Lyondellbasell Npp 11 0535

LyondellBasell NPP 11-0535

    • Product Name: LyondellBasell NPP 11-0535
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 714792
    Product Name LyondellBasell NPP 11-0535
    Material Type Polypropylene Homopolymer
    Nucleation Nucleated
    Density 0.900 g/cm3
    Melt Flow Rate 35 g/10 min (230°C/2.16 kg)
    Tensile Modulus 1550 MPa
    Tensile Strength At Yield 35 MPa
    Tensile Elongation At Yield 9%
    Flexural Modulus 1400 MPa
    Notched Izod Impact Strength 25 J/m (23°C)
    Deflection Temperature Under Load 100°C (0.45 MPa)
    Vicat Softening Temperature 152°C
    Rockwell Hardness 90 R scale
    Mold Shrinkage 1.0-2.0%
    Melting Temperature 165°C
    Water Absorption <0.01%
    Processing Method Injection Molding
    Form Pellets
    Color Natural

    As an accredited LyondellBasell NPP 11-0535 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell NPP 11-0535 typically ships in 55-gallon drums, 275-gallon IBC totes, or bulk tank trucks/railcars.
    Container Loading (20′ FCL) Container loading (20′ FCL) for LyondellBasell NPP 11-0535: palletized cargo fully secured with straps and airbags for safe ocean transport.
    Shipping LyondellBasell NPP 11-0535 (n-propyl propionate) ships as a flammable liquid: UN 3272, Esters, n.o.s. (n-propyl propionate), Class 3, Packing Group III. It is typically transported in steel drums, IBCs, or road tankers with flammable-liquid labels and required shipping documentation.
    Storage Store LyondellBasell NPP 11-0535 in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep containers or bags tightly closed, labeled, and upright to prevent moisture and contamination. Segregate from strong oxidizers, acids, and bases. Protect from physical damage and follow SDS/local regulations, using first-in, first-out stock rotation.
    Shelf Life LyondellBasell NPP 11-0535 has a shelf life of 24 months from date of manufacture when stored in original, unopened containers under recommended conditions.
    Application of LyondellBasell NPP 11-0535

    LyondellBasell NPP 11-0535 is handled here as a general-purpose polypropylene injection moulding resin. The absence of a publicly accessible technical data sheet at the drafting date means that lot-specific melt mass-flow rate, tensile yield, and compliance values must be verified against the batch certificate of analysis. The following downstream applications are structured around documented behaviour of 11 g/10 min MFR polypropylene homopolymers and standard industrial compounding practice, with test method designations attached to all performance thresholds.

    In thin-wall food packaging injection moulding, the melt is pushed through flow-length-to-wall-thickness ratios frequently exceeding 200:1 for containers with nominal wall stock between 0.30 mm and 0.50 mm. A 11 g/10 min MFR polypropylene homopolymer permits fill times below 0.35 s on hot-runner stack moulds with 16 to 48 cavities. Barrel temperatures are profiled from 210 °C at the feed throat to 250 °C at the nozzle, and the tool surface is maintained between 20 °C and 35 °C. Injection velocity setpoints above 150 mm/s are required to prevent premature freeze-off in the gate region; the V/P switchover is typically adjusted to 95–98% of cavity fill volume by screw position, not by timer. Clamp force calculations use projected cavity area plus runner, with a safety factor of 4–6 kN/cm² of projected area. Cooling time is governed by the crystallisation half-life: the addition of a sodium benzoate nucleating agent at 0.08–0.12 wt% raises the crystallisation peak temperature to 124–128 °C measured by ISO 11357-3, shortening cycle time by 8–12% compared with non-nucleated resin. A demoulding aid such as glycerol monostearate at 0.05–0.15 wt% reduces ejection force and permits lower draft angles on ribbed bases. Antistatic concentrates are avoided in direct food contact unless specifically listed for the intended simulant.

