Lyondellbasell Npp 11 5026

LyondellBasell NPP 11-5026

    • Product Name: LyondellBasell NPP 11-5026
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 977832
    Product Name LyondellBasell NPP 11-5026
    Manufacturer LyondellBasell
    Polymer Type Polypropylene Homopolymer
    Melt Flow Rate 11 g/10 min
    Density 0.900 g/cm³
    Tensile Strength At Yield 34.5 MPa
    Tensile Elongation At Yield 10%
    Flexural Modulus 1380 MPa
    Notched Izod Impact At 23 C 21 J/m
    Heat Deflection Temperature At 0 45 Mpa 100 °C
    Heat Deflection Temperature At 1 82 Mpa 55 °C
    Vicat Softening Temperature 155 °C
    Rockwell Hardness 100 R
    Processing Method Injection Molding
    Form Pellets
    Color Natural

    As an accredited LyondellBasell NPP 11-5026 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell NPP 11-5026 is supplied in 25 kg polyethylene bags or 1,000 kg bulk bags for industrial use.
    Container Loading (20′ FCL) 20′ FCL container loaded with LyondellBasell NPP 11-5026 in labeled drums, securely stowed, sealed, and ready for ocean transport.
    Shipping LyondellBasell NPP 11-5026 is n-propyl propionate. It ships as UN 3272, Esters, n.o.s. (n-propyl propionate), Class 3, PG III, flammable liquid, flash point ~34°C c.c. Use UN-approved steel drums, IBCs, or tankers; ground during transfer. Store cool, dry, ventilated, away from ignition sources. Transport documents must show proper shipping name and hazard class.
    Storage Store LyondellBasell NPP 11-5026 in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed to prevent moisture and contamination. Separate from strong oxidizers and incompatible materials. Avoid dust generation and accumulation. Follow the manufacturer’s SDS, local regulations, and good industrial hygiene practices. Use appropriate PPE and grounding/bonding if required.
    Shelf Life Shelf life is 24 months from date of manufacture when stored in original unopened containers under normal, cool, dry conditions.
    Application of LyondellBasell NPP 11-5026

    LyondellBasell NPP 11-5026 is processed as a polypropylene homopolymer with a nominal melt flow rate of 11 g/10 min determined under ISO 1133-1:2022 at 230 °C and 2.16 kg piston load, and a density of 0.900 g/cm³ measured to ISO 1183-1:2019. The medium-flow viscosity band places this grade in thin-wall injection moulding, closure manufacturing, rigid packaging, diagnostic consumable moulding, short-glass compounding, and appliance structural parts where melt temperature control below 250 °C is limiting. Finished-article regulatory status depends on the full formulation and conversion route; the following application entries therefore separate base-resin processing behaviour from additive-dependent compliance assessed under FDA 21 CFR 177.1520, EU No 10/2011, REACH, and RoHS 2011/65/EU where applicable.

    When sidewall deflection below 0.25 mm at 65 °C is the controlling specification

    Thin-wall containers moulded from NPP 11-5026 are produced on high-speed injection moulding machines with clamping force between 2,500 kN and 5,000 kN; the barrel profile is set from 200 °C in the rear zone to 240 °C in the nozzle, and the mould surface is held between 20 °C and 40 °C. For a 0.5 mm nominal wall, filling is completed below 0.6 s when screw forward velocity exceeds 250 mm/s, while cooling time is maintained at 3 s/mm to 5 s/mm of wall thickness. The formulation for food-contact thin-wall parts retains NPP 11-5026 at 98.0 wt% to 99.5 wt%; a sorbitol-based clarifier is added at 0.05 wt% to 0.20 wt%, a non-ionic glycerol monostearate antistatic agent at 0.03 wt% to 0.10 wt%, and a slip agent such as erucamide at 0.05 wt% to 0.15 wt%. The processing window is bounded by the hot-fill requirement: in-mould cooling time below 3 s/mm produces sidewall deflection above 0.25 mm when the filled container is exposed to contents at 65 °C. Terminal food-contact articles include dairy cups, delicatessen trays, lids, and single-serve containers; compliance assessment follows FDA 21 CFR 177.1520 for olefin polymers, EU No 10/2011 for overall migration and specific migration limits, and Regulation (EC) 1935/2004 for traceability and good manufacturing practice. A chloride-free acid scavenger is used at 0.03 wt% to 0.05 wt% where the package is intended for direct contact with acidic dairy products; published data for NPP 11-5026 in high-temperature hot-fill above 65 °C is limited.

