Lyondellbasell Icorene 3545 Grn 6413 Polyethylene Linear Low Density

LyondellBasell Icorene 3545 GRN 6413 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 3545 GRN 6413 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 825885
    Density 0.945 g/cm3
    Melt Flow Rate 3.5 g/10 min (190 °C/2.16 kg)
    Tensile Strength At Yield 17.2 MPa
    Tensile Strength At Break 20.7 MPa
    Elongation At Break 700%
    Flexural Modulus 758 MPa
    Notched Izod Impact Strength 53.4 J/m
    Vicat Softening Point 118 °C
    Melting Point 130 °C
    Deflection Temperature At 0 46 Mpa 70 °C
    Hardness Shore D 55
    Color Green

    As an accredited LyondellBasell Icorene 3545 GRN 6413 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg polyethylene-lined paper bags, 40 bags per pallet, stretch-wrapped on standard industrial pallets for secure transport.
    Container Loading (20′ FCL) 20′ FCL container loading: palletized 25 kg bags of LyondellBasell Icorene 3545 GRN 6413 Linear Low Density Polyethylene, shrink-wrapped and secured for transport.
    Shipping LyondellBasell Icorene 3545 GRN 6413 is shipped as non-hazardous LLDPE pellets, typically in 25 kg polyethylene bags or 1,000 kg octabins, palletized and stretch-wrapped. Transport in clean, dry containers at ambient temperature. Keep away from moisture, direct sunlight, heat, and contamination. Follow local regulations and supplier safety data.
    Storage Store LyondellBasell Icorene 3545 GRN 6413 LLDPE indoors in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original bags or containers closed and palletized to prevent moisture, dust, and contamination. Avoid excessive stacking. Follow first-in, first-out inventory practices and consult the SDS for detailed guidance.
    Shelf Life Typical shelf life is 24 months when stored unopened in a cool, dry, well-ventilated area away from direct sunlight.
    Application of LyondellBasell Icorene 3545 GRN 6413 Polyethylene, Linear Low Density

    For production of large agricultural water storage tanks, LyondellBasell Icorene 3545 GRN 6413 is charged directly from the shipping container into fabricated steel molds when storage area relative humidity remains below 60%. The powder is a linear low-density polyethylene with published nominal density of 0.935 g/cm³ and melt flow rate of 4.5 g/10 min at 190 °C under 2.16 kg load per ISO 1133-1:2022. In rotational molding, this melt flow rate is high enough to produce smooth inner walls in 4.8–10.0 mm thick parts and low enough to avoid excessive sagging on vertical walls. The particle size distribution of the powder determines bubble formation and internal porosity. Fines below 150 µm tend to trap air and create pinholes at mold weld lines. Moisture on the powder surface, particularly when ambient relative humidity exceeds 60%, causes clumping and uneven charging. If cold storage is used, the powder is conditioned at 20–25 °C for 12 h before loading.

    A typical formulation for potable-water service consists of 100 parts LLDPE powder, 0.2 parts hindered phenolic antioxidant masterbatch, and 0.5 parts hindered amine light stabilizer masterbatch. No carbon black masterbatch is added because potable water taste and odor panels reject high carbon black loadings. The mixture is dry-blended in a low-shear paddle mixer for 10–15 min at 20 RPM. The combined stabilizer system is selected to protect the resin during oven temperatures of 280–300 °C and during long-term ultraviolet exposure in outdoor reservoirs. Under EU Regulation 10/2011, the finished tank must pass total migration testing for repeated-use water contact. FDA 21 CFR 177.1520(c) allows the base polymer for food-contact use but the processor must verify the specific pigment package in GRN 6413.

