    Specifications
    HS Code 127164
    Density 0.935 g/cm³
    Melt Flow Rate 3.5 g/10 min
    Tensile Strength At Yield 14.0 MPa
    Tensile Strength At Break 10.0 MPa
    Elongation At Break 700%
    Flexural Modulus 586 MPa
    Tensile Modulus 483 MPa
    Vicat Softening Point 104 °C
    Melting Point 124 °C
    Hardness Shore D 55
    Color Green
    Material Type Polyethylene, Linear Low Density

    As an accredited LyondellBasell Icorene 3545 GRN 6425 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg polyethylene-lined bags, palletized on 1,000 kg shrink-wrapped pallets for safe handling.
    Container Loading (20′ FCL) 20′ FCL container loading of LyondellBasell Icorene 3545 GRN 6425 Linear Low Density Polyethylene: palletized bags, dry container, secured stowage.
    Shipping LyondellBasell Icorene 3545 GRN 6425 is shipped as non-hazardous linear low density polyethylene resin, typically in 25 kg polyethylene bags on stretch-wrapped pallets. Transport in clean, dry trucks or containers, protected from moisture, direct sunlight, and contamination. Store in a cool, dry, ventilated area away from ignition sources.
    Storage Store LyondellBasell Icorene 3545 GRN 6425 Polyethylene, Linear Low Density, in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and strong oxidizers. Keep original packaging closed, off the floor on pallets, and protect from moisture, dust, and contamination. Avoid excessive stacking. Maintain first-in, first-out rotation and good housekeeping. Do not store near food, feed, or drinking water.
    Shelf Life Shelf life is typically 12 months when stored unopened in original packaging under cool, dry, well-ventilated conditions, away from direct sunlight.
    Application of LyondellBasell Icorene 3545 GRN 6425 Polyethylene, Linear Low Density

    Agricultural chemical storage and sprayer tank production consumes the supplied green LLDPE powder in monolayer rotational molding programs. Icorene 3545 GRN 6425 is assessed against ISO 16101:2004 Annex B for standard liquid compatibility when dilute acids, ester-containing adjuvants, and surfactant-based wetting agents are to be held in the same vessel; full-scale vertical tanks are specified under ASTM D1998-21 for hydrostatic strength and hoop-stress rupture behavior. In-plant formulation practice limits repulverized regrind from trimmed manways, fitting bosses, and vent cutouts to 20–30 wt%, with the regrind co-mixed in a low-shear ribbon blender at 30–50 rpm for 20 min before mold charging. Where aggressive ester solvents or chlorinated carriers are expected, wall section is increased to 8–12 mm rather than attempting monolayer barrier modification, because barrier additives are not incorporated in this rotomolding feedstock. Rotational molding is carried out in multi-axis carousel machines with oven set points between 260°C and 300°C, peak internal air temperature of 190–210°C, primary-to-secondary tooling rotation ratios of 4:1, and staged cooling from forced air to mist until mold surface temperature drops below 70°C. Field failure analysis of rotomolded agricultural tanks has repeatedly associated chemical stress cracking with residual stresses at the tank floor knuckle radius and with fitting boss pull-out; these failures are controlled by maintaining a minimum knuckle radius of 25–50 mm, by specifying machined insert bosses with a 45° taper, and by limiting cooling rate through the 90–70°C interval to 2°C/min. Where published data for this specific grade configuration is limited, converter qualification is performed using the surrounding density envelope of 0.930–0.935 g/cm³ according to ISO 1183-1:2019 and melt flow index of 3.0–4.0 g/10 min under 190°C/2.16 kg according to ISO 1133-1:2022. Terminal outputs include 1,000–10,000 L vertical storage tanks, skid-mounted sprayer sumps, and 200–800 L saddle-style induction reservoirs.

