| HS Code | 191602 |
| Material Type | Polyethylene, Linear Low Density (LLDPE) |
| Density | 0.935 g/cm³ |
| Melt Flow Rate | 35 g/10 min (190°C/2.16 kg) |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 7.58 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 0.310 GPa |
| Vicat Softening Point | 88.0 °C |
| Melting Point | 124 °C |
| Hardness Shore D | 48 |
| Color | Green |
As an accredited LyondellBasell Icorene 3545 GRN 6210 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 3545 GRN 6210 LLDPE is typically packaged in 25 kg polyethylene bags, 40 bags per pallet (1,000 kg). |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): LyondellBasell Icorene 3545 GRN 6210 Polyethylene, Linear Low Density in 25 kg bags; approx. 20 MT net. |
| Shipping | LyondellBasell Icorene 3545 GRN 6210 is shipped as non-hazardous LLDPE resin pellets, commonly in 25 kg bags, octabins, or bulk trucks/railcars. Keep containers closed, dry, and away from heat, sunlight, and contamination. No special transport hazard classification; follow SDS and local regulations. Store cool and ventilated. |
| Storage | Store LyondellBasell Icorene 3545 GRN 6210 Polyethylene, Linear Low Density in a cool, dry, well-ventilated area at moderate temperatures, away from direct sunlight, heat, sparks, and open flames. Keep containers or bags closed to prevent moisture, dust, and contamination. Avoid contact with strong oxidizing agents. Maintain good housekeeping, control static, and follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Shelf life: 24 months when stored in original packaging, in a cool, dry, well-ventilated area, away from direct sunlight. |
Icorene 3545 GRN 6210 is a green-compounded linear low-density polyethylene rotational molding grade with published nominal density of 0.934 g/cm³ (ISO 1183-1) and melt flow rate of 5.0 g/10 min (ISO 1133-1:2022). The material is intended for ambient-temperature mold charging in biaxial rotational molding equipment. It is not specified for injection molding, blown film, or extrusion profiles; those processes do not provide the sintering environment required to achieve the designed wall density and impact performance. The following application scenarios are limited to sectors where this density and flow envelope is commercially specified for rotationally molded LLDPE articles.
Potable water storage tanks and cisterns are produced by charging the LLDPE powder into closed or vented cast aluminum molds. For a 6 mm nominal wall tank, shot weight is calculated from part surface area, wall thickness, and 0.93 g/cm³ melt density, with 2–3 wt% added for flash and powder spillage. Powder particle size distribution is controlled by ambient pulverization and sieve classification; a top size near 500 µm and fines below 25 wt% through 150 µm are typical rotational molding quality benchmarks to maintain dry flow and minimize pinholing. The mold rotates biaxially at a primary-to-secondary speed ratio between 2:1 and 5:1, depending on tank geometry. Oven air setpoints between 270 °C and 290 °C are used. Peak internal air temperature is held between 190 °C and 205 °C for complete sintering. Cooling begins with forced air and transitions to water mist after the polymer has solidified, keeping warpage below assembly tolerance. Compliance for potable water contact requires testing of the finished tank under NSF/ANSI/CAN 61 or AS/NZS 4020:2018; the base resin falls within the olefin polymer scope of FDA 21 CFR 177.1520 and EU 10/2011 when migration testing confirms overall migration below 10 mg/dm². Formulation is typically 100 wt% Icorene 3545 GRN 6210 when a green tint is acceptable; if a different color is required, a food-contact-approved masterbatch is added at 1–2 wt%. For outdoor installations, a carrier-compatible HALS/UV stabilizer masterbatch is incorporated at 0.5–2.0 wt%. Finished product types include closed-top potable water tanks from 100 L to 10,000 L, caravan water tanks, rainwater collection cisterns, and livestock drinking troughs. Operational boundaries include avoiding continuous service above 60 °C and avoiding concentrated aromatic hydrocarbon disinfectants that can act as stress-cracking agents.