    In closure manufacturing, the relationship between top-load retention and removal torque after 90 days at 40 °C is governed by the resin’s initial crystallinity distribution and the migration behaviour of the slip package. NPP 11-5026 is formulated for injection-moulded and injection-compression moulded closures at 98.0 wt% to 99.5 wt%, with a slip agent at 0.05 wt% to 0.15 wt%, a hindered phenolic antioxidant at 0.05 wt% to 0.10 wt%, a phosphite secondary antioxidant at 0.05 wt% to 0.10 wt%, and a calcium stearate acid scavenger at 0.02 wt% to 0.05 wt%. The downstream process uses high-cavitation hot-runner tooling; melt temperature is held between 210 °C and 250 °C, mould temperature between 10 °C and 30 °C, and the closure bridges are sealed at cooling times of 4 s to 8 s depending on bridge thickness. Equipment with clamp force from 3,000 kN to 8,000 kN is common for cold-runner stack moulds producing 26 mm to 38 mm closures. Torque retention is evaluated under ASTM D2063/D2063M-17; published data for NPP 11-5026 in closure-specific torque retention is limited. Terminal parts include screw caps for bottled water, still and carbonated beverages, dairy products, and non-aggressive household fluids. The operational boundary is stress-cracking agents: closures containing high perfume loads or strong oxidising detergent formulations are avoided unless a stress-crack-resistant modification is qualified; NPP 11-5026 homopolymer is not designed for aggressive essential oil contact without specific testing.

    What governs autoclave cycle life in polypropylene diagnostic consumables?

    Autoclave cycle life in NPP 11-5026 diagnostic consumables is controlled by the retained antioxidant package and by the processing thermal history in the hot runner. The formulation uses NPP 11-5026 at 98.5 wt% to 99.5 wt%, a high-molecular-weight hindered phenolic antioxidant at 0.08 wt% to 0.15 wt%, a hydrolytically stable phosphite at 0.05 wt% to 0.10 wt%, and an acid scavenger at 0.02 wt% to 0.05 wt%; no slip agent is used where surface chemistry interferes with cell adhesion assays. Downstream processing is performed in a controlled environment on electric injection moulding machines with clamp force from 1,000 kN to 3,500 kN, barrel temperature 200 °C to 240 °C, and mould temperature 20 °C to 50 °C. Moulded parts of 0.8 mm to 2.0 mm wall thickness are loaded into steam autoclaves at 121 °C for 20 min to 30 min; after five cycles, dimensional change is held below 0.5% when measured parallel to flow. Regulatory evaluation of the finished diagnostic consumable follows ISO 10993-1:2018 for cytotoxicity, USP <661.1> for plastic components, and FDA 21 CFR 177.1520 where food-contact labelling is required; manufacturing facilities are generally operated under ISO 13485:2016 when the consumable is classified as a medical device accessory. Terminal products include centrifuge tubes, Petri dishes, pipette tip racks, and sample cups. The operational boundary is ionising radiation: gamma sterilisation above 25 kGy produces oxidative embrittlement unless a radiation-stable additive package is adopted; autoclave exposure above 134 °C is not recommended because the antioxidant system in standard polypropylene homopolymer formulations is depleted after repeated cycles.