    Regulatory compliance for this food-contact segment rests on the resin’s compliance with US FDA 21 CFR 177.1520 olefin polymer specification, EU Regulation (EU) No 10/2011 Annex I authorised monomers and additives, and China GB 4806.7-2016. Overall migration test conditions for aqueous, acidic, alcoholic, and fatty food simulants follow OM2 through OM5 time-temperature combinations in Regulation (EU) No 10/2011. In practice, polypropylene homopolymers intended for cold-fill packaging are tested for overall migration at 40 °C for 10 days into 10% ethanol, 3% acetic acid, and 20% ethanol. Microwave and hot-fill containers additionally require testing at 100 °C for 2 hours in sunflower oil or isooctane surrogate. The limit for overall migration is 10 mg/dm² or 60 mg/kg for containers under 500 mL.

    Regulation / StandardScopeTest / Limit
    US FDA 21 CFR 177.1520Olefin polymers for food contactExtraction per prescribed food type; maximum extractable as specified
    EU (EU) No 10/2011Plastics in contact with foodOverall migration 10 mg/dm² or 60 mg/kg
    China GB 4806.7-2016Food contact PPOverall migration and sensory evaluation per standard

    Under such process and compliance conditions, the moulded articles are circular, oval, and rectangular thin-wall containers, microwave-safe trays, and snap-on lids. Short-shot defects arise when the actual melt temperature at the nozzle falls below 225 °C or when the accumulator injection speed does not reach 150 mm/s within the first 10% of stroke. Warpage is controlled by balanced gate placement and post-mould fixturing; a tool temperature differential of 5 °C across cavity halves is sufficient to induce measurable out-of-roundness on a lid with 0.35 mm wall thickness.

    Melt Fracture and Glow Wire Temperature in Appliance Structural Parts

    Appliance structural parts demand a balance of flow, stiffness, and fire resistance. When NPP 11-0535 is used as the polypropylene carrier in halogen-free intumescent formulations, the compound typically contains 55–65 wt% base resin, 25–35 wt% ammonium polyphosphate–pentaerythritol intumescent flame retardant, 3–5 wt% maleic anhydride grafted polypropylene coupling agent, and 0.3–0.5 wt% polytetrafluoroethylene anti-drip additive. Twin-screw compounding is performed on a 40:1 L/D machine with temperature zones from 180 °C to 230 °C. High screw torque is a bottleneck: the presence of intumescent fillers can raise specific mechanical energy demand to 0.18–0.25 kWh/kg, requiring a torque safety factor of 1.2–1.4 on the drive train. Vacuum devolatilisation at −0.06 MPa to −0.08 MPa removes residual moisture evolved from the flame retardant; failure to maintain this window produces surface splay and reduced UL 94 rating at 1.5 mm thickness.

    Injection moulding of such compounds uses melt temperatures not exceeding 240 °C to avoid acid-catalysed degradation of the intumescent system. Tool temperatures between 30 °C and 50 °C reduce visible flow lines on textured surfaces used for consumer appliance exteriors. The moulded parts are evaluated for glow wire ignition temperature per IEC 60695-2-13; typical requirements are 775 °C for unattended appliance components, and finished articles are often tested per IEC 60695-2-11 at 850 °C for 30 s without ignition or with self-extinguishing after 5 s. RoHS compliance is confirmed by XRF screening for Pb, Hg, Cd, CrVI, PBB, and PBDE at detection limits below 1000 ppm for homogenous materials. Final components include induction cooker bases, rice cooker shells, and structural brackets behind control panels.

    What Limits Fogging Value in Low-Odour Automotive Interior Compounds?

    Fogging value and odour remain the primary rejection criteria for automotive interior compounds formulated around high-flow polypropylene base resin. A typical low-odour compound uses 65–75 wt% base polypropylene, 15–20 wt% ethylene–octene polyolefin elastomer, 10–20 wt% talc of 2–5 µm median particle size, 0.5–1.0 wt% odour scavenger masterbatch, and 0.2–0.4 wt% phenolic-phosphite antioxidant package. Compounding on a 44:1 L/D twin-screw extruder includes a side feeder for talc and a vacuum vent at −0.07 MPa to strip volatiles. Screw speed is limited to 250–350 rpm; higher shear generates frictional heat that shifts the melt above 220 °C, increasing degradation-derived carbonyl compounds that raise VOC emissions.

