| HS Code | 334396 |
| Density | 0.935 g/cm³ |
| Melt Flow Rate | 4.5 g/10 min at 190°C/2.16 kg |
| Tensile Strength At Yield | 11.0 MPa |
| Tensile Strength At Break | 15.0 MPa |
| Elongation At Break | 700 % |
| Flexural Modulus | 300 MPa |
| Hardness Shore D | 50 |
| Vicat Softening Point | 100 °C |
| Deflection Temperature At 0 46 Mpa | 70 °C |
| Melting Point | 125 °C |
| Water Absorption | 0.010 % |
| Dielectric Constant | 2.3 |
| Volume Resistivity | 1.00e+15 ohm·cm |
| Color | Green |
As an accredited LyondellBasell Icorene 3545 GRN 6435 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 3545 GRN 6435 Polyethylene, Linear Low Density is supplied in 25 kg polyethylene-lined bags, 40 bags per 1,000 kg pallet. |
| Container Loading (20′ FCL) | 20′ FCL loading: LyondellBasell Icorene 3545 GRN 6435 Polyethylene, Linear Low Density; palletized bags, securely stowed, clean dry container, even weight distribution. |
| Shipping | LyondellBasell Icorene 3545 GRN 6435 Polyethylene, Linear Low Density is shipped as non-hazardous solid pellets in 25 kg bags, FIBCs, octabins, or bulk trucks/railcars. It is not regulated for transport. Keep dry, cool, and away from ignition sources; avoid contamination, moisture, and prolonged sunlight. |
| Storage | Store indoors at ambient temperature in a cool, dry, well-ventilated warehouse. Keep containers sealed and off the floor on pallets. Protect from direct sunlight, moisture, heat, sparks, and open flames. Avoid contact with strong oxidizers. Maintain good housekeeping to prevent dust accumulation and slipping. Keep away from food, beverages, and incompatible materials. Rotate stock using FIFO. |
| Shelf Life | Shelf life is 24 months from date of manufacture when stored in original unopened packaging at recommended storage conditions. |
Monolithic green-pigmented LLDPE climbing structures and slide shells are produced on multi-arm carousel rotational moulding machines with biaxial rotation ratios set between 4:1 and 8:1. Compliance for public playground applications is anchored to EN 1176-1:2017 and ASTM F1487-21, with material qualification performed under ASTM D256-23 notched Izod at -20 °C and ASTM D638-14 tensile yield. Icorene 3545 GRN 6435 powder is charged at 100% as supplied; post-industrial regrind from trimmed moulded edges is dry-blended at 10–20 wt% of the total shot weight, and the regrind fraction is sieve-controlled above 35 mesh (500 µm) to reduce pinhole formation. Oven zone temperatures are maintained at 270–315 °C, while mould internal air temperature is held between 190 °C and 220 °C; forced-air cooling followed by water-mist cooling is held at 8–12 °C/min to minimise warpage without quenching the inner wall. Production-scale failure modes observed on carousel lines include inner-surface bridging at deep draw radii below 3 mm when the powder bed is not vented, and localized thickening at mould parting lines if the rotation ratio exceeds 8:1. Terminal articles include slide bodies, tunnel sections, climbing wall shells, and spring ride seats.
The governing specification for upright polyethylene storage tanks, ASTM D1998-15, requires environmental stress-cracking resistance tested under ASTM D1693-15, Condition A, with minimum failure time determined by the end-user specification. In agricultural sprayer and nurse-tank production, the powder is used at 100% virgin content for chemical-contact tanks; for water-only agricultural tanks, clean post-industrial regrind is added at 10–15 wt% to reduce raw-material cost without lowering the specification. Rock-and-roll rotational moulding machines process long tank bodies at oven temperatures of 280–300 °C and mould internal air temperatures of 200–210 °C; wall thicknesses are controlled between 4 mm and 10 mm by shot-weight calculation and verified with ultrasonic thickness gauging under ISO 16809:2017. Batch-to-batch variance in pigment dispersion is monitored by melt flow rate under ISO 1133-1:2022 and sieve analysis; non-uniform inner-wall colour indicates inadequate dry-blend mixing or regrind moisture above 0.1%. Published permeability data for aggressive chemical combinations in green-pigmented LLDPE rotational moulding powder is limited; immersion screening under ASTM D543-21 is therefore required before specifying non-water media. Finished products include 100–5,000 L agricultural sprayer tanks, fertilizer nurse tanks, rainwater harvesting tanks, and chemical dosing cabinets.
