| HS Code | 924497 |
| Product Name | LyondellBasell Icorene 3545 GRN 6628 |
| Polymer Type | Polyethylene, Linear Low Density |
| Density | 0.934 g/cm³ |
| Melt Flow Rate | 4.5 g/10 min |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 17 MPa |
| Elongation At Break | 750% |
| Flexural Modulus | 0.400 GPa |
| Hardness Shore D | 50 |
| Vicat Softening Point | 100 °C |
| Brittleness Temperature | -70 °C |
| Melting Point | 125 °C |
| Color | Green |
| Processing Method | Rotational Molding |
| Uv Stabilization | Yes |
As an accredited LyondellBasell Icorene 3545 GRN 6628 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 3545 GRN 6628 is supplied in 25 kg bags, 40 bags per pallet, totaling 1,000 kg. |
| Container Loading (20′ FCL) | 20′ FCL loading: Icorene 3545 GRN 6628 LLDPE, 25 kg bags, palletized or floor-loaded, approx. 20 MT net, securely stowed. |
| Shipping | LyondellBasell Icorene 3545 GRN 6628 is a non-hazardous linear low-density polyethylene resin. Ship in original sealed bags, boxes, or octabins, palletized and stretch-wrapped. Keep dry, away from heat, sunlight, and contamination. No special UN classification; follow standard freight and handling procedures. Maintain load stability and avoid puncturing packaging. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep containers tightly closed to prevent moisture and contamination. Avoid contact with strong oxidizers. Use appropriate grounding to prevent static buildup. Maintain good housekeeping to minimize dust. Follow the manufacturer’s SDS and local regulations for safe handling and storage. |
| Shelf Life | Shelf life is 12 months from manufacture when stored in original packaging under cool, dry conditions, away from direct sunlight. |
For potable water vessels, LyondellBasell Icorene 3545 GRN 6628 Linear Low Density Polyethylene is charged as a 100.0 wt% virgin powder without external lubricants or calcium stearate. Water-contact compliance is assessed under NSF/ANSI 61, EU 10/2011, and FDA 21 CFR 177.1520(c); tank design follows ASTM D1998-21. Where extended outdoor exposure above 1,200 h/year ultraviolet radiation is specified, a hindered amine light stabilizer masterbatch with an LLDPE carrier is dry-blended at 1.5–2.5 wt%, but the green 6628 pigment system itself must be covered by the relevant NSF 61 formulation listing before the moulded part is cleared for potable contact.
The mould is mounted on a biaxial rotomoulding machine with a 4:1 arm ratio; primary rotation is held at 8–12 rpm and secondary rotation at 2–4 rpm. Oven temperature is maintained at 285–315 °C, and a direct PIAT probe inserted through the vent riser is used to stop heating at 195–210 °C internal air temperature. Deviations below 185 °C leave partially sintered powder at the inner wall, producing pinholes, while PIAT above 220 °C initiates oxidative embrittlement and discolouration in the green compound. After forced-air cooling to 90 °C and water-mist cooling to 40 °C, the component is stripped from the mould. Terminal parts include vertical storage tanks of 500–10,000 L, conical-bottom dosing tanks, and rectangular transport tanks for potable water.
Because agrochemical storage tanks are routinely placed outdoors under UV-intensive conditions, the 3545 GRN 6628 powder is selected only after confirming the as-supplied compound retains an ESCR value above 500 h under ASTM D1693 Condition B. Compliance for transport and storage of liquid pesticides and fertilisers is aligned to UN Model Regulations Chapter 6.5 for rigid plastics IBCs and EN 13575-1:2016 for plastics drums. Formulation practice permits 100.0 wt% virgin powder or up to 20.0 wt% clean in-house regrind derived from rejected tanks with no more than two heat histories; regrind addition beyond 20.0 wt% reduces low-temperature impact and narrows the PIAT window. A UV masterbatch is added at 2.0 wt% maximum when tanks are stored in regions exceeding 120 kLy/year solar irradiance. Amine-based antistatic concentrates are not added to the 3545 GRN 6628 compound because they can antagonise the hindered phenol stabilizer system and shorten oven life.
Production uses preheated steel moulds fitted with drop-in stainless steel threaded inserts; the inserts are installed prior to charging and are not exposed to secondary operations after moulding. The oven is set at 290–310 °C and the mould is held until the internal air reaches 195–205 °C, followed by slow cooling to avoid warpage in long rectangular tanks. For tanks with wall sections of 8–12 mm, post-mould annealing at 70–80 °C for 30 min is applied to relieve residual stress before hydrostatic testing. Terminal finished products include 1,000–20,000 L horizontal nurse tanks, cone-bottom sprayer tanks, mixing hoppers, and secondary containment basins.
