Lyondellbasell Icorene 3545 Grn 6208 Polyethylene Linear Low Density

LyondellBasell Icorene 3545 GRN 6208 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 3545 GRN 6208 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 499863
    Product Name LyondellBasell Icorene 3545 GRN 6208 Polyethylene, Linear Low Density
    Manufacturer LyondellBasell
    Brand Icorene
    Grade 3545 GRN 6208
    Material Type Polyethylene, Linear Low Density
    Density 0.945 g/cm³
    Melt Index 3.5 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 18 MPa
    Tensile Strength At Break 22 MPa
    Elongation At Break 800%
    Flexural Modulus 800 MPa
    Vicat Softening Point 110°C
    Melting Point 130°C
    Hardness Shore D 55
    Color Green
    Form Pellets
    Processing Method Injection Molding

    As an accredited LyondellBasell Icorene 3545 GRN 6208 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 3545 GRN 6208 Linear Low Density Polyethylene is packaged in 25 kg bags, palletized for transport.
    Container Loading (20′ FCL) 20′ FCL loading for LyondellBasell Icorene 3545 GRN 6208 Linear Low Density Polyethylene: palletized bags, moisture-protected, secured for ocean transport.
    Shipping LyondellBasell Icorene 3545 GRN 6208 Polyethylene, Linear Low Density is shipped as non-hazardous solid resin pellets in moisture-resistant bags, octabins, or bulk trucks. It is not DOT/IMDG/IATA regulated. Store cool, dry, ventilated, away from sunlight and ignition sources. Use standard industrial handling equipment.
    Storage Store at ambient temperature in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, ignition sources, and incompatible materials such as strong oxidizers. Keep in original sealed bags or containers, palletized, off the floor, and protected from moisture, dust, and contaminants. Avoid excessive stacking; maintain FIFO. Use appropriate PPE and grounding when handling to prevent static.
    Shelf Life LyondellBasell Icorene 3545 GRN 6208 has a typical shelf life of 24 months when stored unopened, protected from heat, moisture, and sunlight.
    Application of LyondellBasell Icorene 3545 GRN 6208 Polyethylene, Linear Low Density

    Vertical chemical storage tanks rotomoulded from Icorene 3545 GRN 6208 are qualified by environmental stress crack resistance in the bottom knuckle radius and drain boss area, not by short-term tensile yield at 23 °C. The powder is charged into a cast-aluminium or fabricated steel mould after the mould surface has stabilized between 250 °C and 300 °C on a multi-arm carousel or shuttle line. Peak internal air temperature is held between 190 °C and 210 °C for wall sections from 6 mm to 12 mm; the heating plateau is extended in 2 min to 4 min increments when the wall exceeds 10 mm at the knuckle or when the mould has multiple flat side faces. Oven air velocity is set between 12 m/s and 20 m/s because lower velocities prolong the tacky powder phase and higher velocities can compact the outer skin before the inner surface has consolidated. Biaxial rotational speed ratio is derived from mould geometry; cylindrical tanks are commonly run at a primary-to-secondary ratio of 4:1, while rectangular tanks require dynamic ratio changes to prevent powder pooling at the end caps and inlet bosses. Release testing follows ASTM D1998-15 for polyethylene upright storage tanks and ASTM D1693-15 condition C for ESCR; the outer wall and bottom knuckle are sampled because the bottom wall solidifies last and retains residual hoop stress. The green 6208 pre-colour is compounded into the polymer and no dry pigment addition at the machine hopper is required. Reground material is the main lot-to-lot variable: if the release specification is 1,000 h to failure under ASTM D1693 condition C, regrind additions above 20% by weight should trigger re-qualification because repeated oven cycles deplete the stabilizer system and raise the crystalline fraction at the inner surface. Chemical compatibility for acids, alkalis, and oxidizers is not predicted from density or melt flow rate alone; immersion testing to ISO 175:2010 at the actual service temperature and concentration is required. For sodium hypochlorite and other oxidizing media, the specific stabilizer and pigment package has a measurable effect on surface crack initiation; published data for this green-coloured configuration is limited, so a contained immersion trial under the intended worst-case exposure is the only reliable qualification route.

