| HS Code | 719445 |
| Density | 0.935 g/cm³ |
| Meltflowrate | 3.5 g/10 min |
| Tensilestrengthatyield | 14 MPa |
| Tensilestrengthatbreak | 24 MPa |
| Elongationatbreak | 800% |
| Flexuralmodulus | 550 MPa |
| Hardnessshored | 55 |
| Vicatsofteningpoint | 115 °C |
| Meltingpoint | 125 °C |
| Thermalexpansioncoefficient | 1.5E-4 1/°C |
| Specificheatcapacity | 2.0 J/g·°C |
| Thermalconductivity | 0.35 W/m·K |
| Dielectricconstant | 2.3 |
| Volumeresistivity | 1E15 ohm·cm |
| Dielectricstrength | 20 kV/mm |
| Waterabsorption | 0.01% |
| Oxygenindex | 17% |
| Linearmoldshrinkage | 0.020 cm/cm |
As an accredited LyondellBasell Icorene 3545 GRN 6421 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 3545 GRN 6421 Linear Low Density Polyethylene supplied in 25 kg polyethylene bags, palletized and stretch-wrapped. |
| Container Loading (20′ FCL) | LyondellBasell Icorene 3545 GRN 6421 LLDPE: 20′ FCL, 25 kg bags, palletized, stretch-wrapped; approx. 18–20 pallets, 18–20 MT net, securely strapped. |
| Shipping | LyondellBasell Icorene 3545 GRN 6421 Polyethylene, Linear Low Density is a non-hazardous, non-regulated solid resin. Ship in original sealed bags, octabins, or bulk containers. Protect from moisture, heat, sunlight, and contamination. No UN number, hazard class, or transport label required. Store cool and dry. |
| Storage | Store LyondellBasell Icorene 3545 GRN 6421 Polyethylene, Linear Low Density, in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and incompatible materials. Keep original containers sealed and palletized to prevent moisture, dust, and contamination. Avoid excessive stacking, prolonged UV exposure, and rough handling. Follow local regulations and supplier storage recommendations. Use first-in, first-out stock rotation. |
| Shelf Life | Recommended shelf life is 24 months when stored in original unopened packaging, dry, cool, and away from direct sunlight. |
During rotomolding of vertical agricultural chemical storage tanks in the 1,000–15,000 L class, the pre-colored green 6421 system removes a separate pigment dispersion step, shifting process control to pulverizer screen condition, charge blending time, and peak internal air temperature repeatability. The powder is charged through a 35-mesh (500 µm) sieve after ambient disc pulverization and dry-blended with reground flash in a low-shear ribbon blender for not less than 15 min; this prevents particle size segregation that otherwise appears as localized thinning at the lower knuckle radius. Compliance for stationary above-ground polyethylene tanks is evaluated under ASTM D1998-15, and where the vessel is certified as a transport IBC, UN 31H1 with ADR/RID 6.5 is applied; environmental stress crack resistance is checked per ASTM D1693 Condition B in 100% Igepal CO-630 at 50 °C, and oxidation induction time is measured per ISO 11357-6 at 200 °C in oxygen. Formulation addition ratio is 100 wt% of this pre-colored compound for certified first-life shells; internally generated flash regrind is permitted at 20–30 wt% maximum, provided the regrind is re-sieved and the melt flow rate of the blend is verified at 190 °C/2.16 kg against ISO 1133-1:2022. The production process on a double-shuttle rotomolder uses an oven set point of 280–300 °C, a peak internal air temperature of 190–200 °C, a biaxial rotation ratio of 4:1, forced-air cooling to 85 °C, and demolding at 60 °C; water mist is introduced only after the shell has fallen below 100 °C to limit warpage at the flanged manway. Terminal product types include vertical storage tanks, secondary containment basins, sprayer sumps, and conical-bottom static mix tanks for crop protection formulations.
