| HS Code | 189740 |
| Density | 0.932 g/cm3 |
| Meltindex | 3.5 g/10 min (190°C/2.16 kg) |
| Tensilestrengthatyield | 11.0 MPa |
| Tensilestrengthatbreak | 24.0 MPa |
| Elongationatbreak | 750% |
| Flexuralmodulus | 300 MPa |
| Vicatsofteningtemperature | 100 °C |
| Meltingpoint | 125 °C |
| Crystallizationtemperature | 110 °C |
| Shoredhardness | 50 |
| Thermalconductivity | 0.33 W/m·K |
| Linearthermalexpansion | 1.5E-4 cm/cm/°C |
| Specificheatcapacity | 2.3 J/g·°C |
| Waterabsorption | <0.01% |
| Dielectricconstant | 2.3 |
| Dissipationfactor | 0.0003 |
As an accredited LyondellBasell Icorene 3545 BUE 5915 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 3545 BUE 5915 Linear Low Density Polyethylene is packaged in 25 kg bags, 40 per pallet (1,000 kg). |
| Container Loading (20′ FCL) | Container Loading (20′ FCL) for LyondellBasell Icorene 3545 BUE 5915 LLDPE: palletized 25 kg bags, securely stowed and export-ready. |
| Shipping | LyondellBasell Icorene 3545 BUE 5915 is a non-hazardous linear low-density polyethylene resin. It is typically shipped in 25 kg bags, bulk bags, or bulk trucks/containers. Keep packages dry, sealed, and away from heat, moisture, and direct sunlight. No special transport classification; handle to avoid contamination and damage. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and strong oxidizing agents. Keep containers closed and pallets stable to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive temperatures, which may cause degradation or pellet blocking. Use first-in, first-out stock rotation, and follow local regulations and the safety data sheet. |
| Shelf Life | Typically 12 months when stored in original packaging in a cool, dry, ventilated area away from direct sunlight and heat. |
On a cast stretch-film line with a 2.8 m automatic die, a 0.8–1.2 mm lip gap, and a 20 ± 2 °C matte-finish chill roll, Icorene 3545 BUE 5915 is processed inside a melt-temperature window of 238–246 °C when the certified melt index falls in the 3.5–4.5 g/10 min band. The melt-index value is verified per ISO 1133-1:2022 at 190 °C and 2.16 kg before start-up, and the lot certificate density of approximately 0.935 g/cm³ is checked against ASTM D1505. The extruder configuration is a barrier screw with 30:1 L/D and a Maddock mixing section, with the feed throat held at 35–40 °C to prevent pellet bridging. Die pressure is maintained below 18 MPa by gear-pump control. Chill roll temperature is held at 20 ± 2 °C; air knife pressure is set at 12–15 kPa and the vacuum box at −2.0 to −3.0 kPa relative to ambient. The draw ratio is held between 28:1 and 34:1, producing a final film gauge of 18–25 µm without edge encapsulation. Operating experience on comparable cast-film lines indicates that neck-in stabilizes at 35–45 mm per edge when the die-lip gap is 0.9 mm; reducing air-knife pressure to 8 kPa allows the melt curtain to wander laterally, increasing transverse gauge standard deviation from ±0.8 µm to ±1.5 µm and raising edge trim from 4% to 7% of web width.
Film tensile properties are evaluated per ASTM D882-18 at a crosshead speed of 500 mm/min; for a 23 µm film, machine-direction elongation at break is typically 350–450% and transverse-direction elongation at break is 600–750%. Elmendorf tear is measured per ISO 6383-2, with machine-direction values above 2.5 N. A laser gel counter mounted after the winder monitors cumulative gel counts for defects of 250 µm² and larger; at 18 µm thickness, the running standard is below 5/m². If gel count exceeds 12/m², the screen pack is changed from 100 mesh to 150 mesh and the die-lip wipe interval is shortened to 30 min. Winding tension is limited to 0.5 N/mm of film width at the core and reduced to 0.25 N/mm at the outside of the roll. Roll hardness is checked with a durometer to maintain 80–85 Shore A near the core and 70–75 Shore A at the outer layer.
