| HS Code | 977382 |
| Polymer Type | Polypropylene Impact Copolymer |
| Nucleation | Nucleated |
| Antistatic | Yes |
| Density | 0.905 g/cm³ |
| Melt Flow Rate | 11 g/10 min (230°C/2.16 kg) |
| Tensile Strength At Yield | 25 MPa |
| Tensile Elongation At Yield | 8% |
| Flexural Modulus | 1200 MPa |
| Notched Izod Impact Strength At 23 C | 6 kJ/m² |
| Notched Izod Impact Strength At 20 C | 3 kJ/m² |
| Heat Deflection Temperature At 0 45 Mpa | 95°C |
| Vicat Softening Temperature | 150°C |
| Rockwell Hardness | 85 R scale |
| Ul 94 Flammability | HB |
| Processing Method | Injection Molding |
As an accredited LyondellBasell NPP 11-3225 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell NPP 11-3225 is supplied in 25 kg polyethylene bags, typically palletized for industrial transport and storage. |
| Container Loading (20′ FCL) | Container loading (20′ FCL): LyondellBasell NPP 11-3225 chemical cargo securely stowed, sealed, and prepared for ocean freight transport. |
| Shipping | LyondellBasell NPP 11-3225 is a non-hazardous polypropylene impact copolymer resin supplied as pellets. Ship in sealed 25 kg polyethylene bags or bulk containers on pallets. Not regulated by DOT, IMDG, IATA, or ADR. Store cool, dry, away from heat and sunlight. Use standard PPE and avoid dust. |
| Storage | Store LyondellBasell NPP 11-3225 in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep original containers tightly closed and off the floor. Protect from moisture, dust, and contamination. Avoid contact with strong oxidizing agents. Store at ambient temperature, preferably below 50°C, and follow local regulations and SDS recommendations. |
| Shelf Life | Shelf life is 12 months from date of manufacture when stored in original, unopened containers under cool, dry, well-ventilated conditions. |
On high-cavitation moulds producing thin-wall dairy cups and freezer trays, LyondellBasell NPP 11-3225 is processed at melt temperatures of 230 °C to 250 °C, mould coolant temperatures of 10 °C to 35 °C, and injection pressures of 80 MPa to 120 MPa. The resin is not pre-dried unless bulk storage humidity exceeds 60 % RH, in which case 2 h at 80 °C with a desiccant dryer at -20 °C dew point is applied before processing. Before continuous production campaigns, incoming lot melt-flow-rate is verified under ISO 1133-1:2022 at 230 °C and 2.16 kg; converters maintain internal acceptance limits against the moulding window rather than relying on absolute nominal values. Thin-wall containers with nominal wall sections below 0.6 mm are moulded using valve-gated hot runners at manifold setpoints of 235 °C to 245 °C, because premature freeze-off at lower manifold temperatures increases short-shot rates on 32-cavity and 64-cavity tools. Colour masterbatch with a polypropylene carrier and 60 % titanium dioxide or carbon black loading is metered at 2 wt% to 4 wt% by gravimetric dosing units; when 4 wt% titanium dioxide masterbatch is used for high-opacity dairy applications, screw back pressure is limited to 0.5 MPa to avoid pigment agglomerates. In-house regrind is limited to 20 wt% of total feed and is revalidated for food-contact migration under EN 1186-1:2002; converters operating under Commission Regulation (EU) No 10/2011 maintain overall migration below 10 mg/dm², while United States distribution is covered by FDA 21 CFR 177.1520(c) for olefin polymers. Terminal product types produced under this regime include 450 mL dairy cups, 750 mL deli containers, and 500 mL freezer-safe trays.
Beverage closure manufacture on 96-cavity hot-runner tools uses melt temperatures of 230 °C to 245 °C with mould temperatures of 15 °C to 25 °C and cycle times of 6 s to 9 s. The standard formulation uses erucamide slip masterbatch with 5 % active content in a polypropylene carrier at 1.0 wt% to 2.0 wt%, resulting in 0.05 wt% to 0.10 wt% active erucamide in the moulded closure. At active erucamide below 0.05 wt%, removal torque on 29/25 mm PCO 1881 closures measured under ASTM D2063 after 72 h of cap-bottle aging on filled lines can exceed 1.5 N·m, while above 0.15 wt% the additive migrates excessively to the surface, causing vent-pin plate-out and reducing gate-vestige cleanliness on high-cavitation tools. Coefficient of friction is monitored on compression-moulded plaques under ISO 8295:1995; the target kinetic coefficient is below 0.25 after 72 h to ensure consistent cap application and removal without threatening seal integrity. Hot-runner needle-shut-off valves and cylindrical core pins with air-assisted ejection are used to prevent ovality; cavity-pressure sensors are maintained at 25 MPa to 35 MPa peak cavity pressure to control tamper-evident band elongation. Compliance for food-contact closures is managed under Commission Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520(c); organoleptic conformity is evaluated by the converter because Article 3 of Regulation 10/2011 requires no unacceptable sensory change without prescribing a single test method. Terminal products include 29/25 mm PCO 1881 carbonated soft drink closures, 30/25 mm water closures, and tamper-evident dairy caps.
