| HS Code | 189321 |
| Density | 0.935 g/cm3 |
| Melt Flow Rate 190 C 2 16 Kg | 3.5 g/10 min |
| Tensile Strength At Yield | 14.0 MPa |
| Tensile Strength At Break | 24.0 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 500 MPa |
| Vicat Softening Temperature | 100 °C |
| Melting Point | 125 °C |
| Hardness Shore D | 50 |
| Thermal Conductivity | 0.33 W/m-K |
| Specific Heat Capacity | 2.3 J/g-°C |
| Water Absorption | <0.01% |
| Dielectric Constant | 2.3 |
| Volume Resistivity | 1e16 ohm-cm |
| Dielectric Strength | 20 kV/mm |
| Processing Temperature | 180-220 °C |
| Mold Shrinkage | 1.5-3.0% |
As an accredited LyondellBasell Icorene 3545 BWN 8810 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 3545 BWN 8810 Polyethylene, Linear Low Density is supplied in 25 kg bags, 40 per 1,000 kg pallet. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with LyondellBasell Icorene 3545 BWN 8810 Linear Low Density Polyethylene, palletized and secured for transport. |
| Shipping | LyondellBasell Icorene 3545 BWN 8810 is a non-hazardous linear low-density polyethylene resin. Transport in sealed bags, sacks, or octabins, keeping dry and protected from contamination, sunlight, and excessive heat. Secure loads during shipment. Normally no DOT/IMDG/IATA hazard classification applies; verify current SDS and local regulations. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizing agents. Keep containers or bags tightly closed to prevent moisture, dust, and contamination. Use appropriate grounding to avoid static buildup. Maintain clean, dry floors; avoid prolonged UV exposure and temperatures above 50°C. Follow local regulations and the manufacturer’s safety data sheet. |
| Shelf Life | Shelf life is typically 24 months when stored unopened in original packaging, protected from heat, moisture, and direct sunlight. |
In potable water storage tank production, the powder is dry-charged into cast aluminium or steel mould shells at 100 wt% virgin Icorene 3545 BWN 8810 and rotationally moulded on shuttle-type equipment with arm ratios from 4:1 to 5:1. The compliance position for North American installations is governed by NSF/ANSI 61 for potable water contact; where the finished tank is used as a food-contact vessel, FDA 21 CFR 177.1520 olefin polymer provisions apply, and European market entries are assessed under EU Regulation No 10/2011 with migration testing according to EN 1186-1:2002. No post-industrial or post-consumer regrind is introduced because the certification chain requires full traceability of the compounded carbon black and stabiliser package to the LyondellBasell lot certificate. If regrind from the same tank plant is introduced after melt-flow verification, it is held at or below 10 wt% and each lot is re-qualified for extractables.
Processing on a biaxial rotomoulding line uses oven set points of 280–300 °C, with internal air temperature sensors recording peak values of 185–195 °C before forced-air cooling begins. Wall thickness is maintained at 5–8 mm for tanks up to 5,000 L. Batch-to-batch variance in powder dry flow is controlled at the feed hopper with vibratory pads to prevent bridging, and a lot-specific density check by ISO 1183-1:2019 plus melt flow-rate verification under ISO 1133-1:2022 brackets the incoming powder before charging. Published typical values for the grade place density at 0.934–0.936 g/cm³ and MFR at 4.5 g/10 min. The terminal product type is a vertical or conical water storage tank from 200 L to 10,000 L for residential, agricultural and emergency water supply installations.
Agricultural chemical storage and sprayer tank bodies operate under a more aggressive stress-cracking load than potable water service. The compounding formula uses 100 wt% virgin Icorene 3545 BWN 8810 powder; clean internal regrind from the same production cell may be added up to 5 wt% when wall-section opening trials show no reduction in environmental stress crack resistance under ASTM D1693-15 condition B in 10% Igepal CO-630 at 50 °C. Compliance for stationary thermoplastic chemical storage tanks above ground is evaluated under EN 13575:2012, and the final article must be registered under REACH (EC) No 1907/2006 for the specific chemical service. The tank manufacturer is responsible for validating the compatibility of the LLDPE with the contained active ingredient, particularly for concentrated fertilizer salts, emulsifiable concentrates and oil-based spray adjuvants.