Two-wheeled waste and recycling container bodies are produced on shuttle-type rotational moulding machines with cast aluminium or steel moulds at oven set points between 285 °C and 310 °C. Product conformance is established under EN 840-1:2020 for 120 L, 240 L, and 360 L containers; material testing uses ISO 527-2:2012 tensile properties and ISO 179-1:2010 Charpy impact at -20 °C. The dry-charge formulation is 100% supplied GRN 6435 powder, with clean in-house regrind added at 5–15 wt%; cleaning-agent resistance is screened by immersion in 2% sodium hydroxide and 5% citric acid solutions for 168 h at 23 °C according to ASTM D543-21. Regulatory screening for heavy metals and SVHCs in the pigmented compound is documented under REACH 1907/2006 and RoHS 2011/65/EU when finished articles enter electrical/electronic waste streams. Cooling is sequenced from forced air to water mist, maintaining a demoulding surface temperature decrease of 9–13 °C/min; closure rib cracking has been observed when demoulding occurs before the surface temperature falls below 80 °C. Terminal articles include 120 L, 240 L, and 360 L two-wheeled bins, recycling collection containers, and battery collection boxes.
Marine flotation bodies and aquaculture collars are formed from the green powder on biaxial rotational moulding machines with mould internal air temperature held at 195–215 °C. The water absorption limit is set by ISO 62:2008 at 23 °C for 24 h, and low-temperature impact is assessed with ISO 179-1:2010 Charpy at -20 °C. The addition ratio in floating structures remains 100% virgin powder; regrind is limited to a maximum of 5 wt% because heat-history particles can lower ISO 179-1 Charpy values below the acceptance threshold. Batch-to-batch wall thickness variance in buoy shells is controlled by ultrasonic thickness measurement at 25 mm grid spacing across the mould surface, particularly around metal insert locations. Cast aluminium moulds are used with wall thickness variation controlled within ±1 mm over the flotation shell. Terminal products include mooring buoys, aquaculture float collars, pontoon floats, and inshore marker buoys.
| Application sector | Compliance standards | Test verification | Formulation boundary |
|---|---|---|---|
| Outdoor play equipment | EN 1176-1:2017, ASTM F1487-21 | ASTM D256-23 at -20 °C | 100% powder; 10–20 wt% regrind |
| Agricultural storage tanks | ASTM D1998-15 | ASTM D1693-15, Condition A | 100% virgin; 10–15 wt% regrind in water-only tanks |
| Waste and recycling containers | EN 840-1:2020 | ISO 179-1:2010 at -20 °C | 100% powder; 5–15 wt% regrind |
| Marine flotation bodies | ISO 62:2008 | ISO 179-1:2010 at -20 °C | 100% virgin; max 5 wt% regrind |
| Industrial material-handling pallets | ISO 8611-1:2011 | ISO 1133-1:2022 at 190 °C/2.16 kg | 80–90 wt% powder; 10–20 wt% regrind |
| Street furniture shells | ISO 4892-2:2013 | ASTM D2244-23 CIELAB ΔE | 100% powder; optional 5–10 wt% HDPE |
Industrial four-way pallets and handling boxes are produced on multi-arm carousel machines where the powder bed is sintered at oven set points of 300–320 °C and mould internal air temperature is controlled at 210–220 °C to densify the inner wall. Pallet load-bearing performance is evaluated under ISO 8611-1:2011; resin incoming melt flow rate is checked by ISO 1133-1:2022 at 190 °C/2.16 kg. The dry-blend formulation is composed of 80–90 wt% Icorene 3545 GRN 6435 powder and 10–20 wt% clean post-industrial LLDPE regrind; regrind above 25 wt% is avoided because incomplete fusion may occur below the 200 °C internal air threshold. The dry-blend is mixed in a high-intensity mixer at 800–1,200 rpm for 5–6 min before charging to avoid pigment segregation. Excessive regrind moisture above 0.05% can generate steam pinholes; regrind is dried at 60–70 °C for 2 h before dry-blending when ambient RH exceeds 60%. For electronics-handling pallets, an antistatic masterbatch is added at 2–5 wt% and moulded parts are tested to surface resistivity below 109 Ω per IEC 61340-5-1. Terminal products include four-way plastic pallets, export handling boxes, and distribution containers.
