Lyondellbasell Icorene 3545 Grn 6238 Polyethylene Linear Low Density

LyondellBasell Icorene 3545 GRN 6238 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 3545 GRN 6238 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 291698
    Density 0.935 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 4.5 g/10 min
    Tensile Strength At Yield 14.0 MPa
    Tensile Strength At Break 20.0 MPa
    Ultimate Elongation 800%
    Flexural Modulus 400 MPa
    Notched Izod Impact 100 J/m
    Shore D Hardness 50
    Vicat Softening Point 95°C
    Melting Point 124°C
    Crystallization Temperature 110°C
    Color Green

    As an accredited LyondellBasell Icorene 3545 GRN 6238 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 3545 GRN 6238 Polyethylene, Linear Low Density is supplied in 25 kg sealed bags, palletized and stretch-wrapped.
    Container Loading (20′ FCL) 20′ FCL loading: LyondellBasell Icorene 3545 GRN 6238 LLDPE in 25 kg bags, palletized, shrink-wrapped, and secured for ocean freight.
    Shipping LyondellBasell Icorene 3545 GRN 6238 (linear low-density polyethylene) ships as a non-hazardous solid resin in sealed bags, octabins, or bulk trucks/railcars. It is not DOT/IMDG/IATA regulated. Protect from moisture, contamination, direct sunlight, and excessive heat; keep packaging intact and labeled during transport.
    Storage Store LyondellBasell Icorene 3545 GRN 6238 Polyethylene, Linear Low Density in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original containers or bags closed, clean, labeled, and palletized. Prevent moisture, dust accumulation, and static discharge. Use first-in, first-out rotation. Consult the SDS and local regulations for specific requirements.
    Shelf Life Shelf life is 12 months when stored in unopened original packaging under cool, dry conditions, away from direct sunlight.
    Application of LyondellBasell Icorene 3545 GRN 6238 Polyethylene, Linear Low Density

    In agricultural sprayer tank and liquid fertilizer containment production, LyondellBasell Icorene 3545 GRN 6238 is charged directly into cast aluminium or steel clamshell moulds at wall-thickness targets between 4 mm and 8 mm. Incoming powder conformance requires a melt flow rate of 3.0–6.0 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022 and density within 0.930–0.940 g/cm³ under ISO 1183-1:2019; these limits preserve the low-shear viscosity required for bubble removal without excessive sag on vertical tank walls. The powder is dry-blended with 0.1–0.3 wt% silicone-based internal release agent before charging; loadings above 0.5 wt% migrate to the mould surface and impair post-mould welding of pipe couplings. Oven setpoint is held between 290 °C and 310 °C, while the peak internal air temperature is maintained at 195–215 °C for 2–4 min to complete sintering of the 35 mesh powder fraction. Deep tank cavities above 1.5 m length require the secondary rotation speed to remain below 4 rpm to prevent powder bridging at internal baffle lines. Venting is achieved with a PTFE tube of 3–5 mm internal diameter; a blocked vent can raise cavity pressure and produce pinholes at weld lines. Hydrostatic proof testing follows ASTM D1998 and EN 13575 at 1.3 times maximum service pressure, and environmental stress cracking resistance is evaluated under ASTM D1693, Condition B, 100% Igepal with a minimum service-acceptable F50 above 500 h. For concentrated fertilizer solutions above 30% nitrogen by mass, immersion screening at 40 °C for 90 days is required because published data for this specific green-pigmented grade in hot ammonium nitrate service is limited.

    Process variableLLDPE rotomoulding windowMeasurement/control reference
    Melt flow rate3.0–6.0 g/10 min at 190 °C/2.16 kgISO 1133-1:2022
    Density0.930–0.940 g/cm³ISO 1183-1:2019
    Peak internal air temperature195–215 °CVented air probe, thermocouple
    Oven setpoint290–310 °CForced convection zone controller
    Rotational ratio4:1 to 8:1Direct-drive encoder
    Vent tube internal diameter3–5 mm PTFEMould insert verification
    Demould temperature≤70 °CIR pyrometer

    Why Does Peak Internal Air Temperature Govern Impact Strength in Marine Buoyancy Modules?