In rotationally molded chemical containment, the limiting failure mode is environmental stress cracking rather than short-term impact. Icorene 3545 GRN 6210 is charged at 100 wt% or with 1–3 wt% of a carbon black/UV masterbatch for outdoor service. The additive loading is kept below 3 wt% because excessive masterbatch dilution can reduce the short-chain branch network responsible for environmental stress-cracking resistance. The downstream process uses cast aluminum molds with radiused corners no smaller than 25 mm; sharp internal corners create residual stress concentrations that promote chemical crack initiation. Molds are rotated at primary-to-secondary speed ratios from 3:1 to 5:1, with oven air at 270–290 °C and a peak internal air temperature of 195–210 °C. For walls of 6–12 mm, oven dwell ranges from 20 min to 40 min depending on shot weight up to 80 kg. Cooling is deliberately slowed below 10 °C/min after solidification to allow amorphous-phase relaxation; rapid water quench is avoided because it freezes in residual stresses near molded-in metallic inserts. Compliance for transportable chemical containers may involve UN 31H1/Y design type testing under ADR 6.5.4 and IMDG Code Chapter 6.5 for liquid dangerous goods of Packing Group II or III up to 1.5 g/cm³ relative density. The grade is not suitable for concentrated aromatic hydrocarbons or strong oxidizing acids above 40 °C; compatibility with specific chemical formulations must be verified by ESCR testing per ASTM D1693 condition B rather than inferred from neat-resin datasheets. Finished product types include 120–1,000 L dosing tanks, secondary containment pallets, acid neutralization basins, scrubber tanks, and static chemical storage vessels.
Because agricultural sprayer tanks carry both mechanical load from boom attachments and chemical load from crop protection formulations, post-mold residual stress around inserts becomes the controlling variable. The standard charge is 100 wt% Icorene 3545 GRN 6210; where UV stabilization is required for long outdoor service, a HALS/UV masterbatch is added at 1.5–2.5 wt%, and a color masterbatch is added at 0.5–2.0 wt% if non-green identification is required. Total non-resin components are not increased beyond 4 wt% because higher additive loads can reduce impact in the ribbed base areas. Downstream production uses fabricated steel or aluminum molds with stainless steel threaded inserts that are preheated to 120–150 °C before mold charging. Oven setpoints of 270–290 °C and peak internal air temperature of 190–205 °C are maintained for wall thicknesses between 5 mm and 10 mm; oven dwell is held until the inner surface reaches the sintering plateau for at least 2–3 min. After demolding, tanks are placed in cooling jigs to prevent boss-area warpage; wall thickness around fittings is designed at 1.5–2.0 times the nominal sidewall. Compliance for liquid agrochemical transport uses UN 31H1/Y design type qualification under ADR 6.5 for Packing Group II and III liquids; dual-use potable water tanks must separately meet NSF/ANSI/CAN 61. Pesticide formulations containing xylene, toluene, or other aromatic solvents can swell the LLDPE amorphous phase, so the operational boundary requires a 60-day compatibility immersion test at 40 °C before specifying this grade. Finished product types include tractor-mounted sprayer tanks, fertilizer nurse tanks, seed treatment mix tanks, and agricultural foamer tanks.
Process envelope comparison for Icorene 3545 GRN 6210 across selected rotational molding applications. Values are representative and must be re-validated for each mold geometry, shot weight, and part thickness.
