Lyondellbasell Icorene 3545 Grn 6657 Polyethylene Linear Low Density

LyondellBasell Icorene 3545 GRN 6657 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 3545 GRN 6657 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 546218
    Density 0.935 g/cm³
    Melt Flow Rate 4.5 g/10 min
    Tensile Strength At Yield 12 MPa
    Tensile Strength At Break 17 MPa
    Elongation At Break 800%
    Flexural Modulus 400 MPa
    Vicat Softening Point 90 °C
    Melting Point 125 °C
    Hardness Shore D 50
    Color Green
    Specific Gravity 0.935
    Brittleness Temperature < -70 °C

    As an accredited LyondellBasell Icorene 3545 GRN 6657 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg polyethylene bags, palletized and stretch-wrapped; also available in 1,000 kg bulk bags.
    Container Loading (20′ FCL) 20′ FCL loading: LyondellBasell Icorene 3545 GRN 6657 Linear Low Density Polyethylene in 25 kg bags, palletized and securely stowed.
    Shipping LyondellBasell Icorene 3545 GRN 6657 Polyethylene, Linear Low Density is a non-hazardous polymer shipped as pellets in 25 kg bags, octabins, or bulk. It is not DOT/IMDG/IATA regulated. Transport in clean, dry, covered containers at ambient temperature, away from moisture, heat, contamination, and direct sunlight.
    Storage Store LyondellBasell Icorene 3545 GRN 6657 Polyethylene, Linear Low Density in a cool, dry, well-ventilated area in tightly closed original containers. Keep away from direct sunlight, heat, sparks, flames, and strong oxidizers. Protect from moisture, dust, and contamination. Palletize securely, avoid excessive stacking. Use first-in, first-out inventory. Follow manufacturer’s SDS and local regulations for safe handling and storage.
    Shelf Life Stable under normal storage conditions; typical shelf life is 12–24 months when kept dry, sealed, and away from direct sunlight.
    Application of LyondellBasell Icorene 3545 GRN 6657 Polyethylene, Linear Low Density

    Icorene 3545 GRN 6657 is supplied as a pre-coloured green LLDPE rotational moulding powder. The particle-size distribution is monitored under ASTM D1921-18; fractions larger than 500 µm are normally kept below 2 wt% because oversized particles create pinholes at thin boss roots. Melt-flow-rate testing at 190 °C with a 2.16 kg load under ISO 1133-1:2022 returns a nominal value near 4.5 g/10 min. Powder temperature control matters at the charging station: cold powder moved from storage below 10 °C into a moulding hall at 25 °C can form surface condensation, and the resulting steam pinholes appear as internal voids rather than visible surface defects. The powder is therefore preconditioned to 20–25 °C before charging when ambient relative humidity exceeds 60%. Rotational moulding does not provide the dispersive mixing of a twin-screw extruder; the green 6657 colour distribution depends on box tumbling, pneumatic transfer, and static charge control. Segregation can occur in silo-to-box transfer, so lot-to-lot screen analysis and colour consistency are recorded before the first production cycle. Up to 25 wt% clean same-grade roto-moulded regrind may be dry-blended in non-regulated applications; published impact-retention data for higher regrind loadings in this exact green formulation are limited. The grade is processed on carousel, shuttle, rock-and-roll, and open-flame machines, but the thermal endpoint is always measured through the mould wall rather than set by oven timer alone.