In three-layer blown silage wrap, Icorene 3545 BUE 5915 is used in the core layer at a layer ratio of 1:2:1 or 1:3:1, while the two skins contain 8–12 wt% of an ethylene-vinyl acetate copolymer with 18–28% vinyl acetate to generate the required cling force without melt-phase separation. The die gap is set at 1.6–2.0 mm, the blow-up ratio is held at 2.8:1 to 3.2:1, and frost line height is maintained at 700–800 mm. When the BUE 5915 additive package contains an ultraviolet stabiliser, the outer-skin UV absorber and hindered amine light stabiliser concentrations are adjusted by fractional melt-flow ratio to avoid surface bloom on the chill roll; the nip roll surface temperature is kept below 35 °C to prevent cling-agent migration into the embossed pattern. If the frost line is lowered below 500 mm, the film reaches the nip with an elevated surface temperature, and cling-force retention after 24 h declines by more than 30% when tested per ASTM D5458 on a 23 °C test surface. Non-amine antifog additives in the skin are limited to 1.0–1.5 wt% because higher loadings can antagonise the UV stabiliser and accelerate carbonyl index increase after 2,000 h of QUV exposure per ISO 4892-3 cycle 2.
| Property | Test Method | Acceptance Range for 25 µm Film |
|---|---|---|
| Film thickness | ISO 4593 | 25 ± 2 µm |
| Dart impact | ASTM D1709 method A | ≥ 450 g |
| Elmendorf tear | ISO 6383-2 | MD ≥ 3.0 N, TD ≥ 4.0 N |
| Puncture resistance | ASTM D5748 | ≥ 14 N |
| Tensile strength at break | ASTM D882-18 | MD ≥ 30 MPa, TD ≥ 28 MPa |
| Cling force after 24 h | ASTM D5458 | ≥ 3.5 N/25 mm |
| Haze | ISO 14782 | ≤ 28% |
With a 70 mm grooved-feed extruder at 120 rpm, line output is limited to 180–220 kg/h by bubble stability rather than by melt temperature. Internal bubble cooling air temperature is set at 8–12 °C to reduce frost-line variation. If the casting rolls are run above 35 °C, cling-agent transfer to the roll surface increases and the roll must be cleaned at intervals shorter than 8 h to maintain consistent film release.
When Icorene 3545 BUE 5915 is applied as a 20–30 g/m² extrusion coating onto corona-treated woven polypropylene, the first measurable limit is substrate moisture, because steam generated at the nip creates pinholes and delamination. The resin is heated to 295–315 °C at the die to promote oxidative adhesion to the fabric; the air gap between die exit and pressure roll is set at 120–150 mm, and the chill roll is held at 12–18 °C. Corona treatment on the fabric is verified at 42–46 dyn/cm per ASTM D2578; below 40 dyn/cm, adhesion fails in the heat-seal zone during bag conversion. The substrate is preheated by a contact roll to 45–55 °C and dried to a moisture content below 0.1%; at 0.3% moisture, pinhole density can exceed 2/m² and peel adhesion falls below 2 N/15 mm when tested per ASTM D1876. Coating-weight variation is scanned with a beta gauge and controlled within ±3% of the target.
Draw resonance is the second operating boundary. As line speed exceeds 330 m/min, the melt curtain develops periodic gauge bands in the 8–14 Hz range that are visible on the chill roll; the oscillation is damped by increasing melt temperature to 310 °C or by closing the air gap to 100 mm without exceeding chill-roll cooling capacity. Edge neck-in is typically 30–50 mm per side at 300 m/min when the die-lip gap is 0.5 mm. If die-lip cleanliness is not maintained, oxidised micro-gels from the 310 °C melt stream accumulate at the lip edge and create coating-weight stripes; the die lip is wiped when transverse coating-weight deviation reaches 3–5%. Heat-seal strength on the coated side is measured per ASTM F88/F88M-21 using a 25.4 mm strip; seal initiation is observed near 105 °C, and the acceptance threshold for woven sack conversion is 35 N/25.4 mm.