Rotational molding of outdoor playground panels and recreational components from this green linear low-density grade places a premium on low-temperature ductility and accelerated weathering response. The pre-pigmented 6421 system is charged at 100 wt% for load-bearing shells; granulated flash regrind is re-inserted at 15–20 wt% maximum after 35-mesh screening, because higher regrind fractions have been observed on multi-arm carousel machines to produce void concentrations at edge radii where nominal wall thickness falls below 3 mm. Compliance is assessed under EN 1176-1:2017 for playground equipment and EN ISO 4892-2 with UVA-340 lamps for weathering; Charpy notched impact is measured per ISO 179-1 at −30 °C, and falling-weight multiaxial impact is tested according to ASTM D3763 on flat specimens cut from the sidewall. Addition ratio when external properties are modified: no external color concentrate is required; if flame-retardant or antistatic masterbatch is requested, the addition is limited to 2–5 wt%, which predictably lowers Charpy notched impact and must be re-validated before serial production. The process uses clamshell or shuttle machines with PTFE-coated aluminum molds, oven temperature 300–315 °C, peak internal air temperature 205 °C, rotation ratio 4.5:1, and forced-air cooling to 70 °C; mold release is applied at 0.8–1.2 g/m² per coat to avoid surface defects on textured panels. Terminal product types include slide hoods, modular tunnel sections, climbing feature components, and rotationally molded outdoor play shells.
Historically, rainwater harvesting tanks and reserve storage bodies have been molded from natural polyethylene, but green-tinted 6421-filled systems are used for non-potable irrigation and greywater storage where light infiltration must be minimized. The compound is fed as a dry powder with a melt flow rate in the rotomolding window near 4.5 g/10 min at 190 °C/2.16 kg when measured by ISO 1133-1:2022; batch-to-batch MFR variation is specified within ±0.5 g/10 min to maintain consistent wall thickness distribution. Compliance for rainwater harvesting systems is evaluated under EN 16941-1:2018 and BS 8515:2009; fabricated thermoplastic tanks are assessed under EN 12573-1:2000, and buried tanks are subjected to long-term hydrostatic strength regression testing according to ISO 9080. Formulation addition ratio is 100 wt% virgin compound for single-layer cylindrical shells; clean in-house regrind may be incorporated at 25 wt% maximum, and if additional black masterbatch is required for opacity, its addition is held at 1.0–2.5 wt% to avoid a measurable drop in ESCR. Production on a rock-and-roll rotomolder for vessels above 3,000 L uses oven temperatures of 290–320 °C, peak internal air temperature of 195–205 °C, rotation ratio 4:1, and controlled air cooling to 80 °C before water fogging; unmonitored cooling can distort the lid flange beyond ±2 mm on diameters over 1,600 mm. Terminal product types include non-potable irrigation tanks, greywater holding tanks, and underground rainwater collection cisterns.
For marine buoy shells and floating dock floats, the saturated hydrocarbon backbone of this linear low-density compound provides resistance to hydrolysis and a water absorption value below 0.02% after 24 h immersion when tested per ASTM D570; the practical design limit is not water uptake but slow crack growth under repeated flexure caused by wave loading. Compliance is evaluated under ISO 1183-1:2019 for density, ASTM D570 for water absorption, ISO 178 for flexural modulus, and ISO 179-1 for Charpy notched impact at −20 °C; long-term creep is screened by ISO 899-2 at 23 °C/1,000 h, though published data for this specific pre-colored 6421 configuration is limited and vessel-specific validation is required. Formulation addition ratio is 100 wt% for the outer shell; regrind is not recommended above 10–15 wt% in the submerged half of the mold because low-temperature crack propagation has been observed along the mold parting line when regrind particles are inadequately fused. The process uses a carousel rotomolder with a two-piece mold, oven temperature 290–310 °C, peak internal air temperature 195 °C, rotation ratio 4:1, and post-mold cooling jigs to hold the part at 70 °C during solidification; rotational speed variation should remain within ±0.5 rpm to avoid asymmetric wall distribution. Terminal product types include mooring buoys, floating dock segments, and pontoon flotation elements.
Where processors retain the foam-filled double-wall construction for insulated fish tubs and cold-chain distribution containers, the grade serves as the outer thermoplastic skin because its rotomolding melt flow enables uniform coalescence in deep draw areas. Food-contact compliance is evaluated under FDA 21 CFR 177.1520 for olefin polymers and EU 10/2011 with overall migration testing in 10% ethanol and 3% acetic acid; cold-temperature impact retention is checked per ASTM D1790 at −40 °C. Formulation addition ratio is 100 wt% for both inner and outer skins; if regrind is used, it is limited to 15 wt% and placed only in the outer skin, because the inner skin requires unimpaired ESCR during repeated washdown with quaternary ammonium sanitizers. The process is a two-stage rotomolding sequence: the outer skin is molded at 285–310 °C oven temperature with peak internal air temperature 195 °C, then the cavity is filled with a rigid polyurethane foam system at 0.35–0.45 MPa internal pressure before the inner skin is fused; cooling is slowed to 2 °C/min between 120 °C and 60 °C to reduce shrinkage anisotropy. Terminal product types include insulated fish tubs, food cold-chain pallet boxes, and temperature-controlled distribution containers for seafood processing lines.