When thick-section housewares such as storage bins and kitchen tools are moulded, NPP 11-3225 is run at melt temperatures of 220 °C to 240 °C, mould temperatures of 20 °C to 40 °C, and pack/hold pressures of 60 % to 80 % of injection pressure to compensate for sink marks in wall sections of 2.0 mm to 4.0 mm. Colour masterbatch is added at 2 wt% to 4 wt%; for outdoor storage articles, a UV stabilizer masterbatch containing hindered amine light stabilizer at 0.5 wt% to 1.0 wt% total article weight is metered into the throat to reduce surface chalking after 1,500 h of accelerated weathering under ISO 4892-2:2013. Mould fill uses screw stroke volumetric control with cushion maintained at 3 mm to 5 mm to prevent gas traps at rib intersections, and ejection is delayed until part surface temperature falls below 70 °C to avoid post-mould warpage. Compliance for kitchen tools and food-contact storage is maintained under Commission Regulation (EU) No 10/2011, with documentation for specific migration of primary aromatic amines where coloured masterbatches are used; articles destined for children’s use are evaluated under EN 71-3:2019+A1:2021 for migration of elements. Terminal part types include drawer organizers, stackable storage boxes, kitchen utensils, and reusable household hangers.
Cleanroom injection moulding of diagnostic packaging and laboratory consumables uses NPP 11-3225 without recycled content in ISO Class 8 or better environments; melt temperature is held at 220 °C to 240 °C, and mould temperature is maintained at 20 °C to 30 °C for dimensional consistency of narrow reservoir geometries. Additive loading is limited to antistatic masterbatch at 0.1 wt% to 0.3 wt%; no external mould release, stearate-based process aids, or pigment systems containing heavy metals are introduced unless the specific grade conforms to USP <661> extraction limits for physicochemical testing and ISO 10993-5:2009 cytotoxicity requirements. For sterile diagnostic consumables, gamma irradiation at doses above 25 kGy may embrittle polypropylene; converters running 25 kGy to 40 kGy cycles validate post-irradiation notched Izod impact retention under ISO 180/A and tensile elongation at break under ISO 527-2:2012 before release. Terminal products include 0.2 mL to 10 mL specimen collection cups, pipette tip racks, microcentrifuge tube arrays, and diagnostic reagent reservoirs.
| Downstream sector | Regulatory instrument | Test method designation | Limit or reference |
|---|---|---|---|
| Thin-wall food packaging | Commission Regulation (EU) No 10/2011 | EN 1186-1:2002 | Overall migration 10 mg/dm² |
| Beverage closures | FDA 21 CFR 177.1520(c) | ASTM D2063 | Torque retention per converter specification |
| Housewares and toys | EN 71-3:2019+A1:2021 | EN 71-3 clause 4 | Element migration limits for category III materials |
| Laboratory consumables | USP <661> | ISO 10993-5:2009 | Cytotoxicity not greater than grade 2 |
| Small appliances | RoHS Directive 2011/65/EU | IEC 62321-5:2013 | Lead 1000 mg/kg; cadmium 100 mg/kg |
| Compounding base resin | Regulation (EC) No 1907/2006 | ISO 178:2019 | No SVHC above 0.1 wt% |
For small-appliance structural brackets and housings where load-bearing requirements are limited to short-term static loads and assembly stresses, NPP 11-3225 is processed with talc masterbatch at 10 wt% to 30 wt% to raise flexural modulus measured under ISO 178:2019. The replacement of an impact copolymer with an unfilled or lightly filled polypropylene requires attention to notch sensitivity: radii below 0.5 mm are not recommended at ribs and screw bosses because stress concentration under assembly torque increases cracking risk; screw boss pull-out tests are run according to ISO 527-2:2012 on moulded bosses rather than standard tensile bars. Moulding uses melt temperatures of 220 °C to 250 °C, mould temperatures of 30 °C to 50 °C, and clamp force calculated from projected area at 3.0 kN/cm² to 5.0 kN/cm²; weld-line tensile strength drops by 25 % to 40 % when filled melts converge at opposing flow fronts, so gate placement is simulated with sequential valve gating to shift weld lines into low-stress zones. Compliance is maintained under RoHS Directive 2011/65/EU with lead below 1000 mg/kg and cadmium below 100 mg/kg, and under IEC 60335-1:2020 for household appliance safety; flammability class is verified under UL 94 horizontal burn classification. Terminal parts include washing machine detergent drawer frames, refrigerator shelf brackets, and vacuum cleaner motor housing supports.