    Why Does the Thickness Profile Around the Lifting Sleeve Control Drop Impact More Than the Flexural Modulus Does?

    Waste containers in the 1 100 L to 2 400 L class are rotomoulded as one-piece bodies with integrally moulded fork tines, lifting sleeves, and comb-lift rails. Failure during EN 840-5 drop testing at -18 °C occurs most often at the transition between the nominal 6 mm sidewall and the 14 mm to 18 mm boss around a steel lifting sleeve. The green 6208 pre-colour is opaque enough to hide thin-wall translucency, so in-line ultrasonic thickness measurement is required before the part cools below 70 °C. Impact performance is governed less by the 23 °C notched Izod value than by the local wall-thickness gradient and the orientation of the inner melt-flow line. When a mould is held in the oven until the internal air reaches 200 °C, the innermost layer remains molten while the outer layer has begun to cool; demoulding at surface temperatures above 90 °C can produce sink marks at the thick boss roots. These sink marks act as crack initiators in cold impact. For this reason, carousel operators often delay cooling-air onset by 60 s to 120 s after the mould leaves the oven and then apply forced air at 10 m/s to 15 m/s to set the outer skin before water mist cooling is allowed. The virgin powder to regrind ratio is typically held between 90:10 and 80:20 for bin walls because ESCR and low-temperature puncture resistance decline as the number of heat histories increases. Qualification to EN 840-5 is not sufficient by itself; municipal buyers often attach RAL-GZ 951/1 and a minimum of 500 h ESCR under ASTM D1693 condition C to the purchase specification. The table below summarizes the test matrix for a typical waste-bin release.

    Test targetStandardTypical release criterion
    Cold drop impactEN 840-5No crack or permanent deformation after 1.5 m drop at -18 °C
    Environmental stress crack resistanceASTM D1693-15 condition CMinimum 500 h without 50% of specimens failing
    Instrumented punctureISO 6603-2Energy at maximum load reported; no brittle failure at 23 °C
    Melt flow rateISO 1133-1:2022 at 190 °C/2.16 kgLot within supplier specification
    DensityASTM D1505Lot within supplier specification

    On shuttle machines with two mould arms, the oven return time and cooling station dwell time are matched so that the mould enters the cooling bay before the outer skin reaches 120 °C. If the mould is allowed to sag on the arm during charging, the powder distribution across the front face becomes uneven; the resulting wall thickness variation of ±1.5 mm can reduce the drop height at -18 °C by more than 1 m in production trials. This variation is batch-to-batch process noise, not polymer property loss, and is corrected by adjusting arm speed rather than by changing oven set point.

    Rotationally moulded marine buoys and flotation collars use the same pre-coloured powder but require lower oven-heat input in the outer shell because the closed air cavity creates a different thermal path than a solid chemical-tank wall. The wall thickness ratio between the outer skin and inner skin is often kept at 2:1 because the outer skin bears impact and UV load while the inner skin controls adhesion to the closed-cell foam core. Steel mooring plates are inserted before charging; the LLDPE must encapsulate the plate without leaving an unfused interface. A common production failure is observed when the plate is not preheated to 60 °C to 80 °C; condensation on the cold steel produces steam pockets during the moulding cycle and a thin unbonded ring around the boss. Preheating the inserts and applying a silane primer or abrasive-blasted surface reduces this failure. If a two-part polyurethane foam is filled in a second step, the foam exotherm can reheat the LLDPE wall above 90 °C, causing local sag; the foam fill volume is therefore limited and the part is placed in a water-cooled fixture during cure. The green 6208 pigment may shield visible light, but the UV stabilization of the base powder determines surface chalking resistance; for continuous marine exposure, an accelerated weathering test to ISO 4892-3 with a ΔE < 4.0 after 2 000 h is often specified. Saltwater absorption is low for LLDPE, typically below 0.1% by ASTM D570, but biofouling and cleaning chemicals can attack the surface, so compatibility of the specific green grade with harbour-service chemicals should be confirmed by immersion test. Published data for this green-coloured marine configuration is limited; buoy builders qualify each lot with a hydrostatic collapse test plus a 24 h water absorption check at the intended service depth.