The absence of a defined molecular orientation in rotationally molded parts of this grade places the flexural modulus in the range of 500–700 MPa when measured on 4 mm plaques per ISO 178, and tensile yield in the range of 15–20 MPa per ISO 527-2; these values are used to design fastening bosses for stable panels. Chemical resistance is screened by ISO 175 after 7-day immersion in 10% citric acid and 5% sodium hypochlorite solutions, and food-contact-capable grades are referenced to Regulation (EC) 1935/2004 and FDA 21 CFR 177.1520. Formulation addition ratio is 100 wt% pre-colored compound for the first-pass shell; washed and dried regrind is limited to 20 wt% maximum because surface pinholes form at higher concentrations when powder particles carry residual sanitizer or moisture. The process uses rotomolding equipment with oven temperature 285–300 °C, peak internal air temperature 190 °C, rotation ratio 4:1, and forced-air cooling to 65 °C; flame treatment is not applied before demolding, and cooling jigs are used on flat stable panel sections to hold flatness within ±1.5 mm per linear meter. Terminal product types include horticultural trays, animal feed troughs, equine stable wall panels, and farrowing pen dividers.
Competitive LyondellBasell Icorene 3545 GRN 6421 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 3545 GRN 6421 is a linear low-density polyethylene powder supplied for rotational moulding applications. The base resin, identified by the grade designation Icorene 3545, is an LLDPE copolymer with a controlled density of 0.934–0.936 g/cm³ and a melt flow rate of 4.5–5.5 g/10 min measured at 190°C/2.16 kg according to ISO 1133-1:2022. The suffix GRN 6421 identifies a green pigmentation package and possible stabiliser formulation; because the exact pigment loading and carrier concentrate are lot-level variables, the supplier’s co-certificate for the pigmented lot is the controlling specification. The material is used in rotational moulding of water storage tanks, agricultural chemical hoppers, industrial material handling bins, outdoor enclosures, and playground structures. In these applications the powder is charged at ambient temperature onto biaxial rotational moulding equipment, and its dry flow, bulk density, and particle size distribution support reproducible wall thickness in deep ribs and closed cavities. Published data for the unpigmented base resin typically list tensile stress at yield from 16–18 MPa, tensile strain at break above 750%, flexural modulus between 600–700 MPa, and environmental stress crack resistance above 1000 h when evaluated under ASTM D1693 Condition B in 100% Igepal. The polymer melting peak determined by differential scanning calorimetry according to ISO 11357-3 is commonly reported between 122°C and 128°C, while the Vicat softening temperature A50 is typically 116–120°C under ISO 306. These values are generated on compression-moulded or rotomoulded specimens and do not automatically transfer to finished part geometry; weld lines, internal cooling rate, mould release residue, and local wall thickness each shift the final mechanical response.
Lot verification for Icorene 3545 GRN 6421 should include melt mass-flow rate under ISO 1133-1:2022, density under ISO 1183-1 or ASTM D1505, and environmental stress crack resistance under ASTM D1693 Condition B. For outdoor service, low-temperature impact should be evaluated using ISO 6603-2 or ASTM D746, and notched impact resistance should be measured according to ISO 180 or ASTM D256. These coupon tests describe the material under a particular thermal history; they do not by themselves predict the performance of a green-pigmented rotomoulded tank after years of ultraviolet exposure. Outdoor weathering depends on the pigment and stabiliser package. The supplier’s weathering data for the GRN 6421 system should be reviewed rather than assuming that natural or black-pigmented grades transfer directly. A lot-specific certificate of analysis may report density in the range 0.934–0.936 g/cm³, nominal MFR close to 5.0 g/10 min, and elongation at break above 750%. These values should be read as production envelopes, not guaranteed finished part properties, because laboratory specimen preparation differs from the slow unpressurised cooling of a 6–10 mm rotomoulded wall. For finished tanks, ASTM D1998 is often applied to polyethylene upright storage tanks; hydrostatic test pressure, wall thickness verification, and inspection of weld areas provide more direct acceptance evidence than coupon data alone. Potable water and food-contact suitability must be documented for the pigmented formulation. A manufacturer may supply declarations under EU Regulation 10/2011, FDA 21 CFR 177.1520, or NSF/ANSI 61, but the green pigment system must be included in the submitted formulation.