    Rotational Moulding of 800-L Agricultural Spray Tanks: Control of Peak Internal Air Temperature and Impact Properties

    Agricultural spray-tank tooling is usually fabricated from mild steel sheet with a 2B finish or from cast aluminium when localised ribbing and undercut drain bosses require tighter replication. The mould is charged to a mass calculated from mould surface area multiplied by target wall thickness and a nominal solid density of 0.934 g/cm³ at 23 °C; a 4.5 m² cavity with a 5.0 mm wall therefore requires approximately 21 kg of powder. Primary arm speed is set between 5 and 7 rpm; the secondary arm runs at 1.2–1.8 rpm to maintain a nominal 4:1 rotational ratio. The oven set point is established at 290 °C, but the controlling thermal variable is the peak internal air temperature measured by a through-mould thermocouple. For this grade, a PIAT of 190–200 °C is required to fully coalesce the powder around blind thread inserts and at the root of outlet stubs. When PIAT falls below 185 °C, the part develops unfused powder in the last-formed ribs; the failure mode appears as a sharp drop in low-temperature tensile impact under ISO 8256:2004. When PIAT exceeds 205 °C, oxidative degradation of the inner wall increases, and the green pigment exhibits a measurable hue shift under ISO 11664-4:2008. Cooling is staged: forced-air to 90 °C, then water mist to 65 °C, then free-air to demould at 50–55 °C. Excessively fast water-quench below 60 °C creates localised differential shrinkage at bung bosses; cooling-rate symmetry around openings is verified by post-mould diameter checks after 48 h at 23 °C and 50% RH under ISO 291:2008. Metal thread inserts are preheated to 60 °C and use 316 stainless steel or brass; the boss is thickened to at least 2.5 times the insert diameter to compensate for LLDPE creep. Weld rod for fitting attachment is extruded from the same powder on a single-screw extruder with a 24:1 L/D barrel profile. Spin welding is performed under an axial pressure of 0.2–0.5 MPa and a rotational speed of 500–1000 rpm until a uniform melt bead appears at the interface. Chemical-contact suitability is screened by ASTM D543-14 immersion in representative service fluids at 40 °C for 30 days; acceptance is a mass change below 0.5 wt% and no visible grazing at the weld. End products are 300–2000 L side-mount and tractor-mounted spray tanks, chemical dosing tool boxes, and secondary containment sumps.

    Single-piece mono-hull kayak shells are moulded from the same green powder in split aluminium cavities with a textured inner surface to ease air release and reduce visible knit lines. Charge mass for a 3.2 m hull is in the range 8–12 kg, yielding a wall thickness of 4–6 mm. The part is demoulded at 50 °C and conditioned at 23 °C and 50% RH for 48 h before post-machining. Holes for carry handles, rudder lines, and deck fittings are radiused to at least 1.0 mm; drilling with high-helix, sharp tools prevents a smeared low-impact edge. Low-temperature Charpy impact is evaluated at -20 °C under ISO 179-1:2010; rotomoulded LLDPE of this density class generally fails by ductile deformation rather than crack propagation. Two-part closed-cell polyurethane foam may be injected inside the hull for stiffness, but the foam exotherm must remain below 80 °C to avoid print-through on the outer skin. Water absorption of the polymer is below 0.01% under ISO 62:2008, so weight gain is driven by fittings and entrapped water, not polymer moisture. Long-term insert retention is governed by creep modulus measured under ISO 899-2:2003; the 1000 h creep modulus governs the backing-plate diameter and bolt torque. Moulded-in 316 stainless steel deck-line inserts require polyethylene backing plates because LLDPE creeps at room temperature under sustained tensile load. UV stabilisation is not automatically proven by the green 6657 pigment; accelerated weathering by ISO 4892-2:2013 is required for a commercial outdoor warranty. End products include recreational kayak hulls, sit-on-top paddlecraft shells, and shallow-water dinghy bodies.