    Outdoor playground and recreational equipment programs use the pre-compounded green LLDPE for rotationally molded slide bedways, tunnel segments, climbing handholds, and roof fascia panels. The components are specified for consumer safety under ASTM F1487-21 and EN 1176-1:2017; the latter requires protrusion, entrapment, and accessible-opening tests on as-molded surfaces. Because the grade is supplied with a UV stabilizer package already incorporated, no additional UV masterbatch is added under standard weathering exposure; if color adjustment is needed for fleet reconfiguration, 1–2 wt% of a polyolefin-based color concentrate is dry-blended, and regrind from rejected parts is limited to 30 wt% to maintain falling-weight impact retention. Molding is performed on rock-and-roll machines for long slide tubes and on carousel machines for multi-part climbing systems, with oven set points of 280–320°C, peak internal air temperature of 200–220°C, and mold cavity texture held below 1.0 mm Ra to balance slip resistance against cleanability. UV package function is verified after molding by ASTM D4329-21 Cycle A for 2,500 h, with retained tensile strain at break compared to unexposed controls rather than color shift alone. Finished products include slide bedways, tunnel housings, angled climbing segments, and green roof canopy end caps.

    What Limits Shell Wall Integrity in Insulated Fish Box Rotomolding?

    A thinned corner at the impingement plate is the dominant shell-wall defect in insulated fish box rotational molding, occurring where the LLDPE powder must sinter after the mold has rotated past the bulk fill zone and the powder bed has become locally depleted. Icorene 3545 GRN 6425 is processed into non-food and food-contact totes; for food-contact configurations, compliance is verified against 21 CFR 177.1520(c) for olefin polymers and EU 10/2011 migration requirements, with the converter responsible for selecting only food-grade internal mold release agents. Formulation practice permits 10–20 wt% of traceable in-house regrind for food-contact shells, but no external reprocessed market material is introduced. The outer shell is rotationally molded to 4–7 mm, cooled, and then a two-part polyurethane foam core is injected at 35–45 kg/m³ core density through pre-molded fill ports. Machine parameters include oven set points of 290–310°C, peak internal air temperature of 210–230°C, and rotational speeds selected to maintain a 4:1 primary-to-secondary ratio with secondary speed not exceeding 6 rpm. Terminal products include 600 L insulated fish boxes, 1,200 mm × 1,000 mm hygienic pallet totes, and 150–300 L ingredient handling containers.

    When Diesel Exhaust Fluid Contact Is Specified for Rotational Molded Polyethylene Sump Reservoirs

    When Diesel Exhaust Fluid contact is specified, the rotomolded structure must avoid contaminating AUS 32 with total organic carbon, basic metal cations, and leached oligomers; material and washing acceptance therefore follow ISO 22241-1:2019 quality requirements and test procedures in ISO 22241-2:2019 for trace elements and total organic carbon. Icorene 3545 GRN 6425 is used in unpainted monolayer sumps; no internal mold release agent is applied because silicone- or metallic stearate releases can raise leachate conductivity, and regrind is limited to 5–10 wt% from fully traceable production batches. The molding process uses passivated aluminum or stainless steel tooling, nitrogen-purge cooling to minimize surface carbonyl formation, and a peak internal air temperature of 190–210°C with wall sections of 3–6 mm for DEF sumps; post-mold leaching is reduced by a 60°C conditioned water flush for 2 h before assembly. Terminal parts include diesel exhaust fluid pump sump reservoirs, dosing cabinet catch basins, and ISO 22241-5 refill neck adapters.

    Application scenarioCore compliance verificationProcess boundary verified on line
    Agricultural chemical tanksISO 16101:2004, ASTM D1998-21Wall thickness 8–12 mm, PIAT 190–210°C
    Playground equipmentASTM F1487-21, EN 1176-1:2017ASTM D4329-21 Cycle A 2,500 h, regrind ≤30 wt%
    Insulated fish boxes21 CFR 177.1520(c), EU 10/2011Shell wall 4–7 mm, foam core 35–45 kg/m³
    DEF sump reservoirsISO 22241-1:2019, ISO 22241-2:2019Regrind 5–10 wt%, wall 3–6 mm
    Secondary containmentEPA 40 CFR 264.175, 40 CFR 112.7Floor plate 6–9 mm, leak test 35–50 kPa
    Park and site furnitureEN 581-1:2017Wall 4–6 mm, regrind ≤20 wt%