| Verification item | Standard designation | Typical target or note |
|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | 4.5–5.5 g/10 min |
| Density | ISO 1183-1 / ASTM D1505 | 0.934–0.936 g/cm³ |
| Tensile strain at break | ISO 527-2 / ASTM D638 | >750% |
| Flexural modulus | ISO 178 / ASTM D790 | 600–700 MPa |
| Environmental stress crack resistance | ASTM D1693 Condition B | >1000 h |
| Low-temperature brittleness | ASTM D746 | <-70°C |
| Food-contact suitability | FDA 21 CFR 177.1520 | Lot-specific declaration required |
| EU food-contact compliance | EU Regulation 10/2011 | Pigmented formulation to be verified |
| Potable water contact | NSF/ANSI 61 | Finished component testing commonly required |
| Accelerated weathering | ISO 4892-2 / ASTM D2565 | Colour retention and retained elongation for green grade |
Production-scale rotational moulding lines processing Icorene 3545 GRN 6421 typically operate with oven air temperatures between 260°C and 300°C. The tool rotates biaxially at a rotation ratio of 4:1 to 6:1, and the powder bed temperature is monitored by an internal air probe. The target peak internal air temperature is commonly between 190°C and 210°C, although the optimum depends on wall thickness, mould metal, oven efficiency, and ambient plant temperature. A fixed residence time is less repeatable than PIAT measurement because heat transfer varies with tool steel thickness and heating capacity. A part removed too early, below 180°C internal air temperature, may contain unfused powder, microvoids, low ESCR, and reduced tensile elongation. An overheated cycle above 230°C PIAT accelerates thermo-oxidative chain scission and may lower impact resistance; the green pigment can darken or shift in hue. For thick walls of 10 mm and greater, a lower initial oven temperature and longer soak time are preferred because a high heat flux at the outer wall can oxidise polyethylene near the mould surface before the inner powder reaches fusion temperature. Moulders record mould surface temperature at demoulding as a secondary control point. The pigmented grade may absorb infrared radiation differently from natural powder, so oven settings, residence time, and PIAT should be re-established after every pigment lot change. Powder storage should remain below 60% relative humidity. Moisture condensation on cold powder reduces dry flow and contributes to steam-induced porosity; if condensation is visible, the powder can be dried at 70°C for 1–2 h in a dehumidified hopper. Polyolefin moisture absorption is low, so the concern is surface condensation rather than bulk moisture uptake.
Powder handling has a direct effect on part quality. The bulk density of a rotational moulding LLDPE powder typically falls between 0.30–0.40 g/cm³, and dry flow time through a standard funnel should be controlled to maintain reproducible cavity filling. Excessive fines may produce local overheating and pinholes; excessive coarse particles may starve narrow ribs. The green pigmentation can shift bulk density and dry flow by several percent. Moulders should measure bulk density under ISO 60 and dry flow under ASTM D1895 on each incoming lot. These measurements do not replace melt flow rate or density but provide early warning of handling changes. If the powder is pneumatically conveyed, segregation can occur; the sample used for quality release should be taken at the charging point rather than from the top of a silo. The melt rheology of the base LLDPE also governs bubble removal and knitting. The single-point MFR measured at 190°C/2.16 kg under ISO 1133-1:2022 does not define the full low-shear viscoelastic response relevant to rotational moulding. Rotational moulding powders are stabilised to withstand long oven cycles, but the stabiliser is depleted by repeated regrind use. Blending regrind of the green compound with virgin powder is common; however, regrind should generally be limited to 20% in thin-wall parts and 10% in maximum-ESCR applications. The permissible level depends on previous heat history and should be confirmed by retained elongation after moulding.
Air cooling and water cooling produce different part properties. Water mist or air-water cooling reduces cycle time and warpage but can increase internal residual stress and reduce ESCR at the inner surface. For large flat panels, a two-stage cooling cycle beginning with 2–4 min of air cooling followed by mist cooling at 30–50°C is often used to balance dimensional stability and mechanical integrity. Demoulding temperature also influences warpage: parts removed while the polymer is still soft may deform under their own weight, while parts left too long in a rigid steel mould can shrink onto cores and create local stress. Waxes and silicone-based release agents are effective, but excessive film prevents welding and coating adhesion in post-moulding operations. The green surface can conceal visual evidence of oxidation or pigment migration, so destructive sampling of the moulded part is recommended during process qualification. Tooling design affects material performance more than a datasheet value. In rotational moulding, tight radii, sharp corners, and deep ribs create thin-wall zones that cool faster and may retain higher internal stress. A radius-to-wall-thickness ratio below 1:1 can promote bridging and unfused corners; ratios between 1.5:1 and 2:1 are common for LLDPE powders in tank moulds. Venting must be provided to prevent compressed air from distorting soft inner surfaces, and vents should be sized to avoid powder loss while allowing gas exchange. These tooling requirements are not altered by the green compound, but pigment separation and flow lines may become more visible if the mould is underfilled or contaminated.
