 m × 25 m folded panels. The product is tested against EN 13207, which specifies tensile strength and tear resistance after outdoor exposure; the outer white layer must maintain specified opacity when cross-checked by thickness-weight measurement. In the EU, Regulation (EU) No 10/2011 applies when harvested feed is considered direct food contact; the overall migration limit of 10 mg/dm² is calculated from total contact area. The downstream process requires no corona treatment on the black inner layer; covers are assembled by hot-knife sealing at 120–140 °C. Antiblock in the resin prevents reel blocking during outdoor storage between fabrication and installation, but pre-drying at 70 °C for 2 h is required when pellets are stored at relative humidity above 60%.
In extrusion coating of aseptic liquid packaging board, NPP11-0119 is applied as a 15–30 g/m² barrier tie layer at a melt temperature of 290–315 °C through a 1200 mm slot die with 0.8 mm die gap. The resin is used at 100% or blended with LDPE at 40:60 for reduced neck-in during high-speed coating. Downstream converting comprises corona treatment, extrusion coating onto board in a tandem line at 120–250 m/min, followed by heat sealing into gable-top and brick cartons. Compliance for direct food contact is evaluated under FDA 21 CFR 176.170(c) for paper and paperboard components and EU Regulation (EU) No 10/2011; the polyolefin coating layer must also meet FDA 21 CFR 177.1520(c). End products include 250 mL, 500 mL, and 1 L dairy and juice cartons with 12–16 µm aluminum foil and board. Adhesion is checked according to ASTM F904-16 after heat-seal simulation at 160 °C and 0.3 MPa jaw pressure. The processing window is constrained: below 285 °C peel strength falls below 4 N/15 mm, while above 320 °C polymer chain degradation generates odour that exceeds organoleptic limits under EN 1230-1. The resulting 35 °C window requires die-temperature control of ±3 °C to maintain consistent polymer-foil adhesion.
Vertical form-fill-seal conversion of 45–70 µm frozen-food film using NPP11-0119 at 60–70 wt% in the sealant layer of a coextruded structure is run with a 1.8 mm die gap, 2.2:1 blow-up ratio, and 200–220 °C melt temperature on a 75 mm extruder. End products include 250 g–2 kg frozen-vegetable pouches, ice-making pouches, and refrigerated food bags. The sealant layer is qualified under FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011 for plastic food-contact materials. Heat-seal strength is measured according to ASTM F88/F88M-21, with minimum 6 N/15 mm on the reciprocating jaw sealer at 140 °C and 0.4 MPa. The antiblock in the sealant layer prevents unwind blocking at high speed and reduces dust adhesion to corona-treated surfaces. Corona treatment must not exceed 42 mN/m on the sealant side; documented line failures show that in-line treaters above 45 mN/m can re-wet the surface and create blocking despite the antiblock package.
When NPP11-0119 is used as a 20–30 wt% impact-modifying fraction in injection moulding of flexible lids, the blend base is typically a high-flow HDPE or PP; the injection machine should deliver clamp force of 150–350 tonnes and barrel temperatures from feed to nozzle of 180/190/200/210 °C. The mould temperature is maintained at 15–30 °C; controller injection pressure generally reaches 70–90 MPa. The downstream process includes melt plastification, injection, cooling, and ejection. Terminal products are 110–125 mm snap-on lids, overcaps for paint pails, and flexible covers for household chemical containers. Mechanical evaluation is performed under ISO 527-2 for tensile yield and ISO 178 for flexural modulus. For food-contact lids, EU Regulation (EU) No 10/2011 imposes an overall migration limit of 10 mg/dm², and FDA 21 CFR 177.1520(c) covers the polyethylene fraction. The antiblock silica acts as a low-level mould-release aid, but at blend ratios above 35 wt% surface haze increases and gloss measured at 60° under ASTM D2457-13 may fall below 20 GU, making the part unsuitable for clear overcaps. Published data for this specific configuration is limited; batch-specific additive retention must be confirmed by lot certificate.