    When Groundwater Buoyancy Exceeds the Dry Weight of a Roto-Moulded Chamber

    Underground irrigation valve enclosures and cable draw pits are moulded as rectangular or cylindrical single-piece shells with a wall thickness between 6 and 10 mm. The tool includes demountable cores for knock-out cable windows, and core surfaces are given draft angles of 1.5–3° because LLDPE shrinkage of around 2–3% can lock the part on long cores if the angle is lower. Soil-load resistance is assessed by parallel-plate crush testing under ASTM D2412-21; the part is loaded to 5% diametric deflection without visible cracking. The wall-thickness-to-mean-diameter ratio should remain above 0.02 for unsupported vertical walls; below this value, flexural stiffness drops enough that backfill compaction produces visible panel deflection. In high-groundwater installations, buoyancy rather than crush is the controlling failure mode. A dry-weight calculation shows that a 500 mm diameter chamber with 8 mm walls is buoyant, so the installation must include concrete anchor blocks, reinforced-concrete collars, or stainless-steel straps. If the chamber is placed under pedestrian traffic, load class A15 under EN 124-1:2015 is used; vehicular load classes are not normally assigned to the LLDPE body, and the lid is replaced by a ductile-iron or steel grating. Impact at -20 °C is checked by falling-weight impact under ASTM D5420-21; no visible fracture or leak path is accepted. Demoulding is performed after free-air cooling to 50–55 °C; forced demoulding below that temperature improves short-term cycle time but increases residual stress around the cable window. The material is insulating, with surface resistivity typically above 1014 ohm under IEC 60093:1980. End products include irrigation valve boxes, cable pull pits, meter chambers, and silt-pit liners.

    What Limits the Use of Green 6657 in Potable Water Contact Applications?

    Rainwater harvesting tanks and agricultural washdown reservoirs are rotationally moulded from the green 6657 grade, but direct potable water contact should not be assumed from the base polymer alone. Published migration data for this exact pre-coloured grade under Regulation (EU) 10/2011 or NSF/ANSI 61 are limited; the moulder must obtain written verification from LyondellBasell and the masterbatch supplier before specifying the grade for drinking-water contact. For non-potable rainwater storage, wall thicknesses of 5–8 mm are used, and watertightness is checked by filling to capacity at 23 °C for 24 h with no visible leakage. Welded outlet stubs and moulded-in O-ring grooves are tensile-tested on coupons cut from butt-welded joints under ISO 527-2:2012; failure outside the weld zone is preferred. The green pigment reduces light transmission through thin sections, but if a light transmission limit is required, moulded plaques should be tested under ASTM D1003-13. Oxygen permeability increases at elevated service temperature; the comparison between 23 °C and 40 °C under ASTM D3985-17 is used when water quality retention is specified over summer storage. For potable service, organoleptic testing under EN 1622:2006 or ISO 8795-1:2001 is required in addition to migration testing. If the exact green 6657 formulation lacks certification, the part should be downgraded to non-potable service or lined with a certified barrier. End products include garden rainwater tanks, temporary construction-site water storage, and non-potable washdown reservoirs.

    Compliance verification matrix for the primary application segments:

    Application segmentStandard designationTest conditionAcceptance control
    Agricultural spray tanksISO 8256:2004; ASTM D543-14Tensile impact at -20 °C; immersion at 40 °C for 30 daysNo brittle failure; mass change <0.5 wt%
    Marine hull shellsISO 179-1:2010; ISO 62:2008Charpy impact at -20 °C; water absorption at 23 °CPlastic deformation only; water absorption <0.01%
    Underground chambersASTM D2412-21; EN 124-1:2015Parallel-plate deflection; vertical load class5% deflection without crack; A15 non-traffic
    Rainwater tanksISO 527-2:2012; EN 1622:2006Weld tensile; organoleptic thresholdFailure outside weld zone; certification required for potable
    Outdoor furnitureISO 4892-2:2013; ASTM D5420-21Xenon 2000 h; falling weight at -20 °CΔE ≤5.0; no brittle failure
    Granular hoppersASTM D4060-19; IEC 60093:1980CS-17 wheels, 1000 g load; surface resistivityWeight loss 10–30 mg/1000 cycles; resistivity >1014 ohm

