| HS Code | 591410 |
| Density | 0.935 g/cm³ |
| Melt Flow Rate | 3.5 g/10 min |
| Tensile Strength At Yield | 11.0 MPa |
| Tensile Strength At Break | 25.0 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 310 MPa |
| Vicat Softening Point | 102 °C |
| Melting Point | 125 °C |
| Haze | 10% |
| Gloss | 75% |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 250 g/mil |
| Elmendorf Tear Strength Td | 400 g/mil |
As an accredited LyondellBasell Icorene 3545 BWN 8001 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 3545 BWN 8001 Polyethylene, Linear Low Density supplied in 25 kg bags, palletized and stretch-wrapped for secure transport. |
| Container Loading (20′ FCL) | 20′ FCL container loading: LyondellBasell Icorene 3545 BWN 8001 LLDPE, palletized 25 kg bags, shrink-wrapped, secured for ocean freight. |
| Shipping | LyondellBasell Icorene 3545 BWN 8001 Polyethylene, Linear Low Density is a non-hazardous polymer resin, not regulated for transport. It is typically shipped in 25 kg bags, palletized and stretch-wrapped, or in bulk lined containers/railcars. Store dry, cool, away from sunlight and ignition sources; avoid dust generation. Handle per SDS. |
| Storage | Store LyondellBasell Icorene 3545 BWN 8001 Polyethylene, Linear Low Density in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed to prevent moisture and contamination. Avoid contact with strong oxidizers. Maintain good housekeeping, dust control, and grounding to prevent static. Inspect containers regularly. Follow the SDS and local storage regulations. |
| Shelf Life | Typically 24 months when stored unopened in original packaging under cool, dry conditions, away from direct sunlight, moisture, and heat. |
In rotational moulding of above-ground agrochemical storage tanks above 5,000 L, LyondellBasell Icorene 3545 BWN 8001 linear low density polyethylene powder is specified principally for stress-crack resistance in the presence of surfactant-containing formulations and for low-temperature impact retention after outdoor exposure. The governing finished-tank standards are EN 13575:2012 for static thermoplastic tanks above ground and ASTM D1998-15 for polyethylene upright storage tanks; chemical compatibility is screened by immersion testing adapted from ASTM D543-21 for the specific fertiliser, pesticide, or adjuvant matrix. The formulation is built on 100 wt% powder dry-blended with 2–5 wt% hindered amine light stabiliser masterbatch and 0.5–2.0 wt% carbon black or approved pigment masterbatch. Post-consumer recyclate is not introduced in this service because a loss of environmental stress crack resistance under hydrostatic load is considered a critical failure. On carousel rotational moulding machines with arm diameters of 4.0–5.0 m, the powder is charged into cast aluminium or fabricated steel moulds and heated at oven air temperatures of 280–300 °C; peak internal air temperature is maintained at 195–210 °C for 12–18 min depending on wall thickness. The biaxial rotation ratio is set near 4:1 for cylindrical vertical tanks and adjusted to 9:1 on cube-like tanks. Production-scale failure modes observed include pinholes when oven air exceeds 310 °C and wall-thickness variation above ±1.5 mm when powder is charged below 20 °C. Controlled cooling at 6–8 °C/min until 90 °C wall temperature, followed by forced air, reduces warpage at the top manway flange.
Batch-to-batch variation in dry flow is controlled through poured bulk density and sieve residue. A shift in bulk density of 0.03 g/cm³ is sufficient to require recalibration of the metering hopper and may extend oven residence by 2–4 min. Wall sections removed from the upper manway area are considered acceptable when the thickness gradient is below 10 % of nominal; values above 15 % indicate incorrect rotation ratio or insufficient peak internal air temperature. Terminal components include 1,000–50,000 L vertical storage tanks, cone-bottom tanks, and transport tank inserts for liquid fertilisers, pesticides, and adjuvant containment.
Arc-shaped and cylindrical flotation shells made from this rotomoulding grade require a narrow particle size distribution because dry-flow behaviour controls the uniformity of the powder layer that forms on the internal surfaces of a closed marine mould before sintering. The resin is evaluated for long-term outdoor service using ASTM D1693-15 environmental stress crack resistance, ASTM D256-23 notched Izod impact at -20 °C, and ISO 4892-2:2013 accelerated weathering. The compensation formulation is 100 wt% base powder with 4–7 wt% UV/HALS masterbatch and 1–2 wt% carbon black masterbatch; when black shells are not desired, a non-carbon black UV package at the same addition level is used. Moulders process closed aluminium moulds on carousel or shuttle machines at oven air temperatures of 285–300 °C and hold peak internal air temperature at 200–210 °C for wall thicknesses of 4–8 mm. After demoulding, the shell is filled with closed-cell polyurethane foam of 35–60 kg/m³ density to provide buoyancy redundancy in case the outer shell is punctured. Brass or 316L stainless steel mooring inserts are moulded in; published data for this exact powder/insert combination is limited, so prototype pull-out and thermal-cycling tests are performed before production batches. UV masterbatches are qualified by measuring tensile retention after 2,000 h of ISO 4892-2 exposure; loss above 25 % triggers reformulation. Sustained contact with aromatic hydrocarbons or ketones is outside the recommended service envelope. Typical end products include navigation buoys, aquaculture cage floats, docking fender shells, and flotation pontoons.