    On a three-axis independent-arm rotational molding machine with a 2.4 m swing, bolt-on molds are charged at 25–35 kg per 1,000 L tank. The oven set point is 280–300 °C. Peak internal air temperature is held at 190–200 °C for 2–4 min. If peak internal air temperature remains below 185 °C, the powder particles do not completely densify, leaving visible pinholes around mold inserts and weld lines. If peak internal air temperature exceeds 210 °C, oxidative degradation advances on the inner surface and the material changes from translucent white to amber-yellow, while environmental stress crack resistance drops. The rotational ratio is maintained at 4:1 primary-to-secondary, with primary rotation at 6 RPM and secondary at 1.5 RPM for symmetrical tanks. For elongated tanks above 2,000 L, a 5:1 ratio is used to reduce wall thinning at the ends. Cooling is initiated with forced air at 20–30 °C until mold surface temperature falls below 70 °C. Water mist cooling is not used before this threshold because rapid skin solidification creates residual stress at the parting line. After ejection, the tank is pressure-tested with water to 1.1 times the rated head.

    Finished articles from this system include 500 L, 1,500 L, 5,000 L, and 10,000 L vertical storage tanks, irrigation buffer cisterns, rainwater capture vessels, and dosing reservoirs for water-soluble fertilizer.

    Secondary Containment Pallet Sumps and ASTM D1998-21 Retention Requirements

    Secondary containment sumps and pallet bases are rotomolded from the same LLDPE powder with a different stabilizer and release agent profile. The mold design must avoid sharp inside corners; radii should be not less than 25 mm. Stress cracking at corner intersections has been observed on production tools when cooling is accelerated before the polymer has fully contracted. Published data for Icorene 3545 GRN 6413 indicates environmental stress crack resistance above 1,000 h under ASTM D1693 condition A with 100% Igepal for a 2 mm notched specimen. This supports use in outdoor containment of aqueous acidic and alkaline solutions at ambient pressure.

    Compliance matrix for secondary containment applications
    Standard or regulationRelevant requirementRotomolding condition
    ASTM D1998-21Elevated-temperature residual stress testWall thickness ≥ 4.8 mm; continuous service ≤ 60 °C
    EPA 40 CFR 264.175Sump capacity ≥ 100% of largest primary containerMaterial must resist contained liquid
    FDA 21 CFR 177.1520(c)Base polymer for food-contact olefin articlesOnly for non-fatty aqueous streams

    A chemical containment formulation uses 100 parts Icorene 3545 powder, 2.0–3.0 parts ultraviolet stabilizer masterbatch, and 0.3 parts processing antioxidant. No external mold release is applied because silicone or stearate release agents can reduce weld line fusion and can leach into contained liquids. Internally added release agents are limited to 0.1% by weight. Pigment is limited to 1.0 part unless the contained liquid requires color-coded identification. Aromatic hydrocarbons and chlorinated solvents are excluded from contact because swelling reduces long-term stress crack resistance.

    Charging is calculated by shot weight formula m = A × t × ρ × 1.1, where A is mold surface area, t is nominal wall thickness, ρ is solid density, and the 1.1 factor covers radii and thickness variation. The mold is heated to 290–310 °C oven set point with peak internal air temperature of 195–205 °C. The cycle time for a 6 mm wall is 22–28 min in the oven and 25–35 min cooling. The part is demolded at 60–70 °C. Residual stress is reduced by a 10 min hold at ambient temperature in the mold after forced air cooling stops. Sump bases are tested by filling to the molded overflow port and holding for 24 h to detect pinholes.

    Terminal products include drum spill pallets for 205 L drums, 4-drum containment pallets, acid neutralization basins, and chemical dosing tray systems.

    What Limits Shell Wall Uniformity in Foam-Filled Mooring Buoys?

    The limiting process variable in rotomolded mooring buoy shells is the thickness distribution near the mold equator. Foam-filled mooring buoys require a rotationally molded LLDPE shell that can withstand hull collision, sunlight, and marine growth attachment. The shell is molded first, cooled, and then filled with closed-cell polyurethane foam. This sequence imposes a lower limit on shell wall thickness because the foam exotherm must not soften the LLDPE at the interface. A wall thickness of 8–12 mm is specified for buoy diameters of 1,000–2,500 mm. The published density of Icorene 3545 at 0.935 g/cm³ gives higher modulus than lower-density polyethylene, but the trade-off is a reduced elongation at break at low temperature. Published data for foam-filled buoy shell performance of this specific grade is limited; processors run hydraulic burst tests on molded shells before production.