    In marine float moulding, the failure mode that limits service life is low-temperature crack propagation from the mould parting line, which is governed by interfacial sintering rather than bulk tensile yield measured at 23 °C under ISO 527-2. Peak internal air temperature must exceed the melting region of the grade by 20–35 °C; at PIAT values below 180 °C, powder particles coalesce only partially and multiaxial impact at −20 °C under ISO 6603-2 typically falls by 15–30%. Above 225 °C, oxidative degradation increases the melt flow rate and lowers puncture resistance; industrial ovens therefore set chamber air at 300 °C maximum and use forced convection with airflow above 4 m/s across the mould surface. Mould charging for a 250 L buoyancy module typically consumes 18–22 kg of powder, and the cycle is terminated only after the internal air thermocouple reads 205 °C for two consecutive minutes. When a polyurethane core is injected after shell demoulding, the LLDPE skin must retain a minimum corner thickness of 6 mm; otherwise the PU exotherm above 120 °C softens the polyethylene and causes localised collapse. Ultraviolet stabilisation in the green-pigmented system must be verified by xenon-arc exposure under ISO 4892-2, with a retained elongation at break of at least 50% after 2,000 h. Published data for this specific colour concentrate loading in marine service is limited; a lot-specific accelerated weathering panel run is therefore required before deployment of production floats.

    For underground utility chambers and drainage sumps, the critical processing variable is not only full sintering but also flatness across the access opening after demoulding; cooling-induced warpage exceeding 3 mm/m causes gasket seating failure on site. Moulds for chambers above 1 m in diameter are run on shuttle-type machines rather than fixed-arm carousels because independent cooling-station control reduces differential shrinkage between the frame insert and the polyethylene wall. The powder is charged to produce a nominal wall of 5–7 mm, and local thinning at the knock-out rib is controlled by adding a static charge reduction agent at 0.05–0.1 wt% to limit powder clumping in deep corners. Oven cycle time for a 60 kg shot is extended by 15–25% relative to a flat panel because the steel frame insert delays the peak internal air temperature; thermocouple placement in the deepest cavity is mandatory. Cooling after PIAT is staged: forced air at 10–12 °C/min to 100 °C, followed by water mist at 3–5 °C/min to 60 °C. Demoulding above 70 °C produces permanent post-mould shrinkage and flange bowing. Vertical proof load class is verified under EN 124-1, and flatness is checked with a calibrated straightedge over the full opening perimeter. The green-pigmented grade must also be checked for oxidative induction time at 200 °C under ISO 11357-6; values below 20 min indicate insufficient stabiliser for multiple regrind cycles in underground service.

    Waste and Recycling Container Lids Require a Narrow Warp-Avoidance Cooling Curve

    Green-pigmented LLDPE for mobile waste containers and recycling carts is processed with a lid-to-body shrinkage differential that must be held below 1.5% to maintain hinge alignment. The nominal body wall is moulded at 4–6 mm, while the lid edge is thickened to 8–10 mm for impact resistance; this thickness difference changes the cooling rate between sections by more than 5 °C/min and induces sink marks if cooling is not staged. In production-scale carousel moulding, the mould is removed from the oven at PIAT 195–210 °C and transferred to the cooling station within 30 s; delayed transfer allows continued exotherm, increases crystallinity in the lid rim, and raises warpage by 40–60% compared with immediate forced-air cooling. The cooling station uses differential airflow: 8 m/s directed at the lid rim and 3 m/s at the body cavity through variable-frequency drive fans. Demoulding is initiated only after the part reaches 80 °C; earlier demoulding distorts hinge-pin holes irreversibly. Impact and structural verification follows EN 840-1:2020, with the corner weld region tested by a 10 kg steel ball drop at −20 °C. The green pigment in GRN 6238 must not increase melt viscosity by more than 5% relative to the unpigmented base; incoming powder conformance is checked by capillary rheometry at 190 °C and 10 s⁻¹ under ISO 11443. Because the pigment may shift the crystallisation onset, a differential scanning calorimetry trace under ISO 11357-3 is used to confirm that the cooling curve does not accelerate crystallisation in the thickened lid rim.

