    Specifications
    HS Code 476426
    Density 0.945 g/cm³
    Melt Index 190 C 2 16 Kg 3.5 g/10 min
    Tensile Strength At Yield 17.0 MPa
    Tensile Strength At Break 25.0 MPa
    Elongation At Break 700 %
    Flexural Modulus 0.700 GPa
    Vicat Softening Point 110 °C
    Melting Point 130 °C
    Hardness Shore D 58
    Thermal Conductivity 0.35 W/m·K
    Brittleness Temperature < -70.0 °C
    Water Absorption 0.010 %

    As an accredited LyondellBasell Icorene 3545 BUE 5594 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 3545 BUE 5594 is packaged in 25 kg moisture-resistant bags, 40 bags per pallet, totaling 1,000 kg per pallet.
    Container Loading (20′ FCL) Container loading (20′ FCL): LyondellBasell Icorene 3545 BUE 5594 LLDPE, 25 kg bags, palletized, shrink-wrapped, secured for ocean freight.
    Shipping LyondellBasell Icorene 3545 BUE 5594 Polyethylene, Linear Low Density is a non-hazardous thermoplastic resin. It is typically shipped in sealed bags, octabins, or bulk containers. No UN number, hazard class, packing group, or special transport labels are required. Store dry and keep away from heat and ignition sources.
    Storage Store LyondellBasell Icorene 3545 BUE 5594 Polyethylene, Linear Low Density in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep original containers or bags tightly closed to prevent moisture and contamination. Avoid contact with strong oxidizers. Maintain good housekeeping and use first-in, first-out stock rotation. Do not store outdoors unprotected.
    Shelf Life Shelf life is 24 months from date of manufacture when stored in a cool, dry place in original unopened packaging.
    Application of LyondellBasell Icorene 3545 BUE 5594 Polyethylene, Linear Low Density

    LyondellBasell Icorene 3545 BUE 5594 Polyethylene, Linear Low Density is a rotational-moulding powder whose downstream applications are selected where biaxial, low-shear oven processing controls wall densification. The nominal density of 0.934 g/cm³ under ISO 1183-1 and melt flow rate of 5.5 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022 place the material in the LLDPE rotomoulding range. The application sectors below are limited to documented industrial end-uses; no unfilled high-pressure injection-moulding, blown-film, or structural-pipe claims are included.

    The conversion of Icorene 3545 BUE 5594 into agricultural sprayer and storage tanks places the highest demand on environmental stress crack resistance, because pesticide emulsifiable concentrates and liquid fertilizers accelerate crack propagation in LLDPE if wall-stock crystallinity is overdeveloped during slow cooling. In biaxial rotational moulding, the powder is charged into a closed aluminum tool mounted on a carousel machine; the primary oven is maintained at 280–300 °C, and the internal air temperature is brought to 190–205 °C before the mould is indexed into the cooling chamber. The rotation speed ratio is held at 4:1 on the primary axis, with secondary-axis speed between 6 rpm and 12 rpm, a range that reduces pinhole formation in corners while avoiding excessive wall thinning. Compliance for above-ground agricultural tanks is assessed under ASTM D1998-21, with dangerous goods packaging additionally subjected to hydraulic pressure and stacking tests according to the applicable national transport code. Formulation adjustment for outdoor agricultural tanks consists of adding a carbon black or hindered amine stabilizer masterbatch at 0.5–2.0 wt%; black compounds are maintained at 1.0–1.5 wt% to limit sidewall impact-strength loss. The terminal product range includes horizontal sprayer tanks, vertical storage tanks, fertiliser induction hoppers, and secondary containment liners produced by the same oven cycle but with a removable foam core. A failure mode observed on production lines is wall-thickness thinning below 4 mm at the threaded filling boss, which can require a second powder charge during the stationary mould phase or an insert-heating step; this is not a resin deficiency but a mould-fill limitation when a single-shot cycle is forced beyond the bulk density of the 35-mesh powder.