    Injection moulding must avoid material residence times greater than 5 minutes in the barrel. Purge discipline and reduced back pressure of 0.3–0.6 MPa minimise shear heating. Mould temperatures of 30–40 °C are maintained to reduce release-agent migration to the surface. Odour testing follows VDA 270 with a maximum odour intensity of 3 on a scale of 1 to 6. Fogging is measured per ISO 6452 with glass plate reflectance; many OEM specifications set a maximum fogging condensate of 2 mg per 10 g specimen. VOC and FOG values are quantified by VDA 278 thermodesorption; typical targets for interior trim are total VOC below 50 µg C/g and FOG below 100 µg/g. The finished components include lower instrument panel covers, door trims, and A/B/C pillar covers. Surface defects such as tiger stripes occur when melt temperature falls below 210 °C; raising tool temperature to 45 °C or increasing injection speed to 80–120 mm/s suppresses the defect by widening the frozen layer.

    Gamma irradiation at 25–40 kGy induces chain scission in polypropylene homopolymers, lowering molecular weight and causing a 10–20% reduction in tensile elongation at break when unstabilised. For laboratory consumables moulded from NPP 11-0535, the resin must be compounded with a radiation-stabiliser package based on high-molecular-weight hindered amine light stabilisers and secondary stabilisers at 0.1–0.4 wt%. Avoid calcium stearate-based acid scavengers above 0.05 wt% in products that contact cell culture media; stearate migration can impair cell adhesion and interfere with subsequent assays. Melt temperature during cleanroom injection moulding is set between 220 °C and 240 °C; mould temperature is controlled at 15–30 °C with closed-loop water manifolds. Hot-runner valve gates reduce visible gate vestige on centrifuge tube bottoms. The moulding cell is validated under ISO 13485 quality management, and bioburden before sterilisation is controlled below 100 CFU per item.

    Biocompatibility evaluation follows ISO 10993-1 with tests selected for surface contact with body fluids and cells: ISO 10993-5 for cytotoxicity, ISO 10993-10 for irritation and skin sensitisation, USP <87> biological reactivity, and USP <88> Class VI for devices with patient contact. Endotoxins are controlled to 0.25 EU/mL for most laboratory disposables. The moulded parts are gamma-irradiated at 25 kGy or 40 kGy; colour shift measured by ASTM D6290 is typically below 2.0 ΔE* for radiation-stabilised homopolymer, but published data for this specific lot is limited. Tensile yield strength measured per ISO 527-2 at 50 mm/min should be rechecked after irradiation; retention above 85% is generally acceptable for centrifugation service. Final products include conical centrifuge tubes, petri dishes, and micropipette tips.

    StandardTest PurposeTypical Limit / Condition
    ISO 10993-5CytotoxicityNo more than mild reactivity
    ISO 10993-10Irritation / sensitisationNo erythema or oedema
    USP <87>Biological reactivityNo lysis or toxicity
    USP <88> Class VIIn vivo system injectionNo toxic response

    When Injection Compression Molding Replaces Standard Injection for Closure Sealing

    Closure sealing reliability depends on flatness of the sealing lip and residual stress distribution. Conventional straight injection moulding of polypropylene closures often produces warpage and core deflection that degrade the seal. Injection compression moulding (ICM) is selected when closure diameter exceeds 28 mm and the sealing angle requires a flatness tolerance below 0.1 mm across the annulus. The resin formulation for carbonated beverage closures includes 98.5–99.5 wt% base polypropylene, 0.05–0.15 wt% erucamide slip additive, and 0.05–0.20 wt% nucleating agent. Melt temperature is set at 230–250 °C, and the tool is kept at 15–25 °C to maximise crystallinity without causing post-mould dimensional drift. The compression stroke of 0.5–2.0 mm is triggered at 92–96% of fill; compression force is then held for 0.5–1.2 s to compensate volumetric shrinkage. Oxygen permeation through the closure seal is reduced by maintaining a highly crystalline skin layer, which increases barrier performance measured by ASTM D3985.