In heavy-duty form-fill-seal sack production on a grooved-feed extruder with an 80 mm barrier screw and 30:1 L/D, Icorene 3545 BUE 5915 is blown at a die gap of 1.6–2.0 mm, a blow-up ratio of 2.5:1 to 3.2:1, and a frost line height of 600–850 mm for a 140 µm three-layer film. At a melt temperature of 205 ± 5 °C and a main screw speed of 95 rpm, bubble diameter coefficient of variation is held below 1.5% using an internal bubble cooling lance with 8–12 °C air and an external bubble cage. If the frost line is allowed to fall below 500 mm, transverse-direction Elmendorf tear falls below 4 N and the sack fails the 600 g dart-impact threshold per ISO 7765-1 method A. Tensile properties are tested per ASTM D882-18: machine-direction yield strength of the 140 µm film should remain above 18 MPa, with machine-direction elongation at break above 650%.
Without a polymer processing aid, line output is limited to 220–250 kg/h because melt fracture appears as chevron patterns at the die lip; adding a fluoropolymer processing aid at 300–500 ppm shifts the melt-fracture onset above 300 kg/h but requires a 30–45 min conditioning period before the surface defect clears. The screen pack is replaced when the pressure differential exceeds 12 MPa between the extruder head and the screen changer, because higher differentials indicate gel accumulation from the edge-trim refeed loop. For low-temperature drop resistance, sacks are conditioned at −20 °C for 48 h and then subjected to a 1.2 m drop test; the acceptance criterion is no weld seam rupture when filled to 25 kg.
Flat-die extrusion of a 1.5 mm LLDPE geomembrane from Icorene 3545 BUE 5915 uses a 3.5 m wide flat die with a 1.2 mm lip gap, but line speed is restricted to 4–6 m/min because gauge control at this thickness is limited by melt-temperature variation across the die width. The polishing roll stack is maintained at 60–80 °C; lower roll temperatures reduce sheet gloss but increase flatness deviation, while higher temperatures produce antiblock plate-out on the rolls. If the base resin is not supplied with carbon black, a 40–50% carbon black masterbatch is added to achieve 2.0–2.5% carbon black content per ASTM D1603. Melt temperature is held at 220 ± 5 °C to balance stable web drawing against thermal degradation; die-pressure variation across the width is kept below 1.2 MPa by independent cartridge heaters in the die-lip zones.
| Property | Test Method | Acceptance Range for 1.5 mm Sheet |
|---|---|---|
| Thickness | ASTM D5199 | 1.5 ± 0.15 mm |
| Density | ASTM D1505 | 0.930–0.945 g/cm³ |
| Tensile yield | ASTM D6693 | ≥ 11 MPa both directions |
| Elongation at break | ASTM D6693 | ≥ 800% |
| Tear resistance | ASTM D1004 | ≥ 125 N |
| Puncture resistance | ASTM D4833 | ≥ 360 N |
| Carbon black content | ASTM D1603 | 2.0–3.0% |
| Oxidative induction time | ASTM D3895 | ≥ 100 min at 200 °C |
Oxidative induction time is measured by differential scanning calorimetry at 200 °C with 50 mL/min oxygen flow per ASTM D3895; the unaged sheet should exceed 100 min before the roll is released for field installation. If OIT falls below 80 min, the antioxidant package is judged insufficient for the intended service life and the lot is downgraded to non-geomembrane use. Low-temperature brittleness is checked per ASTM D746; the 1.5 mm sheet should not fail at −50 °C in five parallel specimens. Wrinkling at the roll stack is controlled by maintaining web tension at 0.8–1.2 N/mm; tension above 1.5 N/mm creates machine-direction gauge bands that become visible in the field as thickness striping after thermal expansion.