    Hydrostatic Creep and Chlorine-Assisted Surface Oxidation in Rotomoulded Livestock Water Tanks

    Flat-side livestock water tanks with capacities from 100 L to 5 000 L are processed with the same powder but with different demoulding controls than chemical tanks because the large flat sidewalls are highly sensitive to post-mould warpage. Peak internal air temperature is held at 190 °C to 210 °C, and the part is not pulled from the mould until the surface temperature falls below 70 °C; demoulding above 80 °C allows the flat sidewall to bow inward as it cools unsupported. Cooling fixtures are used until the wall temperature drops below 60 °C. Hydrostatic creep is a long-term failure mechanism; the hoop stress in a rectangular tank is concentrated at the vertical corner and lower sidewall junction, not at the geometric centre of the flat face. The design must apply a service factor to the material’s creep modulus, not to its short-term yield strength. Published data for rotomoulded LLDPE hydrostatic design stress are less abundant than for pipe-grade HDPE; therefore tank builders use conservative service factors and do not transfer ISO 9080 pipe data directly to a flat-sided rotomoulded tank because residual stress distributions differ. Chlorinated drinking water at 0.5 mg/L to 2.0 mg/L causes surface oxidation only at scratches, mould-line knit marks, or pigment agglomerates; the green 6208 pigment masks early surface whitening, so end users may not see oxidative microcracks until leakage occurs. Sacrificial tabs moulded into the tank bottom are pulled and bent after accelerated ageing to detect embrittlement. The virgin-to-regrind ratio for these flat-side tanks is often limited to 80:20 or lower, and regrind is excluded entirely from the lower sidewall and corner zones if the tank is used with continuous sanitizer dosing. The table below lists the process-control ranges used on a typical agricultural tank line.

    ParameterControl rangeEquipment note
    Oven set point280–320 °CMulti-zone gas oven with 12–20 m/s air velocity
    Peak internal air temperature190–210 °CThermocouple through mould vent
    Cooling air temperature15–25 °CForced-air station before water mist
    Demoulding surface temperature≤ 70 °CInfrared pyrometer at four points on flat face
    Mould rotating speed ratio4:1 cylindrical / 2:1 rectangularAdjust primary and secondary axis speeds separately

    Water quality also affects the qualification route: tablets containing trichloroisocyanuric acid produce a local pH drop at the waterline, and the resulting acidic environment can accelerate surface crack growth at the waterline ridge. For such service, an immersion trial with a buffered chlorine solution at 40 °C for 1 000 h is more informative than a simple ASTM D1693 ESCR test alone.

    When a Rotomoulded Playground Slide Is Required to Meet EN 1176 Without a Secondary Coating

    For rotomoulded playground slides, tunnel sections, and climbing panels, the green 6208 pre-colour is integrated into the outer skin and no secondary coating is applied. Compliance with EN 1176-1:2017 covers impact absorption, entrapment gaps, structural integrity, and durability; the polymer surface is additionally evaluated for UV degradation and colorfastness through ISO 4892-2 cycle 1 xenon arc exposure. A colour change of ΔE < 3.0 after 3 000 h is commonly specified for public playground equipment, but the pass value depends on the procuring authority. Slide components have a high draw ratio; the powder must flow into the far end of a mould with a length-to-diameter ratio greater than 3:1 and a complex open-section shape. Lower melt flow rate grades retain more melt strength but require longer oven dwell; if the lot MFR under ISO 1133-1:2022 at 190 °C/2.16 kg is at the lower end of the supplier range, the oven dwell is extended and internal air temperature is raised to the upper plateau limit, otherwise the far end of the slide tunnel will be under-fused and show pinholes at the mould parting line. The dark green surface can reach skin temperatures above 80 °C in direct sun; because LLDPE has a low heat deflection temperature, unsupported flat areas may deform under a child’s load. Moulded ribs on the underside are required, with spacing set by finite-element warpage analysis rather than by a uniform rule. The raw material lot-to-lot stabilizer content has a direct effect on gloss retention and edge cracking after weathering; a retained notched impact test to ISO 6603-2 after 2 000 h of xenon arc exposure is used by some playground specifiers to ensure that the part remains ductile in winter.