    ApplicationReference standardCritical technical verification
    Agricultural chemical storage tankEN 13575 / ASTM D1998Hydrostatic proof at 1.3× service pressure; ESCR per ASTM D1693, 100% Igepal
    Marine buoyancy moduleISO 4892-2Retained elongation at break after 2,000 h xenon-arc exposure
    Underground utility chamberEN 124-1Vertical proof load class verification; flatness ≤3 mm/m
    Waste and recycling containerEN 840-1:2020Lid-body shrinkage differential ≤1.5%; drop test at −20 °C
    Material handling binISO 2248Drop height 1.2 m at −10 °C; cracking threshold 25 mm
    Playground componentEN 1176-1:2017Entrapment openings; accelerated weathering per ISO 4892-2

    Material handling bins and pallet boxes are rotomoulded with flat drop gates and fork pockets where the main technical risk is stress whitening at the gate hinge after repeated drop cycles. The Icorene 3545 powder is processed without pre-drying unless stored at relative humidity above 60%, in which case surface moisture condenses on cold powder from outdoor silos and produces steam pinholes at the mould wall; drying for 2 h at 70 °C in a fluid-bed dryer restores moisture content below 0.01 wt%. The mould is a fabricated aluminium box with a pneumatically operated gate insert; the hinge area is designed with a radius of not less than 3 mm because radii below 2 mm create a notch that reduces notched constant tensile load performance under ASTM F2136 by more than 30%. Shot size is calculated from a powder bulk density of 0.37–0.42 g/cm³ and a wall thickness of 6 mm, with an additional 8–12% charge weight to account for corner build-up at the fork pockets. The rotational ratio is maintained at 4:1, but primary rotation speed is reduced to 2–3 rpm when bin length exceeds 1.2 m to avoid powder sliding rather than tumbling, which produces thin end panels. Steel fork pocket inserts are preheated to 80 °C before charging; cold inserts quench the melt prematurely and create a crystalline halo at the insert wall. The finished bin is evaluated by a drop test of 1.2 m onto a concrete floor at −10 °C after conditioning for 24 h; failure is defined as any crack longer than 25 mm at the gate hinge.

    Playground Panel Skin Hinge and UV Weatherability Limits

    Rotational moulding of playground panels, roof caps, and tunnel sections uses the same pigmented LLDPE powder but demands lower surface gloss and higher resistance to UV-induced chalking than utility parts. The mould is textured with 50–80 µm average roughness to mask flow lines; smoother surfaces show visible weld lines at the powder contact boundary when PIAT drops below 190 °C. The panel is moulded to a nominal wall of 5 mm, while thickened bosses around bolt holes are designed with a local wall thickness not exceeding 12 mm because heavier sections increase cooling time by 20% and reduce impact resistance at −20 °C. UV stabilisation in the green grade is assessed by monitoring the carbonyl index change after 1,500 h in a xenon-arc weatherometer under ISO 4892-2; a carbonyl index increase above 0.1 indicates surface degradation sufficient to lower elongation at break below 50% of the unweathered value. Where the moulded panel is accessible to children under 36 months, heavy metal migration is screened against EN 71-3; the pigment masterbatch used in GRN 6238 requires documentation of colourant composition because some inorganic green pigments can contain chromium species above the 60 mg/kg migration limit. Structural performance of the panel is tested under EN 1176-1:2017, including head and neck entrapment openings and impact attenuation of accessible surfaces. Published data for this specific green-pigmented grade in thin playground sections is limited; a pre-production weathering panel run at 2,000 h is therefore retained as the standard qualification route before series production.

    Free Quote

    Competitive LyondellBasell Icorene 3545 GRN 6238 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 3545 GRN 6238 is a pigmented linear low-density polyethylene compound supplied as a rotational moulding powder. The base polymer belongs to the Icorene 3545 family and is classified as a linear low-density polyethylene under ASTM D883. The GRN 6238 suffix identifies a green colourant package incorporated into the powder before final particle size control. Because the material is designed for rotational moulding, it is supplied in powder form rather than as uniformly pelletised feedstock. The polymer matrix is a low-pressure polymerised LLDPE with a density near 0.934 g/cm³ and a melt flow rate around 4.5 g/10 min under ISO 1133-1 at 190 °C with a 2.16 kg load. These values are typical reference data, not contractual specifications; lot-specific certificates govern production release.