| Application | Typical wall thickness | Oven air setpoint | Peak internal air temperature | Cooling sequence | Primary compliance anchor |
|---|---|---|---|---|---|
| Potable water tanks | 6–10 mm | 270–290 °C | 190–205 °C | Forced air to water mist | NSF/ANSI/CAN 61 |
| Chemical containment | 6–12 mm | 270–290 °C | 195–210 °C | Slow cool below 10 °C/min | UN 31H1/Y |
| Agricultural sprayer tanks | 5–10 mm | 270–290 °C | 190–205 °C | Cooling jig after demolding | UN 31H1/Y |
| Playground and site furniture | 3–5 mm | 270–285 °C | 190–200 °C | Forced air only | EN 71-3:2019+A1:2021 |
| Marine hulls and buoyancy | 4–7 mm | 270–290 °C | 195–210 °C | Air to water mist | 33 CFR 183.105–183.114 |
| Material handling bins | 6–10 mm | 270–290 °C | 190–205 °C | Flat cooling racks or jigs | ISO 8611-1:2011 |
For outdoor playground structures and site furniture, the green-pigmented LLDPE grade is processed without a separate base resin pre-drying step unless powder has been stored in unheated silos below the ambient dew point; condensation on powder can otherwise create pinholes. The production process uses CNC-machined cast aluminum molds with textured interior surfaces to hide shrinkage variations. Molds are charged at 100 wt% Icorene 3545 GRN 6210 or with 1–3 wt% of a UV-stabilized color masterbatch. Use of undried powder is acceptable when relative humidity is below 60%; at higher humidity, the powder is pre-dried at 60 °C for 1–2 h or kept in sealed containers. Oven air temperature is set between 270 °C and 285 °C, with peak internal air temperature between 190 °C and 200 °C. For walls from 3 mm to 5 mm, oven dwell is short, but insufficient dwell produces surface porosity and weld-line weakness at multi-part mold interfaces. Compliance for playground articles requires elemental migration testing under EN 71-3:2019+A1:2021, restriction compliance under REACH Regulation (EC) No 1907/2006 Annex XVII, and, for plastic components without electrical function, RoHS Directive 2011/65/EU where applicable. Impact and entrapment performance is verified on the finished structure under ASTM F1487-17 or EN 1176-1:2017. Operational boundaries include limiting dark-colored parts in high-solar-irradiance regions because surface temperatures can exceed 70 °C and reduce local stiffness. Finished product types include crawl tubes, slide hoods, climbing panels, sandbox shells, and rotationally molded site furniture components.
Unlike potable water tanks, marine hull shells experience reversed flexural loading with every wave cycle, making fatigue and UV retention the decisive material selection criteria. The grade is used at 100 wt% or blended with 1–3 wt% of a marine-grade UV/antioxidant masterbatch and 2–4 wt% color concentrate for bright topside colors. The downstream process uses machined aluminum molds with wall thickness from 4 mm to 7 mm. Oven air at 270–290 °C and peak internal air temperature of 195–210 °C are used; the mold is cooled initially by forced air at 0.2–0.5 m/s face velocity until the inner surface reaches 110–120 °C, then by water mist to reduce bowing along long hull sections. Secondary operations include router trimming of the parting line, bonding of foam bulkheads with compatible polyolefin adhesive after flame treatment, and installation of deck fittings with large-diameter backing washers to prevent point loading. Compliance for small craft flotation invokes 33 CFR 183.105–183.114 for boats under 20 ft and Directive 2013/53/EU for recreational craft placed on the European market; the material itself is not a compliance certificate, and full craft buoyancy testing remains required. The grade is not specified for hull sections requiring wall thickness above 10 mm because cycle time and centerline porosity risk increase. Published cyclic fatigue data for this specific green-pigmented compound at marine thicknesses is limited; hull validation should include instrumented drop tests and flexural fatigue cycling. Finished product types include sit-on-top kayaks, canoe hulls, floating dock segments, buoyancy chambers, and marina fenders.