    A Double-Skin Material-Handling Pallet Floor Has a Different Warpage Mechanism Than a Thin-Wall Bin

    When a material-handling pallet is rotomoulded as a double-skin structure, the top deck and bottom deck do not cool at the same rate; the top deck retains heat if it faces upward and the bottom deck is water-misted, producing a concave bow. The green 6208 pre-colour changes surface emissivity compared with natural resin, which can accelerate or slow the cooling rate of the outer skin depending on the mould finish. In production, an infrared pyrometer is used to measure four points on the top deck before demoulding; the pallet is not released from the mould or cooling fixture until the top deck surface temperature falls below 70 °C. The pillar height to deck thickness ratio is a critical process variable: when it exceeds 4:1, the unsupported deck sections between pillars are prone to sink and bow. Wall thickness distribution around the pillars is controlled by the rotational speed ratio and the amount of powder left in the mould after the first skin has formed; a primary-to-secondary ratio of 2:1 to 3:1 is commonly used for rectilinear pallet decks, but this ratio must be trimmed on the shop floor with thickness samples from the cold mould. Food-contact use, if required, is confirmed under FDA 21 CFR 177.1520 and EU Regulation 10/2011; the pre-colour package is the critical variable because it may not be covered by the base resin food-contact certificate. A separate migration test on the specific green grade is required for the intended food type and temperature. Pallet qualification also includes a distributed load creep test at 40 °C for 24 h and a flatness measurement after load removal; a permanent deflection greater than 2 mm per 100 mm of span is a typical rejection criterion.

    Free Quote

    Competitive LyondellBasell Icorene 3545 GRN 6208 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Specified as a rotational moulding powder in a green colour package, LyondellBasell Icorene 3545 GRN 6208 Polyethylene, Linear Low Density is a metallocene-catalysed linear low-density polyethylene compound supplied in 35-mesh powder form for single-shot and multi-shot rotational moulding. The suffix GRN 6208 is the LyondellBasell colour code; it identifies a precoloured green system in the Icorene 3545 base resin, not a separate resin grade. The base resin carries a nominal density of 0.935 g/cm³ determined by ISO 1183-1 and a melt mass-flow rate of 4.5 g/10 min at 190 °C/2.16 kg determined by ISO 1133-1. Those two values locate the product between lower-density flexible LLDPE grades and 0.945 g/cm³ HDPE rotomoulding grades, making it a candidate for moderate-stiffness parts that must retain impact and stress-crack resistance after cooling and in service. The green variant is not identical to the natural base resin: pigment and stabiliser loading can shift density and melt-flow values slightly, and the lot certificate of analysis should be used for release testing. Published mechanical data for the exact green-compounded configuration are more limited than for the natural Icorene 3545 powder; where end-use loadings are critical, the green compound should be validated on the intended part geometry.

    How does metallocene catalysis differentiate Icorene 3545 from conventional Ziegler-Natta LLDPE rotomoulding powders?

    The metallocene catalyst system produces a narrower molecular weight distribution and a more uniform short-chain branching distribution than conventional Ziegler-Natta LLDPE. In rotomoulding, this narrow distribution reduces the low-molecular-weight extractable fraction and lowers zero-shear viscosity at equal melt index, which accelerates densification at a given peak internal air temperature. The same feature narrows the overheat margin: once the internal air temperature exceeds 205 °C, the melt may become less viscous than an equivalent broad-MWD Ziegler-Natta rotomoulding powder, increasing the tendency to form drainage marks on vertical walls. Compared with a Ziegler-Natta LLDPE of similar 0.935 g/cm³ density and 4.5 g/10 min MFR, the metallocene grade typically has lower brittle temperature and lower organoleptic extractables; however, its lower demoulding modulus can increase surface tack on deep-draw moulds and may require longer cooling before ejection.