    In material selection, the grade occupies a middle density range between high-pressure LDPE and high-density polyethylene. The lower crystalline fraction relative to HDPE reduces stiffness but improves stress-crack resistance and low-temperature impact. The green pigment system may contribute minor nucleation effects; crystallisation, shrinkage, and part cooling behaviour should therefore be qualified with the actual pigmented lot rather than inferred from an unpigmented base resin. Published data for this specific green configuration is limited, so end-use qualification is required for critical dimensions and mechanical performance.

    What distinguishes an LLDPE rotomolding powder from traditional LDPE and HDPE?

    Linear low-density polyethylene is produced by low-pressure polymerisation using transition-metal catalysts, in contrast to high-pressure LDPE, which uses free-radical initiation. The absence of long-chain branching in LLDPE results in a narrower molecular weight distribution, lower melt extensional strain hardening, and typically higher tensile strength and environmental stress-crack resistance at equivalent density. For rotational moulding, the melt flow rate of Icorene 3545 GRN 6238 is in the intermediate flow class for LLDPE powders, which permits reasonable oven dwell times but reduces zero-shear viscosity compared with fractional-melt rotomolding grades. During rotomolding, lower zero-shear viscosity can improve particle coalescence, but excessive flow can produce non-uniform wall thickness in complex mould cavities.

    Compared with a high-pressure LDPE grade of the same nominal melt flow rate, the LLDPE grade generally requires a higher peak internal air temperature to achieve full densification because its predominantly linear chains resist shear-free melt coalescence more than long-chain branched LDPE at equivalent oven conditions. This is a critical processing conflict: the operator must keep peak internal air temperature high enough to eliminate bubbles and pinholes but low enough to avoid thermal degradation of the green pigment and antioxidant system. Compared with an HDPE rotomolding powder of melt flow 3.5–6.5 g/10 min and density 0.944–0.952 g/cm³, this LLDPE grade shows reduced flexural modulus, higher elongation at break, and better low-temperature ductility. The trade-off is lower heat deflection behaviour and lower creep resistance under continuous load.

    Rheology, density, and mechanical benchmarks for rotomolding powders

    The nominal melt flow rate is measured under ISO 1133-1 at 190 °C with a 2.16 kg load. The value places the material in the intermediate flow class for rotational moulding, not in the fractional-melt class used for ultra-high ESCR HDPE. The density of 0.934 g/cm³ is below that of high-density rotomolding grades and above that of very-low-density plastomers; this range is commonly selected for chemical-tank and agricultural-container applications where part stiffness can be traded for stress-crack resistance. Representative published property values for the Icorene 3545 family are summarised below. They are reference values, not guaranteed lot-specific specifications.

    PropertyTypical reference valueTest method
    Melt flow rate4.5 g/10 minISO 1133-1
    Density0.934 g/cm³ISO 1183-1
    Tensile stress at yield17 MPaISO 527-2
    Tensile strain at break>700 %ISO 527-2
    Flexural modulus0.59 GPaISO 178
    Vicat softening point, A50116 °CISO 306
    Low-temperature brittleness-75 °CASTM D746
    Environmental stress-crack resistance, 100% Igepal CO-630>1000 hASTM D1693

    The tensile and flexural data indicate a semi-rigid LLDPE with high elongation at break. The low-temperature brittleness value near -75 °C suggests that the material retains ductility in cold-climate installations, although impact resistance in a moulded part is also governed by wall thickness, cooling rate, and internal stress. The ESCR value is a comparative ranking under ASTM D1693; it does not directly predict service life in a specific chemical environment. For parts containing moulded-in stress, welded regions, or pinch-off seams, ESCR should be validated on prototype parts because stress concentration can reduce time to crack onset by orders of magnitude relative to standard test coupons.