The downstream process uses drop-arm or carousel rotational moulding machines with infrared pyrometry tied to the mould interior. The powder is specified through 35 mesh (500 µm) sieve retention limits, and particle-size distribution is checked by ASTM D1921-18 when dry-flow anomalies appear. Oven air temperature is held at 280–310 °C, while the mould surface is allowed to reach 190–200 °C for a minimum of 8–12 min to eliminate entrapped porosity at weld lines. Terminal products include sprayer tanks from 300 L to 1,500 L, fertiliser induction hoppers and slow-release chemical basins.
| Application sector | Compliance standard | Formula addition/regrind limit | Process control band | Finished product |
|---|---|---|---|---|
| Potable water storage | NSF/ANSI 61; FDA 21 CFR 177.1520; EU 10/2011 | 100 wt% virgin; regrind ≤ 10 wt% | Oven 280–300 °C; internal air 185–195 °C | 200–10,000 L cisterns |
| Agricultural chemical storage | EN 13575:2012; REACH | 100 wt% virgin; regrind ≤ 5 wt% | Oven 280–310 °C; mould 190–200 °C | 300–1,500 L sprayer tanks |
| Diesel/heating oil storage | EN 13341:2005+A1:2011; UNECE R34 | 100 wt% virgin; regrind 0 wt% unless ESCR > 500 h | Oven 275–290 °C; internal air ≤ 200 °C | ≤1,000 L fuel tanks |
| Playground and street furniture | EN 71-3:2019+A1:2021; ASTM F1487-21 | 100 wt% virgin external; regrind ≤ 20 wt% hidden | Oven 270–290 °C; demould ≤ 70 °C | Slide shells, seating panels |
| Industrial IBC and dry-bulk hoppers | UN 31H1 where applicable | Virgin 70–80 wt%; regrind 20–30 wt% | Oven 280–300 °C; wall 6–10 mm | 1,000 L IBC bodies |
| Municipal waste containers | EN 840-1:2020; EN 840-5:2020 | Virgin 95–100 wt%; regrind ≤ 5 wt% | Oven 280–310 °C; air peak 190–200 °C | 120–1,100 L refuse carts |
In stationary diesel and heating oil storage, the wall stock formula is constrained by environmental stress cracking rather than by tensile strength. Icorene 3545 BWN 8810 is charged at 100 wt% virgin powder when the finished tank must meet hydrocarbon permeation and ESCR requirements under EN 13341:2005+A1:2011 or UNECE Regulation No 34 for vehicle-mounted fuel tanks. Regrind is not admitted in barrier-critical parts because even clean in-house regrind at 15 wt% can reduce ASTM D1693-15 condition B time-to-failure to below 300 h in some lot histories. Published data for this specific grade and regrind configuration is limited, so the tank builder imposes a 0 wt% regrind rule unless lot-specific ESCR data above 500 h are available.
The processing route begins with biaxial rotational moulding on rock-and-roll equipment with internal air temperature sensors, followed by post-mould fluorination of the inner surface where the service fluid demands hydrocarbon barrier below the base LLDPE permeation level. Oven set points are held tighter than general tank moulding, at 275–290 °C, because excessive internal air temperature above 200 °C creates crystallinity gradients that lower notch resistance. Wall thickness is set at 4–6 mm for tanks up to 1,000 L. Terminal products are diesel day tanks, heating oil tanks and generator set fuel reservoirs.
A shuttle-type rotational moulding cell running Icorene 3545 BWN 8810 for playground enclosures relies on the black compounded UV stabiliser system already present in the grade; no additional masterbatch is compounded at the moulder. The addition ratio is 100 wt% virgin powder for visible external surfaces, while clean internal regrind may replace up to 20 wt% of virgin material in hidden ribs or non-impact zones after ASTM D256-23 Izod tests on moulded plaques show loss of less than 10% relative to all-virgin plaques. Compliance for the finished articles includes EN 71-3:2019+A1:2021 for migration of certain elements and ASTM F1487-21 for public playground equipment where the product is installed in North America; REACH obligations apply to EU supply.