Directly transferrable from the heavy-duty sack line is the three-layer coextrusion of 200 µm industrial liners for non-food chemical packaging. Icorene 3545 BUE 5915 is run in all three layers with a die gap of 2.2 mm, a blow-up ratio of 2.0:1, and a melt temperature of 218 ± 3 °C. The lower blow-up ratio improves machine-direction stiffness but requires retraction of the external bubble cage during start-up to prevent drag-induced gauge bands. Output is ramped over 30 min from 80 kg/h to 180 kg/h to allow the bubble to stabilise. The film is tested for environmental stress-crack resistance per ASTM D1693 condition B in 10% Igepal CO-630; failure should occur after more than 400 h for the liner to be assigned to surfactant and mild acid-containing products. Published data for the permeation of aromatic hydrocarbons through this specific grade configuration are limited; such service requires additional gravimetric permeation testing per ASTM F739 before certification. Weld seam strength of the finished liner is measured per ASTM F88/F88M-21 on a 25.4 mm strip; the seal should exceed 45 N/25.4 mm before the liner is accepted for palletised export packaging. Direct contact with strong oxidisers above 40 °C is not recommended unless compatibility is confirmed by immersion testing per ISO 175 for the specific chemical mixture and concentration.
Competitive LyondellBasell Icorene 3545 BUE 5915 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 3545 BUE 5915 is a linear low density polyethylene supplied as a free-flowing powder intended for rotational molding. The grade designation carries process-relevant information: the 3545 segment is consistent with a nominal density near 0.935 g/cm³ and a nominal melt flow rate near 4.5 g/10 min at 190 °C/2.16 kg, while the BUE 5915 suffix identifies a stabilization and color package whose exact composition is proprietary. The product is differentiated from high-density polyethylene rotomolding grades by its lower flexural modulus and higher environmental stress crack resistance, and from butene-based linear low density polyethylene powders by its balance of low-temperature ductility and processability. Manufacturers publish property ranges rather than single values; lot-specific data must be confirmed against the producer’s technical data sheet before setting charge weights, oven set points, or cooling rates.
The controlling variable is density-driven stiffness. Under ASTM D790-17, linear low density polyethylene in the 0.933–0.937 g/cm³ band commonly exhibits a flexural modulus in the range of 450–650 MPa, whereas high-density rotomolding grades at 0.945–0.965 g/cm³ typically exceed 900 MPa. The lower modulus reduces buckling resistance in large flat walls but improves impact toughness and environmental stress crack resistance. Against medium-density polyethylene, the difference is narrower because some MDPE grades overlap the same density range; selection therefore shifts to melt flow, comonomer distribution, and stabilizer package. Compared with butene-based LLDPE, performance depends on comonomer identity. If the producer’s technical data identify a higher α-olefin comonomer, the short-chain branch distribution may be more uniform, typically raising dart impact strength under ASTM D5420-21 and reducing brittleness temperature under ASTM D746-14. When comonomer identity is not disclosed, substitution testing under the end-use validation plan is required.
In a single-arm shuttle rotational molding machine running water-cooled aluminium moulds, powder charge weight is determined by cavity surface area and desired wall thickness, not by volume alone. For a nominal wall thickness of 6 mm, a charge weight of 17–19 kg per cavity is typical for a large rectangular tank mould with 8.5 m² internal surface area and powder bulk density of 0.34–0.38 g/cm³. Oven set-point temperatures from 270–290 °C are used, with peak internal air temperature held between 185 °C and 205 °C. Rotational speed ratios of 4:1 on the primary axis and 1.5:1 on the secondary axis are maintained to distribute the melt across deep-cavity geometries; deviation from these ratios can produce thick rims at the parting line and thinning at bottom corners. Powder bridging in gravity hoppers is a recurring failure mode when fines content rises above 15 wt% below 150 µm or when storage humidity exceeds 70% RH. Operators report charge-weight variation of ±0.5 kg between cycles under such conditions, producing wall thickness deviations of approximately ±1 mm. Pre-drying at 60 °C for 2 h can restore dry flow, but drying above 80 °C may soften the polymer and cause agglomeration.
