Lyondellbasell Icorene 3545 Bue 5513 Polyethylene Linear Low Density

LyondellBasell Icorene 3545 BUE 5513 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 3545 BUE 5513 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 210907
    Density 0.935 g/cm³
    Meltmassflowrate 3.5 g/10 min
    Tensilestrengthatyield 10.3 MPa
    Tensilestrengthatbreak 21.4 MPa
    Elongationatbreak 800%
    Flexuralmodulus 276 MPa
    Vicatsofteningtemperature 100 °C
    Meltingpoint 124 °C
    Dartdropimpact 120 g
    Elmendorftearstrengthmd 200 g
    Elmendorftearstrengthtd 300 g
    Haze 10%
    Gloss 80%
    Coefficientoffriction 0.2
    Comonomer Butene-1

    As an accredited LyondellBasell Icorene 3545 BUE 5513 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 3545 BUE 5513 is packaged in 25 kg polyethylene bags, with 40 bags per 1,000 kg pallet.
    Container Loading (20′ FCL) 20′ FCL: LyondellBasell Icorene 3545 BUE 5513 LLDPE in 25 kg bags, palletized, stretch-wrapped, ~18–20 MT net, secured for transport.
    Shipping LyondellBasell Icorene 3545 BUE 5513 Polyethylene, Linear Low Density is a non-hazardous plastic resin, not regulated for transport by DOT, IMDG, or IATA. Ship in clean, dry containers; protect from moisture, heat, and sunlight. Keep bags sealed, palletized, and secured. Follow SDS and carrier requirements.
    Storage Store LyondellBasell Icorene 3545 BUE 5513 Polyethylene, Linear Low Density in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, flames, and moisture. Keep original containers tightly closed, palletized, and protected from physical damage. Avoid dust accumulation and static discharge. Use first-in, first-out stock rotation; do not store near oxidizers. Follow local regulations.
    Shelf Life Typically 24 months from manufacture when stored in original, unopened packaging under cool, dry conditions, away from direct sunlight.
    Application of LyondellBasell Icorene 3545 BUE 5513 Polyethylene, Linear Low Density

    In chemical storage tank production, LyondellBasell Icorene 3545 BUE 5513 Polyethylene, Linear Low Density is processed on a carousel-type independent-arm rotational moulding machine with cast aluminium moulds operated in a forced-air oven. The powder is charged directly to the closed mould without pre-drying when storage relative humidity is below 60% RH and surface moisture remains below 0.05 wt%; higher moisture levels produce steam-induced pinholes along the inner wall below the top fill port. A vented thermocouple is inserted through the parting line, and the oven set point is maintained at 280–295 °C while the internal air temperature is driven to 190–210 °C and held for 20–30 min after the thermocouple first reaches that band. This schedule is used for wall thicknesses from 6 mm to 12 mm in vertical chemical storage vessels. In the cooling segment, forced ambient air at 2–4 °C/min is applied until the mould surface falls below 100 °C; water fog is introduced only after that threshold because early quench creates differential shrinkage at the manway flange and locks in cylindrical wall bowing. For vertical polyethylene chemical storage tanks, mechanical acceptance is assessed under ASTM D1998-21, tensile properties under ASTM D638-22, and environmental stress crack resistance under ASTM D1693-15 Condition B at 50 °C in Igepal CO-630. When potable water contact is specified, the fabricated article is additionally evaluated under NSF/ANSI/CAN 61, and for incidental food contact under FDA 21 CFR 177.1520 paragraphs (c) 1.1 and (d) depending on extractive end-use conditions. Typical end products include vertical cylindrical storage tanks from 200 L to 20,000 L, dosing cabinets, and double-wall containment basins for aggressive liquid intermediates.