In potable water storage, the critical requirement is that the migrated organic fraction from stabiliser systems, catalyst residues, and pigment carriers remains below the extraction thresholds established by NSF/ANSI/CAN 61 and AS/NZS 4020:2018; for applications requiring United States compliance, the base resin must meet FDA 21 CFR 177.1520 as an olefin polymer. The dry blend is restricted to 100 wt% virgin powder plus 1–2 wt% of a food-contact-approved blue or black masterbatch. Post-consumer recyclate is excluded, and external mould release agents based on metallic stearates are not used because they are known to alter taste-and-odour profiles and can push total organic carbon values above potable water limits. Large shuttle or rock-and-roll rotational moulding machines with mould lengths up to 5.0 m process these tanks at oven air temperatures of 280–295 °C and peak internal air temperatures of 195–205 °C. Cooling is held at 6–8 °C/min until the wall reaches 90 °C, then forced air is used to bring the part to demoulding temperature. The lower cone wall is not allowed to fall below 5 mm to keep hydrostatic stress within design allowables. Terminal products include 500–20,000 L domestic rainwater tanks, underground potable water cisterns, and water transport tanks.
In moulded playground slides, crawl tunnels and outdoor seating, the grade is acceptable only when the processor controls heavy-metal pigments and maintains a documented weathering baseline. The governing chemical restriction is EN 71-3:2019+A1:2021 migration of certain elements, with additional limits from 16 CFR 1303 for lead in surface coatings and structural performance expectations under ASTM F1487-21. The formulation is normally 100 wt% base powder with 2–4 wt% UV/HALS masterbatch and 1–3 wt% pigment masterbatch; lead, cadmium, and hexavalent chromium pigments are excluded from the supply chain. The weathering baseline is verified by ISO 4892-2 exposure for 1,500–2,000 h, with tensile retention above 70 % and delta E below 4. Small multi-arm carousel machines with mould widths up to 1.5 m produce thin-wall sections of 3–5 mm at oven air temperatures of 285–300 °C. The biaxial rotation ratio is held at 4:1 and demoulding is not performed above 75 °C because thin-wall edges distort. The resulting components include slide shells, crawl tunnels, climbing steps, and outdoor tables and bench seats.
For industrial bins, pallets and insulated fish tubs, the specification pressure is on stiffness retention after repeated washdown with dilute cleaning agents and hot water up to 60 °C. The finished parts are tested under ASTM D638-14 tensile, ASTM D790-17 flexural, and ASTM D1525-17 Vicat softening temperature; food-contact articles additionally comply with FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011. The powder is compounded at 100 wt% base with 15–25 wt% closed-loop post-industrial regrind from the same grade where permitted, and 0.5–1.5 wt% antioxidant masterbatch to control melt history. Regrind loading above 25 wt% is avoided because it reduces environmental stress crack resistance and increases pinhole incidence at corner radii. When regrind is used, it is passed through a 2,000 µm screen and metal detection; powder melt flow rate is retested to ensure no more than 10 % drift from virgin grade. Multi-arm carousel machines produce double-wall or foam-filled constructions with wall thicknesses of 6–12 mm; oven air temperature is 285–300 °C and peak internal air temperature is 200–210 °C. After cooling, parts are transferred to flatness fixtures until the wall temperature drops below 60 °C to prevent edge curvature. Production output includes 200–1,000 L conical bins, 1.2 m × 1.0 m pallets, and insulated fish tubs.
Buried wastewater tanks derive structural capacity from uniform wall thickness and the absence of internal voids at rib intersections. Finished tanks are tested to EN 12566-1:2000+A2:2013 for small wastewater treatment systems and ASTM D1998-15 for polyethylene upright tanks; EU market material certification under REACH 1907/2006 is standard. The formulation is 100 wt% base powder with 2–3 wt% carbon black masterbatch and 0.5–1.0 wt% UV stabiliser masterbatch. Post-consumer reclaim is excluded from buried load-bearing walls because soil deflection and hydrostatic loading can expose signs of oxidative degradation at stress concentrations. Rock-and-roll machines with a major-to-minor axis ratio of 4:1 process walls of 8–20 mm with structural ribs. Oven air temperature is maintained at 280–300 °C, peak internal air temperature at 190–205 °C, and cooling in a full support fixture continues until the wall temperature is below 55 °C. Demoulding above 70 °C is a common source of flange warpage and subsequent installation leakage. Hydrostatic test pressure for small tanks is typically 5 kPa at the shell, with deflection measured at the rib midpoint; deflections above 3 % of span indicate insufficient wall thickness or premature demoulding. Terminal products include underground septic tanks, pump chambers, grease interceptors, and water retention cisterns.