    How Does Marine Buoyancy Moulding Test Low-Temperature Ductility After Water Absorption?

    Marine buoyancy shells and floating dock modules produced from the same LLDPE powder are evaluated under ISO 179-1 Charpy impact at −20 °C and after 7 days of water immersion, because wave-loading flexural fatigue and freeze-thaw cycling near the waterline drive crack initiation in semicrystalline polyethylene. The powder is dry-blended with a UV stabilizer concentrate at 0.7–1.5 wt%; high-visibility yellow or orange pigments are introduced as a 50% loaded masterbatch at 1.0–2.5 wt% relative to the base powder, and the dry blend is mixed in a low-speed ribbon blender for 15–25 min to prevent segregation. During moulding, a cast aluminum or fabricated steel tool is filled to achieve a nominal wall thickness of 6–10 mm; peak internal air temperature is held between 195 °C and 210 °C, and forced-air cooling is delayed until the internal temperature falls below 120 °C to reduce warpage on long flat deck sections. Compliance documentation for floating modules references ISO 4892-2 for accelerated UV weathering, ISO 179-1 for impact acceptance, and REACH for imported component registration. Finished part types include foam-filled dock floats, navigation buoy hulls, pontoon end caps, and modular floating walkway sections. A documented processing limitation is that water-spray cooling must be interrupted at 90–110 °C to prevent tensile residual stress that lowers the −20 °C impact energy by approximately 10–15%; published data for this specific configuration is limited, and validation should be performed on production-scale parts rather than compression-moulded plaques.

    In playground slide and play-panel manufacture, the selection of Icorene 3545 BUE 5594 is governed less by stiffness than by control of specific migration limits when colour concentrates are combined with the powder. The dry blend is prepared with a polyolefin-based colour masterbatch at 0.8–3.0 wt%; below 0.8 wt%, dark blue and red shades show inconsistent colour saturation on flat sections, while above 3.0 wt% the viscosity differential between masterbatch carrier and base resin can produce surface swirl in thin ribs. The mould is heated in a shuttle machine to an internal air temperature of 185–200 °C, with a maximum oven dwell of 20–25 min for 10 mm nominal wall sections. Aluminium moulds with a draft angle of at least 2° are used for double-wall slide beds; the second wall is produced by sequentially charging a controlled mass of powder into the still-rotating mould after the first layer has sintered but before full densification. The process avoids post-mould trimming that can expose stress-concentrating cut edges. Compliance records for the finished components include EN 71-3:2019+A1:2021 and ASTM F963-17 for elemental migration from toy-contact surfaces, while REACH Annex XVII restrictions for phthalates and polycyclic aromatic hydrocarbons are applied to the compound. Mechanical acceptance is documented under ASTM D638-14 tensile yield and ISO 179-1 Charpy notched impact at 23 °C. Terminal types include curved slide tubes, climbing tunnel sections, roof panels, and sandbox surrounds. A production-level failure mode reported by rotational moulders is the formation of pinholes along the parting line when clamp pressure is reduced to avoid flash; this is addressed by maintaining a minimum 0.5 MPa mould-closing pressure and cleaning the parting surface after every third cycle, not by increasing oven temperature.

    Material Handling Bins, Creep Resistance, and Sanitary Cold-Storage Liners

    Material handling containers and insulated fish bins expose the LLDPE to cyclic top-load compression and repeated steam cleaning; performance is therefore specified by creep modulus under ISO 899-2 and by low-temperature impact after conditioning at −30 °C. The polymer powder is blended with a food-contact-approved processing stabilizer at 0.1–0.4 wt% and, where required for freezer storage, with a white masterbatch at 1.0–2.0 wt% to raise surface reflectivity. The formulation is maintained below the overall migration limit of 10 mg/dm² under EU Regulation (EU) No 10/2011; for United States cold-storage use, the finished wall is covered by FDA 21 CFR 177.1520 for olefin polymers. Rotational moulding is performed on independent-arm machines with oven set points at 270–290 °C; the peak internal air temperature is limited to 195–205 °C, and the cooling cycle is extended with forced air at 5–10 °C for 30–45 min to achieve a wall crystallinity that balances stiffness and impact. Finished product categories include nestable distribution pallets, insulated fish tubs, bread trays, and sanitary hoppers. A recurring process bottleneck on production lines is bulk-powder bridging in the feed hopper when the powder temperature falls below 10 °C; a fluidized-bed pre-heater at 30–40 °C restores uniform feeding without altering particle-size distribution.

