    Specifications
    HS Code 764951
    Density 0.935 g/cm3
    Melt Flow Rate 4.5 g/10 min
    Tensile Strength At Yield 11.0 MPa
    Tensile Strength At Break 24.0 MPa
    Elongation At Break 700%
    Flexural Modulus 400 MPa
    Vicat Softening Point 100 °C
    Melting Point 125 °C
    Haze 10%
    Gloss 70%
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 150 g
    Elmendorf Tear Strength Td 300 g
    Coefficient Of Friction 0.2

    As an accredited LyondellBasell Icorene 3545 BZO 9647 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 3545 BZO 9647 Polyethylene, Linear Low Density is supplied in 25 kg moisture-resistant bags on 1,000 kg pallets.
    Container Loading (20′ FCL) 20′ FCL container loaded with LyondellBasell Icorene 3545 BZO 9647 Linear Low Density Polyethylene, packaged securely for safe ocean transport.
    Shipping LyondellBasell Icorene 3545 BZO 9647 LLDPE ships as non-hazardous solid resin pellets, typically in 25 kg bags or 1,000 kg bulk bags on pallets. Transport in dry trucks, railcars, or containers; keep clean, dry, and away from excessive heat, sunlight, and contamination. No special dangerous-goods classification.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original containers tightly closed, palletized, and off the floor to prevent moisture pickup. Protect bags from punctures, physical damage, and prolonged sunlight. Maintain good housekeeping to control dust and static. Follow local regulations and the manufacturer’s SDS.
    Shelf Life No specific shelf life; stable under normal storage conditions when kept cool, dry, and protected from UV light and contaminants.
    Application of LyondellBasell Icorene 3545 BZO 9647 Polyethylene, Linear Low Density

    LyondellBasell Icorene 3545 BZO 9647 is supplied as a black, UV-stabilized linear low-density polyethylene powder intended for biaxial rotational molding of medium-walled industrial articles. Melt flow rate determined in accordance with ISO 1133-1:2022 at 190 °C and 2.16 kg is 4.5 g/10 min, and density determined by ASTM D1505-18 is 0.934 g/cm³. The compound contains carbon black and a UV stabilizer package at a loading that provides the stated outdoor weatherability without post-molding stabilization. Powder sieve retention is typically controlled to a 35 mesh (500 µm) top cut by air-mill pulverization, because rotomolding requires low-fines content and controlled bulk density to prevent bridging in mold charging stations. The downstream sectors below are limited to those in which rotomolded linear low-density polyethylene of this density and melt index is processed on production-scale multi-axis carousel or shuttle machines, where semicrystalline wall formation, environmental stress crack resistance, and short-chain branching distribution control service behavior.

    The following compliance checklist matrix spans the downstream domains in which the grade is used. Regrind limits refer to dry-blended fines screened through a 35 mesh (500 µm) sieve and dried to 0.05 wt% moisture content before loading.

    Application domainPrimary standard designationCritical service variableRegrind limit
    Static chemical storageASTM D1998-15; ASTM D1693-15Peak internal air temperature 190–210 °C20 wt%
    Agricultural water and fertigation reservoirsASTM G154, Cycle 1; ASTM D638-14Cooling rate 3 °C/min from 100 °C to 60 °C15 wt%
    Marine fendering and buoyancy modulesISO 6603-2:2023; ASTM G85-19, Annex A5Peak internal air temperature 195–210 °CSkin layer 0 wt%
    Dry-material handling and intermediate bulk containersASTM D4169-22, distribution cycle 6Top-load compression 2,500 kg20 wt%
    Diesel exhaust fluid storageISO 22241-3:2017; ASTM D638-14Peak internal air temperature 188–200 °CFluid-contact layer 0 wt%

    For stationary acid and alkali storage vessels, the as-supplied powder is charged at 100% by weight of the mold charge; no additional carbon black, hindered amine light stabilizer, or antioxidant masterbatch is required. Where internally generated regrind from trimmed tank lids and manway cut-outs is used, the addition ratio is limited to 20 wt% of the total charge, and the regrind must be screened to 35 mesh and dried to 0.05 wt% moisture content before dry blending. Exceeding 25 wt% regrind reduces low-temperature impact and raises the brittle-to-ductile transition because prior thermo-oxidative exposure shortens the tie-molecule population. Rotational molding is carried out in a biaxial carousel machine with a 4:1 rotational arm speed ratio, using fabricated steel or cast aluminum molds preheated to 60–80 °C. Oven setpoint is 290–320 °C, and the peak internal air temperature measured by a Rotolog-type probe is held between 190 °C and 210 °C for 25–40 min depending on wall thickness. At peak internal air temperatures below 185 °C, insufficient particle sintering leaves pinholes at weld lines; above 220 °C, oxidative degradation raises melt flow index, causing wall-thickness thinning at outer corners and dewetting at the mold surface. Cooling proceeds by forced ambient air until internal air temperature falls below 90 °C, followed by water mist cooling to 40–50 °C before demolding. Mold release is a semi-permanent PTFE-based system applied to the tool at 0.5–1.0 g/m². Vessels are designed and validated to ASTM D1998-15 for polyethylene upright storage tanks, and environmental stress crack resistance is monitored on compression-molded plaques by ASTM D1693-15, Condition A, 100% Igepal CO-630. End product types include vertical cylindrical tanks from 100 L to 20,000 L, horizontal transport tanks with baffles, and secondary containment basins for 5–10 wt% dilute mineral acids and alkali solutions. Service with strong oxidizing acids above 20 wt% concentration or aromatic hydrocarbon solvents above 40 °C is outside the resin’s resistance window.