    When prolonged environmental stress-crack resistance and low-temperature ductility outweigh high flexural modulus

    Material substitution should be based on part-level requirements rather than single-point datasheet comparisons. If a rotationally moulded tank currently produced in a 0.944 g/cm³ HDPE fails by environmental stress cracking at pinch-off seams or in areas of moulded-in stress, an LLDPE with lower density may reduce the cracking frequency because lower crystalline fraction reduces the number of tie-chain strain concentrations. ASTM D1693 data are useful as ranking values but do not directly predict service life; the moulded part stress history, chemical exposure, and wall thickness also control failure. For a 6 mm nominal wall thickness, increasing the ESCR by an order of magnitude from a fractional-melt HDPE to a 0.934 g/cm³ LLDPE can extend the time to crack onset in 10% Igepal environments, but published field data for this specific GRN 6238 configuration is limited.

    Conversely, replacing HDPE with this grade will reduce tensile modulus by roughly 150–300 MPa, which may require ribbing or increased wall thickness if the part is under internal hydrostatic pressure. The lower heat deflection performance also restricts continuous under-load service at elevated temperatures. In cold-climate installations, the low-temperature brittleness value near -75 °C supports consideration of this material for tanks and containers that must survive impact during winter handling. However, part-level low-temperature impact should be measured on moulded panels with the actual cooling rate and wall thickness because laboratory brittleness testing does not fully capture residual stress and pigment-related nucleation effects.

    On a single-arm carousel rotomolding machine with an oven set point of 260–316 °C, the powder is placed in closed steel or cast-aluminium moulds rotating about two axes at a speed ratio commonly between 3:1 and 5:1. Heat transfer through the mould wall raises the powder from ambient to the melting range; the resin then passes through tackification, sintering, and densification stages. The target internal air temperature for an LLDPE of this melt flow is generally 180–200 °C; a thermocouple inside the mould should be used to terminate the heating cycle. If the peak internal air temperature remains below 170 °C, incomplete coalescence can appear as pinholes, poor inner-surface finish, and low weld strength at part corners. If peak internal air temperature exceeds 210 °C for this class of material, antioxidant consumption accelerates, and the green colour may shift or gas bubbles may appear at gate areas. Published data for this specific grade is limited, so process capability studies should map the relationship between peak internal air temperature and part impact strength.

    Cooling rate is another process variable with a disproportionately large effect on warpage and impact. Fast forced-air cooling followed by water mist can reduce cycle time but creates high thermal gradients through the wall; this can produce differential shrinkage and sink marks at thick bosses. Slow cooling in still air at ambient temperature yields lower part stress but can increase crystallinity and shrinkage. For pigmented LLDPE, the same cooling rate may not produce identical gloss or colour because pigment particles can act as heterogeneous nucleants. The moulder should therefore validate colour and warpage together, not separately.

    The GRN 6238 colour designation is a supplier pigment code, not a generic colour standard. If the part must match a defined RAL or Pantone target, the converter should establish a colour masterbatch tolerance using a spectrophotometer and CIE L*a*b* coordinates. Pigment dispersion can be assessed on moulded plaques by ISO 18553 or supplier optical methods. The green pigment package may affect weathering performance; UV stabilisation of the base resin and pigments should be specified separately if the part is exposed to sunlight.

    Food-contact status is not assumed from the base polymer alone. The base LLDPE may fall under FDA 21 CFR 177.1520 and EU Regulation No 10/2011 if unpigmented and manufactured under appropriate good manufacturing practice, but the green concentrate must have its own compliance documentation. Because GRN 6238 is a coloured compound, converters must request the supplier’s food-contact declaration or REACH/RoHS statement before using it in potable-water or toy applications. The final article must also pass end-use migration and organoleptic testing according to applicable national standards.

    The product is not recommended for continuous service above 60–70 °C under load; LLDPE exhibits lower creep resistance and heat deflection than HDPE. It is also not suitable for high-shear processes such as injection moulding or extrusion without adjustment because the powder morphology and stabilisation package are designed for rotational moulding. Avoid storage in direct sunlight or at relative humidity above 60% if condensation forms; polyolefin powders are not hygroscopic, but surface moisture can cause bubble defects and inconsistent flow in the mould.

    Top