    Secondary containment bunds and spill pallet platforms are rotomolded from the LLDPE grade for chemical and electrolyte storage areas. The governing containment capacity follows EPA 40 CFR 264.175, which requires 110% of the largest container volume or 100% for single vessels, with additional SPCC requirements under 40 CFR 112.7 applied at site level. Floor plate thickness is set at 6–9 mm to handle steel drum chime puncture, and pallet sump walls are molded with a 3–5° draft angle to release from shuttle machine tools. Regrind is limited to 25 wt% for general oil-containing sumps and is eliminated when oxidizing acids are to be stored, because reprocessed LLDPE can carry carbonyl groups that accelerate stress crack propagation under residual molding stresses. Production uses shuttle-type rotational molding machines with independently controlled oven and cooling stations, weld-on fittings attached by hot-plate welding at 210–230°C and 0.15–0.30 MPa interface pressure, and leak testing by air pressure differential at 35–50 kPa after assembly. Terminal products include two-drum and four-drum spill pallets, IBC catchment bunds, and rectangular battery rack containment trays.

    Underground Enclosure Cover Pressure Ratings and Cold-Impact Specification

    Park and site furniture components require a sustained balance between cold-weather impact behavior and resistance to surface stress whitening when installed with threaded metal inserts. The parts are specified under EN 581-1:2017 for outdoor furniture safety and stability; for public seating, load tests are conducted on the completed assembly rather than on isolated shells. The rotomolding formulation keeps regrind below 20 wt% in cold-climate configurations to reduce low-temperature crack nucleation at insert bosses, and no additional UV masterbatch is introduced beyond the supplied package unless a non-green color match is required. Molding uses multi-axis carousel tooling with oven set points of 280–300°C, peak internal air temperature of 200–220°C, and wall thickness held between 4 mm and 6 mm to preserve stiffness without raising cooling-time-driven warpage. Terminal products include backless bench shells, table tops, litter ring covers, and planter base rings.

    Free Quote

    Competitive LyondellBasell Icorene 3545 GRN 6425 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 3545 GRN 6425 Polyethylene, Linear Low Density is a green-pigmented linear low-density polyethylene powder formulated for single-layer rotational molding. The product designation separates the base resin identifier 3545 from the controlled color identifier GRN 6425; this separation is process-relevant because the pigment package shifts melt rheology and final part density relative to the natural polymer. The base resin is a copolymer with a published nominal density of 0.934 g/cm³ and a melt flow rate of 4.5 g/10 min under 190°C/2.16 kg as determined by ASTM D1238. The material is supplied as a dry-flow powder with a controlled top size, typically below 500 µm, to support uniform particle packing against the mold wall. Published data specific to the green-pigmented configuration are limited; values presented in the following table refer to the base resin unless the pigmented condition is explicitly identified.

    PropertyStandardNominal value
    DensityASTM D1505 / ISO 1183-10.934 g/cm³
    Melt flow rate, 190°C/2.16 kgASTM D1238 / ISO 1133-14.5 g/10 min
    Tensile yield strength, Type IV, 50 mm/minASTM D63817 MPa
    Tensile elongation at breakASTM D638900%
    Flexural modulus, 1% secantASTM D790550 MPa
    Vicat softening temperature, A/120ASTM D1525117°C
    Brittleness temperatureASTM D746-76°C
    Environmental stress crack resistance, 100% IgepalASTM D1693 Condition A>1000 h

    Specimen preparation for the tensile and flexural values used rotomolded plaques machined to ASTM D638 Type IV geometry. The cooling rate on the tool affects crystallinity; fast cooling at mold surface temperatures below 60°C can reduce flexural modulus by 5–10% relative to slow cooling in still air. Therefore the tabulated values are not intrinsic polymer constants but depend on the thermal history of the test plaque. Rotational molding laboratories commonly prepare flat panels on a cast aluminum mold with a cavity thickness of 3 mm and an oven residence sufficient to reach a peak internal air temperature of 200°C. The environmental stress crack resistance value is based on compression-molded specimens according to ASTM D1693; rotomolded parts can show different failure times depending on wall thickness, inner-surface roughness, and residual stress at the mold surface.