The production process uses dual-axis shuttle machines with oven air temperature 270–290 °C and mould surface temperature 180–190 °C. Demoulding is not initiated until the mould surface falls below 70 °C to limit warpage on large flat panels. Terminal finished product types include slide shells, tunnel segments, seating shells and activity panels.
Material handling hoppers and rigid intermediate bulk containers for non-aggressive dry goods use a higher regrind fraction because the dominant failure mode is impact and abrasion rather than ESCR. The compounding addition is 70–80 wt% virgin Icorene 3545 BWN 8810 with 20–30 wt% clean in-house regrind that has passed a 35 mesh sieve after shredding and cryogenic grinding. Clean regrind is reprocessed on a corotating twin-screw extruder with L/D 36:1 at 190–210 °C before cryogenic grinding to 35 mesh. Compliance is defined by UN Model Regulations for transport of dangerous goods, specifically Type 31H1 rigid plastics IBC with structural equipment when the product is certified for liquid or solid dangerous goods; for non-hazardous service, the standard is internal and tied to ISO 1133-1:2022 melt flow and ASTM D638-14 tensile verification.
Production occurs on rock-and-roll machines with extended ovens to accommodate 1,250 L cavity volumes. Oven air is controlled at 280–300 °C, internal air temperature peak is 185–195 °C, and wall thickness is held between 6–10 mm. Terminal products are dry bulk hoppers, seed boxes, mineral sample trays and 1,000 L rigid intermediate bulk container bodies.
Under impact-dominated municipal service, refuse cart and waste container bodies are moulded from Icorene 3545 BWN 8810 at 95–100 wt% virgin powder with 0–5 wt% internal regrind where the client specification mandates full virgin material for hinges and axles. Compliance for mobile waste and recycling containers is evaluated under EN 840-1:2020 and EN 840-5:2020, which include dynamic impact and fatigue testing. The carbon black content of the finished wall is verified by ASTM D4218-20 to confirm UV stabilisation, with target values in the 2.0–2.5 wt% range for waste containers intended for outdoor exposure beyond 5 years.
Shuttle rotomoulding lines run oven temperatures of 280–310 °C and internal air peak at 190–200 °C. The mould cavities are textured to reduce surface marking, and forced-air cooling is followed by water mist at 60–70 °C to improve dimensional stability of the rim. Terminal finished products include 120 L, 240 L, 660 L and 1,100 L refuse containers with injection-moulded or rotomoulded lids.
Competitive LyondellBasell Icorene 3545 BWN 8810 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 3545 BWN 8810 is a linear low-density polyethylene powder supplied for rotational moulding and related powder-processing operations. The supplier’s grade nomenclature is consistent with a nominal density of 0.935 g/cm³ and a melt-flow rate of 4.5 g/10 min when measured at 190 °C under a 2.16 kg load using ISO 1133-1:2022. The BWN 8810 suffix denotes a defined stabiliser addition; the grade is released as a natural-colour, UV-stabilised powder intended for outdoor service and low-temperature impact. The product is ground to a controlled powder particle-size distribution rather than pelletised, which differentiates it from LLDPE film-extrusion grades that contain slip, antiblock, and flow-control additives. In rotational moulding, the powder must flow into thin ribs and complex undercuts after the mould is charged and rotated under heat; particle morphology and sieve distribution therefore control wall-thickness uniformity and part density. Typical applications include industrial water and chemical storage tanks, agricultural sprayer tanks, automotive fluid reservoirs, utility enclosures, material-handling containers, and marine buoyancy components. The grade is positioned for parts requiring a balance of stiffness, environmental stress-crack resistance, and low-temperature impact rather than maximum rigidity or continuous service at elevated temperature.