    Park benches, bollard sleeves, play equipment panels, and planter liners are rotationally moulded from the green 6657 grade where low-temperature ductility and falling-weight toughness are required. The primary outdoor risk is photo-oxidation, not tensile yield. The pigment package may reduce light attack relative to natural LLDPE, but it does not eliminate weathering. Accelerated ageing is run under ISO 4892-2:2013, Method A with filtered xenon arc, and colour change is measured by CIELAB under ISO 11664-4:2008; an agreed ΔE limit of 5.0 after 2000 h is common for municipal components. Gloss retention under ASTM D523-14 creates a test-method conflict: the textured roto-moulded surface diffuses light and gives lower numerical gloss than a smooth plaque, even when field appearance is acceptable. Gloss is therefore judged on flat witness plaques produced in the same cycle, not on the textured part. Additional UV stabiliser masterbatch may be dry-blended at 0.5–1.5 wt% when extended warranty is specified, but this changes shrinkage and colour, requiring re-qualification. Play equipment parts must meet structural and entrapment requirements of EN 1176-1:2017; the LLDPE component is only a shell, and the impact-attenuating surface is a separate material. Metal inserts are 316 stainless steel or hot-dip-galvanized steel isolated with a polypropylene washer to avoid galvanic corrosion. Falling-weight impact is run at -20 °C under ASTM D5420-21; no brittle fracture is accepted. Batch-to-batch pigment dispersion is checked by taking moulded samples from the first and last cavity of each multi-cavity run and comparing tensile impact values under ISO 8256:2004. End products include seating slats, climbing tunnel sections, litter bin liners, and protective bollard covers.

    Granular Fertilizer Hopper Bins, Abrasion Resistance, and Static Control

    Bulk storage hoppers and transfer bins for granular fertilizers, seed, and mineral additives are rotationally moulded as one-piece shells to eliminate seam leakage. A 1000 L hopper uses 6–8 mm wall thickness on vertical faces and 10–14 mm at the outlet transition where the cone is welded or bolted to a steel frame. Abrasion screening uses ASTM D4060-19 with CS-17 wheels and a 1000 g load; LLDPE of this density class generally falls in the 10–30 mg/1000 cycles weight-loss range, but the limiting failure mode in granular service is impact fatigue at the outlet weld. The outlet is therefore lined with a replaceable 316 stainless steel or polyurethane insert. The material is electrically insulative; surface resistivity is typically above 1014 ohm under IEC 60093:1980. For combustible organic dust applications, all conductive inserts, frame members, and flexible connections require grounding; antistatic additives are not normally specified for this grade. The hopper outlet is fastened to a butterfly valve or slide gate through a moulded flange; bolt-hole creep is controlled by embedding a steel torque ring on the back side of the flange. Metal inserts are preheated to 60–70 °C before charging; a cold insert creates a local quench zone that reduces wall thickness and produces a visible sink mark. Dimensional inspection is delayed for 48 h at 23 °C under ISO 291:2008 because LLDPE continues to shrink after demoulding. Published data for this exact green 6657 grade in highly acidic fertilizer solutions are limited; immersion testing under ASTM D543-14 in the actual formulation at 40 °C for 30 days is recommended before long-term contact with ammonium nitrate or urea solutions. End products include seed hoppers, fertilizer storage cones, mineral additive intermediate bulk containers, and feed transfer bins.

    Free Quote

    Competitive LyondellBasell Icorene 3545 GRN 6657 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 3545 GRN 6657 is a linear low-density polyethylene powder supplied as a green compound for rotational moulding. The numeric suffix 3545 maps to a nominal density of 0.935 g/cm³ and a nominal melt flow rate of 4.5 g/10 min at 190°C/2.16 kg; the suffix GRN 6657 designates a green colour compound. Because the product is a ground powder rather than pelletised feedstock, it can be charged directly into hollow tooling and sintered by conduction from the heated mould surface under biaxial rotation. Density is evaluated by ASTM D1505, melt flow rate by ASTM D1238, and tensile properties of sintered plaques by ASTM D638. The pigmented compound may differ from natural Icorene 3545 in infrared absorption and crystallisation behaviour; the current manufacturer datasheet is authoritative for lot-specific values.