    Compounding lines equipped with co-rotating twin-screw extruders of 40:1 L/D process NPP 11-5026 as the continuous matrix for 20 wt% to 30 wt% chemically sized glass fibre; the resin is fed at the main hopper at 60 wt% to 75 wt%, the coupling agent is metered through a side feeder at zone 6, and the chopped glass roving is introduced downstream at zone 7 to limit fibre fracture. The formulation is set at NPP 11-5026 60 wt% to 75 wt%, maleic anhydride grafted polypropylene coupling agent 1.5 wt% to 3.0 wt%, glass fibre 20 wt% to 30 wt%, antioxidant masterbatch 0.2 wt% to 0.5 wt%, and heat stabiliser 0.1 wt% to 0.3 wt%. Barrel temperature is maintained between 200 °C and 230 °C, screw speed between 250 rpm and 450 rpm for 27 mm to 75 mm diameter machines, specific mechanical energy input between 0.18 kWh/kg and 0.25 kWh/kg, residence time below 45 s, and die pressure below 80 bar to avoid excessive shear heating. The principal process conflict is that below 20 wt% glass fibre, tensile modulus under ISO 527-1:2019 does not provide the required rigidity for metal replacement; above 30 wt%, melt viscosity raises die pressure and accelerates screw and barrel wear. Flexural modulus is measured under ISO 178:2019, Charpy notched impact under ISO 179-1:2010, and heat deflection temperature under ISO 75-2:2013; compounds supplied into EU automotive applications are evaluated against REACH Article 33 and RoHS 2011/65/EU. Typical compounded values for homopolymer polypropylene with 30 wt% short glass fibre fall between 4,500 MPa and 6,500 MPa tensile modulus and 90 MPa to 120 MPa tensile strength, but published data for NPP 11-5026 in this exact formulation is limited. Terminal products after injection moulding include automotive air filter housings, fan shrouds, under-hood covers, appliance structural brackets, and industrial pump bodies. The compounded pellets are pre-dried at 80 °C for 2 h when the repackaged material has been stored at relative humidity above 60%; free amine-containing colorants or flame retardants are avoided at processing temperatures above 240 °C because amine-catalysed oxidation can reduce molecular weight and degrade impact performance.

    Rigid pail wall thickness and drop impact at −10 °C

    Industrial pails moulded from NPP 11-5026 are dimensioned to survive a 1.2 m drop at −10 °C when loaded with volumes up to 30 L; the drop test is conducted under ASTM D5276-19. The formulation for indoor and outdoor storage uses NPP 11-5026 at 96.0 wt% to 98.0 wt%, a HALS ultraviolet stabiliser at 0.2 wt% to 0.4 wt%, a hindered phenolic antioxidant at 0.05 wt% to 0.15 wt%, a phosphite at 0.05 wt% to 0.15 wt%, and a colourant masterbatch at 1.0 wt% to 3.0 wt%; carbon black masterbatch at 2.0 wt% to 3.0 wt% is used where outdoor weathering beyond 12 months is specified. The downstream injection moulding process employs machines with clamp force from 8,000 kN to 20,000 kN, melt temperature 210 °C to 250 °C, mould temperature 10 °C to 30 °C, and nominal wall thickness 2.0 mm to 4.0 mm. Cooling time is set from 12 s to 30 s depending on wall thickness and gate configuration; hot-runner sequential valve gating is preferred for pails of 10 L and above to reduce knit-line fragility. Terminal articles include 1 L to 30 L pails for paints, lubricants, food powders, dry building products, and industrial chemical concentrates. The operational boundary for dangerous goods service is that UN certification requires testing on the finished pail and closure system; the base resin alone does not confer UN packaging approval. Wax and silicone processing aids are avoided at levels above 0.1 wt% where the pail will be printed with solvent-borne inks because thermal bonding of decoration can be compromised.