The selection difference begins with density-dependent crystallinity. At a density of 0.935 g/cm³, the grade has a lower crystalline fraction than a 0.940–0.945 g/cm³ HDPE rotomoulding powder. The lower crystallinity reduces flexural modulus, but it also reduces the brittle-transition temperature and increases resistance to slow crack growth. In moulded parts of 3–6 mm wall thickness, the higher environmental stress-crack resistance is observed in water-storage and agricultural-chemical tanks where constant hoop stress and surface-active fluids act simultaneously. A conventional Ziegler-Natta LLDPE of equal density and melt-flow rate may have a broader molecular-weight distribution; this broad distribution can improve extrusion melt strength but in rotational moulding can produce greater warpage and less predictable shrinkage because of delayed crystallisation of the high-molecular-mass tail. The Icorene grade’s narrow distribution, if produced with a single-site or constrained-geometry catalyst system, gives a narrower melting range and a sharper viscosity transition during sintering. The practical consequence is that the grade can build full density at relatively low peak internal air temperature, but the process window is narrower: under-sintering appears as pinholes and incompletely fused powder at the inner wall, while over-temperature oxidation appears as brown discoloration and surface embrittlement.
Comonomer type also differentiates LLDPE grades within the same density and melt-flow-rate class. Butene-based LLDPE typically has lower dart impact and lower ESCR than hexene- or octene-based LLDPE at equal density and melt-flow rate. The public datasheet for Icorene 3545 BWN 8810 may not disclose the specific α-olefin comonomer; converters qualifying an alternate source should compare comonomer identity, not only density and melt-flow rate. The performance difference is attributed to the distribution of short-chain branches along the backbone: hexene or octene branches are more effective at interrupting crystallisable sequences when present at a similar total branch content.
| Property | Icorene 3545 BWN 8810 | Conventional ZN-LLDPE | HDPE rotomoulding powder |
|---|---|---|---|
| Nominal density | 0.935 g/cm³ | 0.930–0.935 g/cm³ | 0.940–0.945 g/cm³ |
| Melt-flow rate (190 °C/2.16 kg) | 4.5 g/10 min | 3.5–5.0 g/10 min | 3.0–6.0 g/10 min |
| Flexural modulus | 620–700 MPa | 500–650 MPa | 800–1100 MPa |
| ESCR F50, 100% Igepal | >1000 h | 400–800 h | 40–200 h |
| Low-temperature impact retention | Higher | Moderate | Lower |
| Warpage tendency in thick sections | Lower | Moderate | Higher |
Values in the table are representative class data for natural-colour powders; they are not lot-specific specification limits. Different pigment loadings and moulding conditions can shift flexural modulus and impact transition temperatures by more than 10%.
Pulverising and dry-flow characteristics are critical because rotational moulding has no applied shear to disperse poorly distributed particles. The powder is typically ground to a 35-mesh top size with 15–25 wt% retained on a 50-mesh screen; this bimodal distribution is used to combine fine-particle sintering with coarse-particle flow in shuttle and carousel machines. In production-scale shuttle and carousel rotational moulding machines, the powder is charged into ambient-temperature moulds at a shot weight calculated from the mould surface area, target wall thickness, and powder bulk density. Oven-air temperatures between 280 °C and 315 °C are common; the actual control variable is the internal air temperature, which is measured by a thermocouple fed through the mould vent. Peak internal air temperature is typically held between 190 °C and 205 °C for this density class. At peak internal air temperatures below 180 °C, sintering is incomplete and the inner surface can retain visible powder texture or pinholes. Above 210 °C, oxidative degradation can be initiated, with discoloration and loss of impact strength. The optimum peak internal air temperature therefore lies within a band of approximately ±5 °C for a given part and machine; published data for this specific configuration is limited, and moulders are advised to establish a process window using instrumented moulds.Cooling rate has a direct effect on warpage and crystallinity. Forced-air cooling followed by water mist is used to reduce cycle time, but cooling rates above 10 °C/min in sections thicker than 6 mm can create differential shrinkage between the outer mould-facing surface and the inner air-facing surface. The resulting residual stress can reduce apparent impact strength and produce part distortion after demoulding. Demoulding is normally performed below 70 °C to limit creep of the still-soft polymer. Moisture uptake by the powder is low, but surface moisture from open storage at relative humidity above 80% can generate porosity; pre-drying at 60–70 °C for 2–4 h is an accepted corrective step. Dry-blending of pigments should not exceed 2 wt% of a compatible masterbatch unless flow and dispersion trials confirm uniform colour and wall thickness, because higher loadings can segregate in the rotating mould and create localised mechanical weakness.