    How Does a Rotomoulding-Grade LLDPE Differ from Injection-Moulding or Film-Grade Polyethylene?

    Rotational moulding resins are specified first by particle morphology. Injection-moulding and film grades are pelletised and processed under high shear; Icorene 3545 GRN 6657 is a dry-flowing powder with a controlled sieve profile that permits distribution into thin ribs, bosses, and kiss-off features. Rotomoulding powders in this class are commonly controlled to a maximum particle size near 35 mesh (500 µm) with a limited fraction below 200 mesh (75 µm); coarse particles can generate pinholes, while excessive fines reduce bulk density and create dust in pneumatic transfer lines. The melt flow rate of 4.5 g/10 min is lower than that of many injection-moulding LLDPE grades because the process requires sufficient melt strength to limit sag during slow cooling, yet still low enough to release bubbles and knit at the polymer-tool interface. With a density of 0.935 g/cm³, the product sits between LDPE and HDPE: it offers higher stiffness than LDPE while retaining higher environmental stress-crack resistance and ductility than many HDPE rotomoulding grades of similar melt flow.

    A further difference is the additive system. Film and injection grades may contain slip agents, antiblocking additives, or processing aids that are unnecessary or detrimental in rotational moulding. The GRN 6657 variant includes a green pigment and a weathering package intended for outdoor service; such compounds can shift the thermal-oxidative induction period, and oxidation induction time may be monitored by ASTM D3895 or ISO 11357-6.

    CharacteristicIcorene 3545 GRN 6657LDPE Rotomoulding GradeHDPE Rotomoulding GradeMetallocene LLDPE Rotomoulding Grade
    Nominal density (ASTM D1505)0.935 g/cm³0.920–0.930 g/cm³0.940–0.955 g/cm³0.934–0.940 g/cm³
    Melt flow rate (ASTM D1238, 190°C/2.16 kg)4.5 g/10 min4–6 g/10 min6–9 g/10 min3–6 g/10 min
    ESCR (ASTM D1693)High; published comparative values for the natural grade family commonly exceed 500 hModerateModerate to lowHigher relative to conventional LLDPE
    Low-temperature impact behaviourDuctile at −20°C in drop-weight testing when wall thickness is adequateDuctile but lower modulusLower baseline ductility unless comonomer-modifiedDuctile with high puncture toughness
    Weatherability packageGreen pigment plus UV stabilisation in GRN 6657Often limitedOften limitedOptional

    The table rows describe general polyethylene class behaviour. GRN 6657-specific values should be confirmed with the manufacturer because pigment loading and antioxidant content can change mechanical, thermal, and weathering responses.

    Sintered plaque testing for Icorene 3545 is typically conducted on rotationally moulded plaques rather than injection-moulded specimens. Publicly available representative property data for butene-LLDPE rotomoulding powders in the 0.935 g/cm³ density class place tensile yield stress in the 14–18 MPa band, elongation at break above 800%, and flexural modulus near 500 MPa under ASTM D638 and ASTM D790. Icorene 3545 GRN 6657 may fall within this envelope, but the green compound may show somewhat lower elongation and a slight increase in modulus if the pigment acts as a nucleating agent; acceptance testing should therefore be performed on the pigmented compound. Environmental stress-crack resistance is commonly evaluated by ASTM D1693 with 100% Igepal CO-630 at 50°C; published values for the natural grade family commonly exceed 500 h. Because pigment particles can act as stress risers, prototype parts in GRN 6657 should be tested in the final wall thickness and tooling location. Low-temperature impact is assessed by drop-weight procedures such as ASTM D5276 or ASTM D5628; published data for this specific green configuration at −20°C is limited, so qualification should include multiple specimens across the moulded part.