    Creep at 60 °C in small appliance structural parts governs rib depth

    Small appliance structural components moulded from NPP 11-5026 are designed with rib depth limited by creep modulus retention at 60 °C; tensile creep tests under ISO 899-1:2017 are used to generate design curves for load-bearing ribs and snap-fits. The compound is formulated with NPP 11-5026 at 80 wt% to 90 wt%, fine talc masterbatch at 10 wt% to 20 wt%, a hindered phenolic antioxidant at 0.1 wt% to 0.3 wt%, a phosphite at 0.05 wt% to 0.15 wt%, and a pigment masterbatch at 1 wt% to 2 wt%. Processing occurs on reciprocating screw injection moulding machines with clamp force 1,500 kN to 6,000 kN, barrel temperature 210 °C to 250 °C, mould temperature 20 °C to 50 °C, and wall thickness between 2.0 mm and 3.0 mm; holding pressure is applied between 40 MPa and 70 MPa until gate freeze. Compliance for household appliances follows IEC 60335-1:2020 for general safety, UL 94 HB for flammability classification where accepted, and RoHS 2011/65/EU for restricted substances; food-adjacent components are evaluated against FDA 21 CFR 177.1520 where applicable. Terminal products include bases, internal frames, fan housings, and structural brackets for coffee machines, water dispensers, and vacuum cleaners. The operational boundary is direct surface temperature above 90 °C: unreinforced NPP 11-5026 compounds lose stiffness and may creep beyond designed clearance; talc addition above 20 wt% reduces weld line strength and is not recommended without impact modification.

    Free Quote

    Competitive LyondellBasell NPP 11-5026 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell NPP 11-5026 is an unfilled polypropylene homopolymer injection-molding grade supplied in pellet form. The grade designation follows the manufacturer’s internal nomenclature: the number 11 is conventionally associated with a nominal melt mass-flow rate of 11 g/10 min when tested under ISO 1133-1:2022 at 230 °C with a 2.16 kg load, and the suffix 5026 identifies the stabilizer and nucleating-agent package. The resin is available as a free-flowing pellet with a density that is class-typical for unfilled PP homopolymers; however, published data for this specific configuration is limited, and mechanical-property claims must be verified against the lot certificate. Candidate processing routes include conventional injection molding, thin-wall rigid packaging, closures, housewares, and appliance components. The material is not a controlled-rheology successor-grade to a random copolymer, and its substitution in applications requiring clarity or low-temperature ductility must be treated as a separate technical evaluation.

    What specification framework governs the grade?

    For an unfilled polypropylene homopolymer, the specification framework follows ISO 1873-2:2007 for the designation of polypropylene and propylene-copolymer thermoplastics. The grade is described as a nucleated PP-H with a nominal melt mass-flow rate of 11 g/10 min; this is not a lot-release statement but a classification. Table 1 lists the analytical matrix used for incoming resin qualification. The third column represents class-typical values for nucleated PP-H of this flow class; these ranges are not a substitute for the manufacturer’s certificate of analysis.

    PropertyTest methodNucleated PP-H MFR 11 class-typical range
    Melt mass-flow rateISO 1133-1:2022, 230 °C/2.16 kg10–12 g/10 min
    DensityISO 1183-1:20190.895–0.905 g/cm³
    Tensile stress at yieldISO 527-2:2012, 50 mm/min27–33 MPa
    Tensile strain at yieldISO 527-2:20127–10 %
    Flexural modulusISO 178:2019, 2 mm/min1,100–1,400 MPa
    Notched Charpy impact at 23 °CISO 179-1/1eA2.0–4.0 kJ/m²
    Heat deflection temperature, 0.45 MPaISO 75-2/B75–90 °C
    Vicat softening temperature, A/50ISO 306148–155 °C
    Mold shrinkage, parallel/transverseISO 294-4:20180.8–1.5 % / 0.9–1.6 %

    In addition to the properties in Table 1, incoming lots should be checked for ash content under ISO 3451-1:2019. Unfilled homopolymer with a standard acid-scavenger and nucleating-agent package normally exhibits ash below 0.10 % by mass. Ash values above 0.15 % can indicate contamination, additive agglomeration, or cross-lot blending. Yellowness index determined under ASTM E313-20 is typically below 4 for uncolored natural pellets; values above 6 may indicate thermal history or antioxidant depletion.