    Compliance checklist matrix by downstream application
    ApplicationStandard or regulationEssential test or scope
    Agricultural sprayer and storage tanksASTM D1998-21Self-supporting PE upright tanks; wall thickness, hydrostatic resistance, and chemical exposure documentation
    Marine buoyancy and floating dock shellsISO 4892-2, ISO 179-1, REACHUV weathering and Charpy impact after immersion; European chemical inventory compliance
    Playground slides and panelsEN 71-3:2019+A1:2021, ASTM F963-17, REACH Annex XVIISpecific elemental migration; phthalate and PAH restrictions; mechanical acceptance
    Cold-storage containers and palletsFDA 21 CFR 177.1520, EU (EU) No 10/2011Olefin polymer food-contact compliance and overall migration limit
    Outdoor site furnitureEN 581-1, REACHSeating stability and chemical compliance of the finished component
    Secondary containment linersEPA SW-846 Method 9095B, ASTM D1693-CFree-liquid penetration and environmental stress crack resistance under chemical load
    Thin-wall instrument cabinetsIEC 60529, NEMA 250 Type 4, UL 94 HBIngress protection, weather resistance, and horizontal burn rate

    Outdoor site furniture such as benches, planters, and litter bins is rotomoulded from the same 35-mesh powder with a UV-stabilizer masterbatch at 0.5–1.5 wt%, using a mould internal air temperature of 185–200 °C and a wall thickness of 5–8 mm; compliance is recorded under EN 581-1 for seating stability and REACH for chemical registration of the finished component.

    If Secondary Containment Liners Must Withstand Diesel, Fertilizer, and UV in the Same Part

    Secondary containment liners for generator sets and agricultural chemical fill stations are a demanding application because the same polyethylene wall is exposed to hydrocarbons, aqueous fertilizer salts, and ultraviolet radiation for the entire service life. The powder is compounded on a 40:1 L/D twin-screw extruder only where a converter elects to pre-disperse additives; otherwise the additive package is tumble-blended at 0.5–1.8 wt% using a hindered amine light stabilizer and a phenolic antioxidant. The rotomoulding cycle uses a steel fabricated mould with an internal release coating, and the peak internal air temperature is maintained at 190–205 °C for 18–22 min; a higher temperature above 210 °C accelerates oxidative degradation at the inner wall and reduces long-term crack resistance under ASTM D1693-C. Compliance is recorded under ASTM D1998-21 for chemical storage tanks, EPA SW-846 Method 9095B for free-liquid penetration testing of the containment wall, and REACH for import documentation. Finished part types include rectangular secondary containment basins, pump-skid drip trays, and cylindrical double-wall sumps. A limitation of the resin is that prolonged contact with strong oxidizing acids or aromatic solvents is not recommended; published data for these specific configurations is limited, and compatibility testing under the actual chemical concentration and temperature must be performed before production release.