Static mechanical loads, rather than chemical exposure, govern material handling bin life. Industrial material handling containers made from Icorene 3545 GRN 6210 are specified for food-contact and general logistics applications where creep and impact loads define service life. Formulation is normally 100 wt% virgin powder; if color coding is required, 1–2 wt% of a food-approved masterbatch is added for non-green bins. For cleanroom or ESD applications, conductive carbon black masterbatches are used only at levels validated by surface resistivity testing because carbon black loadings above 5 wt% can reduce low-temperature impact. The downstream production process uses cast aluminum molds with integrally molded ribs, gussets, and fork slots. Wall thickness ranges from 6 mm to 10 mm; oven air is set at 270–290 °C, and peak internal air temperature is controlled between 190 °C and 205 °C. Demolded parts are placed on flat cooling racks or jigs and cooled with forced air; post-mold shrinkage of 1.5–2.5% is accommodated by mold scaling. Load-bearing performance is verified under ISO 8611-1:2011 for pallets and ASTM D4169 for distribution shock and vibration. Food-contact conformity is assessed under FDA 21 CFR 177.1520 and EU 10/2011; overall migration testing follows EN 1186-1:2002 with simulant selection per EU 10/2011. Operational boundaries include avoiding stacked service above 45 °C unless the load is reduced, because LLDPE modulus declines with temperature and long-term creep accelerates near the vicat softening region. Finished product types include 200–1,200 L bulk bins, pallet boxes, insulated fish tubs, meat lugs, and cleanroom bins.
Competitive LyondellBasell Icorene 3545 GRN 6210 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 3545 GRN 6210 is a polyethylene, linear low density compound supplied in a factory-colored green powder form for rotational molding and related low-shear consolidation processes. The numeric designation 3545 identifies the base resin within the Icorene LLDPE portfolio, while GRN 6210 is a manufacturer color code for a green pigmented variant. The material is polymerized in a low-pressure coordination process, which produces short-chain branching along the polyethylene backbone and distinguishes the resin from high-pressure low density polyethylene. Published typical values associated with the Icorene 3545 base resin include a nominal density of 0.934 g/cm³ and a melt flow rate of 4.5 g/10 min at 190 °C and 2.16 kg. The colored GRN 6210 formulation may exhibit minor shifts in density, rheology, and oxidative stability relative to the natural powder, so lot-specific certificate of analysis data should be used for final process setup.
Characterization of the material for incoming inspection normally follows ISO 1183-1 or ASTM D1505 for density and ISO 1133-1:2022 or ASTM D1238 for melt flow rate. These two parameters alone do not define rotational molding behavior. The particle size distribution, bulk density, dry flow, and oxidative induction time of the pigmented powder also determine whether the material will densify into a void-free part without color shift. For rotational molding powders, the base resin is pulverized rather than pelletized, and the resulting particle geometry influences how uniformly the powder fills mold recesses and how quickly air evacuates during sintering.
The technical difference between high-pressure LDPE and LLDPE is architectural, not merely a shift in density. High-pressure LDPE produced in autoclave or tubular reactors contains both short-chain and long-chain branches, which depress crystallinity, reduce tensile strength, and increase melt elasticity. Conventional LLDPE such as the Icorene 3545 base resin introduces short-chain branching through an α-olefin comonomer. The branching arrangement allows higher tensile yield stress, higher puncture resistance, and higher environmental stress crack resistance at equivalent density. These properties are typically compared under ASTM D638-14 or ISO 527-2 for tensile response, ASTM D1693 for environmental stress crack resistance, and ISO 6603-2 for multiaxial impact.
Metallocene-catalyzed mLLDPE carries a narrower composition distribution and more uniform comonomer placement than conventional Ziegler–Natta LLDPE. If the Icorene 3545 base resin is produced using a conventional catalyst system, its broader composition distribution may produce a broader melting range and different organoleptic or low-temperature impact behavior than an mLLDPE of the same density. In rotational molding, that difference can be observed as a wider peak internal air temperature window for complete sintering but potentially less sharpness in color or surface reproduction. The density of 0.934 g/cm³ places Icorene 3545 near the transition between LLDPE and medium-density polyethylene, balancing stiffness against low-temperature ductility. The melt flow rate of 4.5 g/10 min is moderate for rotomolding; lower-flow grades typically improve toughness but extend cycle time and may retain bubbles, while higher-flow grades fill narrow ribs more easily but may sacrifice stress crack resistance.
Rotational molding grades are not selected for melt strength in the same way as blown-film grades. In blown film, long-chain branching is desirable for bubble stability. In rotational molding, the powder is heated inside a biaxially rotating mold without external pressure, so densification depends on powder particle coalescence, melt surface tension, and bubble diffusion. LLDPE generally has lower melt strength than high-pressure LDPE because it lacks long-chain branching. This is not necessarily a deficiency in rotomolding, but it can affect melt flow from thin sections into thicker sections when the part wall thickness varies.