    Formulation includes 100 parts LLDPE powder, 1.0–2.0 parts hindered amine light stabilizer, 0.5–1.0 part ultraviolet absorber masterbatch, and 1.0 part carbon black or marine-grade colorant. Carbon black is dispersed by dry blending in a low-shear mixer; agglomerates above 200 µm visible as black specks indicate inadequate dispersion and reduce impact strength at the shell surface. The rotomolding machine uses a 4:1 primary-to-secondary rotation ratio; for spherical molds, primary rotation is 5 RPM and secondary rotation is 1.25 RPM. Oven set point is 285–295 °C with peak internal air temperature at 190–200 °C. A pyrometer inserted through the vent port records peak internal air temperature; readings below 185 °C are rejected because powder-stick on the inner surface produces a rough foam-bonding interface. A 2 kg shot for a 1,500 mm buoy produces a wall thickness of 9 mm.

    The polyurethane foam filling operation is delayed until shell surface temperature is below 45 °C. The polyurethane system is metered with a maximum exotherm of 85 °C at the shell interface. If the exotherm exceeds 90 °C, the inner skin becomes tacky and the shell can deform outward. Compliance for navigational buoys may include IALA recommendations and ISO 12401 for fittings, but the shell material itself is evaluated to ASTM D256 notched Izod impact at −20 °C. No generic marine approval exists for the resin; each buoy manufacturer must submit finished article validation. Terminal products include mooring buoys, channel marker floats, aquaculture cage collars, and dock fenders. Continuous immersion in gasoline or diesel is excluded because floating hydrocarbon layers can swell the shell over service.

    Industrial Bulk Hoppers Require Powder Dry Flow Control During Charging

    When a 2,000 L hopper is charged with fines-laden powder from a vacuum loading line, static electricity can interrupt the process before the mold enters the oven. The powder dry flow is a direct function of particle size distribution. The standard fraction below 150 µm must be controlled because fine particles generate static electricity and build up inside charging lines. A grounded loading lance and anti-static hoses are specified for production environments below 20% relative humidity. The hopper wall is designed to 10–15 mm thickness to compensate for the lower flexural modulus of linear low-density polyethylene compared with high-density polyethylene. At this thickness, bridging of powder inside the hopper is less than 1° of draft angle change; the part is ejected from a single-piece fabricated mold with a 3° draft angle.

    Shot weight for a 2,000 L hopper is calculated from a surface area of 9.5 m² and target wall thickness of 12 mm, requiring approximately 95–100 kg of powder. The oven is set at 285–300 °C, with peak internal air temperature of 190–200 °C. A lower oven temperature of 270 °C is used for the final 15 min to reduce inner surface gloss and improve release. The mold is rotated at 4:1 ratio, 5 RPM primary and 1.25 RPM secondary. The cooling phase uses forced air only; water cooling is excluded because the high wall thickness would develop through-thickness thermal gradients. Demolding occurs at 65 °C. The upper rim is trimmed with a router after 24 h at ambient temperature to prevent post-molding shrinkage distortion.

    The material is not recommended for abrasive mineral ores because its surface wear resistance is lower than UHMWPE; the hopper requires a replaceable liner if quartz sand or fired clay granules are processed. Terminal products include conical-bottom feeding hoppers, fertilizer batch bins, seed transfer hoppers, and mineral supplement dispensing cones.

    When UV Stabilizer Loadings Exceed 3 wt% in Outdoor Furniture Rotomolding

    Outdoor furniture shells and playground panels are molded from dry-blended UV-stabilized LLDPE powders. The combined masterbatch loading should not exceed 3.0 wt% of the dry blend. Above this threshold, particle size distribution shifts to a higher fine fraction and powder dry flow becomes erratic during charging. The result on a four-arm turret machine is longer loading time and non-uniform wall thickness in deep-draw seat molds. A typical weather-resistant formulation uses 100 parts Icorene 3545 GRN 6413, 1.5 parts hindered amine light stabilizer masterbatch, 0.8 parts benzotriazole ultraviolet absorber masterbatch, and 2.0 parts pigment masterbatch. The mixture is tumbled for 20 min at low speed before loading.