    On a carousel, shuttle, or rock-and-roll machine, the powder is loaded at ambient temperature into a mould that rotates biaxially through an oven zone set between 260°C and 300°C. Direct control uses the peak internal air temperature measured by infrared pyrometry or thermocouple; for Icorene 3545 GRN 6657, a PIAT between 190°C and 220°C is typically required for complete sintering without degrading the green pigment. If PIAT remains below 185°C, incomplete densification can create microvoids at internal corners and moulded-in inserts; if PIAT exceeds 230°C, oxidative degradation may reduce elongation at break and impact resistance, and colour shift toward yellow may appear. Cooling through the crystallisation range is a second threshold. Forced-air or water-mist cooling at 10–20°C/min through the 120–90°C band limits warpage, but excessively rapid cooling increases internal stress and can produce sink marks across ribs. The powder absorbs negligible water, but storage at relative humidity above 60% for more than 24 h may allow surface condensation; drying at 60°C for 2–4 h before charging reduces steam-induced porosity.

    Typical biaxial rotation ratios for hollow tanks are 4:1 primary-to-secondary axis, with primary axis speeds of 4–8 rpm and secondary axis speeds of 1–2 rpm for cylindrical parts. On a shuttle machine with two arms, oven dwell time for a 5 mm wall in this density class can range from 20 to 35 min depending on tooling mass and heat-transfer coefficient. The green compound can absorb infrared radiation differently from natural powder, so oven time may be 5–15% shorter; cycle settings should be transferred only after PIAT confirmation. Oxidation induction time of the powder should be monitored by ASTM D3895 or ISO 11357-6; a free-powder OIT below 10 min at 200°C indicates antioxidant depletion. A drop of more than 50% after a single oven pass suggests that the cycle is too aggressive or the mould is overcharged.

    Dry handling of Icorene 3545 GRN 6657 requires attention to bulk density and segregation during pneumatic transfer. The powder is not hygroscopically sensitive, but it can segregate by particle size in hoppers and pipelines, producing inconsistent charge weights and wall thickness variation. A volumetric cup feeder or loss-in-weight feeder with low shear should be used to maintain constant charge mass. Charge weight is calculated from part surface area, required wall thickness, polymer melt density, and a process factor; for a 5 mm wall, the approximate charge mass is surface area × wall thickness × 0.935 g/cm³ × 1.05–1.10. The process factor accounts for powder retained on the mould surface, loss through vents, and densification differences. Variation in charge weight greater than ±1% can produce measurable wall-thickness scatter in multi-cavity biaxial tools.

    Field data from rotational moulding lines indicate that pigmented polyethylenes can show accelerated heat absorption in thin-walled sections, leading to over-sintering of the outer wall while the inner wall has not reached full densification. This imbalance may appear as internal bubbles or delamination along the wall centreline. Moulders typically adjust oven time downward by 5–15% for the green compound and verify the internal air temperature rather than relying on the oven timer alone. In addition, tooling release agents containing silicone or fluoropolymer can migrate into the powder and reduce weld-line strength; release-agent selection should be validated by ASTM D638 tensile tests on plaques prepared with the same mould-release protocol used in production.

    A Stabilised Green Compound for Outdoor and Chemical Storage Service

    The GRN 6657 designation combines the Icorene 3545 polymer with a green pigment and a weathering stabiliser. Outdoor performance is not limited to colour retention; the stabiliser package is specified to preserve tensile elongation and impact after xenon-arc exposure under ISO 4892-2 or ASTM D2565. Because the green pigment absorbs infrared radiation differently from unpigmented polyethylene, heat-up rates in the mould can be 5–15% faster at the same oven setpoint. Moulders should validate PIAT and not assume that natural-grade cycle times transfer directly. The material is used in rotational moulded tanks, secondary containment, and agricultural chemical reservoirs where environmental stress-crack resistance is a design requirement. Chemical compatibility must be assessed with the intended fluid, concentration, and service temperature under ISO 175 or ASTM D543; published data for this specific green compound in oxidising acids, aromatic hydrocarbons, and chlorinated solvents is limited.