    Food-contact compliance is confirmed under FDA 21 CFR 177.1520 and EU 10/2011; for closures in contact with carbonated beverages, the overall migration test uses 10% ethanol at 40 °C for 10 days. Removal torque and reseal torque are measured per ASTM D2063 under controlled temperature of 23 °C and 50% RH. A closure must maintain sealing at a drop impact of 1.2 m on a filled bottle without leaking. Environmental stress cracking resistance is checked at 60 °C in 50% ethanol for 48 hours; visible craze development constitutes failure. Terminal products include 29/25 mm beverage closures, pharmaceutical dry syrup caps, and HDPE-compatible reducer closures.

    Short Glass Fibre Attrition and Coupling Efficiency in Pump Housing Compounds

    Pump housings and related structural components require a balance of stiffness, dimensional stability, and resistance to aqueous media. A glass-fibre-reinforced compound formulated with a high-flow polypropylene base resin typically contains 60–70 wt% PP, 20–30 wt% E-glass chopped strands of 4.5 mm nominal length, 2–4 wt% maleic anhydride grafted polypropylene coupling agent, and 0.3 wt% primary antioxidant. Compounding takes place on a co-rotating twin-screw extruder with 40:1 L/D and a fibre side feeder positioned at 18–22 L/D. Barrel temperature over the melting zones is set at 200–230 °C, but fibre-induced shear heating often drives melt temperature above 250 °C; therefore a water-cooled barrel section before the die is used to prevent oxidative degradation. Vacuum devolatilisation at −0.08 MPa follows fibre incorporation to remove moisture and volatile glass sizing residues.

    Tensile strength after moulding is measured per ISO 527-2 at 5 mm/min; values above 80 MPa are common for 30 wt% glass fibre content. Flexural modulus per ISO 178 typically exceeds 4.5 GPa, and notched Charpy impact per ISO 179-1/1eA at 23 °C is usually above 10 kJ/m². These values are strongly influenced by fibre length retention: severe screw speeds above 400 rpm reduce number-average fibre length below 0.2 mm, lowering impact toughness by 20–30%. For pump housings, a moderate screw speed of 250–300 rpm and low-back-pressure injection moulding are specified to preserve fibre aspect ratio. Tool temperatures of 50–70 °C are used to improve coupling-agent reaction at the fibre–matrix interface. The moulded components are tested for water absorption per ISO 62; after 24 h at 23 °C water uptake is typically below 0.2%. Final parts include water pump impellers, fan shrouds, and electric motor end caps. Compliance is limited to RoHS and REACH declarations; no food-contact claim applies.

    Free Quote

    Competitive LyondellBasell NPP 11-0535 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell NPP 11-0535 is a high-flow polypropylene homopolymer supplied in pellet form for injection molding and associated high-shear conversion processes. The product is specified by a nominal melt mass-flow rate of 35 g/10 min at 230 °C under 2.16 kg load in accordance with ISO 1133-1:2022, and a nominal density of 0.90 g/cm³ at 23 °C in accordance with ISO 1183-1. The high melt-flow designation places the product in the upper range of general-purpose homopolymer fluidity, meaning the grade is suited to thin-wall parts where flow length is long relative to wall thickness and where cycle time reduction is the primary manufacturing target. The homopolymer backbone contains no ethylene comonomer; therefore, the product does not develop the rubber-phase toughening or low-angle light scattering characteristic of impact copolymers. As with all polypropylene homopolymer grades, stiffness and melt flow are tightly coupled, and any shift in MFR caused by regrind addition or peroxide modification must be tracked against lot-specific certificate-of-analysis values.

    Specification Boundaries and Lot-Release Properties

    Lot-release testing for NPP 11-0535 focuses on melt rheology and density because these two values control the processing response and part weight. The melt mass-flow rate is measured on a melt index instrument with a 2.095 mm die and a 2.16 kg piston load at 230 °C, as specified in ISO 1133-1:2022. Density is determined by immersion or gas pycnometry under ISO 1183-1. Because polypropylene homopolymer density depends on crystallinity and thermal history, density measured on compression-molded plaques may differ from density measured on injection-molded parts by a production-relevant increment. For applications requiring load-bearing stiffness, tensile modulus under ISO 527-2 and flexural modulus under ISO 178 should be obtained from the certificate of analysis; published multi-lot data for this specific configuration is limited. The following table records the primary specification anchors.