Marine buoy shells require a slightly different cooling profile than water tanks because the green outer surface must remain colour-stable after prolonged salt spray and wave impact. Surface colour is verified against IALA Recommendation E-108 for visual signal colours, and weld-line tensile properties of moulded-in steel chain plates are checked under ASTM D638-14 at 50 mm/min. The outer shell is moulded from 100.0 wt% Icorene 3545 GRN 6628; if additional UV stabilisation is required for equatorial deployment, a UV/HALS masterbatch is blended at 1.0–2.0 wt%. The formulation is not modified with talc or calcium carbonate because flexural fatigue under wave loading accelerates cracking.
The outer shell is rotomoulded on a bobbed arm machine with oven temperature 275–295 °C, and PIAT is deliberately held at the lower end of 190–200 °C to minimise thermal warpage of long cylindrical geometry. Wall thickness is maintained at 5–10 mm depending on impact zone; after demoulding, closed-cell polyurethane foam of 35–60 kg/m³ density is injected to occupy 70–90 % of the internal cavity, with a two-part mixing head delivering 3.5–5.0 kg/min throughput. The moulded skins are cooled with a compressed air ring to avoid water ingress into the vent ports. Finished parts include 600–2,000 mm diameter channel markers, mooring buoys, floating dock fenders, and aquaculture collar floats.
Logistics sector tubs are produced with a triple-layer rotational moulding sequence rather than a single charge, because recycled material can be embedded in the core without migrating to the food-contact surface. The exterior and interior skins are 100.0 wt% Icorene 3545 GRN 6628; the core may contain up to 25.0 wt% post-industrial regrind of the same grade with no odour or previous chemical load. Compliance for pallet boxes is evaluated under ISO 8611-1:2021 pallet load tests, and food-contact surfaces are assessed under EC 1935/2004 and FDA 21 CFR 177.1520 for fatty and aqueous foods.
Triple-layer charging is performed by introducing the green outer skin powder first, followed by the regrind-containing core powder, and finally the inner skin powder, with no additional binder; the sequential charge is sintered at oven temperature 280–300 °C to PIAT 195–210 °C. Multi-piece steel moulds with side cores produce undercuts for fork pockets; water-cooled side plates are engaged after demoulding to control shrinkage. Wall thickness ranges from 8–15 mm, with 4–6 mm virgin skin layers on both surfaces. Terminal products are 500–1,500 L insulated fish tubs, bulk bins, nestable distribution crates, and rotomoulded pallet boxes.
The critical difference in playground parts is not the resin chemistry but the wall-thickness distribution across concave slide geometries. Playground components are moulded from 100.0 wt% as-supplied Icorene 3545 GRN 6628; no separate pigment is added, because the 6628 green is already dispersed and additional masterbatch causes colour drift between production batches. Where play structures are installed above 2,000 m elevation, a HALS/UV stabilizer masterbatch is added at 1.0–2.0 wt%. Chemical compliance is tested under EN 71-3:2019 for migration of elements, mechanical safety under EN 1176-1:2017, and US playground systems under ASTM F1487-21.
Cast aluminium moulds with highly polished concave surfaces are used to minimise drag marks on slide beds. The machine runs a 3:1 arm ratio at primary 6–9 rpm and secondary 2–3 rpm, with oven temperature 280–300 °C and PIAT 190–210 °C. Wall thickness is held at 5–7 mm for slide beds, but rope attachment points are locally thickened to 8–10 mm using removable mould inserts. Forced-air cooling with a venturi ring is used instead of water mist to avoid surface stress whitening. Terminal finished products include slide beds, tunnel sections, climbing wall panels, spring rider bodies, and sand-play tables.
Underground chambers are rotomoulded with the highest wall thickness in the LLDPE application range, typically 8–18 mm, because live-load deflection controls the design rather than internal pressure. The compound is processed as 80.0 wt% virgin Icorene 3545 GRN 6628 and 20.0 wt% clean post-industrial regrind; no high-aspect-ratio fillers are permitted because creep modulus gains are offset by premature stress cracking under ASTM D1693 Condition B. Structural evaluation for shallow burial is performed under AASHTO LRFD live-load provisions with an H-25 wheel load, and long-term creep is checked under ASTM D2990 at 23 °C and 50 % RH.
Arch-shaped steel moulds with internal water-cooled rib forms are used to create corrugated sidewalls and internal stiffeners. Oven temperature is set at 285–305 °C and PIAT is terminated between 195–210 °C; the powder is pre-dried to 0.05 wt% maximum surface moisture when storage humidity exceeds 60 % RH for more than 48 h before charging. Post-mould deflection testing applies an H-25 equivalent load and records diametric deflection of less than 5 % without wall buckling. Terminal parts include stormwater detention and infiltration chambers, catch basin inserts, utility vault liners, and water meter pits.