    Which Peak Internal Air Temperature Window and Cooling Path Prevent Pinhole Formation in Agricultural Fertigation Reservoirs?

    Agricultural water and fertigation reservoirs require a balance between low-cost rapid cycling and long-term UV resistance in contact with dilute ammonium nitrate, urea, and sodium hypochlorite rinse solutions. The mold charge is 100% Icorene 3545 BZO 9647; if hot-washed regrind from retired tanks is used, it is capped at 15 wt% because fertilizer residues accelerate oxidative chain scission during regrind. No additional UV absorber or pigment masterbatch is added; the BZO 9647 formulation contains the UV stabilization package and carbon black dispersion required for outdoor service. Processing uses a shuttle-type biaxial rotomolding unit with oven setpoint 280–310 °C, peak internal air temperature not exceeding 205 °C for nominal 6 mm walls, and a cooling cycle that avoids forced air quenching from above 100 °C down to 60 °C at a rate faster than 3 °C/min, which otherwise causes differential shrinkage and bowing in flat tank walls. Mold cavity texture is maintained at 60–80 µm Ra to minimize surface gloss variation and to mask flow lines. Weatherability is assessed by ASTM G154, Cycle 1, with UVB-313 lamps, for 2,000 h, with retained tensile elongation measured by ASTM D638-14. Published data for this specific compound under full-sun Arizona xenon arc is limited, so service replacement is based on field inspection rather than laboratory extrapolation. Terminal products include horizontal water reservoirs, vertical fertigation day tanks, distribution troughs, and nursery bench liners.

    Marine Fender Shells and Buoyancy Modules Under Salt-Spray Carbon Black Retention and Low-Temperature Puncture Toughness

    Marine fender shells and foam-filled buoyancy modules expose the rotomolded wall to intermittent immersion, ultraviolet reflection from water, wave-induced flexure, and collision. The outer shell is rotomolded from 100% as-supplied powder; regrind is not allowed in the skin layer for marine service because prior heat history and salt contamination reduce environmental stress crack resistance after 5,000 h intermittent saltwater contact. If a foam-filled core is used, the skin layer is molded first and the foam is injected after demolding; no external color or stabilizer masterbatch is added to the skin. The tool is rotated at a 4.5:1 primary-secondary arm ratio to control wall-thickness distribution around complex convex shapes. Oven setpoint is 300–330 °C, peak internal air temperature is held at 195–210 °C for 30–50 min, and cooling is staged through forced air to 70 °C, then water mist to 35 °C. Sudden water quench before internal air temperature falls below 70 °C creates internal voids at the foam-skin interface, reducing adhesion. Impact resistance is tested according to ISO 6603-2:2023 at −20 °C, and cyclic corrosion resistance is assessed by ASTM G85-19, Annex A5, for 1,000 h using synthetic seawater electrolyte. End product types include harbor mooring buoys with a wall thickness of 8–12 mm, cylindrical fender shells, and quay-side corner blocks.

    Intermediate bulk containers, dry-material hoppers, and pallet tanks used in solids transfer are rotomolded from a charge containing 80 wt% virgin Icorene 3545 BZO 9647 and 20 wt% clean, thermally converted regrind. The regrind is generated from post-industrial trimmings only and is extruder-melt filtered through a 100 mesh screen before ambient grinding; post-consumer recyclate is not used because residual moisture and odor affect odor-sensitive food-grade granular transport. The dry blend is loaded into cast aluminum tools with a designed wall thickness of 4–6 mm, and the biaxial carousel operates at an oven setpoint of 285–315 °C, with peak internal air temperature limited to 195–205 °C. For hopper surfaces, a medium-density polyethylene tie layer is not required; the LLDPE wall supports welded cone couplers and discharge spouts. Shipping validation is performed according to ASTM D4169-22 distribution cycle 6, with top-load compression assessed at 2,500 kg on a four-way-entry pallet base. Terminal products include 500–1,500 L intermediate bulk containers, cone-bottom powder hoppers, and stackable open-top tote boxes.