    Comparative formulation addition ranges and recorded processing limits
    ApplicationAdditive systemAddition ratioObserved processing limit
    Agricultural sprayer and storage tanksCarbon black or HALS masterbatch0.5–2.0 wt%Black batches kept at 1.0–1.5 wt% to retain sidewall impact strength
    Marine buoyancy shellsUV stabilizer and pigment masterbatch0.7–1.5 wt% plus 1.0–2.5 wt%Water-spray cooling interrupted at 90–110 °C to reduce residual stress
    Playground slides and panelsPolyolefin-based colour masterbatch0.8–3.0 wt%Minimum mould-clamp pressure 0.5 MPa to prevent parting-line pinholes
    Cold-storage containersFood-contact processing stabilizer and white masterbatch0.1–0.4 wt% plus 1.0–2.0 wt%Powder pre-heated to 30–40 °C to stop hopper bridging
    Outdoor site furnitureUV-stabilizer masterbatch0.5–1.5 wt%Wall thickness held at 5–8 mm without supporting frame
    Secondary containment linersHALS and phenolic antioxidant package0.5–1.8 wt%Peak internal air temperature capped at 190–205 °C to avoid oxidative degradation
    Thin-wall instrument cabinetsConductive carbon black masterbatch2.0–3.5 wt%Cryogenic powder warmed to 20–25 °C before charging to avoid condensation

    Cryogenic Grinding Adjusts Particle-Size Distribution for Thin-Wall Instrument Cabinets

    For outdoor telemetry and instrument cabinet housings, the moulded wall is reduced to 4 mm to allow heat dissipation and lower part mass; this shifts the process-control burden to the particle-size distribution of the rotomoulding powder. The as-supplied 35-mesh powder is further cryogenically ground at −70 °C using liquid nitrogen to produce a bimodal distribution with 70–80 µm median particle size, which increases packing density in sharp corners. The formulation includes a conductive carbon black masterbatch at 2.0–3.5 wt% when static dissipation is specified, though this addition lowers elongation at break; the resulting compound is screened through a 200 µm sieve to remove agglomerates. Moulding is performed in a shuttle machine with mould internal air temperature 180–195 °C, and the oven dwell is shortened to 12–16 min to prevent over-sintering of the thin wall. Compliance for finished enclosures is stated under IEC 60529 for ingress protection, NEMA 250 Type 4 for weather resistance, and UL 94 HB for horizontal burn rate. Finished part types include telemetry cabinets, pump control boxes, and roadside battery housings. A production limitation is that cryogenic powder must be allowed to warm to 20–25 °C before charging to prevent condensation on the mould surface; published data for this specific configuration is limited, so first-article thermal mapping is required.

    Free Quote

    Competitive LyondellBasell Icorene 3545 BUE 5594 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 3545 BUE 5594 is a linear low density polyethylene grade supplied as a pigmented rotational moulding powder. The BUE 5594 designation identifies a blue colorant and stabilizer package within the manufacturer’s material code system; the base polymer is an ethylene/alpha-olefin copolymer with a short-chain branching distribution characteristic of LLDPE reactor technologies. Because the product is delivered in powder form, its bulk handling, dry-flow, and particle-size distribution are as relevant to process control as its melt-state properties.

    The grade carries a nominal density of 0.934 g/cm³ when tested in accordance with ISO 1183-1:2019 and a melt mass-flow rate of 5.0 g/10 min determined at 190 °C under a 2.16 kg load according to ISO 1133-1:2022. These two values define the basic compromise between flow and stiffness. A density below 0.940 g/cm³ keeps the crystalline fraction moderate, which preserves flexibility and stress-crack resistance; the MFR of 5.0 g/10 min is high enough to assist particle coalescence in thin ribs but still low enough to maintain melt integrity during the low-shear conditions of rotational moulding.

    PropertyRepresentative valueTest method
    Density0.934 g/cm³ISO 1183-1:2019
    Melt mass-flow rate5.0 g/10 minISO 1133-1:2022, 190 °C/2.16 kg
    Tensile yield strength17.0 MPaISO 527-2:2012
    Elongation at break800%ISO 527-2:2012
    Flexural modulus550 MPaISO 178:2019
    Environmental stress crack resistance>1000 hASTM D1693-15, Condition B
    Vicat softening temperature118 °CISO 306:2022 A50
    Brittleness temperature-76 °CASTM D746-14

    Values in the table are representative single-point data for material selection. They are not batch release limits. Batch certification should be consulted for lot-specific results because density, MFR, and additive dispersion can vary within the supplier’s specification band.