Competitive LyondellBasell Icorene 3545 BWN 8001 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 3545 BWN 8001 is classified as a linear low density polyethylene supplied primarily as a rotational moulding powder. The grade designation decodes the nominal density as 0.935 g/cm³ when tested under ISO 1183-1:2019 and a nominal melt flow rate of 4.5 g/10 min at 190 °C with a 2.16 kg load under ISO 1133-1:2022. The BWN 8001 suffix identifies the additive and stabilisation package rather than a colour designation; natural, white, and black variants may use related suffix codes within the same density and melt flow family. Because the material is supplied as a powder, incoming inspection typically includes bulk density by ASTM D1895 and particle-size retention by ASTM D1921. Published third-party summaries do not consistently disclose the comonomer type, but the density and melt flow combination places the product in the medium-density LLDPE segment used for chemical tanks, hoppers, and outdoor industrial parts.
The resin is not a pelletized blown film grade. Substitution with film-grade pellet resin requires grinding and re-stabilisation, which can alter bulk density, fines content, and gel level. The powder form is selected because rotational moulding depends on particle coalescence during slow heating rather than screw-driven plastication. This distinction is relevant when comparing the product with injection moulding or blown film grades carrying a similar nominal density.
The sintering behaviour of this polymer is governed by the zero-shear viscosity associated with a melt flow rate of 4.5 g/10 min. In a production-scale carousel-type rotational moulding machine operating with a biaxial rotation ratio of 4:1 to 5:1, oven air temperature is typically held between 260 °C and 290 °C. The critical measured variable is peak internal air temperature, or PIAT, obtained with a thermocouple or infrared sensor inside the mould cavity. For wall sections between 3 mm and 6 mm, PIAT generally needs to remain between 180 °C and 220 °C for complete densification. If PIAT remains below 180 °C, entrapped air and moisture form microvoids that reduce impact strength and create pinholes in thin ribs. If PIAT exceeds 220 °C, thermo-oxidative chain scission increases carbonyl index, lowers elongation at break, and produces discolouration in natural parts. The effective processing window can narrow to ±5 °C when tooling contains deep pockets or when wall thickness varies because the local powder loading changes heat-transfer rate.
Controlled cooling is also a boundary condition. Differential shrinkage between inner and outer surfaces causes warpage when forced-air cooling exceeds 12 °C/min on large flat panels. Mould release agents and internal air pressure can reduce warpage but alter surface gloss and release consistency. Published data for the optimum cooling profile of this exact grade is limited; trial runs on the specific shop floor are required to define a repeatable cooling curve for a given tool and charge weight.
For service in chemical storage at 23 °C, environmental stress crack resistance is the primary discriminator against high-density polyethylene rotational moulding grades. Third-party summaries for this LLDPE commonly report slow-crack-growth resistance under ASTM D1693-15 condition B exceeding 1,000 h in 100% Igepal CO-630; the manufacturer’s certificate of analysis should be consulted for lot-specific values because ESCR is sensitive to comonomer distribution and cooling history. Tensile yield strength is generally reported in the range 15–19 MPa under ASTM D638, with elongation at break above 600%. Flexural modulus is typically clustered around 500–620 MPa under ASTM D790. Low-temperature brittleness temperature under ASTM D746 is commonly below -40 °C. These values are screening data, not design allowables, and must be confirmed for the specified colour, wall thickness, and moulded part geometry.
Oven setpoint alone does not determine PIAT because mould geometry, wall thickness, shot weight, and rotation ratio alter the rate of heat transfer. In a large flat tank lid with wall thickness 4 mm, PIAT may lag oven air by 40–70 °C during the middle of the cycle depending on mould surface emissivity and the presence of release agent. On production lines using infrared pyrometers, operators commonly observe PIAT variation of 5–15 °C between winter and summer campaigns when oven exhaust dampers are not adjusted. This variation is sufficient to move the process outside the 180–220 °C window if the oven setpoint remains fixed. A melt flow rate of 4.5 g/10 min lowers viscosity relative to 2.0–3.5 g/10 min rotational moulding LLDPE grades, accelerating bubble migration in the molten layer, but it also promotes sagging in thick sections when PIAT is too high. Verification should include a thermocouple placed in the worst-case thin wall and a record of ambient temperature, charge weight, and oven residence time for each cycle.