In production-scale shuttle and carousel rotational molding machines, the powder is charged into a mold that rotates in an oven. Oven set points for LLDPE powders are commonly between 280 °C and 300 °C. The internal air temperature is monitored through a vent, and the peak internal air temperature is the primary control variable. For LLDPE densities near 0.934 g/cm³, typical peak internal air temperature values fall between 200 °C and 220 °C. Operating below the densification threshold can leave pinholes, microvoids, and poorly fused powder at the mold surface. Operating above the oxidative threshold can shift the green color and embrittle the part. Because the GRN 6210 variant contains a green colorant, the upper temperature limit may be reduced if the pigment lowers oxidative induction time.
A common failure mode on production lines is under-densification at the mold parting line or at the end of deep ribs. The powder may appear fused but still contain gas bubbles that collapse into pinholes during cooling. Temperature probes and infrared pyrometers reduce but do not eliminate the need for part-section validation. Thick sections above 6 mm require longer heat soak to reach the peak internal air temperature, while thin sections below 3 mm are more sensitive to surface defects and powder-coating irregularities. Cooling rate is a second critical variable. Water fog or compressed air cooling can reduce warpage but may increase internal stress and reduce low-temperature impact. Validation should include falling dart impact per ASTM D3763 or ISO 6603-2, not only visual inspection.
The sintering window for rotational molding polyethylene is narrow because the mold is heated from the outside while the powder layer is a moving, conductive medium. If the peak internal air temperature is lowered to avoid color degradation in the green compound, the inside surface of thick regions may remain porous. A temperature reduction of only 5–10 °C below the validated peak can leave unmelted domains or reduce interparticle diffusion enough to lower elongation at break. The effect is more severe in areas with low thermal mass, such as thin ribs or inserts, because heat is dissipated into the mold body. Production process validation should therefore establish a peak internal air temperature corridor with a tolerance of approximately ±5 °C, based on molded plaque testing rather than powder data alone.
Melt rheology at low shear rates controls bubble collapse and particle coalescence. Oscillatory rheometry under ISO 6721-10 or dynamic mechanical analysis can provide storage modulus and loss modulus crossover data, but these tests are not routine in a molding shop. In practice, the melt flow rate gives an inverse indicator of molecular weight; a value of 4.5 g/10 min generally allows sufficient flow for moderate wall thickness without excessive sag. A lower melt flow rate would improve impact and environmental stress crack resistance but require a higher peak internal air temperature or longer oven residence time. A higher melt flow rate would fill complex geometry faster but may reduce ESCR and allow more melt migration into thick sections, creating sinks and dimensional variation.
Thermal stability under oxidative conditions is assessed by ASTM D3895, which measures oxidative induction time by differential scanning calorimetry at 200 °C. Natural LLDPE rotomolding grades typically require a minimum oxidative induction time to survive the oven cycle. Pigmented grades may have different stability because the colorant or its carrier resin can interact with the stabilization package. The GRN 6210 material should not be assumed to have the same oxidative induction time as natural Icorene 3545. Published data for this specific colored configuration is limited, so oven residence time should be validated by molded part impact and color measurements.
Powder dry flow is also a function of particle size distribution, surface moisture, and static charge. Pulverized LLDPE powders are not spherical; the grinding process creates angular particles and a broad distribution. Excessive fines below 75 µm can produce dust and static adhesion to mold surfaces, causing uneven wall thickness and pinholes. Coarse particles above 500 µm may not pack tightly into fine surface details, reducing mold reproduction. Production lines often use vibrational feeders, grounded mold frames, and controlled low-humidity handling below 30% RH to reduce static. Surface moisture above 0.05–0.1 wt% can create steam during heating and generate pinholes. If condensation occurs during storage, drying at 60–70 °C for 1–2 h may be required, but the manufacturer’s colored-grade guidance should be followed because excessive heat can agglomerate powder or shift the pigment hue.