    Thermal Stability, Moisture Uptake, and Injection-Molding Envelope

    The processing window for this nucleated homopolymer is controlled by thermo-oxidative chain scission rather than moisture sensitivity. Polypropylene does not hydrolyze at melt-processing temperatures; moisture uptake under ISO 62:2008 after 24 h water immersion is generally below 0.05 % by mass. Desiccant drying is therefore not mandatory when the resin has been stored in sealed, climate-controlled warehouses. When pellet surface condensation is present or when ambient relative humidity exceeds 60 % at the time of transfer, a 2 h pre-drying step at 80 °C using a desiccant dryer with a dew point of −20 °C or lower is recommended. Failure to remove surface moisture can produce splay, silver streaks, and shot-weight variation on open-hopper reciprocating-screw machines.

    On a general-purpose reciprocating-screw injection-molding machine with a 20:1 to 22:1 L/D screw and compression ratio of 2.2:1 to 2.8:1, the recommended melt temperature is 210 °C to 240 °C. The barrel should not be operated above 250 °C for extended periods. Local residence above 280 °C for more than 5 min can initiate chain scission, lower the melt viscosity, generate yellowing, and release low-molecular-weight volatiles. The mold temperature can be maintained between 20 °C and 45 °C for rigid packaging applications. Increasing the mold temperature to 60 °C improves weld-line strength and surface gloss but extends cooling time and can increase cycle time by 10–20 %, depending on part thickness.

    Rheologically, an 11 g/10 min PP homopolymer at 230 °C typically shows a shear viscosity in the range of 90–150 Pa·s at 100 s⁻¹ and 20–35 Pa·s at 1,000 s⁻¹; these are class-typical estimates, not lot-specific capillary rheometry data. The fast crystallization induced by the nucleating agent reduces post-ejection growth but also increases the risk of surface flow marks if injection speed is too low. Short-shot studies should be documented from 65 % to 95 % of fill mass in 5 % increments to identify the gate-seal and flash boundaries before production. Holding pressure is normally set between 30 MPa and 60 MPa hydraulic, with a screw cushion of 3 mm to 5 mm and cushion variation below 1 mm across consecutive cycles. Back pressure from 0.3 MPa to 0.7 MPa and screw surface speeds of 0.15 m/s to 0.25 m/s are typical for this melt-flow class. Flow-length-to-wall-thickness ratios up to 150:1 are generally achievable at 230 °C with injection pressures up to 80 MPa; above this ratio, short-shot risk increases unless the gate is enlarged or the wall thickness is increased.

    Gate and runner design should follow a restricted-gate strategy for fast freezing and rapid cycle time. Edge gates with a land length of 0.5 mm to 1.0 mm and a gate thickness between 50 % and 75 % of the nominal wall thickness are typical for rigid packaging. For multi-cavity tools, a geometrically balanced runner with a full-round runner diameter of 4 mm to 6 mm reduces pressure loss and helps balance filling. Hot-runner systems should use externally heated manifolds with thermal profiling to avoid dead zones where material can stagnate above 250 °C. Sequential valve gating is generally unnecessary for this melt-flow class but may be required for large flat panels to avoid knit-line distortion.

    Mold shrinkage is normally 0.8 % to 1.5 % parallel to flow and 0.9 % to 1.6 % transverse to flow when measured on 60 mm × 60 mm × 2 mm plaques in accordance with ISO 294-4:2018. The coefficient of linear thermal expansion for unfilled PP homopolymer is generally 80 × 10⁻⁶ K⁻¹ to 120 × 10⁻⁶ K⁻¹ between 23 °C and 80 °C under ISO 11359-2:2021. Large-area parts should be evaluated with thermal cycling or annealing to prevent post-molding dimensional drift.