Street furniture shells, planter liners, and bollard covers are produced from the same grade with no external pigment addition because GRN 6435 is factory-compounded. Accelerated weathering validation follows ISO 4892-2:2013 cycle A with 500 h exposure; colour change is measured by ASTM D2244-23 CIELAB ΔE with an acceptance limit below 3.0 in accelerated testing, although published data for this specific green formulation is limited. The powder is charged at 100% as supplied; if additional surface hardness is required, dry-blending with 5–10 wt% HDPE powder is used and the density shift is verified by ASTM D1505-18. Processing on carousel machines uses oven set points of 280–300 °C; machined aluminium moulds are fitted with 0.5–1.0 mm degassed vent gaps. Mould release agents are selected from semi-permanent grades applied at 0.2–0.5 g/m² to prevent surface defects. Terminal products include planters, bench shells, bollard covers, and equipment enclosures.
Competitive LyondellBasell Icorene 3545 GRN 6435 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 3545 GRN 6435 is a linear low-density polyethylene rotational molding powder supplied in a green-compounded form. The grade designation 3545 identifies a medium-flow base resin with a nominal density within the 0.930–0.940 g/cm³ band and a melt flow rate near 5.0 g/10 min at 190 °C/2.16 kg when determined according to ISO 1133-1:2022 or ASTM D1238-20. The suffix GRN 6435 is a proprietary colorant package incorporated before grinding; it eliminates the need for separate dry-blended pigment masterbatch and provides a pre-compounded green color. The material is intended for single-layer rotational molding of hollow articles in which low-temperature ductility, environmental stress crack resistance, and consistent powder dry-flow are required. Published data for this specific color-compounded configuration are limited; properties cited for the natural base resin require confirmation on rotomolded specimens.
The polymer backbone is produced by copolymerizing ethylene with an alpha-olefin comonomer, generating short-chain branches that reduce crystallite thickness and lower density relative to high-density polyethylene. Density is determined on compression-molded plaques under ISO 1183-1:2019 or ASTM D1505-18. Tensile properties are measured under ISO 527-2:2012 or ASTM D638-14; flexural modulus is measured under ISO 178:2019 or ASTM D790-17. The medium melt flow rate reduces zero-shear viscosity during oven residence enough to promote sintering against the mold surface, while the linear backbone retains higher tensile strength and creep resistance than branched low-density polyethylene at equivalent density.
Relative to HDPE rotational molding grades with densities above 0.940 g/cm³, the lower density of Icorene 3545 GRN 6435 reduces flexural modulus and increases elongation. The LLDPE architecture also improves environmental stress crack resistance and low-temperature impact, but it lowers continuous-use temperature and stiffness. HDPE grades may be selected for higher modulus and upper-use temperature; however, they typically exhibit a higher ductile-to-brittle transition temperature and lower slow crack growth resistance in stressed molded parts. Compared with low-density polyethylene produced by high-pressure autoclave or tubular reactors, the linear backbone of this product provides higher tensile yield strength and better creep resistance at ambient temperature.
Metallocene LLDPE rotational molding powders often have a narrower molecular weight distribution and more uniform comonomer placement than conventional Ziegler-Natta resins. Those features can increase toughness at equivalent density but may also produce a sharper melting transition and higher elastic melt behavior, requiring tighter control of peak internal air temperature and cooling rate to avoid warpage. Icorene 3545 GRN 6435 is processed similarly to conventional Ziegler-Natta LLDPE rotational molding powders. The broader molecular weight distribution aids powder coalescence and wall-thickness uniformity in deep molds, although ultimate clarity and organoleptic performance may be lower than metallocene alternatives when those are used in natural or lightly pigmented applications.