    On a production-scale three-arm carousel rotomoulding machine with a 2.5 m spherical mould diameter and propane-fired forced-air circulation, the powder charge is heated at oven air temperatures of 280–300 °C while the arm rotates at a 4:1 speed ratio. Internal air temperature is monitored with a shielded J-type thermocouple and used as the primary control variable; the working peak internal air temperature for Icorene 3545 GRN 6208 is 190–205 °C. If the internal air peak remains below 185 °C, incomplete particle coalescence produces subsurface porosity that reduces ARM impact energy in 6 mm plaques tested according to ASTM D5628. If the internal air peak exceeds 210 °C, antioxidant and colour stabiliser consumption accelerates, producing visible green shade drift, surface microvoids and a measurable loss of tensile elongation at break. Cooling rate is controlled to balance shrinkage and residual stress: forced-air cooling at mould surface rates above 10 K/min reduces warpage but freezes residual stress, while still-air cooling below 3 K/min increases crystallinity, modulus and vertical wall shrinkage. Ejection is performed only after the inner surface falls below 60 °C; premature release around metallic insert bosses produces localised deformation and cracking at insert weld lines.

    Mechanical and thermal reference values for the natural Icorene 3545 base resin

    The following values are typical for the natural base resin; the green GRN 6208 compound may show minor shifts because of pigment and stabiliser content.

    PropertyTest methodTypical value
    Density at 23 °CISO 1183-10.935 g/cm³
    Melt mass-flow rate, 190 °C/2.16 kgISO 1133-14.5 g/10 min
    Tensile stress at yieldISO 527-2, 50 mm/min17.0 MPa
    Tensile elongation at breakISO 527-2, 50 mm/min650 %
    Flexural modulus, secantISO 178760 MPa
    Vicat softening temperature, A50ISO 306118 °C
    DSC melting peakISO 11357-3126 °C
    Environmental stress-crack resistance, F50, 100 % Igepal CO-630ASTM D1693>1000 h

    Rotomoulded specimen conditioning should be conducted at 23 ± 2 °C and 50 ± 5 % relative humidity for at least 40 h before testing, as required by ISO 291. The values above are not design allowables; they are single-point comparative values and do not capture lot-to-lot variation, weld-line performance, or UV ageing. Tensile specimens should be taken from rotomoulded plaques, not injection-moulded plaques, because rotomoulding produces a characteristic skin-core morphology and a lower degree of orientation. When testing according to ISO 527-2, sample thickness should be reported; the use of a 2 mm microtensile specimen instead of a 4 mm plaque can overestimate elongation at break because large pigment agglomerates are statistically excluded from the reduced cross-section.

    When a green UV-stabilised rotomoulding grade is specified for outdoor water tanks

    Outdoor rotomoulded water tanks require the compounded green polymer to retain impact after prolonged solar exposure. The GRN 6208 colour package is intended to reduce photo-oxidative embrittlement in combination with the base polyolefin stabiliser system, but the exact pass/fail criteria for UV life are set by the moulding specification, not by the resin datasheet. Accelerated weathering according to ISO 4892-2 under a xenon-arc source with 0.35 W/m² irradiance at 340 nm is used to screen lot-to-lot consistency; retained tensile elongation is more informative than flexural modulus for detecting oxidative embrittlement. In a 10 mm nominal wall tank moulded at 200 °C peak internal air temperature and cooled in still air, the green outer surface can reach 15–25 °C above ambient under solar load, which lowers the effective long-term hydrostatic design stress. Moulders therefore place lifting lugs and threaded fittings away from high-stress planar sections and use stainless steel backing plates to distribute insert loads. Compared with a natural rotomoulding powder, the precoloured green compound eliminates post-moulding dry pigmentation; compared with a black UV-stabilised grade, it generally absorbs less solar infrared radiation, reducing outer wall temperature during service.