Differential heating and cooling create the central process conflict in rotomolded LLDPE parts. Thin sections reach peak internal air temperature earlier and cool faster than thick sections, producing differential shrinkage and residual stress. The green pigment can act as a nucleating agent, altering crystallization temperature and potentially changing mold shrinkage. Crystallization behavior should be measured by differential scanning calorimetry under ISO 11357-3, and mold shrinkage can be quantified under ASTM D955. If the pigment raises crystallization temperature, the part may demold with higher apparent dimensional stability but also higher internal stress in thick sections. The result can be warpage, sink marks, or stress cracking around molded-in inserts.
The melt flow rate of 4.5 g/10 min provides adequate particle coalescence but does not eliminate the need for pressure-free bubble removal. In thick sections, the skin can densify before the core is fully sintered, trapping bubbles that expand during cooling. This failure is exacerbated when peak internal air temperature is reached too quickly. A plateau step in the oven cycle, rather than a continuous ramp, can allow the core to reach temperature without overheating the surface. In thin-wall sections, the same plateau can cause excessive color shift or oxidative degradation. The practical processing window for Icorene 3545 GRN 6210 is therefore geometry-dependent and must be established on the production tooling rather than on a flat plaque alone.
Mechanical testing of rotomolded parts should use specimens cut from molded sections, not injection-molded plaques, because the rotomolding process produces different porosity, orientation, and surface structure. Tensile properties are reported under ISO 527-2 or ASTM D638-14. Falling weight impact under ISO 6603-2 or ASTM D5420 is more relevant than notched Izod because rotomolded parts often fail by ductile puncture rather than sharp crack propagation. Environmental stress crack resistance is a critical differentiator for tanks and containers. The standard bent-strip test ASTM D1693 is commonly cited, but the notched constant tensile load test ASTM D5397 or the full-notch creep test ISO 16770 may better discriminate long-term performance under stress. Published data for the green GRN 6210 compound in these long-term tests is limited; qualification should use molded articles produced on the intended machine.
The colored formulation introduces separate regulatory requirements from the natural polymer. Food-contact suitability for the polyethylene base resin may be established under FDA 21 CFR 177.1520 for olefin polymers, but the green pigment and its carrier must also be suitable under 21 CFR 178.3297 or an equivalent colorant provision. In the European Union, food-contact plastics are assessed under EU Regulation 10/2011, which sets an overall migration limit of 10 mg/dm² for general food contact and includes specific migration limits for colorant components. A food-contact statement from LyondellBasell for the exact grade and color is required; the absence of such a statement means the material is not automatically cleared for food-contact applications.
For industrial and consumer applications, compliance with REACH Regulation (EC) 1907/2006 requires confirmation that the pigments and additives are registered or exempt and that no substance of very high concern exceeds 0.1% w/w. Restriction of hazardous substances compliance under Directive 2011/65/EU requires lead, cadmium, mercury, hexavalent chromium, PBB, and PBDE concentrations to remain below the thresholds in Annex II. Colorants are a common source of heavy metals, so the green pigment used in GRN 6210 should be covered by a RoHS certificate. Dust explosion hazards in processing are addressed under ATEX Directive 2014/34/EU or NFPA 652. The supplier safety data sheet is the binding document for dust explosion parameters, not the technical data sheet.
| Standard or regulation | Application boundary | Required evidence |
|---|---|---|
| FDA 21 CFR 177.1520 | Food-contact olefin polymer | Manufacturer food-contact statement for pigmented grade |
| EU Regulation 10/2011 | Food-contact plastics in EU | Overall migration and specific migration test data |
| REACH (EC) 1907/2006 | European chemical registration and SVHC | SDS and SVHC declaration |
| RoHS Directive 2011/65/EU | Electrical and electronic equipment | Heavy-metal and brominated flame retardant certificate |
| ATEX Directive 2014/34/EU | Dust explosion hazard in processing | Dust explosion data from SDS |
Compared with natural Icorene 3545, the GRN 6210 compound removes the need for dry blending a color masterbatch at the molding machine. Dry blending in automated rotational molding cells can cause pigment segregation, color streaks, and uncontrolled additive distribution. Factory coloring incorporates the pigment into the powder or compound under controlled conditions, improving batch-to-batch consistency. However, factory-colored powder can differ from natural powder in dry flow, bulk density, and static behavior because the colorant particles occupy space between polymer particles and can alter surface friction. No generic correction factor should be applied; the colored material must be tested as supplied.