    Molds are heated at 270–290 °C. Peak internal air temperature is held at 185–195 °C for 3 min. The lower peak internal air temperature window of 185–195 °C is used to maintain impact strength in furniture parts with irregular cross-sections. If peak internal air temperature exceeds 200 °C, the thinner edges oxidize and develop surface cracks after one summer of ultraviolet exposure. The mold uses a 4:1 rotational ratio. For chair shells with deep concave pockets, the primary rotation is 6 RPM and secondary is 1.5 RPM; for long bench tops, the primary rotation is reduced to 4 RPM and secondary increased to 2 RPM to distribute powder evenly. Cooling is forced air to 70 °C, then ambient for 10 min. Ejection pins must have large pads to avoid localized stress whitening.

    Playground structural components in the United States must meet ASTM F1487-21 and CPSC guidance. Under the CPSC lead content rule, accessible substrates in children’s products are limited to 100 ppm total lead. Under EN 71-3, the finished polymer must pass aqueous migration limits for 19 elements, independent of the raw resin certification. The processor is responsible for testing the finished colorant package; the base LLDPE cannot guarantee migration compliance by itself. Terminal products include modular outdoor seating shells, picnic table tops, rotomolded cooler benches, and playground tunnel segments.

    In livestock feeding trough and creep feeder applications, the LLDPE powder is processed into thick-walled trays that resist repeated hot-water cleaning and alkaline detergent attack. The GRN 6413 colorant package is used as supplied; separate pigment masterbatch is not required if the customer accepts the standard green tone. Wall thickness is set at 5–8 mm to balance weight and impact resistance in unheated barns where winter temperatures may reach −40 °C. Rotational molding proceeds at an oven set point of 280–295 °C and peak internal air temperature of 190–200 °C. The 4:1 rotational ratio is maintained for rectangular trough molds; for long narrow troughs, the secondary rotation is briefly paused during initial powder distribution to prevent material accumulation at the ends. The powder is not pre-dried unless condensation is visible. After demolding at 65 °C, the trough is flame-treated on the inner surface to improve cleaning release and reduce feed residue adhesion.

    The base resin may be acceptable for repeated food-contact use under FDA 21 CFR 177.1520(c), but the finished trough is not food-equipment certified unless tested as a finished article. Feed supplements containing propionic acid can cause surface swelling at elevated concentration; the processor should test a filled tray for one month at 40 °C before approving long-term use. Terminal products include creep feeders, farrowing pen partitions, mineral feed trays, and water bowls.

    Free Quote

    Competitive LyondellBasell Icorene 3545 GRN 6413 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 3545 GRN 6413 is a pre-compounded green linear low-density polyethylene supplied as a 35-mesh rotational moulding powder. The base grade, Icorene 3545, is designed for dry-flow processing and is distinguished from injection-moulding or blown-film LLDPE by its particle morphology, controlled particle-size distribution, and rotational-moulding-specific stabilization. Lot release documentation for the 3545 designation normally reports melt mass-flow rate according to ISO 1133-1:2022 at 190 °C/2.16 kg, density according to ISO 1183-1:2019, and sieve retention values according to ASTM D1921 or an equivalent dry-sieve method. Because the 6413 green designation is a pre-colored variant, published datasheets for the exact color-modified system are limited; the values applicable to a specific shipment must be taken from the manufacturer’s certificate of analysis, not from generic base-resin literature. The product is used primarily in rotational moulding of tanks, agricultural components, outdoor enclosures, and material-handling parts where a green color is required at the surface and through the wall. Compared with natural LLDPE powders of the same base melt flow, the green 6413 variant introduces pigment particles and possibly additional light stabilizers, which can alter dry flow, bulk density, impact response, and heat absorption during oven residence.

    What Distinguishes Icorene 3545 GRN 6413 from Natural LLDPE and HDPE Rotational Moulding Feedstocks?