    Compliance matrix for rotationally moulded articles using Icorene 3545 BUE 5513
    Application zoneStandard designationCritical test or conditionNumerical acceptance reference
    Chemical storage tankASTM D1998-21Hydrostatic resistance at full rated volumeNo leakage at 110% rated head
    Chemical storage tankASTM D1693-15ESCR, Condition B, Igepal CO-630Failure time not below reservoir specification, commonly 500 h
    Agricultural sprayer tankASTM D543-21Chemical immersion at 40 °C for 30 daysChange in tensile elongation below acceptance limit
    Marine float shellISO 25649-1:2017Floating leisure article safety requirementsLoad retention after 24 h water immersion
    Municipal waste containerEN 840-1:2012Dimensional compatibility and performanceDimensional tolerance at comb lift interface
    Municipal waste containerISO 4892-2:2013Xenon-arc accelerated weatheringRetained elongation at 2,000 h exposure

    How Does Powder Dry Flow Govern Wall Uniformity in Narrow-Neck Agricultural Sprayer Assemblies?

    Agrochemical sprayer tanks with threaded narrow necks impose a direct relationship between powder dry flow and wall thickness scatter because the powder must travel through a restricted opening before sintering into the lower mould cavity. The powder fraction is screened to reject particles larger than 500 µm, and pourability is measured by a funnel method based on ASTM D1895-17 Method C so that bridging at the neck does not reduce charge weight in the far end of the mould. Pre-drying is not routinely required below 60% RH, but if water content exceeds 0.05 wt%, the oven cycle is extended by 10–15% to prevent steam porosity at the threaded insert weld plane. Threaded inserts for drain ports and pump fittings are backed with annular flanges rather than point-loaded washers because the LLDPE moulded boss must distribute hoop stress around the opening. The process window uses an internal air temperature of 195–210 °C with a peak internal air hold of 18–25 min for a 5 mm to 8 mm wall, followed by forced-air cooling at 3 °C/min until the insert boss stabilises below 95 °C. Chemical compatibility is tested according to ASTM D543-21 using the specific agrochemical formulation at 40 °C for 30 days; because published third-party data for this exact grade and pesticide formulation is limited, a pre-production immersion trial is required. Mechanical properties after exposure are measured by ISO 527-2:2012 at 50 mm/min, and outdoor weathering is evaluated under ASTM G154-16 Cycle 1. End products include saddle-style horizontal sprayer tanks from 200 L to 1,500 L, nurse tanks, seed hoppers, and fertigation reservoirs with moulded-in fitting bosses.

    When a floating body carries both a closed-cell polyurethane core and a moulded-in stainless steel mooring boss, the LLDPE shell must be cooled slowly enough to preserve insert concentricity within ±0.25 mm, otherwise the finished float develops asymmetric bearing stress at the ocean-side shackle. Marine buoyancy modules are rotationally moulded with wall thicknesses from 5 mm to 12 mm, depending on hydrostatic collapse resistance and mooring load class. The peak internal air temperature is deliberately pushed to 210–220 °C because the UV-stabilised formulation requires additional heat history to fully consolidate around stainless steel inserts. Forced-air cooling at 20–25 m/s is maintained until the inner wall reaches 80 °C; water quench is not applied above this threshold because differential contraction between the metal boss and the LLDPE shell enlarges the insert hole and initiates microcracks during subsequent swell-shrink cycles. Weathering acceptance is normally set at 1,000–3,000 h under ASTM G154-16 Cycle 1, with retained elongation measured by ASTM D638-22 and colour shift measured by ISO 11664-4. Published data for the BUE 5513 stabilizer package in this specific marine configuration is limited, so a trial plaque should be exposed before volume production. End products include aquaculture float collars, segmented fender shells, closed-cell foam-filled mooring buoys, and marker floats that must remain serviceable after prolonged saltwater immersion.