    What Separates Icorene 3545 GRN 6425 from Unpigmented 3545 in Rotational Molding Control?

    The GRN 6425 pigment package is not an inert colorant at the process level. Green inorganic pigments raise complex viscosity and can lower melt flow rate by 3–8% relative to natural Icorene 3545 at equivalent temperature. As a result, a pigmented charge can require a peak internal air temperature increase of 5–10°C or an oven dwell extension of 60–120 s to reach the same degree of interparticulate fusion in wall sections above 4 mm. On production-scale shuttle-type rotational molding machines with a 4:1 arm speed ratio, the viscosity increase also reduces drainage from vertical walls during the first cooling stage, which can suppress pinhole formation but may increase warpage if the part is pulled before the mold surface drops below 80°C. Batch-to-batch variation is most detectable in dry-flow and bulk-density measurements; pigment dispersion quality should be verified by melt filtration or by observing the inner surface of a thin dome test section.

    In single-layer rotational molding, the product is specified for agricultural sprayer tanks, water storage containers, playground components, kayaks, and material handling bins. The core technical justification for selecting this LLDPE over a high-density polyethylene is the combination of low-temperature impact resistance and environmental stress crack resistance measured by ASTM D1693 Condition A; the nominal value exceeds 1000 h in the base resin. This property is critical for tanks that store dilute fertilizer mixtures or surfactant-containing liquids, which can initiate slow crack growth in lower-molecular-weight HDPE rotomolding grades. The green coloration of GRN 6425 is used in outdoor recreational equipment and industrial enclosures where a dark green finish is specified or where the pigment package contributes to ultraviolet screening in combination with the grade’s light stabilizer package. Food-contact status is not automatically conferred by the base polymer classification under 21 CFR 177.1520; the green pigment package must be cleared for the specific end-use article. Tanks produced from this grade can be evaluated under ASTM D1998 for polyethylene upright storage tanks, but long-term hydrostatic design basis is application-specific.

    Processing Window, Particle Size Distribution, and Moisture Constraints in Single-Layer Rotational Molding

    For this powder, the practical processing window is controlled by the interaction of oven setpoint, peak internal air temperature, and wall thickness. Oven setpoints of 260–300°C are common, with the peak internal air temperature maintained at 195–205°C for unfilled sections up to 6 mm. Below 190°C, the compacted powder layer fuses incompletely, leaving a rough inner surface and subsurface voids that reduce impact toughness. Above 210°C, thermo-oxidative scission accelerates; the outer skin develops discoloration and tensile elongation decreases measurably. The allowable variation around the target peak internal air temperature is therefore no more than ±5°C for load-bearing parts. Powder moisture should be held below 0.1% by weight; higher free moisture creates steam porosity at the parting line where the powder charge is thickest. On carousel-type machines with a 1.5 m swing radius, primary-axis rotation speeds of 6–10 rpm and secondary-axis speeds of 1.2–2.0 rpm are typical for this density; excessive primary-axis speed can collapse the tumbling powder pool and generate wall-thickness gradients in box-shaped tooling. Regrind should be screened through a 35-mesh sieve, with retention held below 5% of charge weight; fines above this threshold inhibit bulk flow and can create unmelted agglomerates in deep cavities. Particle size distribution is a stronger predictor of surface finish than average particle size alone. A powder with a narrow distribution between 150 µm and 425 µm packs more uniformly than a broad distribution with excessive fines below 75 µm; the latter increases bubble entrapment because fine particles sinter early and prevent air escape. A top size exceeding 500 µm requires longer oven residence to completely melt the largest grains and can leave visible orange-peel texture on the outer surface.