Cast hygiene film lines processing NPP11-0119 use 70–85 wt% of the resin in the core layer, with metallocene skin layers for reduced melting point and improved softness. The melt curtain from an 800 mm coat-hanger die with 0.6 mm lip gap is quenched on a 12–16 °C chill roll; line speed is usually 350–500 m/min for 30–40 µm film. Above 500 m/min, web neck-in exceeds 15%, and edge-bead formation causes gauge variation beyond ±5% as measured by ISO 4593. The antiblock reduces reel blocking during storage at 35 °C and 80% RH, but also lowers transparency when downstream masterbatch addition exceeds the pre-compounded level. Regulatory exposure is covered by FDA 21 CFR 177.1520(c) for overwrap contact and EU Regulation (EU) No 10/2011 for food-contact overall migration. End products include hygiene product overwrap, paper towel bundles, and magazine wraps. The film is slit to 400–900 mm rolls and requires static decay verification under IEC 61340-2-3 when used for electronics packaging.
Competitive LyondellBasell NPP11-0119 Linear Low Density Polyethylene with Antiblock prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell NPP11-0119 Linear Low Density Polyethylene with Antiblock is a resin designation that combines a linear low density polyethylene matrix with an inorganic antiblock additive system. Published certificate-of-analysis values for this specific grade are limited; therefore, numerical ranges in this document are stated as standardized class bands for LLDPE film resins unless the measurement is explicitly product-specific. The grade code NPP11-0119 should be confirmed against the supplier's technical datasheet and lot certificate before extrusion trials. Incoming inspection is normally performed using ISO 1133-1:2022 or ASTM D1238 for melt flow rate at 190 °C under 2.16 kg, ISO 1183-1 or ASTM D1505 for density, and ASTM D3354 for blocking load. The antiblock component functions by reducing the real contact area between adjacent film layers through micro-scale surface protrusions, not by chemically altering the polymer backbone.
Because antiblock efficacy is governed by particle size, particle size distribution, refractive index, and loading, the morphological response of the film surface is not a simple linear function of additive weight fraction. Synthetic amorphous silica and natural diatomaceous earth are the common inorganic antiblock classes; their particle diameters typically lie between 2 µm and 10 µm, although tail fractions above 10 µm can dominate visible surface defects in films thinner than 20 µm. After film solidification, the particles protrude from the polyethylene surface, creating roughness that lowers blocking force. Blocking load measured under ASTM D3354 decreases as protrusion density increases until optical degradation becomes unacceptable. Haze measured under ASTM D1003 and 60° gloss measured under ASTM D2457 are the standard indicators of that optical penalty. Because silica has a refractive index near 1.46 and polyethylene near 1.51–1.54, transmitted light is scattered, increasing wide-angle haze. Antiblock is not synonymous with slip. Static and kinetic coefficients of friction measured under ASTM D1894 remain controlled by migratory amide additives when present. A resin containing antiblock without slip may still show high film-to-metal coefficient of friction, so converter trials should separate the two mechanisms.
On monolayer blown-film lines with internal bubble cooling and high-stalk bubble configurations, LLDPE resins of this class are processed at melt temperatures from 190 °C to 240 °C. The lower boundary is set by melt homogeneity and the upper by oxidation risk; actual set points depend on extruder diameter, screw design, and output rate. Typical general-purpose blown-film extruders for LLDPE operate with 24:1 to 30:1 length-to-diameter ratios and use barrier screws with Maddock or spiral mixing sections. Die gap selection for LLDPE is often 1.0–1.5 mm; narrower gaps increase shear stress and may initiate sharkskin melt fracture. Inorganic antiblock particles can promote die lip deposit formation over extended runs, so planned die cleaning intervals should be indexed against pressure drop across the screen pack and die. Blow-up ratios between 2.0:1 and 3.5:1 are common, with frost line height adjusted to balance impact and tear. The processing window is not a narrow ±5 °C boundary; bubble stability, melt strength, and melt fracture typically limit output before a thermal degradation threshold is reached. At film thickness below 20 µm, oversized antiblock particles can act as stress concentrators and generate pinholes, making the top-size fraction of the additive package an important specification.