Competitive LyondellBasell Icorene 3545 GRN 6628 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Designated in producer documentation as LyondellBasell Icorene 3545 GRN 6628, this product is a pre-coloured green linear low density polyethylene rotational moulding powder. The unreinforced base resin, Icorene 3545, is an LLDPE with a nominal density of 0.934 g/cm³ when measured to ISO 1183-1:2019 and a melt flow rate of 5.0 g/10 min when tested to ISO 1133-1:2022 at 190 °C and 2.16 kg. The suffix GRN 6628 denotes a proprietary green colour package; the carrier resin and pigment loading are not fully disclosed in the public datasheet. The as-shipped pigmented powder may show a density offset of a few thousandths of a gram per cubic centimetre relative to the natural base resin, so the batch certificate of analysis must be used for shot-weight and tooling calculations. The grade is used in large hollow components that require low-temperature ductility and environmental stress crack resistance without the excessive stiffness of HDPE. In comparison with a conventional 0.942 g/cm³ hexene HDPE rotomoulding powder, Icorene 3545 GRN 6628 shifts the balance toward higher freeze-impact retention and lower flexural modulus; these differences are measurable in rotomoulded plaques cut to the dimensions required by ISO 527-2 and ISO 178.
A direct substitution from a conventional HDPE rotomoulding grade to Icorene 3545 GRN 6628 affects stiffness, impact, and chemical resistance in measurable directions. HDPE grades with density near 0.940–0.945 g/cm³ typically show flexural moduli in the 700–900 MPa range when machined from rotomoulded plaques and tested under ISO 178. Icorene 3545’s lower density is generally associated with flexural modulus values closer to 600–650 MPa; the precise value depends on cooling rate, wall thickness, and pigment dispersion. Conversely, environmental stress crack resistance of LLDPE materials in this density range commonly exceeds that of unmodified HDPE. Some producer data for Icorene 3545 report ESCR values above 1000 h under ASTM D1693-22 condition B, though the GRN 6628 pigmented variant should be re-tested because pigments can nucleate or alter tie-molecule populations. Freeze-impact behaviour also differs: a properly moulded Icorene 3545 part generally retains ductility at -20 °C to -40 °C, as evaluated by drop-weight testing to ISO 6603-2 or ARM impact tests. This is why the product is selected for agricultural tanks, outdoor equipment housings, and chemical storage where HDPE fails by brittle fracture at low temperature.
On a shuttle or carousel rotational moulding line with closed mould cavities, the material is charged as a dry powder and densified by simultaneous heating and biaxial rotation. A commonly used rotational ratio of 4:1 and mould surface temperatures of 250–300 °C permit the powder to sinter and consolidate. The critical process variable is peak internal air temperature, which for LLDPE powders of this class should generally reach 190–210 °C. If PIAT remains below 190 °C, residual microvoids persist at the inner wall and shrinkage, tensile strength to ISO 527-2, and drop-impact resistance to ISO 6603-2 are degraded. At PIAT above 220 °C, oxidative degradation accelerates, especially in the presence of green pigmentation; the inner surface can become tacky, discoloured, or bubble-laden. Oven residence time required to reach the target PIAT depends on mould material, wall thickness, and powder particle-size distribution. Thick aluminium tools with a wall thickness of 6–8 mm may require 18–30 min in the oven, while thin steel shells may densify more quickly. Cooling should be controlled because rapid water mist cooling of a green LLDPE part increases warpage and differential shrinkage, whereas slow ambient cooling reduces frozen-in stress but lengthens cycle time.
The dry-flow characteristics of Icorene 3545 GRN 6628 are governed by particle shape, bulk density, and the dispersion of the green pigment. Rotomoulding powders of this type are typically supplied with a particle-size distribution controlled to a D50 range of 250–450 µm and an upper sieve fraction below 500 µm, but the exact distribution should be taken from the producer’s certificate of analysis. Bulk density is commonly reported between 0.34 and 0.38 g/cm³ for uncompressed powder; vibrated bulk density may be 0.04–0.07 g/cm³ higher. When the powder is transferred by vacuum conveying or flexible screw from silo to weigh hopper, coarse and fine fractions can segregate; this segregation changes the melt packing behaviour and can produce local pinholing in thin-wall sections. A horizontal ribbon blender with a gentle blending cycle is preferred over high-intensity mixers because high shear can fracture powder particles, increase fines, and shift the sintering onset. If the green concentrate is not fully dispersed, colour streaks appear at part corners and weld lines. A screened sieve pack of 500–1000 µm or a rotary sifter should be used before charging to remove tramp particles. The GRN 6628 variant may require a specific dry-flow test, such as a Hall flowmeter or the method described in ASTM D1895-17, to establish hopper discharge reliability.