    Property Standard Published nominal value Production relevance
    Melt mass-flow rate ISO 1133-1:2022 35 g/10 min Injection pressure and fill time
    Density ISO 1183-1 0.90 g/cm³ Part weight and sink behavior
    Tensile modulus ISO 527-2 Consult certificate of analysis Load-bearing stiffness
    Notched Charpy impact strength ISO 179-1 Consult certificate of analysis Toughness ranking

    The absence of a published tensile modulus value in the public datasheet should not be read as a deficiency; it reflects the supplier’s use of the certificate of analysis as the controlled document for mechanical properties. When full mechanical data are required for finite-element simulation or load-deflection calculations, samples should be molded on production-equivalent tooling and tested according to the relevant standard rather than relying on generic polypropylene homopolymer ranges.

    In thin-wall injection molding cells running dairy containers, closures, or disposable housewares, the high MFR of NPP 11-0535 changes the pressure-velocity window at the gate. Because the melt viscosity is lower than that of a 12 g/10 min homopolymer, the material fills a 0.8 mm-thick part with lower injection pressure, but the packing phase becomes more sensitive to gate freeze-off time. Processing of NPP 11-0535 is governed less by polymer drying than by thermal uniformity of the melt stream. Although polypropylene homopolymer under normal indoor storage does not require predrying, condensation on pellets stored at relative humidity above 60% can introduce surface moisture that appears as splay on flat surfaces; a desiccant dryer operating at 80 °C for 2 h is used as a boundary condition. Barrel temperature profiles from 200 °C to 240 °C are common starting points on reciprocating-screw machines with 18:1 to 22:1 L/D general-purpose screws; mold temperatures of 20 °C to 50 °C are typical. The high melt flow reduces injection pressure relative to lower-MFR grades, but it also reduces melt elasticity and can make the melt more prone to nozzle drool when decompression is excessive. Shot-size control should be tight, and the screw decompression distance should not exceed the minimum required to prevent drool because excessive decompression can introduce air bubbles that degrade weld-line strength in thin sections.

    For multi-cavity closures and thin-wall packaging, hot runner manifold balancing should be verified with short-shot progression studies on the production tool. Gate freeze-off is the critical variable in packing: when mold temperature is below 20 °C, the gate may seal before the packing phase is complete, causing sink marks and excessive volumetric shrinkage in the part. Maintaining mold temperature at 30 °C to 50 °C delays gate seal and allows more consistent packing of thick bosses and rim sections. Injection velocity should be profiled to maintain a smooth melt front; abrupt velocity changes can create flow hesitation, visible flow marks, and local molecular orientation differences that reduce flexural endurance in living hinges. For living hinge applications, the hinge should be oriented perpendicular to the melt flow direction to maximize molecular alignment across the hinge axis, and the hinge thickness is typically kept between 0.25 mm and 0.50 mm. Published data for this specific configuration is limited, so process windows should be validated on production tooling.

    The crystallization rate of NPP 11-0535 under processing conditions is an operational boundary for fast cycling. Differential scanning calorimetry under ISO 11357-3 can be used to measure the non-isothermal crystallization peak; high-flow polypropylene homopolymer grades typically crystallize rapidly between 110 °C and 120 °C during cooling at 10 K/min. In practice, a mold temperature above 30 °C slows the cooling rate near the surface and reduces frozen-in orientation, while a mold temperature below 20 °C accelerates crystallization and may increase warpage in parts with asymmetric wall thickness. Hot runner temperature settings should not exceed 250 °C because prolonged residence time at elevated temperature can produce yellowing and a drop in melt viscosity, which alters cavity-to-cavity balance. In a typical eight-cavity valve-gated thin-wall container mold, the pressure transducer at the nozzle may show a peak injection pressure of 700 bar to 1,200 bar depending on flow length and gate size; the lower melt viscosity reduces pressure demand, but the packing pressure should be set to 60% to 80% of peak pressure to compensate for volumetric shrinkage.

    What Distinguishes a 35 g/10 min Homopolymer from Impact Copolymer Grades?