In converter environments with high winding tension or long roll storage periods, substitution of an antiblock-containing LLDPE changes blocking behavior before it changes tensile or seal strength. Trial protocols should measure blocking after 24 h and 7 days under ASTM D3354 with a defined load, temperature, and aging time because blocking develops under pressure. The expected benefit is a reduction in roll blocking defects and lower unwind tension variation. At equal film gauge, dart impact under ASTM D1709 and Elmendorf tear under ASTM D1922 are governed primarily by the base resin and comonomer type; the antiblock additive effect on these properties is usually secondary but must be confirmed. Heat seal strength under ASTM F88 and hot tack under ASTM F1921 should be checked because inorganic particles at elevated loading can interrupt the fusion bond. Published data for this specific NPP11-0119 configuration in high-winding-tension conversion is limited; converter validation is required.
| Attribute | Test method | Typical class band | Note |
|---|---|---|---|
| Melt flow rate | ISO 1133-1:2022, ASTM D1238 | 0.5–2.0 g/10 min at 190 °C, 2.16 kg | Class range for LLDPE film; lot-specific value required |
| Density | ISO 1183-1, ASTM D1505 | 0.918–0.925 g/cm³ | Class range; not certificate value |
| Antiblock content | Ashing, XRF, or XPS | 500–5000 ppm | Confirm exact additive level with supplier |
| Blocking force | ASTM D3354 | Product-specific | Time, load, and temperature dependent |
| Haze | ASTM D1003 | Higher than unmodified LLDPE | Optical penalty from additive |
| Coefficient of friction | ASTM D1894 | Product-specific | Controlled by slip system |
| Dart impact | ASTM D1709, Method A/B | Product-specific | Comonomer dependent |
| Elmendorf tear | ASTM D1922 | Product-specific | MD/TD anisotropy expected |
| Heat seal strength | ASTM F88 | Product-specific | Validate seal initiation curve |
Film structures containing NPP11-0119 are typically directed toward form-fill-seal food packaging, heavy-duty sacks, industrial liners, and over-wrappers where roll blocking during storage or high-speed unwinding is a known bottleneck. For food-contact applications, the converter must establish compliance under 21 CFR 177.1520 for olefin polymers and, where relevant, European Union Regulation EU 10/2011 with overall migration limits of 10 mg/dm². The inorganic antiblock component must be acceptable under applicable food-contact additive inventories. Because the base resin and additive package influence organoleptic and seal performance, application-specific qualification is mandatory. In heavy-duty sacks at film thicknesses from 70 µm to 120 µm, the antiblock effect is concentrated at the surface, while puncture resistance is governed by the core layers.
For converters running high-speed vertical form-fill-seal equipment, the interaction among film stiffness, surface roughness, and metal surfaces determines transfer efficiency. An antiblock-modified surface may reduce web tracking issues caused by blocking, but it does not necessarily lower film-to-metal friction. If low coefficient of friction is required for forming shoulders or bag guides, a migratory slip additive is added separately. In such lines, the film must also withstand impact and seal requirements; dart impact values should be correlated with fill weight and drop height using ASTM D1709 Method A or B, and seal strength should be correlated with jaw temperature using ASTM F88. Without machine-specific data, a general substitution is not justified.
Differentiation among LLDPE grades with antiblock is primarily a function of comonomer type, molecular weight distribution, and antiblock particle selection. Butene-based LLDPE film grades often exhibit lower dart impact and tear resistance than hexene-based or octene-based grades at equivalent melt index and density because longer comonomers produce more effective tie-molecule formation. The specific comonomer used in NPP11-0119 is not stated in the limited public identifier; the certificate of analysis and supplier datasheet should be consulted. Compared with a standard LDPE film resin, LLDPE is less shear-thinning, so it normally requires higher extruder torque and melt pressure at equivalent output. This difference is more pronounced with narrow die gaps and low melt temperatures. In multilayer coextrusion, the viscosity ratio between skin and core should be monitored; interlayer instability can appear when the ratio exceeds approximately 2:1 at the die-lip shear rate.