    The primary differences arise in density and stiffness, melt-flow and processability, and color-related property shifts. In the LLDPE rotational moulding family, density values typically measured by ISO 1183-1:2019 Method A fall in the 0.930–0.940 g/cm³ band. HDPE rotational moulding grades typically occupy a higher density range of 0.940–0.965 g/cm³, producing parts with higher flexural modulus but often lower environmental stress crack resistance at equivalent melt flow. Icorene 3545 GRN 6413 therefore occupies a lower-stiffness, higher-elongation region compared with HDPE. The 3545 designation is commonly interpreted in rotational moulding trade literature as a 35-mesh nominal powder with a target melt mass-flow rate near 4.5 g/10 min under ISO 1133-1:2022 conditions, although the manufacturer’s coding convention is not a release specification. The green 6413 color package differentiates it from natural Icorene 3545 by removing in-house dry pigment blending. In dry-blended systems, pigment agglomerates and inconsistent dispersion can create localized reductions in impact resistance. Precompounding is intended to reduce batch-to-batch color variance, but final dispersion quality should be verified by optical microscopy on thin sections or by melt-filter pressure rise across a standardized extruder screen pack. Precompounded colors also shift the heat absorption profile of the powder during oven rotation, which may require adjustment of oven set temperature or cycle time relative to the natural base.

    On a production-scale biaxial carousel line with a closed oven zone, the powder enters at ambient temperature and is heated under rotation until the mold surface reaches a temperature sufficient for densification and bubble removal. The processing window for LLDPE rotomoulding is bounded on the low side by incomplete particle coalescence and on the high side by oxidative yellowing and loss of impact. Typical oven setpoints for LLDPE rotational moulding are reported in the range of 260 °C to 320 °C, with the peak internal air temperature often controlled between 180 °C and 220 °C depending on wall section. A 35-mesh powder reduces the time to full densification relative to a 50-mesh or 80-mesh pulverized powder because the coarser particles have lower surface area per unit mass but may require longer time to eliminate trapped air if the wall is thick. Dry-flow performance is measured with ASTM D1895 Method A or ISO 60:1977, and sieve retention with ASTM D1921. Bulk density changes of more than ±3% relative to the qualified baseline should trigger re-establishment of cycle time, because bulk density directly controls the volume of powder in the mold and the heat transfer area during early heating. Static charging and moisture pickup in high-humidity environments are operational boundaries: if the powder is stored in unsealed containers above 60% relative humidity, surface moisture can produce surface porosity and voids, and pre-drying with dry air at 70 °C to 80 °C is required until the moisture content meets the lot certificate specification.

    Material Specifications and Test Methodology for the Green 6413 Variant

    Lot qualification for the green 6413 variant should be based on a controlled list of test methods, because colorants influence multiple rheological and mechanical responses. The following matrix identifies the minimum standard designations and reporting units used in rotational moulding grade qualification. Values are not reproduced because published data for this specific color-modified configuration is limited and lot-specific certificates differ from base-resin literature.

    PropertyStandard designationCondition or unit
    Melt mass-flow rateISO 1133-1:2022190 °C/2.16 kg; g/10 min
    DensityISO 1183-1:2019 Method Ag/cm³
    Apparent densityISO 60:1977g/cm³
    Particle size distributionASTM D1921% retained; µm
    Tensile stress at yieldISO 527-2:2012MPa
    Tensile strain at breakISO 527-2:2012%
    Flexural modulusISO 178:2019MPa
    Vicat softening temperatureISO 306:2022 Method A50°C
    Environmental stress crack resistanceASTM D1693-15 Condition B100% Igepal CO-630; h
    Low-temperature puncture impactISO 6603-2:2000J or J/mm

    The table does not constitute a release specification. A production lot certificate must include actual results and the exact sample preparation history, including annealing time and temperature for density plaques, because density measured on a fast-cooled mold surface may be lower than density measured on a laboratory compression-moulded specimen. For colored grades, the density of the pigmented compound is typically slightly higher than the natural base because pigment particles are higher in density than the polyolefin matrix; the exact shift is a function of pigment loading and is normally below the repeatability uncertainty of routine density measurement if loading is low.