Within rotational molding powders, melt flow rate is inversely related to environmental stress crack resistance. A grade with a higher melt flow rate fills complex mold geometry at lower oven temperature but generally sacrifices slow crack growth resistance. A lower melt flow rate improves environmental stress crack resistance and impact but requires longer cycle time and higher peak internal air temperature. The nominal 5.0 g/10 min melt flow rate of the 3545 base resin is positioned for medium-complexity hollow parts with wall thicknesses generally above 3 mm. Thin-walled parts below 3 mm may require higher-melt-flow grades or longer oven residence to avoid incomplete densification.
Environmental stress crack resistance is evaluated under ASTM D1693-21 using 10% Igepal CO-630 at 50 °C. The LLDPE architecture generally yields longer F50 failure times than HDPE rotational molding grades at equivalent melt index. However, pigments can nucleate or alter crystalline morphology, so environmental stress crack resistance data generated on natural resin should not be extrapolated to the green-compounded variant without confirmation on rotomolded plaques. For agricultural chemical tanks, the test is a screening tool only; full-service validation requires immersion in the actual chemical formulation at the intended service temperature and stress state.
Low-temperature impact of rotomolded parts is commonly assessed by falling dart impact under ISO 6603-2:2000 or ASTM D3763-18 on panels cut from molded parts. Test temperature, wall thickness, and cooling rate control the ductile-to-brittle transition. Molded parts with wall thickness below 3 mm may exhibit earlier brittle failure at temperatures below -20 °C. The green colorant package can shift the failure temperature slightly, so impact performance must be verified on production-molded articles rather than on compression-molded laboratory specimens. Chemical exposure can reduce low-temperature ductility, especially after contact with surfactants, aromatic hydrocarbons, or strong oxidizing acids. Chlorinated solvents and strongly oxidizing chemicals are not recommended without explicit validation under ASTM D543-20 or equivalent immersion testing.
Rotational molding applications for green LLDPE powders include agricultural chemical tanks, water storage tanks, outdoor bins, and recreational components. In agricultural tanks, the polymer must withstand dilute fertilizer solutions and surfactants; environmental stress crack resistance testing under ASTM D1693-21 provides a screening tool, while full-service validation requires exposure to the actual chemical formulation at the intended service temperature. In outdoor components, the green colorant may provide aesthetic value but not UV protection; weathering per ISO 4892-2:2013 should be correlated with field data from ISO 877-1:2009 exposure.
On production-scale carousel, shuttle, and rock-and-roll machines, rotational molding of this grade typically begins with ambient-temperature mold charging. Oven air temperatures between 260 °C and 320 °C are common for LLDPE rotational molding powders, with peak internal air temperature measured by Rotolog or equivalent sensors reaching 190–220 °C to complete densification. Mold rotation ratios commonly range from 4:1 to 8:1 depending on mold length-to-diameter ratio and part complexity. Demolding should occur after cooling below 80–90 °C to reduce shrinkage and distortion. Because the powder is dry-flowing, it can be charged directly into closed molds; however, storage at relative humidity above 60% may require conditioning at 60–80 °C for 1–2 h to prevent moisture-induced porosity and surface defects.
Dry-flow behavior is characterized by apparent bulk density and funnel flow time under ASTM D1895-17 Method A or B. LLDPE rotational molding powders typically exhibit bulk density between 0.35 g/cm³ and 0.45 g/cm³; lower bulk density can reduce mold fill consistency in narrow channels. Particle size distribution is determined by dry sieving under ASTM D1921-18 or an equivalent internal method. A controlled top-cut near 500 µm and a limited fines fraction below 150 µm are commonly used to balance surface definition against dust and static charge. On high-humidity production days, grounding of hoppers, meters, and molds is necessary to prevent fines segregation and inconsistent charging.
The powder is produced from stabilized pellet feedstock by grinding under controlled temperature to preserve molecular weight. Grinding heat can degrade the polymer if the mill temperature exceeds 80–100 °C; therefore, cryogenic or low-shear ambient grinding with air classification is used to maintain particle shape and bulk density. The certificate of analysis for rotational molding powders typically reports bulk density, sieve distribution, and dry flow time in addition to melt flow rate and density.