    Rotational molding grades are evaluated by zero-shear viscosity at 190°C and by sag resistance of a laboratory plaque heated to 210°C. The base resin has a zero-shear viscosity typical of a 4.5-g/10-min LLDPE; this is low enough to promote particle coalescence but high enough to prevent excessive sag on flat tooling. The green-pigmented version shows a slightly higher zero-shear viscosity, which reduces sag but requires longer sintering time. Molders should verify that the oven atmosphere does not exceed 350°C, because radiative heat from the oven walls can degrade the exposed powder layer before the bulk reaches peak internal air temperature.

    Relative to a 0.940 g/cm³ LLDPE rotomolding grade, this product has a lower flexural modulus and better low-temperature impact; compared with a 0.926 g/cm³ LLDPE grade, it has higher stiffness and slower sintering. Its base resin is therefore positioned as a medium-density LLDPE for parts that must balance stiffness, chemical resistance, and freeze-thaw durability without moving to crosslinked high-density polyethylene or a high-flow grade. The compounded green GRN 6425 version is also distinct from natural Icorene 3545 dry-blended with on-site pigments. Precompounded green gives tighter lot-to-lot color consistency—submitted injection-molded plaques typically show CIELAB ΔE*ab variation of ≤0.5—while manual dry coloring in a rotational molding shop can vary by more than 1.0 ΔE*ab across a shift. The precompounded product eliminates dry pigment dust, reduces housekeeping exposure, and avoids the variable melt-flow shift caused by uncontrolled pigment addition at the molding machine.

    The grade is compatible with dilute mineral acids, alkali solutions, and many agricultural chemicals at ambient temperature, but strong oxidizing acids, aromatic hydrocarbons, and chlorinated solvents can cause swelling or stress cracking. Chemical resistance should be validated using ASTM D543 immersion testing on rotomolded plaques at the actual service temperature, not extrapolated from high-density polyethylene data. For diesel or fuel storage, the product is not a substitute for a fluorination-treated or polyamide-containing barrier layer.

    For Wall Sections Exceeding 8 mm, Internal Air Temperature Probes Are Mandatory

    Thick-wall processing changes the heat transfer bottleneck from the mold surface to the polymer core. A nominal 10 mm wall can require 20–30% longer oven dwell than a 5 mm wall, and the peak internal air temperature at the core can lag the mold surface by 8–12°C during heating. If oven timers are used without an internal air probe, the inner wall may remain below the sintering threshold while the outer skin begins to oxidize. Field data from forced-air shuttle machines show that wall thickness variation around a corner can exceed 15% when the mold is not indexed for uniform heat exposure; the powder pool spreads unevenly across vertical ribs, and the inner wall may read below 200°C even though the mold surface thermocouple is above 200°C. For parts with nominal wall above 8 mm, and for any structure that must survive a specified −40°C impact or hydrostatic test under ASTM D1998, an internal air temperature probe is specified as a process control.

    Measuring Oxidative Induction Time After Multiple Regrind Cycles

    Regrind streams in rotational molding can deplete the thermal stabilizer package and reduce long-term service life. Oxidative induction time by ASTM D3895 at 200°C is used to monitor the remaining stabilizer after each heat history. A first-pass part may show an OIT above 20 min, while the same material after three regrind cycles at 285°C may fall below 10 min, indicating that additional stabilizer masterbatch is needed before the regrind fraction exceeds 20% of the charge weight. Blending more than 30% regrind without OIT verification can produce brittle failures in chemical tanks after one outdoor season. For accelerated weathering, the pigmented product should be assessed under ASTM G154 or ISO 4892-2, because some organic green pigments shift shade or fade more rapidly than carbon black or titanium dioxide systems. The weathering response is a function of the full stabilization package, not the pigment alone.

    The material’s operational boundaries include a moisture limit of 0.1%, storage below 50°C away from direct sunlight, and avoidance of blending with amine-based flame-retardant additives that can deactivate phenolic antioxidants and produce yellowing. Continuous load-bearing service above 60°C is not recommended because creep modulus declines with temperature and the part may deform under hydrostatic load. Published data specific to the green-pigmented configuration for food-contact status, ultraviolet rating, and long-term hydrostatic strength are limited; project-specific qualification is required before use in applications governed by NSF/ANSI 61, ASTM D1998, or regional drinking-water directives.