    Rotational Moulding Cycle Parameters Constrain the Useful Melt Flow Range

    The melt flow rate of the base grade influences the lower temperature limit for densification and the upper temperature limit for bubble escape. If the melt flow is too low for a given wall thickness, pinholing and incomplete coalescence occur at the inner surface. If the melt flow is too high, molten resin may sag on vertical walls and produce thickness variation under slow cooling. For Icorene 3545 GRN 6413, the nominal base-resin melt flow rate near 4.5 g/10 min under ISO 1133-1:2022 conditions places it in the medium-flow region of the LLDPE rotational moulding range. This flow band is generally suitable for parts with nominal wall thickness from 3 mm to 12 mm when processed with oven setpoints of 260 °C to 300 °C and with a biaxial rotation ratio between 4:1 and 5:1. The green 6413 pigment can absorb infrared or visible radiation differently from the natural resin, so the actual internal air temperature ramp should be re-qualified rather than transferred directly from a natural-grade cycle. Thermocouple data from a production tool is the preferred method: the peak internal air temperature and plateau time should be adjusted until the inner surface is free of porosity and the outer surface shows no oxidative discoloration. Process records should include mold temperature at release, not only oven setpoint, because the part cooling rate determines warpage and shrinkage compensation.

    Environmental stress crack resistance is a key differentiator between LLDPE rotational moulding grades and HDPE alternatives. In ASTM D1693-15 Condition B testing using 100% Igepal CO-630, linear low-density polyethylene grades generally exhibit longer failure times than high-density grades of similar melt flow when density is reduced. The Icorene 3545 designation, with a density in the LLDPE band and a medium melt flow, is specified for applications where repeated cleaning agents, agricultural chemicals, or hydrocarbon-containing condensates contact the molded wall. The green 6413 pigment package may alter the crack-initiation population at the surface; if the part is used for chemical storage, ESCR specimens should be cut from the actual molded wall rather than from a compression-moulded plaque, because the rotomoulded inner surface contains particle-boundary histories that differ from press-cooled laboratory samples. Low-temperature impact is evaluated by ISO 6603-2:2000 or rotational-moulding-specific ARM impact methods; acceptance values depend on section thickness and conditioning temperature. Published data for this specific green 6413 configuration is limited; users should require lot-specific impact data at the intended service temperature and wall thickness. Coarse powder particle size and pigment-induced nucleation may also influence shrinkage. Mould shrinkage values should be checked on a cavity of production geometry, not on a laboratory plaque, because the biaxial rotation path determines internal orientation.

    When In-House Dry Pigment Blending Is Replaced by the 6413 Precompound

    When the 6413 green precompound is used instead of dry blending a masterbatch or pigment into natural Icorene 3545, the technical benefits and constraints shift. Precompounding moves the dispersion step upstream, so the molder does not create the shear environment required to break down pigment agglomerates. In rotational moulding, the powder is not melted under high shear during the process; therefore, poor dispersion of dry-blended pigment may not be corrected in the mold. The 6413 precompound is intended to reduce the risk of undispersed pigment agglomerates that appear as specks or low-impact initiation points. However, precompounding also creates a material with a different electrostatic and particle-size profile than the natural base. Bulk density may change due to the melt compounding and regrinding step, and the powder may carry a broader or finer particle-size distribution. Dry-flow funnel time and apparent density should be re-established for each silo or hopper, especially if the powder is transferred by vacuum conveying. If the compound contains hindered amine light stabilizers for outdoor weathering, the stabilization package must be verified against ISO 4892-2 or ASTM D2565 exposure criteria, because green pigmentation alone does not guarantee ultraviolet resistance. For food-contact uses, the base polyethylene may be covered under 21 CFR 177.1520, but the green 6413 pigment package may require separate verification. Under EU REACH and RoHS Directive 2011/65/EU as amended, the finished compound must be checked for restricted heavy metals or phthalate carriers used in pigment dispersion. No stated value should be treated as a release limit without a current certificate of analysis.