In thin-wall agricultural hoppers and material-handling containers, wall thickness is often specified between 2.5 mm and 4.0 mm. The lower wall section requires a higher PIAT to eliminate microbubbles, but a higher PIAT increases the risk of degradation and raises peak internal mould pressure. On a typical shuttle-type rotational moulding machine with forced-air oven, the operator may need to raise oven air temperature to 290–300 °C while limiting hold time at PIAT to 2–3 min. Field records from multi-arm carousel machines show that batch-to-batch MFR drift of ±0.3 g/10 min shifts the optimum PIAT by approximately 3–5 °C. This is one reason incoming melt flow rate verification under ISO 1133-1:2022 is not a formality; it establishes whether the control model for a given tool should be adjusted. Powder bulk density also matters because low bulk density can create uneven wall thickness when the mould rotates at 4:1 and the powder slides rather than tumbling.
Outdoor service in agricultural and marine components exposes the polymer to ultraviolet radiation, moisture, and thermal cycling. The BWN 8001 additive package includes stabilisers intended to delay photo-oxidative chain scission, but the exact hindered amine light stabiliser and phenolic antioxidant loadings are not disclosed in third-party summaries. Accelerated weathering under ASTM D2565 or ISO 4892-3 provides a ranked comparison of elongation retention but does not directly state service life. A 50% retention of elongation at break after 4,000 h of xenon-arc exposure is sometimes used as a screening threshold for agricultural tanks, though field data remain necessary for warranty decisions. Surface microcracking and gloss loss proceed faster on the windward exposure side; thickness reduction due to chalking is usually negligible for structural performance until significant chain scission has occurred. The manufacturer’s weathering data should be required for the exact colour and lot because pigment interactions can alter stabiliser effectiveness.
Compared with a conventional 0.945 g/cm³ HDPE rotational moulding grade, the lower density of this LLDPE lowers flexural stiffness but increases slow-crack resistance and low-temperature ductility. HDPE rotational moulding grades often exhibit flexural modulus in the range 800–1,100 MPa, while this LLDPE grade generally falls between 500 MPa and 620 MPa under ASTM D790. That difference makes the LLDPE more suitable for parts that deform without cracking, such as chemical tanks and playground components, and less suitable for unsupported structural panels where stiffness governs buckling. Compared with high-pressure LDPE, the linear backbone provides higher tensile yield and better environmental stress crack resistance. Compared with blown film LLDPE, the rotational moulding grade is supplied as a powder, has a stabiliser package without slip or antiblock additives, and has molecular weight and comonomer distribution tuned for slow sintering in a mould rather than bubble stability in a blown film line. Substitution of film-grade pellets requires grinding, which reduces bulk density and can introduce fines; it also risks gel formation if film additives are incompatible with mould release agents.
The base polyethylene polymer generally falls within the scope of FDA 21 CFR 177.1520(c) for olefin polymers used in contact with food, subject to density, maximum extractable fraction, and intended temperature conditions. Potable water tank manufacturers must also evaluate migration under national standards such as NSF/ANSI 61 or EU 10/2011; the resin supplier’s designation does not automatically certify the finished rotational moulded article because processing temperature, regrind content, and colour concentrates can change migration profiles. REACH registration in the EU and RoHS Directive 2011/65/EU should be confirmed through the safety data sheet and product compliance statement. For medical packaging or pharmaceutical closures, USP 661.1 testing may be required; published data for this specific configuration is limited, and suitability must be determined on the finished part.
Continuous immersion in aggressive fluids is a separate failure mechanism from short-term chemical splash. LLDPE is a semicrystalline polyolefin; aliphatic and aromatic hydrocarbons diffuse into the amorphous phase and reduce yield stress. At 23 °C, short-term splash exposure to diesel or hydraulic oil may produce visible swelling but not immediate fracture; at 60 °C, the same fluids can reduce tensile strength by more than 30%. Oxidising acids such as concentrated nitric acid and chlorinated solvents are outside the recommended service envelope. Detergent solutions containing nonylphenol ethoxylates can accelerate environmental stress cracking, so ASTM D1693 screening should be supplemented with full immersion testing under ISO 175 for the actual chemical concentration and temperature. The upper continuous-use temperature in dry air is generally limited by oxidative stability rather than melting point; published data for this exact grade is limited, but rotational moulding LLDPE of this density class is often not recommended above 60–70 °C under sustained load in air. Parts requiring operation outside these boundaries should be tested under ISO 175 and ASTM D638 after conditioning in the intended service fluid.