    What Processing Constraints Emerge from the 0.934 g/cm³ Density and 5.0 g/10 min MFR?

    In rotational moulding, the MFR of 5.0 g/10 min places the grade in the higher-flow segment of LLDPE powders. Higher-flow grades shorten the time required for powder bed densification, but the same flow behavior can widen wall-thickness variation if the oven soak is extended beyond the point of full void elimination. On multi-arm carousel machines equipped with internal air temperature probes, oven chamber temperatures are commonly set between 260 °C and 290 °C. Peak internal air temperature is typically controlled between 190 °C and 205 °C; sustained PIAT above 210 °C can initiate oxidative degradation and inner-surface discoloration, particularly in vented tools. Tool surface temperatures measured by thermocouple or infrared pyrometer lag the internal air temperature, and the difference between the two is a function of mould material, wall thickness, and oven air velocity.

    Heating rate and cooling rate interact at the part wall. A fast heating ramp may collapse the outer skin before the inner powder bed has sintered, trapping air bubbles at the mid-wall. A plateau at PIAT between 190 °C and 205 °C allows dissolved gases and residual air to diffuse from the melt. The cooling sequence for this grade should begin with forced air until the mould surface temperature falls below approximately 120 °C; water mist or water spray can then be applied. Demoulding is generally initiated at part wall temperatures below 80 °C. Early demoulding at higher temperatures increases the risk of post-mould shrinkage and warpage on large flat panels. These conditions are engineering reference points and require validation on the specific tool because mould parting lines, venting, and wall thickness distribution shift the effective processing optimum.

    Powder handling adds a separate constraint. Rotational moulding powders are dry-flowed into cavity sections, and the particle-size distribution influences bulk density and charge consistency. A top cut near 600 µm is common for rotomoulding powders, while excessive fines below 100 µm can increase static charge, reduce hopper flow, and create non-uniform melt-out. Dry sieve analysis according to ISO 4610:2001 or an equivalent method should be included in incoming quality control when the material is pneumatically conveyed. High-speed mixing of dry-blended pigments or regrind should be avoided because it can generate fines and heat-induced additive segregation.

    Sintering, Void Collapse, and Air Removal in the Cavity

    Rotational moulding densification proceeds through sintering, bubble dissolution, and melt densification. For LLDPE powders, the onset of particle neck formation is governed by polymer viscosity at the particle surface. As the cavity passes through the oven, the powder bed experiences a transition from solid-state contact to viscous sintering; the melt viscosity drops as the internal air temperature rises from 150 °C to 190 °C, allowing contact necks to form. Entrapped air between particles is then expelled or diffuses into the molten polymer. If the outer wall solidifies before the inner powder has fully coalesced, residual bubbles remain as mid-wall porosity, reducing tensile and impact properties. The use of internal air temperature rather than oven time alone is therefore mandatory for process control on thick parts.

    The higher MFR of 5.0 g/10 min reduces the zero-shear viscosity at a given temperature relative to lower-MFR LLDPE grades, which accelerates neck formation. However, too low a viscosity can allow the melt to flow away from corner sections under gravity, producing thin edges and thick lower walls. Mould baffles and internal pressure are not used in standard rotational moulding; wall distribution is controlled almost entirely by thermal history and mould rotation ratio. Typical rotation ratios for deep parts range from 4:1 to 8:1 on the primary axis relative to the secondary axis, but tool geometry determines the optimum. Process engineers should map wall thickness across the part after initial trials and adjust the oven soak, not the rotation ratio alone, to correct thickness variation.

    Chemical storage tanks, water treatment vessels, agricultural hoppers, marine floats, and recreational components are specified with this grade when the part requires a measurable combination of environmental stress crack resistance, low-temperature ductility, and processability in complex tooling. The ESCR value of >1000 h under ASTM D1693-15 condition B provides a standardized ranking benchmark for stressed parts exposed to surfactants; it is not a direct service-life prediction because ESCR testing accelerates failure through a fixed stress and a standard wetting agent. Outdoor components made from the blue-stabilized formulation should be evaluated for UV retention using accelerated weathering under ISO 4892-2 and, where possible, correlated with outdoor exposure data from the application region.