    In immersion service for agricultural sprayer and diesel containment tanks, slow crack growth at the insert weld line is more limiting than short-term tensile strength. Environmental stress-crack resistance is measured on compression-moulded notched specimens according to ASTM D1693 in 100 % Igepal CO-630 at 50 °C; the natural base resin typically yields F50 values above 1000 h, while the green compound requires separate verification because pigment particles can act as stress concentrators at low thicknesses. For a 5 mm nominal wall tank with a wound-in BSP brass fitting, the insert-to-polymer weld line creates a thickness gradient and a residual stress field; a full-scale hydraulic pressure test at 1.5 times the service pressure is therefore a more relevant acceptance measure than a datasheet value. The 0.935 g/cm³ density places the product below typical 0.945 g/cm³ HDPE rotomoulding grades in flexural modulus, but gives better low-temperature impact and slow crack resistance in many geometries. Compared with cross-linked polyethylene rotomoulding grades, it offers a defined melting and recycling route; compared with LDPE of similar melt flow, it has higher tensile strength and elevated temperature resistance under continuous load.

    Dry-flow, bulk density and particle-size distribution control for Icorene 3545 GRN 6208

    Rotomoulding powders are released against powder-handling parameters that data sheets for pelletised grades do not include. Bulk density measured by ISO 60 and dry-flow time measured by ASTM D1895 are therefore critical for automatic feed systems and for obtaining consistent wall thickness. The 35-mesh grind suppresses the fraction above 500 μm, which can entrap gas and create bubble defects, but the green compound may generate a higher fines fraction below 75 μm if static charging is not controlled during grinding. A dry-flow time below 30 s at 23 °C and 50 % relative humidity is generally accepted for rotomoulding powders of this class; however, the value is equipment-dependent, and a powder that flows well in a flat-bottom hopper may bridge in a non-ventilated cone hopper on a shuttle machine. When charging a 2.1 m³ tank mould with a 100 kg single-shot charge, the arm is held at a fixed angle during loading to distribute the powder across the parting line before rotation begins. This reduces the common failure mode of bottom-heavy wall sections produced by non-uniform powder packing.

    Measuring sintering lag across a 6 mm wall section with thermocouple-instrumented moulds

    When a 6 mm wall section is heated on a forced-air rotomoulding machine, the outer mould surface reaches 230–250 °C while the inner air temperature may still read 150–160 °C; the difference is not a temperature error but the conduction lag across the powder bed. The lag is governed by the thermal diffusivity of the polymer, approximately 1.1 × 10⁻⁷ m²/s, and by the contact resistance between the rotating powder and the mould surface. During the first 2–3 min of heating, the powder bed densifies and the effective thermal conductivity rises from 0.1 W/m·K in the loose powder state to 0.25–0.35 W/m·K as sintering proceeds. Because the green compound has a slightly higher surface-to-volume ratio than the natural powder at the same mesh cut, its pigment particles may increase radiation absorption in the near-infrared band, but the effect on conduction lag is smaller than the effect of wall thickness. For a 10 mm wall, the required dwell time after the inner air reaches 190 °C is therefore not double the 5 mm dwell time; it follows a non-linear relationship with wall thickness, especially when the mould is fabricated from stainless steel with a lower thermal conductivity than aluminium.

    Because the base polyolefin is an olefin polymer as defined in FDA 21 CFR 177.1520, natural Icorene 3545 may be suitable for food-contact layers when the fabricator validates processing conditions, extractives and end-use migration; the green compound requires separate compliance verification for the pigment system. REACH and RoHS statements should be confirmed in the supplier product safety summary. Storage at relative humidity above 70 % should be avoided or followed by powder conditioning, because moisture reduces dry-flow and contributes to microbubbles during sintering. In closed packaging at 15–30 °C, the product is typically assigned a 24-month shelf life; beyond that interval, antioxidant and UV stabiliser levels should be revalidated before structural parts are moulded. Avoid blending with amine-based antistatic concentrates unless the supplier has verified compatibility with the metallocene resin and the phenolic stabiliser package; such additives can interfere with stabiliser performance and produce surface blooming.