Compounding trials on a co-rotating twin-screw extruder with L/D 40:1 and side feeder for fillers show that NPP 11-3225 can be used as a base resin for talc-filled compounds when the main screw speed is 300 rpm to 600 rpm and the barrel profile from feed throat to die is maintained at 180 °C to 230 °C. Talc with median particle size 2 µm to 5 µm is introduced through a side feeder at 20 wt% to 40 wt%, while antioxidant masterbatch is added at 0.2 wt% to 0.5 wt% to address thermo-oxidative degradation during subsequent conversion. Dispersion quality is assessed by pressure-rise through a 40/60/80 mesh screen pack; a pressure rise above 0.8 MPa per hour signals unacceptable agglomeration and requires screw reconfiguration. The resulting compounds are characterised under ISO 527-2:2012 for tensile modulus and ISO 178:2019 for flexural modulus; lot acceptance is typically managed with ISO 75-2:2013 heat deflection temperature measurements. REACH compliance under Regulation (EC) No 1907/2006 requires that no SVHC in the polymer, filler, or additive package exceeds 0.1 wt% at article level. Terminal products from this compounding route include mineral-filled polypropylene compounds for appliance back panels, automotive interior trim substrates, and building product profiles.
Competitive LyondellBasell NPP 11-3225 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell NPP 11-3225 is identified in supplier documentation as a natural polypropylene grade supplied in uncolored pellet form. The material is positioned for injection molding and extrusion operations where a controlled melt-state rheology and predictable shrinkage behavior are required. The designation NPP is commonly interpreted as natural polypropylene, indicating that the pellet does not carry a masterbatch colorant and can be self-colored or compounded on site. The numerical identifier is a supplier-specific grade code; it does not directly encode a physical property unless explicitly stated in the certificate of analysis. Publicly available full datasheets for this specific configuration are limited, and equipment qualification should therefore be based on the current LyondellBasell product data sheet and lot-specific release data.
For release testing and incoming inspection, the following methods and specimen configurations are used. Density is verified under ISO 1183-1, melt mass-flow rate under ISO 1133-1 at 230 °C with a 2.16 kg piston, tensile stress at yield under ISO 527-2 or ASTM D638-14, flexural modulus under ISO 178, and notched impact strength under ISO 180/A or ASTM D256-23. Specimen preparation should follow ISO 294-1 or the equivalent ASTM injection-molding procedure. The exact target values and tolerance bands are not published in a universally fixed standard; they are defined by the supplier specification and should be confirmed against the lot certificate before releasing the material to production.
| Parameter | Test Standard | Specimen or Condition | Verification Purpose |
|---|---|---|---|
| Density | ISO 1183-1 | Injection-molded plaque | Uniformity of uncolored PP base resin |
| Melt mass-flow rate | ISO 1133-1 | 230 °C, 2.16 kg | Rheological lot consistency |
| Tensile stress at yield | ISO 527-2 / ASTM D638-14 | Type 1A or Type I | Short-term load-bearing stiffness |
| Flexural modulus | ISO 178 | 80 × 10 × 4 mm | Bending resistance and dimensional predictability |
| Notched impact strength | ISO 180/A / ASTM D256-23 | 4 mm notched specimen | Comparison against impact copolymer grades |
Unfilled polypropylene is not generally hygroscopic, and absorbed water is not the primary source of processing defects. Surface condensation on cold pellets is a more common cause of splay, silver streaks, and intermittent bubble formation in molded parts. When pellets move from a cold silo into a warm production hall, the dew point at the pellet surface may be crossed. At relative humidity above 60 %, a desiccant dryer set to 80 °C for 2 h is used before melt processing. Conveyance air for high-speed thin-wall molding should be dried to a dew point of -20 °C or lower. Sustained storage above 40 °C can shift the melt mass-flow rate downward through oxidative chain scission or long-chain branching, and the resulting lot may show longer fill time at the same barrel setpoints.
In injection molding, a general-purpose polypropylene of this melt-flow class is processed with a barrel profile beginning near 210 °C in the feed zone and rising to 230–240 °C at the nozzle. Mold temperature is maintained between 20 °C and 40 °C. Back pressure is commonly set between 0.5 MPa and 1.5 MPa. A general-purpose polypropylene screw with 20:1 to 24:1 L/D ratio and compression ratio near 2.5:1 is adequate for melt preparation. No pre-drying is required if the pellet surface remains dry and the hopper throat is water-cooled to prevent bridging. The hopper magnet and screen pack should be inspected for black specks that originate from extended purge hold times above 250 °C.