    When Municipal Waste Bin Lids Are Moulded as a Separate Index, Cooling Airflow Control Sets the Dimensional Acceptance Range

    Municipal waste bin bodies are moulded as two-piece shells with integrated comb-lift pockets and a separately moulded lid that must seat without trimming. The main body wall is specified at 4–6 mm, while the lid edge is moulded at 5–8 mm to resist hinge-area impact. Differential cooling between the lid and the bin body creates radial mismatch, so the forced-air nozzle bank in the cooling station is set to 15–25 m/s and the water mist cycle is started only after the parting line temperature falls below 90 °C. Moulded-in hinge pin holes are avoided; the holes are drilled post-mould in a CNC jig because thickness variation around a moulded pinhole initiates stress cracking under sub-zero drop testing. Oven residence time for a 240 L bin body is set according to wall mass and mould charge, with the peak internal air temperature held at 200–210 °C for 20–28 min. Dimensional compatibility and comb lifter interface dimensions are evaluated under EN 840-1:2012, accelerated weathering under ISO 4892-2:2013, and low-temperature impact after conditioning at −20 °C for 24 h. The compound also requires outdoor exposure trials for colour retention because municipal tenders routinely specify a visible service life of 5–10 years without major yellowing. End products include two-wheel bins from 120 L to 360 L and four-wheel bins from 500 L to 1,100 L, including separate lids moulded to the same shrinkage envelope.

    Industrial Bulk Container Bodies with Welded Steel Frames and the Problem of Differential Thermal Expansion

    Rotational moulding of bulk container bodies with encapsulated steel frames places the LLDPE shell against a high-expansion metal support, and the cooling step must be managed so that the polymer does not crack away from the frame corners. The coefficient of linear thermal expansion for polyethylene is substantially higher than that of steel, so the tool is pre-compensated by 1.0–1.5% along the long axis to absorb the shrinkage difference when the moulded part cools from 90 °C demould temperature to a 20 °C warehouse. The mould is mounted on a shuttle-type rotating arm with a load capacity verified for the combined mass of steel frame, aluminium tool, and powder charge. For a 1,200 mm × 1,000 mm pallet box, wall thickness is held at 6–9 mm, with the fork entry ribs thickened to 10–12 mm to resist shear stress at the tunnel openings. Peak internal air temperature is set at 200–215 °C, and the cooling cycle uses staged forced air at 5 °C/min until the frame inserts reach 100 °C, followed by ambient air to prevent warpage at the upper rim. Flat pallet performance is tested under ISO 8611-1:2021 for racking, fork lifting, and stacking, while impact strength after thermal conditioning is tested under ASTM D256-23 Izod notched geometry but with a rotomoulded plaque rather than an injection-moulded specimen because the cooling history differs. End products include weld-frame fruit bins, collapsible sidewall boxes, and heavy-duty pallet containers with conductive or floor-contact gaskets installed after demoulding.

    In food handling, the olefin polymer classification under FDA 21 CFR 177.1520 does not by itself establish food safety for a finished rotationally moulded tote; the stabilizer package in the BUE 5513 formulation must be evaluated under the intended extractive conditions. The mould surface is prepared with a food-grade release agent that does not contain silicone, because silicone migration interferes with subsequent adhesion of product labels and with smokehouse drying cycles. Interior corners are coved to a radius of not less than 20 mm to permit clean-in-place spray removal of organic residues. Moulding uses a peak internal air temperature of 195–205 °C for a 5 mm nominal wall, with slower cooling at 2 °C/min through the crystallization plateau to minimise sink marks on the interior floor. Migration testing is carried out under Regulation (EU) No 10/2011 using food simulants appropriate to the finished article, with overall migration and specific migration limits applied to the stabilizer constituents listed in the supplier certificate. Mechanical properties are verified by ISO 527-2:2012 tensile tests and ASTM D790-17 flexural tests on specimens cut from flat panels moulded in the same cycle. End products include meat lug tubs, cheese boxes, bakery dough trays, and seafood totes that require repeated washdown at 60–80 °C without embrittlement after commercial sanitizer exposure.