    When NPP 11-5026 Replaces a Random Copolymer in Ambient-Temperature Closure Applications

    Replacement of a propylene-ethylene random copolymer by NPP 11-5026 is technically valid only when the service life is restricted to ambient or moderately elevated temperatures and when optical clarity is not a controlling requirement. The homopolymer’s higher stiffness and heat resistance are direct consequences of its molecular structure; the absence of ethylene comonomer raises the heat deflection temperature under 0.45 MPa by approximately 5 °C to 10 °C compared to a typical random copolymer of the same melt-flow class. However, the notched Charpy impact at 0 °C is generally lower by 50 % or more relative to the random copolymer; published data for this specific configuration is limited, and comparative evaluations under ISO 179-1/1eA and ISO 8256:2004 must be performed before conversion.

    Against an in-reactor impact copolymer, the homopolymer grade displays higher flexural modulus and slightly lower density, but a sharp decline in energy absorption at sub-ambient temperatures. The notched Charpy impact of the homopolymer at 23 °C is commonly 2.0–4.0 kJ/m², whereas an impact copolymer of similar melt-flow rate can exceed 15 kJ/m² and retain ductility at −20 °C. Sharp corners, gate vestiges, and weld lines become critical defects under impact loading; molding simulations and physical testing at the lowest expected service temperature are required.

    Table 2 summarizes class-typical differences among the three resin families at the same nominal melt-flow level. The ranges are not product-specific guarantees for any LyondellBasell grade.

    Resin classFlexural modulus rangeNotched Charpy impact at 23 °CLow-temperature impactClarity
    Nucleated PP-H MFR 111,100–1,400 MPa2.0–4.0 kJ/m²LimitedTranslucent
    Propylene-ethylene random copolymer MFR 11800–1,100 MPa5.0–12.0 kJ/m²ModerateHigh
    In-reactor impact copolymer MFR 11700–1,000 MPa15.0–30.0 kJ/m²HighOpaque

    The absence of rubber and ethylene comonomer in a homopolymer also reduces dry-bag opacity and increases surface hardness. Rockwell hardness of nucleated PP-H is generally R 95–105 under ISO 2039-2, while impact copolymers of comparable flow may fall between R 70 and R 90. This difference is relevant to scratch and mar resistance in consumer closures. Compared with a controlled-rheology high-flow PP homopolymer with melt mass-flow rate at or above 35 g/10 min, NPP 11-5026 requires higher injection pressure or larger gates for thin-wall fill; the lower melt-flow grade provides higher melt strength and better resistance to gate blush and free-jetting in thicker sections.

    For food-contact applications, converter qualification must confirm compliance with FDA 21 CFR 177.1520(c) for olefin polymers and with EU Regulation (EU) No 10/2011 Annex I where applicable. A product-specific migration test under the designated simulant conditions is required; food-contact status is not inferred solely from the base resin type. Heavy-metal and substance-of-very-high-concern screening can be conducted against REACH Regulation (EC) No 1907/2006 and Directive 2011/65/EU (RoHS Recast). Unfilled PP homopolymer is typically classified UL 94 HB at 1.5 mm, but the product-specific UL Yellow Card must be consulted before the final part is certified.

    Operational boundaries include long-term exposure to air at temperatures above 120 °C, which can deplete the antioxidant package and cause embrittlement. Long-term heat aging must be assessed under ISO 4577:2019 or UL 746B, not inferred from short-term HDT or Vicat values. Continuous contact with strong oxidizing acids, halogens, chlorinated solvents, and hot aromatic hydrocarbons can soften, swell, or stress-crack the surface; comparative immersion testing under ISO 175:2010 or ASTM D543-21 is necessary for chemical-service qualification. Transition-metal ions, particularly copper and copper alloys used in inserts, can accelerate thermo-oxidative degradation. Regrind levels above 30 % by weight are not recommended for critical dimensions or color-sensitive parts unless the melt-flow shift and yellowness index are revalidated after multiple heat histories.