Compared with another polyethylene family, high-density polyethylene has higher density, higher flexural modulus, and higher heat resistance but lower low-temperature impact and generally lower environmental stress crack resistance. Low-density polyethylene has easier processing in some applications but lower tensile strength and ESCR. Icorene 3545 GRN 6210 at 0.934 g/cm³ occupies an intermediate position, with greater stiffness than lower-density LLDPE and better ductility than HDPE. If a rotational molding application requires high chemical resistance in a large tank, an LLDPE such as Icorene 3545 may be chosen over HDPE for environmental stress crack resistance. If a part requires high dimensional stiffness under load, an HDPE or filled grade may be more appropriate.
| Polyethylene class | Typical density range | Branching architecture | Rotational molding trade-off |
|---|---|---|---|
| High-pressure LDPE | 0.915–0.935 g/cm³ | Long- and short-chain branches | Lower stiffness and ESCR; easier bubble removal |
| Conventional LLDPE | 0.915–0.940 g/cm³ | Predominantly short-chain branches | Higher tensile and ESCR; narrower densification window |
| HDPE | 0.940–0.970 g/cm³ | Low branching | Higher stiffness and heat resistance; lower impact |
| Metallocene LLDPE | 0.915–0.940 g/cm³ | Narrow composition distribution | Improved toughness and organoleptics; higher cost |
Adhesive bonding and painting of LLDPE rotomolded parts require surface oxidation because the polyolefin surface is nonpolar. Flame treatment or air plasma can raise surface energy from below 32 mN/m to above 40 mN/m. Bond strength should be checked by pull-off methods such as ISO 4624 or ASTM D4541. Without surface treatment, acrylic and epoxy adhesives may peel cleanly from the part. The green pigmented surface can also mask oxidation temperature differently than a natural surface, so treatment parameters should be revalidated on the colored compound.
Chemical resistance of polyethylene covers many aqueous acids, bases, and salts, but strong oxidizing acids, aromatic hydrocarbons, and chlorinated solvents can soften or stress crack the polymer. Polar surfactants and detergents may reduce environmental stress crack resistance even when visible swelling is absent. Immersion testing under ISO 175 or ASTM D543 in the intended chemical environment is therefore mandatory for critical tank and container applications. No generic compatibility table replaces testing on a molded part made from Icorene 3545 GRN 6210.
Outdoor use of the green compound requires a separate weathering stabilizer package. The green color may provide some visible light screening, but it does not automatically provide ultraviolet stability. Accelerated weathering can be evaluated under ISO 4892-2 or ASTM G155, with property retention measured by tensile elongation or impact after exposure. A color shift in the green part may occur before mechanical failure, so ΔE color difference should be included in the acceptance criteria. Linear thermal expansion should be measured by ISO 11359-2 or ASTM E831 for parts that must maintain gaps and fastener loads over a range of service temperatures.
Recycling of factory-colored LLDPE is possible but requires segregation by color and melt flow to maintain reproducibility. Reprocessing increases oxidation and may shift viscosity, surface finish, and color. Industrial regrind levels should be validated for impact retention and environmental stress crack resistance. The green colorant complicates sorting in mixed-polyolefin recycling streams; separate collection of production scrap is preferred over post-consumer mixed waste. Incoming inspection should include melt flow rate under ISO 1133-1:2022, density under ISO 1183-1, powder bulk density under ASTM D1895, sieve analysis under ASTM D1921, and color measurement by spectrophotometry using CIELAB coordinates with an agreed maximum ΔE tolerance.