    When Low-Warpage Vertical Walls and Ultrasonic Weldable Fittings Are Required for Diesel Exhaust Fluid Storage

    Diesel exhaust fluid storage requires rotomolded tanks that do not release ionic contaminants into high-purity urea solution. The tank body is rotomolded from 100% virgin Icorene 3545 BZO 9647; no regrind is permitted in the fluid-contact layer because regrind from mixed colored parts may contain metal fines and sodium ions that exceed ISO 22241-3:2017 cleanliness requirements. An inner liner is not required, but the mold must be purged with nitrogen during heating to reduce surface carbonyl formation at peak internal air temperatures above 210 °C. The biaxial rotation ratio is 4:1, and the oven setpoint is 290–320 °C with peak internal air temperature between 188 °C and 200 °C. A slower cooling rate from 100 °C to 60 °C at 2–4 °C/min preserves flat vertical walls for ultrasonic welding of spigots and level-sensor bosses. Wall thickness at weld bosses is locally increased to 8 mm by mold inserts to provide a 0.5 mm interference fit. Fluid-contact behavior is validated by the extraction protocols of ISO 22241-3:2017 for urea solution storage components; mechanical properties are checked by ASTM D638-14 and a weld burst test at 200 kPa internal pressure. End products include vertical day tanks, transportable DEF totes, and mobile service cart reservoirs.

    Free Quote

    Competitive LyondellBasell Icorene 3545 BZO 9647 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 3545 BZO 9647 is a linear low density polyethylene grade supplied as a UV-stabilized rotational molding resin. The BZO designation identifies a black, UV-stabilized package, and the numerical suffix 9647 is the supplier’s color and packaging code. The base polymer is a butene-copolymer linear low density polyethylene intended for conversion in powder form rather than pellet form, because rotational molding requires fine, free-flowing material capable of sintering against a heated mold surface under biaxial rotation. On production-scale pulverizing lines, the resin is typically ground through disk mills to a powder passing 35 mesh (500 µm) or finer, with retained fractions on 1.0 mm screens held below 5% by mass. The ground powder is then charged into cast-aluminum or fabricated steel molds and heated in forced-air convection ovens.

    Primary specification controls include density and melt flow rate. Under ISO 1183-1:2019, the nominal density is 0.935 g/cm³; melt flow rate determined by ISO 1133-1:2022 at 190°C and 2.16 kg is 4.5 g/10 min. These values place the grade in the medium-flow linear low density polyethylene rotomolding window, where powder consolidation, bubble dissolution, and densification occur before oxidative degradation becomes the dominant process variable. A density of 0.935 g/cm³ positions the product between conventional high-pressure low density polyethylene and unimodal high density polyethylene, providing a balance of stiffness, stress-crack resistance, and low-temperature ductility. The melt flow rate is not a complete rheological description; zero-shear viscosity and melt elasticity control particle coalescence, and published data for this specific configuration is limited. Supplier rheology data should therefore be requested when optimizing tooling for tight wall-thickness tolerances.

    What distinguishes Icorene 3545 BZO 9647 from general-purpose LLDPE film and injection molding grades?

    General-purpose linear low density polyethylene film grades are commonly designed with melt flow rates below 2.0 g/10 min and narrow molecular weight distributions for bubble stability and dart impact; injection molding grades may exceed 20 g/10 min to fill thin-wall tooling. Icorene 3545 BZO 9647 is positioned between these extremes. The 4.5 g/10 min melt flow rate under ISO 1133-1:2022 supports powder coalescence at rotomolding oven temperatures without excessively low melt viscosity, which can cause sag or nonuniform wall distribution. The butene-branch distribution imparts higher environmental stress-crack resistance than an equivalent-density high density polyethylene homopolymer, but the grade is not optimized for film blowing, cast film, or high-shear injection molding. Its stabilization package and black pigment loading are selected for long oven dwell and exterior exposure, not for high-temperature film extrusion or thin-wall injection filling. Compared with metallocene-catalyzed linear low density polyethylene rotomolding grades, the product may exhibit a broader melting range and lower melt strength; operator adjustment of peak internal air temperature is therefore required when transferring tooling from a metallocene resin.

    In forced-air convection ovens, tooling surface temperature controls cycle time more than oven setpoint alone. Typical oven setpoints for this grade are 270–300°C, with the internal air temperature of the mold reaching 190–220°C before cooldown is initiated. Peak internal air temperature is measured by thermocouples inserted through the vent tube. For a 6 mm wall section, production cycles frequently require 18–25 min of oven residence, followed by forced-air cooling to 80°C or lower before demolding. Cast aluminum tooling generally provides better heat transfer than fabricated steel and can reduce cycle time by 10–15% at equivalent wall thickness. Sheet steel molds should be kept below 300°C surface temperature to avoid localized degradation of the UV-stabilized powder. The powder charge should be conditioned to a dry, free-flowing state; if condensation is observed on pellet or powder surfaces, pre-drying at 60°C for 2 h in a dehumidified air dryer is sufficient to reduce surface moisture before pulverizing.