    Published data for long-term chemical retention of the specific BUE 5594 pigment package are limited. Chemical compatibility for a stored fluid must be assessed on the finished moulded article using static immersion or stress-rupture tests because the polymer may soften or swell in oxygenated fuels, strong oxidizing acids, and certain surfactants even when the ESCR classification is high. For water storage, potable-water contact approval is not automatically conferred by the resin supplier; the complete article must meet the specific migration and organoleptic requirements of the destination market.

    When Linear Low Density Polyethylene Replaces High Density Polyethylene in Rotational Moulding

    HDPE and LLDPE occupy different property envelopes. HDPE grades at a comparable melt flow generally provide higher flexural modulus and higher heat deflection temperature because of their higher crystallinity. The LLDPE base of Icorene 3545 BUE 5594 has a nominal density of 0.934 g/cm³ and a flexural modulus of 550 MPa; typical rotomoulding HDPE grades with densities above 0.945 g/cm³ can exceed 900 MPa in flexural modulus. Consequently, a tank sidewall designed for HDPE may exhibit greater deflection under hydrostatic load when moulded from this LLDPE grade unless ribbing or wall thickness is adjusted. The LLDPE grade compensates through higher ESCR and lower brittleness temperature, which are valuable in thin-walled parts that experience impact at low service temperatures.

    Compared with high-pressure low density polyethylene, the linear architecture of LLDPE provides higher tensile yield strength and puncture resistance at the same density because long-chain branching is absent and the short-chain branches are more uniformly distributed along the polymer chain. LDPE remains easier to process in some low-shear applications due to higher melt elasticity, but for rotational moulding the LLDPE grade’s balance of flow and mechanical properties is typically preferred for structural parts. Within the broader LLDPE rotomoulding segment, lower-MFR grades may show marginally higher dart impact and better melt strength at the expense of slower densification and reduced detail resolution. The 5.0 g/10 min MFR of Icorene 3545 BUE 5594 positions it for complex mould geometries, provided the oven soak is tightly controlled to prevent uneven wall distribution.

    Regulatory evaluation of the BUE 5594 formulation requires separate review of the base polyolefin and the added colorant/stabilizer system. The base LLDPE polymer is generally covered as an olefin polymer under 21 CFR 177.1520(c) when used in accordance with the specified conditions of use and any relevant migration limits; the blue pigment and UV stabilizer package must be confirmed against the applicable positive lists. In the European Union, plastic food-contact articles must meet the requirements of Commission Regulation (EU) No 10/2011 as amended, including overall migration limits and, where applicable, specific migration limits for the additives. RoHS and REACH obligations are article-level responsibilities; the converter must verify that the supplied formulation does not contain substances of very high concern above the threshold established by Regulation (EC) No 1907/2006.

    Storage and handling boundaries are explicit. The powder should be stored in sealed, moisture-resistant packaging at temperatures not exceeding 40 °C and protected from direct sunlight. Polyolefins are not generally desiccant-dried, but condensation on cold powder surfaces can introduce pinholes when the powder is charged into a heated mould; containers should be allowed to reach ambient temperature before opening. Regrind levels above the converter-validated threshold—commonly 20%—should not be used without re-qualification of ESCR and low-temperature impact because repeated thermal cycles consume the antioxidant package and change the molecular weight distribution. Avoid blending with incompatible polymers outside the polyolefin family; dispersed heterophasic domains can reduce weld-line strength and impact performance.

    Long-term heat aging data for the specific blue-stabilized grade are limited. Continuous service at elevated temperatures above 60 °C should be supported by retained-property testing on moulded parts, including oxidative induction time measurements by ISO 11357-6 or tensile property retention under ISO 527-2:2012. Material selection should not rely solely on the resin datasheet when the application imposes simultaneous stress, temperature, and chemical exposure.