Polypropylene grade selection depends on the balance of stiffness, impact resistance, flow length, and optical clarity. A natural homopolymer such as NPP 11-3225 is expected to show higher tensile stress at yield and higher flexural modulus than a random copolymer of equivalent melt mass-flow rate, because the absence or near-absence of ethylene comonomer preserves chain packing density and crystallinity. It is also expected to show lower notched impact strength and lower elongation at break than an impact copolymer, because it lacks a discrete elastomeric phase. The practical tradeoff is higher stiffness and better demolding consistency, but reduced cold-temperature drop resistance. For rigid packaging, caps, closures, and housewares, this balance favors dimensional stability and predictable ejection. For automotive interior parts exposed to winter impact loading, an impact copolymer grade is preferred.
Rheology is the primary lot-release control parameter for this product type. A melt mass-flow rate near 11 g/10 min, when confirmed under ISO 1133-1, corresponds to a medium-flow polypropylene. At 230 °C and an apparent shear rate of 1,000 s⁻¹, viscosity is lower than that of a 4 g/10 min grade and higher than that of a 35 g/10 min grade. This positions the material for multi-cavity molds that require moderate injection pressure and short cycle times, but it does not eliminate flow hesitation at weld lines. Mold-filling simulations should use pressure-volume-temperature data generated on the specific lot rather than a generic homopolymer library. Shrinkage predictions should also use lot-specific data, because small changes in nucleating additives or residence time can shift the crystallization temperature and alter post-mold shrinkage.
Clamp force requirement is calculated from projected part area and effective cavity pressure. For unfilled polypropylene homopolymers, estimated cavity pressure during hold is typically 30–40 MPa for thick-wall parts and up to 60 MPa for thin-wall parts with high flow-length-to-wall-thickness ratio. A part with a total projected area of 200 cm² and an effective cavity pressure of 40 MPa requires approximately 80 metric tons of clamp force, if mold deflection is ignored. The machine hydraulic pressure profile should maintain injection velocity between 80 mm/s and 150 mm/s for wall thickness below 1.5 mm. An open nozzle or reverse-taper nozzle is preferred; shut-off nozzles may generate dead zones and degrade material during extended cycles. Melt cushion is maintained at 3–6 mm to compensate for check-valve leakage.
Weld-line strength in this type of material is lower than the bulk tensile strength. Gates should be positioned so that weld lines occur away from high-stress regions, and the mold should be vented at the end of fill to avoid gas entrapment. Mold surface temperature may be raised to 45 °C for thin-wall containers to improve weld-line healing, but cycle time will increase. The use of more than 20 % by weight regrind of the same natural grade is possible if the regrind is free of contamination and has not undergone repeated high-temperature extrusion. Separate storage of regrind and virgin pellets prevents stratification in the hopper and color variation in self-colored parts.
Compliance statements for food-contact, medical, or electrical applications are not generic across all supplies of a polymer grade. Each production lot must be evaluated against the applicable regulation and the final formula, including colorants, additives, and processing aids. The following matrix identifies the typical regulatory frameworks that should be checked for a natural polypropylene grade supplied into consumer and industrial markets.
| Regulation or Standard | Scope | Typical Verification |
|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymers for food contact | Monomer and extractables compliance in finished article |
| EU (EU) No 10/2011 | Plastic materials in food contact | Overall migration and specific migration limits |
| REACH | Chemical safety in the European Union | Substance registration and SVHC content below 0.1 % by weight |
| RoHS | Electrical and electronic equipment | Pb, Cd, Hg, Cr(VI), PBB, PBDE limits |
| ISO 1873-2 | Polypropylene designation system | Basis for grade classification and property designation |
For extrusion applications, the same natural polypropylene grade is processed with a melt temperature of 225–245 °C at the die, depending on line speed and back pressure. Screen packs with a 100 mesh or finer retention are used for sheet and film to remove gel contamination. Film and sheet output rates should be set to maintain melt pressure below the extruder manufacturer’s maximum screw design limit. Neck-in and draw ratio are adjusted to the lot-specific melt mass-flow rate, because lower melt viscosity increases drawability but may reduce bubble stability in cast film. An induction-heated die lip is preferred for thickness uniformity when running at line speeds above 30 m/min. For cast film, chill-roll temperature is held at 15–25 °C to control crystallization and surface gloss. For sheet, roll stack temperature is set between 30 °C and 50 °C to prevent sticking while retaining dimensional stability.