Replacing a high-density polyethylene rotational moulding powder with Icorene 3545 GRN 6421 changes stiffness, ESCR, and low-temperature behaviour. A generic HDPE rotomoulding grade with a density of 0.945–0.955 g/cm³ may provide flexural modulus values from 800–1200 MPa, while the lower-density LLDPE base of Icorene 3545 typically sits in the 600–700 MPa range. This stiffness reduction is acceptable only if the part design accounts for deformation under hydrostatic load. The advantage appears in environmental stress crack resistance and ductility: LLDPE grades with the 3545 profile often exceed 1000 h under ASTM D1693 Condition B, whereas many HDPE rotomoulding grades fall into the 50–500 h range under the same condition. At low temperatures, LLDPE generally retains ductility better than HDPE, but the green pigment may modify this behaviour; lot-specific impact data should be obtained. A standard LDPE rotomoulding grade at 0.920–0.930 g/cm³ typically provides lower flexural modulus and lower compressive strength, making the 3545 product a middle-ground choice for tanks requiring both stiffness and crack resistance. Compared with metallocene-catalysed LLDPE rotomoulding powders, Icorene 3545 may offer wider processing latitude on older machines with less precise temperature control while giving up some low-temperature impact performance; published head-to-head data for the specific green configuration is limited. This balance leads to its use in medium-sized vertical tanks, chemical storage vessels, and outdoor housings where continuous hydrostatic stress and weathering are expected. Design calculations should use the lower bound of the property envelope and include a weld factor and a stress concentration factor for metallic inserts.
Outdoor service of a green LLDPE moulded part requires more than colour fastness. Accelerated weathering according to ISO 4892-2 or ASTM D2565 may report Delta-E colour shift, but retained elongation after exposure is the property that indicates polymer degradation. Surface oxidation can be measured by carbonyl index using infrared spectroscopy; an increase in carbonyl index often precedes loss of tensile elongation. For long-term outdoor tank service, the specifier should therefore require retained elongation and ESCR after weathering, not only a colour change limit. The green pigmentation may provide better colour retention than natural or white material, but colour retention does not automatically imply mechanical retention. Migration kinetics in the polymer matrix become relevant for food-contact and toy applications; organic pigments and process aids can migrate slowly under high-temperature contact conditions, and the supplier should provide migration data for the final green formulation if the part is used under EU Regulation 10/2011 or FDA 21 CFR 177.1520.
Chemical compatibility limits follow standard linear low-density polyethylene behaviour. The base polymer resists aqueous acids, alkalis, and salt solutions at ambient temperature but is softened by aromatic solvents, chlorinated hydrocarbons, and some aliphatic hydrocarbons at elevated temperatures. Strong oxidising acids, including concentrated nitric acid, can initiate stress cracking. Immersion testing under ASTM D543 can measure mass and dimensional change after chemical exposure, but property retention should be verified on rotomoulded specimens because compression-moulded coupons have different crystallinity and residual stress. In potable water applications, migration testing under EU Regulation 10/2011 or extraction testing under NSF/ANSI 61 is product-specific, and the green pigment system must be included in the submitted formulation. A REACH declaration may be requested in Europe to confirm that only registered monomers and additives are present. In electrical or electronic applications, a RoHS 2011/65/EU statement should be obtained from the supplier. The material is an olefinic polyolefin and generally contains no phthalate plasticisers or halogenated flame retardants. Weld joints in fabricated assemblies should be made with a compatible LLDPE filler rod from the same colour lot or with a natural grade accepted by the supplier. Weld strength depends on hot-gas temperature, speed, and surface preparation; EN 13067 and ISO 13920 provide guidance for plastics welding but are not direct material property specifications. Because published data for the specific GRN 6421 compounded configuration is limited in the public literature, design load, chemical exposure, and wall thickness should be confirmed with lot-specific manufacturer data before production tooling is cut.