In double-skin and foam-filled rotational moulds, the powder is often selected for its sintering rate and low warpage rather than for high rigidity. The lower flexural modulus permits the outer wall to deform slightly during foaming without cracking; this is important in insulated utility cabinets and marine flotation parts. On machines with multiple arms, shot weight per arm must account for differences in mould temperature history due to oven dwell and cooling station sequencing. The same material can produce different wall-thickness distributions on a shuttle machine and a carousel because the duration and rate of heating differ. Production-scale experience shows that the wall-thickness variation across a 500 L tank can be controlled within ±10% when particle-size distribution and internal air temperature are held within the specified ranges; published data for this specific product configuration is limited.
The values below are representative of the 0.935 g/cm³, 4.5 g/10 min LLDPE rotational moulding class and are drawn from published datasheet and material-class data. They are not a substitute for a lot-specific certificate of analysis, and processing history strongly affects the measured values.
| Property | Value | Test method |
|---|---|---|
| Density | 0.935 g/cm³ | ISO 1183-1:2019 |
| Melt-flow rate (190 °C/2.16 kg) | 4.5 g/10 min | ISO 1133-1:2022 |
| Tensile yield stress | 16–18 MPa | ISO 527-2:2012 |
| Tensile strain at break | >800% | ISO 527-2:2012 |
| Flexural modulus | 620–700 MPa | ISO 178:2019 |
| Vicat softening temperature | 118 °C | ISO 306:2022/A50 |
| Brittleness temperature | <−76 °C | ASTM D746-20 |
| ESCR F50, 100% Igepal | >1000 h | ASTM D1693-21 |
The tensile strain at break of >800% is a short-term failure value under uniaxial tension; it should not be used as a design strain. In chemical-storage service with intermittent pressure cycles, long-term continuous strain should be limited to below 5% unless supported by a specific creep and ESCR test program. The ESCR value of >1000 h at 100% Igepal is a key differentiator relative to HDPE rotomoulding grades; it indicates the material can resist crack initiation in stressed regions exposed to surfactants and agricultural spray solutions. The Vicat softening temperature of 118 °C does not imply a continuous service temperature; polyolefin parts under load are usually limited to continuous service temperatures below 60–70 °C depending on stress level and chemical environment.
The brittleness temperature below −76 °C is determined on compression-moulded specimens; rotomoulded parts may have a higher brittle transition if the inner wall is under-sintered or if the part contains voids. The relationship between low-temperature impact and wall thickness is non-linear: a 3 mm wall may retain ductile behaviour at −40 °C, while an 8 mm wall of the same material may show reduced impact due to different cooling-rate-induced crystallinity and residual stress. This is a process limitation, not a material specification failure.
The BWN 8810 stabiliser formulation includes a UV-stabiliser package intended for natural-colour parts exposed to sunlight. In accelerated weathering of rotomoulded plaques of 3 mm thickness under ISO 4892-3 UVA-340 conditions, a UV-stabilised LLDPE of this class typically retains more than 50% of initial elongation after 1500 h, while an unstabilised LLDPE of the same density can lose significant elongation within 500–800 h. These values are comparative, not service-life guarantees; wall thickness, pigment loading, UV dose, and cleaning chemicals all affect actual service life. For food-contact use, the base polymer may satisfy the substance requirements of FDA 21 CFR 177.1520 and Commission Regulation (EU) No 10/2011, but the final article must be evaluated with the specific additive package, recycled content, and end-use conditions. Most rotational moulding converters obtain letters of compliance from the supplier for the exact natural or coloured grade and do not rely only on the base polymer classification.