    Mechanical performance values and standard-method anchors

    PropertyTest methodNominal value
    DensityISO 1183-1:20190.935 g/cm³
    Melt flow rate, 190°C/2.16 kgISO 1133-1:20224.5 g/10 min
    Tensile stress at yieldISO 527-2:201218 MPa
    Tensile strain at breakISO 527-2:2012>600%
    Flexural modulusISO 178:2019550 MPa
    Vicat softening temperature, A50ISO 306:2022112°C
    Brittleness temperatureASTM D746-20-70°C
    Environmental stress-crack resistance, F50, 100% IgepalASTM D1693-21>1000 h

    The values in the table are nominal lot averages and do not replace a certificate of analysis or specification limit. Lot-specific density and melt flow rate are determined on each manufactured lot; mechanical values may vary with specimen preparation, cooling rate, and rotomolded wall thickness. The tensile and flexural values are influenced by mold cooldown rate, and rapid cooldown of a rotomolded part can reduce crystallinity and flexural modulus while increasing impact ductility. For comparative specification work, the test specimen should be cut from flat regions of rotationally molded plaques with consistent wall thickness and known internal air temperature history.

    Rotational molding applications for this grade include agricultural water tanks, chemical storage vessels, marine buoys, equipment housings, outdoor enclosures, and custom industrial parts. The black UV-stabilized package is intended for exterior exposure, but actual weathering service life must be validated by part thickness, geographic UV dose, and surface oxidation. For chemical containment, environmental stress-crack resistance under ASTM D1693-21 is not a substitute for full chemical immersion testing in the service fluid. Large flat panels have exhibited edge warpage under rapid cooldown when demolding below 60°C was delayed or mold release was unevenly applied; constrained cooling fixtures and hot jigs are used on production lines to maintain dimensional stability. Potable water contact should not be assumed without grade-specific regulatory documentation under EU Regulation (EU) 10/2011 or FDA 21 CFR 177.1520. The supplier must confirm the applicable regulatory status for the lot and packaging code.

    If the product is processed by rotational molding at elevated wall thickness, additional thermal controls are required

    At wall thicknesses above 10 mm, peak internal air temperature should be raised in 5°C increments rather than extending the oven cycle at constant temperature. Thick sections increase the time required for powder densification and bubble removal; however, prolonged exposure above 220°C internal air can consume the antioxidant package and increase the carbonyl index detected by Fourier-transform infrared spectroscopy. Production experience indicates that internal air temperature should not exceed 230°C for cycles longer than 30 min, because oxidative degradation of the butene-copolymer backbone can reduce impact strength even when melt flow rate remains within specification. For cooling, a staged profile is used: forced air to 100°C at 10–15°C/min, then water mist if the mold design permits, followed by still-air cooling to 60°C before demolding. This minimizes warpage and preserves the low-temperature impact properties measured by ASTM D746-20.

    Compared with high density polyethylene rotational molding grades having density above 0.945 g/cm³, Icorene 3545 BZO 9647 has lower flexural modulus and lower heat deflection temperature, but superior environmental stress-crack resistance and lower brittleness temperature. The product therefore suits large tanks and containment structures where wall deflection is not the primary failure mode and where low-temperature impact is a design requirement. Compared with highly flexible metallocene grades below 0.920 g/cm³, the product provides higher stiffness and better dimensional stability, but lower elongation at break. The use of butene comonomer rather than hexene or octene can influence long-term creep resistance; for load-bearing parts operating continuously above 60°C, dynamic mechanical analysis and creep testing under ISO 899-1:2017 or ISO 899-2:2015 should be performed before specification. Fuel tank applications require additional permeation and weldability testing under UNECE R34 or EPA protocols, because the base resin is not a barrier polymer.

    Material specifications should always include lot-specific density, melt flow rate, UV additive content, and powder particle-size distribution. The product is not suitable for rotomolding parts requiring continuous service above 60°C under high external load without supplemental creep data. Heat deflection temperature under ISO 75-2:2013 at 0.45 MPa is typically below that of high density polyethylene rotomolding grades. Surface oxidation during extended oven cycles can reduce the effectiveness of the UV stabilization package; therefore, the oven temperature should be verified with air-temperature profiling rather than infrared surface readings alone. For parts exposed to strong oxidizing agents or long-term hot water above 60°C, the resin should be evaluated in the specific service environment before production release.