Antiblock package selection also differentiates NPP11-0119 from slip-agent-only grades. An erucamide or oleamide slip additive migrates to the film surface over hours to days, reducing coefficient of friction but not necessarily blocking. An antiblock additive reduces blocking immediately after cooling but may not reduce coefficient of friction unless a migratory slip component is present. Many commercial films therefore combine both additive types; the antiblock gives physical separation and the slip agent lowers surface friction. If NPP11-0119 contains antiblock only, the converter should not assume low film-to-metal coefficient of friction values during transfer. Surface resistivity and static decay may need separate antistatic treatment; antiblock additives do not confer antistatic performance.
LLDPE pellets are supplied with the antiblock dispersed in the polymer matrix; no separate liquid additive dosing is required unless additional slip, antistatic, or polymer processing aids are specified downstream. The resin should be stored in dry conditions. Although LLDPE does not hydrolyze, surface condensation can transport fines and antiblock particles into feed ports and contribute to pellet bridging. Pre-drying is not normally required at relative humidity below 60%; above that, hopper drying at 60–70 °C for 2–4 h may be used to remove surface moisture, but temperatures above 80 °C should be avoided if a migratory amide slip additive is present. Regrind reincorporation at 10–30 wt% is common in film plants; higher levels can shift rheology, raise gel counts, and increase screen pack pressure because inorganic antiblock particles are non-melting. Screen pack mesh sizes of 40–100 mesh are typical, with pressure-drop monitoring used to set change intervals.
Three-layer blown film structures can position an antiblock-bearing LLDPE as the outside skin at 10–20% of total film thickness, while the core and sealant skin use resins selected for toughness and sealing. In such structures, the concentration of antiblock in the finished film is diluted by the layer ratio; the outside surface still carries the full additive loading from the skin resin. Multilayer dies with 0.8–1.4 mm die gaps and internal bubble cooling allow the higher-viscosity LLDPE skin to be carried by a higher-melt-strength core. Interlayer flow instability can appear if the viscosity ratio between skin and core exceeds approximately 2:1 at the die-lip shear rate. When NPP11-0119 is introduced into a coextrusion structure, the processing trial should log melt pressure, die lip temperature, and bubble frost line position at each output step.
Because antiblock concentrates can produce haze bands, particle agglomerates, and die-lip deposits under suboptimal dispersion, film defects should be classified by transmitted-light inspection and surface profilometry. Agglomerates form if the additive is not adequately dispersed or if the resin is exposed to high shear at low melt temperature; they appear as fisheyes. Haze measurement under ASTM D1003 catches gross optical differences, but high-resolution surface profilometry or scanning electron microscopy of film surfaces is required to quantify protrusion density and particle distribution. In cast-film lines operating at high line speeds, die lip deposits from inorganic antiblock may appear as streaks; the use of a purge compound with abrasive or scrubbing filler at planned intervals may be necessary, but the purge must be compatible with polyethylene and food-contact requirements where applicable.
In cast-film wrapper lines running at moderate output rates, the value of an antiblock-bearing LLDPE is observed mainly when film is wound at high tension and stored at elevated ambient temperatures. Blocking develops faster when film temperatures exceed 30–35 °C in warehouse environments, so trials should age wound rolls at the maximum expected storage temperature. Tensile elongation under ASTM D882 and puncture resistance under ASTM F1306 are secondary test methods used to compare the NPP11-0119 candidate against the incumbent film on the same line. Processors should obtain lot-specific melt flow and density values before adjusting extruder barrel profiles, because film-grade LLDPE resins with identical nominal designations can vary sufficiently to alter bubble stability and screw feed behavior.