Food-contact and potable-water clearances cannot be transferred automatically from the natural base resin to the pre-coloured powder. The base LLDPE may be manufactured in accordance with US FDA 21 CFR 177.1520(c) for olefin polymers when the end-use temperature and food-simulant conditions are respected, but the GRN 6628 colour package and its carrier must be evaluated separately under applicable colourant regulations or migration testing. For European applications, compliance with Commission Regulation (EU) No 10/2011 on plastic materials intended for food contact requires testing of the finished article because the green pigment may alter overall migration or specific migration behaviour. The material is not recommended for continuous exposure to strong oxidizing acids, aromatic hydrocarbons, or chlorinated solvents at elevated temperatures; these agents attack the polyethylene matrix and may also leach colourant. In outdoor tanks exposed to diesel or agricultural chemicals, the manufacturer should provide chemical resistance data based on ISO 175 immersion testing, and the processor should validate the specific chemical blend because polar co-solvents produce different swelling profiles than neat reagents.
Some processors reduce oven temperature to avoid yellowing or gloss loss in pigmented LLDPE. If the setpoint is lowered from a conventional 290 °C to 260 °C, the heat flux into the mould is reduced and the PIAT may plateau below 190 °C unless residence time is extended. Under this condition, the powder particles sinter but do not fully coalesce; the dominant failure is microvoiding at the inner surface and in the weld lines around inserts, rather than oxidative discolouration. Microvoids act as stress concentrators that reduce tensile elongation at break and may lower ARM impact values by more than 50% in 6 mm plaques. The second failure mode is warp due to temperature gradients across the mould. A thick section may reach densification temperature while the inner surface remains cooler; the resulting differential crystallinity from fast cooling creates internal stress. Dimensional checks on a cast aluminium mould with 8 mm walls should include a shrinkage measurement after 48 h conditioning at 23 ±2 °C and 50 ±5% relative humidity, with reference values taken from the natural 3545 datasheet and adjusted for the green pigment. If cold processing is unavoidable, a 10–15% increase in oven residence time and an increase in rotational speed are sometimes used to improve heat transfer, but the only robust validation is a PIAT recorder placed inside the cavity.
Outdoor service life data for green rotomoulded LLDPE are strongly influenced by the UV stabilisation package, which may or may not be present in the GRN 6628 colour system. If the part is intended for permanent outdoor exposure, accelerated weathering should be conducted according to ISO 4892-2 with Type 1A daylight filters, black-standard temperature 65 °C, and a wet/dry cycle. A change in colour Delta E greater than 10 before 2000 h often indicates insufficient pigment or UV stabiliser performance for long-term agricultural service. Mechanical properties after weathering should be tested by ISO 527-2 and ISO 6603-2 at -20 °C because degraded skin layers nucleate brittle failure even when bulk tensile properties remain within specification. Edge gate areas, mould parting-line flash, and zones with high pigment concentration are typical initiation sites. For chemical storage tanks, the inner wall should be examined for environmental stress cracks after 500 h of contact with the intended chemical at 40–60 °C; ASTM D1693-22 bent-strip testing in the active chemical is not a direct replacement but can be used for ranking formulations. In all cases, the specific green variant must be qualified on the same tool and under the same cycle conditions used in production; data from natural 3545 cannot be substituted.
When the product arrives in bulk deliveries, a composite sample should be withdrawn from at least 10 locations during silo discharge to limit the effect of fines segregation. The composite should be reduced in a spin riffler rather than by cone-and-quartering because a riffler preserves the particle-size distribution. Melt flow rate should be tested to ISO 1133-1:2022 at 190 °C/2.16 kg, and density should be tested to ISO 1183-1:2019 on compression-moulded plaques prepared from the received powder. Powder bulk density and flowability can be screened by ASTM D1895-17, while sieve classification can be checked by ASTM D1921 or ASTM D6913 if the particle-size specification is written into the purchase order. Moisture content of hydrophobic polyethylene is usually low, but condensation can occur when cold powder is discharged in a warm, humid plant at relative humidity above 80%; closed silo storage and 24 h conditioning before processing reduce surface moisture defects. Colour uniformity of the green powder should be verified with a spectrophotometer using 45/0 geometry and a minimum of 3 readings per batch. Rotational rheometry at 190 °C with a 25 mm parallel-plate fixture across an angular frequency sweep of 0.1–100 rad/s can detect pigment-induced viscoelastic shifts that a single melt flow rate value cannot resolve. Cross-contamination with polypropylene or HDPE is critical because even a 2–5% contamination level can alter density, reduce ESCR, and create visible weld-line defects in the final part.