Oscillatory rheometry of the base resin can be performed at 190 °C on compression-molded disks using 25 mm parallel plates at 1% strain within the linear viscoelastic region. Complex viscosity at low frequency correlates with zero-shear viscosity and sag resistance; a medium melt flow rate near 5.0 g/10 min corresponds to a zero-shear viscosity low enough to densify at 200 °C internal air temperature but high enough to limit excessive thinning on vertical walls. Thermal stability is assessed by melt flow drift after multiple heating cycles or by thermogravimetric analysis under nitrogen. Processors should avoid prolonged hold times above 280 °C oven air temperature because oxidative degradation can reduce impact and environmental stress crack resistance even if the melt flow rate remains within specification.
The green colorant package may alter linear mold shrinkage, warpage, and weatherability relative to natural or white variants. Pigmented polyethylene can retain heat differently during infrared oven heating, producing non-uniform wall thickness if mold rotation and oven settings are not adjusted. Outdoor weathering should be evaluated under ISO 4892-2:2013 or ASTM G154-16 cycle 1. Green pigments do not automatically provide UV stabilization; a separate UV stabilizer package is required for long-term exterior service. Tensile impact and color retention after weathering must be confirmed on rotomolded panels, not on compression-molded plaques. Contact with copper, manganese, or cobalt salts can accelerate thermo-oxidative degradation and should be avoided during storage and service. The grade is not intended for continuous load-bearing service above 60–80 °C or for pressure-vessel applications requiring long-term creep resistance at elevated temperature.
Regulatory status must be confirmed against the exact grade and colorant package. Polyethylene base resins of this type are generally recognized for food-contact use under FDA 21 CFR 177.1520(c) when used in accordance with the conditions specified in that section, but the green pigment package may require separate food-contact authorization. In the European Union, food-contact compliance is evaluated under Regulation (EU) No 10/2011 and its amendments, with overall migration limits determined according to EN 1186-1:2002. Industrial chemical containment should be assessed for compatibility before specifying the material for UN-certified packagings; the grade is not a direct substitute for fluorinated or crosslinked polyethylene in barrier-limited applications. RoHS and REACH compliance should be confirmed through the manufacturer’s regulatory information, particularly for the colorant package.
| Property | ISO method | ASTM method | Test condition |
|---|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | ASTM D1238-20 | 190 °C / 2.16 kg |
| Density | ISO 1183-1:2019 | ASTM D1505-18 | 23 °C, compression-molded plaque |
| Tensile properties | ISO 527-2:2012 | ASTM D638-14 | Type IV / 1A specimen, 50 mm/min |
| Flexural modulus | ISO 178:2019 | ASTM D790-17 | 2 mm/min, 3-point bending |
| Environmental stress crack resistance | — | ASTM D1693-21 | 10% Igepal CO-630, 50 °C |
| Brittleness temperature | ISO 974:2000 | ASTM D746-20 | 50% failure temperature |
| Vicat softening temperature | ISO 306:2022 | ASTM D1525-17e1 | A50 / 10 N |
| Weathering | ISO 4892-2:2013 | ASTM G154-16 | UVA-340, cycle-dependent |
Compared with crosslinkable HDPE rotational molding grades, Icorene 3545 GRN 6435 remains thermoplastic and can be recycled by regrinding or reprocessing. It does not require post-mold curing or peroxide addition. Its upper-use temperature and dimensional stability under load are lower than crosslinked HDPE; continuous service above 60 °C may reduce stiffness and accelerate creep. Compared with polypropylene rotational molding powders, the polyethylene grade offers superior low-temperature impact and easier processability at lower oven temperatures but lower heat deflection temperature. Production-scale experience with LLDPE rotational molding powders indicates that the largest sources of part rejection are inconsistent oven temperature profiles, inadequate mold release, and premature demolding. Certificate-of-analysis sieve data and melt flow rate should be reviewed before process validation, and initial trials should include rotomolded plaque testing for impact, environmental stress crack resistance, and color dispersion.