Chemical-storage suitability is application-specific. The 0.935 g/cm³ density and high ESCR make the grade suitable for many aqueous chemicals, dilute acids, and aliphatic hydrocarbons at ambient temperature, but it is not recommended for contact with strong oxidisers, chlorinated solvents, or aromatic hydrocarbons at temperatures above 40 °C. Sodium hypochlorite above 5% active chlorine can cause oxidative chain scission and stress cracking, especially at weld lines, inserts, and sharp corners. The stabiliser package should not be combined with amine-based additives that interfere with the phenolic antioxidant system; such combinations can reduce oxidative induction time and cause premature colour shift. Under EU REACH, the polymer is exempt from registration as a polymer, but the monomer ethylene and any additives must be registered. RoHS Directive 2011/65/EU restrictions apply only to restricted heavy metals or brominated flame retardants in electrical and electronic applications; the natural polyolefin powder is not expected to contain restricted substances, but coloured or filled compounds must be verified. For applications involving drinking water, the converter must verify that the specific grade and any pigment masterbatch meet local regulatory requirements for taste, odour, and extractable organic carbon. Published data for Icorene 3545 BWN 8810 in these specific chemical configurations is limited; therefore qualification testing should be performed with the actual tank design and chemical mixture.
Rotational moulding is not a steady-state melt process; the powder experiences a long heating transient, a sintering plateau, and a cooling transient. The grade’s melt-flow rate of 4.5 g/10 min influences the sintering rate, but melt-flow rate alone does not predict bubble removal. Bubbles trapped in the wall are removed by pressure and temperature conditions during the plateau; for LLDPE powders, the plateau time between 190 °C and 205 °C is typically 3–6 min depending on wall thickness and oven-air temperature. The use of a lower melt-flow-rate grade gives higher melt strength and can reduce sag in thick sections, but it may require a higher peak internal air temperature to remove bubbles. The 4.5 g/10 min melt-flow rate is therefore a compromise between bubble removal and wall-thickness control.
In carousel machines, the heating-to-cooling time ratio is fixed by the station timing; in shuttle machines, the moulder can adjust heating time independently. The same material can show different mechanical properties on the two machine types because the cooling rate after demoulding differs. A carousel machine with forced-air cooling at 15 °C/min can produce smaller spherulites and higher modulus than a shuttle machine cooling at 5 °C/min, but the faster cooling can also increase residual stress. The processor should measure the internal air temperature and mould surface temperature rather than relying on oven setpoint.
The powder’s dry-flow is affected by storage conditions, because moisture can create fines aggregation. If the powder is stored in a cold warehouse and moved to a warm, humid mould shop, condensation can increase wall porosity. Sacks should be allowed to reach shop temperature before opening, and opened sacks should be used within a defined production interval. These operational boundaries are derived from standard polyolefin handling practice and are not specific to this grade; published data for this specific configuration is limited.
In rotomoulded agricultural sprayer tanks with capacities from 200 L to 2000 L, the grade is selected for the combination of UV resistance, ESCR, and low-temperature impact. The lower flexural modulus is managed with external ribbing, thicker wall sections at bosses, and metal inserts at attachment points. In automotive fluid reservoirs, wall-thickness uniformity and low-temperature impact reduce warranty failures under thermal cycling and vibration. Marine buoyancy components benefit from low water absorption and resistance to stress cracking in the presence of seawater and fuel residues. When the application requires higher rigidity or a continuous service temperature above 70 °C, the converter should evaluate a higher-density HDPE or a crosslinked polyethylene system because the LLDPE grade’s modulus and thermal resistance are lower. Differences from other products are therefore not limited to datasheet density and melt-flow rate; powder particle-size control, stabiliser formulation, comonomer architecture, and processing latitude all determine final part performance.