    In a rotationally moulded agricultural tank, the wall must withstand hydrostatic pressure, ultraviolet exposure, and low-speed impact at sub-zero temperatures. Wall sections in this density class are often specified at 4–6 mm for medium-volume vessels, but the exact dimension depends on vessel geometry and unsupported wall area. Impact acceptance is evaluated by ASTM D5276 drop-weight or ASTM D5628 falling-weight procedures at the required minimum service temperature; ductile deformation without brittle fragmentation is the usual acceptance criterion. Because Icorene 3545 is a linear low-density polymer with short-chain branching, it exhibits higher crack growth resistance than a comparable melt index HDPE rotomoulding grade, but it has lower load-bearing stiffness. Designers should not replace HDPE in flat-wall containers without re-evaluating buckling, creep, and deflection under the lower modulus of the LLDPE grade.

    Dispersion quality of the green pigment in Icorene 3545 GRN 6657 affects both appearance and mechanical integrity. Poor pigment dispersion can create agglomerates that act as stress concentrations and reduce low-temperature impact. Rotomoulding powders are typically dry-blended or melt-compounded; incompletely dispersed pigment in dry-blended systems may be detected by optical microscopy or by a low elongation at break relative to the natural grade. If the converter dry-blends green concentrate into natural Icorene 3545 instead of purchasing the GRN 6657 compound, the concentrate must be matched for melt flow rate and particle-size distribution to prevent segregation during rotation.

    When Complex Tooling Demands Rheology and Particle-Size Control

    In tools containing deep ribs, threaded inserts, or narrow kiss-off features, the powder must coat the tool surface early in the cycle and sinter before crystallisation freezes the wall. With a density of 0.935 g/cm³, the crystallisation onset lies near 105–110°C; if a thin feature cools below that range before powder has adhered, the remaining polymer can remain unconsolidated and create internal porosity. Particle-size distribution is therefore as important as melt flow rate. Coarse particles above 35 mesh (500 µm) can settle in pockets and fail to fuse, while an excessive fraction below 200 mesh (75 µm) can segregate during rotation and generate variable wall density. On production-scale twin-arm shuttle machines, batch-to-batch variation in sieve retention and bulk density is a known source of wall-thickness scatter; dry-flow and sieve checks are often performed after each 25–50 kg of material transfer. The green compound may show a slight increase in crystallisation temperature compared with natural powder because pigment particles can act as nucleation sites; the effect should be measured by ISO 11357-3 differential scanning calorimetry before cooling time is optimised.

    Relative to metallocene-catalysed octene LLDPE rotomoulding powders, the butene-based Icorene 3545 grade usually carries a lower raw-material cost and established field history in general-purpose tanks. Metallocene grades can offer higher dart-impact energy at equivalent density and melt flow rate under ASTM D5276, but they may exhibit narrower processing tolerances in some tooling configurations. Converters often select Icorene 3545 for less demanding outdoor containers where moderate stiffness, high ESCR, and reliable sintering are sufficient; when the application requires maximum puncture toughness at −40°C, a metallocene product may be more appropriate. Published data comparing GRN 6657 with specific metallocene green compounds is limited, so comparative moulding trials are required.

    Regulatory assessment of Icorene 3545 GRN 6657 must include both base resin and pigment package. The base polyethylene may be manufactured to meet FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011 for food-contact applications, but the green pigment concentrate may not be covered under all food-contact or potable-water listings. For potable water storage, verification against NSF/ANSI 61 is required for the exact GRN 6657 formulation. Continuous service under load above 50–60°C is outside the normal design envelope for this density class, and steam sterilisation above 100°C is not recommended unless prototype testing demonstrates acceptable creep and oxidative stability. Contact with strong oxidising agents, aromatic solvents, or chlorinated hydrocarbons can reduce service life; long-term evaluation under ISO 175 immersion at the maximum use temperature is required. Published data for this specific green configuration in those environments is limited.

    Top