Because rotational molding applies no mechanical shear, melt flow rate at 190 °C/2.16 kg is used as a proxy for bubble-removal time. A nominal melt flow rate of 4.5 g/10 min under ISO 1133-1:2022 or ASTM D1238-23 is high enough to permit gas-bubble escape during the densification plateau but not so high that the melt drains from vertical walls. Powder particle size distribution controls sintering rate: coarse particles above 500 µm can leave pinholes because internal air channels close before bubbles are released, while excessive fines below 100 µm can compact in the mould and reduce dry flow. A D50 of 250–350 µm is commonly specified for LLDPE rotomolding powders in this melt flow class, although the manufacturer’s certificate of analysis is the controlling document.
| Property | Test standard | Process or service relevance |
|---|---|---|
| Density | ASTM D1505-18, ISO 1183-1:2019 | Controls stiffness, warpage, and chemical resistance |
| Melt flow rate | ISO 1133-1:2022, ASTM D1238-23 | Determines bubble removal and minimum oven time |
| Powder particle size distribution | ASTM D1921-18 | Affects dry flow, scoop weight, and corner fill |
| Bulk density | ASTM D1895-17 Method A | Affects hopper bridging tendency and charge weight per cavity |
| Tensile yield strength | ASTM D638-14 Type IV, ISO 527-2:2012 | Indicates short-term load-bearing capability |
| Flexural modulus | ASTM D790-17, ISO 178:2019 | Differentiates LLDPE from HDPE and MDPE stiffness |
| Notched Izod impact | ASTM D256-10(2018), ISO 179-1:2023 | Low-temperature impact performance for outdoor tanks |
| Environmental stress crack resistance | ASTM D1693-15 | Service life in chemical tank and agricultural spray applications |
| Brittleness temperature | ASTM D746-14 | Cold-weather ductility limit |
At peak internal air temperature below 170 °C, incomplete particle coalescence persists even though the crystalline melting range of linear low density polyethylene is approximately 121–125 °C. Full densification requires a plateau above the melting range. The result is a porous inner surface, reduced elongation at break under ASTM D638-14, and a ductile-to-brittle transition that may shift above 0 °C. At peak internal air temperature above 210 °C, oxidative degradation accelerates, consuming the BUE 5915 stabilizer package and causing yellowing at the inner surface. Cooling rate governs crystalline morphology and residual stress. Forced-air cooling at 4–8 °C/min down to 90 °C is commonly used to minimize warpage in large flat panels. Water mist cooling above 12 °C/min can produce residual stresses, dimensional recovery after demolding, and part pull-in from the mould surface. Process thresholds should be validated for each mould geometry because published data for this specific configuration are limited.
A 5,000 L cylindrical tank with an 8 mm wall illustrates the application envelope. Hydrostatic pressure at the base is approximately 0.08 MPa, below the tensile yield strength of the material, but the limiting condition is often environmental stress crack resistance under ASTM D1693-15 rather than short-term yield. In agricultural spray service, dilute surfactant solutions can initiate stress cracking at sharp radii. Rotational molders typically seek documented ESCR above 500 h in 100% Igepal for such applications; the specific value for Icorene 3545 BUE 5915 must be confirmed from the producer’s data sheet. Field failures are frequently associated with inner-corner radii below 3 mm, insufficient venting, or uneven cooling on multi-cavity arms.
The BUE 5915 suffix indicates that the grade is formulated for outdoor service, but the exact hindered amine light stabilizer and phenolic antioxidant ratios are proprietary. Processors report that excessive oven residence beyond the recommended plateau by more than 8–10 min can deplete stabilizers and shift Yellowness Index. The same limitation applies to high regrind ratios. Regrind fractions above 20–25 wt% can increase fines, reduce dry flow, and carry oxidized surface material into the melt. Fabricators who reuse trimmed flash sieve reclaimed powder through a 600 µm screen and blend for 15–20 min in a ribbon blender before charging. The product is not intended for continuous immersion in strong oxidizing acids, aromatic hydrocarbons, or chlorinated solvents unless chemical compatibility data from the producer demonstrate suitability.
Compliance status is a function of grade formulation and jurisdiction. Polyethylene homopolymers and ethylene copolymers used in food-contact applications may be evaluated under FDA 21 CFR 177.1520 if the specific grade, colorant, and stabilizer package are cleared. European processors must verify REACH registration under Regulation (EC) No 1907/2006 and, where applicable, specific migration limits under Regulation (EU) No 10/2011. The product should not be dry-blended with alkaline or amine-based additives unless validated, because such additives may interact with the stabilization package and shift processing stability. End users must rely on the LyondellBasell product stewardship statement for food-contact, potable-water, and safety-related applications.