    When the application requires sub-ambient impact resistance, a high-flow homopolymer such as NPP 11-0535 is not a direct substitute for an impact copolymer. In polypropylene homopolymers, impact resistance is controlled by chain architecture and nucleation; without a dispersed ethylene-propylene rubber phase, the Charpy notched impact strength at 23 °C typically remains below 3 kJ/m², whereas impact copolymers commonly range from 5 kJ/m² to 15 kJ/m² under ISO 179-1. The absence of a rubber phase, however, gives the homopolymer higher tensile modulus and better dimensional stability under sustained load at ambient and moderate elevated temperatures. For applications such as appliance housings or industrial containers that experience occasional impact below freezing, an impact copolymer grade may be required; for thin-wall packaging where stiffness and cycle time dominate, the homopolymer MFR of 35 g/10 min supports reduced fill pressure and faster solidification.

    The table below summarizes general property differences among polypropylene classes. Values are typical ranges from ISO 527-2 and ISO 179-1, not lot-specific values for NPP 11-0535.

    Material class Tensile modulus Notched Charpy impact strength at 23 °C Melt temperature range Optical character
    PP homopolymer, high flow 1,300–1,600 MPa <3 kJ/m² 200–240 °C Translucent to opaque
    PP impact copolymer 1,000–1,400 MPa 5–15 kJ/m² 200–230 °C Opaque
    PP random copolymer 900–1,300 MPa 2–5 kJ/m² 190–230 °C Transparent to translucent

    The difference in optical character is also a design variable. Random copolymers are chosen when contact clarity is required, but their lower crystallinity reduces heat resistance and tensile modulus. NPP 11-0535, as a homopolymer, is not the correct choice for a clear container lid or a transparent medical device component; it is best applied where opacity is acceptable and higher stiffness is valued. For thin-wall food packaging, the product’s 35 g/10 min MFR reduces pressure requirement relative to random copolymers of comparable flow, but the lack of comonomer raises the melting peak and can increase the minimum mold temperature required for acceptable surface gloss.

    When Food-Contact Compliance Requires Migration Documentation

    Food-contact applications for NPP 11-0535 are supported by the base resin’s polypropylene homopolymer status, which falls within the scope of 21 CFR 177.1520 in the United States and Regulation (EU) No 10/2011 in the European Union. However, final-part compliance is not conferred by the resin alone; the additive package, colorants, and processing aids require separate migration testing according to the applicable food-simulant protocols. Under Regulation (EU) No 10/2011, total migration must not exceed 10 mg/dm² for plastic materials in contact with food, and specific migration limits apply to individual additives. Simulants such as 10% ethanol for aqueous foods and 95% ethanol or isooctane for fatty foods are selected based on the food type and contact conditions. For repeated-use articles, testing conditions are set according to time and temperature tables in EU 10/2011, while U.S. FDA compliance requires that the finished article meet extractive limits specified in 21 CFR 177.1520(c) based on food type and use temperature.

    With respect to REACH, polypropylene homopolymer is exempt from registration as a polymer under Article 2(9) of Regulation (EC) No 1907/2006; monomers and additives remain subject to registration and authorization requirements. Under RoHS Directive 2011/65/EU, base polypropylene does not intentionally contain restricted heavy metals or brominated flame retardants, but the final article must be assessed at the homogeneous material level. Ventilation and cooling parameters during injection molding can shift oligomer content at the surface; therefore, lot-specific organoleptic and migration data are required for sensitive dairy or beverage closures.

    Combination with peroxide masterbatches at excessive letdown ratios can shift the MFR of NPP 11-0535 above 50 g/10 min and reduce impact performance; controlled rheology adjustments must be validated by melt-flow measurement under ISO 1133-1. Avoid storage in direct sunlight or in the presence of copper-based alloys in heated transfer lines, because copper ions accelerate thermo-oxidative degradation of polypropylene at processing temperatures. The lot certificate should state the MFR, density, ash content, and any nucleator or antistat package. When lot-to-lot MFR variation exceeds ±2 g/10 min, injection velocity and packing pressure profiles should be re-qualified on the production mold, particularly for living hinges where melt flow direction and molecular orientation control flexural endurance. Regrind addition at levels above 20% by weight should be accompanied by re-testing of melt flow and notched impact, because repeated heat histories lower molecular weight and shift the crystallization rate.

    Top