    Underground utility vaults and septic access chambers made from Icorene 3545 BUE 5513 are moulded with external corrugations rather than flat ribbing because buried service imposes hoop compression, and inner radii below 3 mm at corrugation valleys become crack initiation sites when backfill load cycles superimpose on the moulded-in shrinkage strain. The shell is moulded at a wall thickness of 8–14 mm to meet soil-load deflection limits, and the mould is charged with pre-weighed powder to avoid thin spots at the apex of the arch. Peak internal air temperature is held at 205–215 °C for 30–40 min because the deeper corrugation fill points require longer heat transfer from the aluminium tool surface. Cooling is slowed to 1–2 °C/min through the solidification range to reduce residual stress at the base-to-sidewall transition. Long-term stiffness is assessed by ISO 527-2:2012 and creep behaviour by ISO 899-1:2017 on creep specimens cut from the buried wall section. External confirmation of raw material density and lot-to-lot consistency is performed by ISO 1183-1:2019. End products include water meter vaults, cable joint chambers, septic access chambers, and pumping station sumps with sealed access lids that must resist ground settlement and occasional vehicle load at grade.

    Free Quote

    Competitive LyondellBasell Icorene 3545 BUE 5513 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 3545 BUE 5513 is a butene-comonomer linear low-density polyethylene rotational moulding powder supplied as a free-flowing pulverised solid. The base resin is characterised by a nominal density of 0.934 g/cm³ when measured in accordance with ISO 1183-1:2019 and a melt flow rate of 4.5 g/10 min at 190 °C under 2.16 kg load according to ISO 1133-1:2022. The suffix BUE 5513 identifies a compounded additive and colour package rather than a modification of the base polymer; published compositional data for this specific suffix is limited, and food-contact or potable-water approvals must be verified against the lot certificate. The material is used mainly in outdoor storage tanks, agricultural hoppers, marine buoys, and moulded parts requiring a balance of low-temperature ductility and environmental stress crack resistance.

    What distinguishes Icorene 3545 BUE 5513 from general-purpose butene-LLDPE rotomoulding powders?

    The differentiation arises primarily from the stabiliser package and the powder morphology rather than from a unique density or melt-flow position. The melt flow rate of 4.5 g/10 min places the grade near the centre of the rotomoulding viscosity window: it is low enough to permit low-shear sintering across complex multi-plane cavities, but high enough to reduce vertical-wall sag during the mould heating cycle. Butene-LLDPE powders in this flow range generally display a broad molecular weight distribution and a wider sintering plateau than metallocene-catalysed alternatives, while producing a lower low-temperature dart impact at equivalent density. Typical pulverised LLDPE particle size falls between 150 µm and 500 µm, with powder flow evaluated by methods such as ISO 6186 or ASTM D1895; the dry-flow profile is controlled to avoid bridging in deep, narrow mould pockets. The BUE 5513 additive package is formulated for exterior weathering; it provides pigment retention and ultraviolet stabilisation that are not present in a natural, unmodified 3545 powder. Published data for the specific pigment concentration of BUE 5513 is limited, and UV retention should be confirmed by ISO 4892-2 or ISO 4892-3 exposure on the finished article.

    Thermal fusion window and machinery-specific processing responses

    Rotational moulding of Icorene 3545 BUE 5513 is controlled by temperature rather than pressure. Industrial practice for LLDPE powders with a density near 0.934 g/cm³ targets a peak internal air temperature of 200 °C to 230 °C. Oven set-points are commonly 280 °C to 320 °C, although the required value depends on wall thickness, mould material, and machine type. In carousel machines with forced-air velocities of 0.5–1.5 m/s, a nominal 6 mm wall section may require 18–24 min heating, whereas shuttle machines with less uniform airflow commonly require 20–28 min for the same thickness. The peak internal air temperature is measured inside the cavity by a thermocouple passing through the vent; it must remain above the crystalline melting peak of 127 °C for sufficient time to achieve full particle coalescence and eliminate gas voids.

    If the internal air temperature is terminated below 200 °C, the outer mould surface may be fully sintered while the inner surface still contains unmelted powder and microporosity. If the peak internal air temperature exceeds 230 °C, oxidative degradation at the inner cavity surface can reduce tensile elongation and generate discolouration. Cooling rate after fusion has a direct effect on shrinkage and warpage. Rapid forced-air cooling to 80 °C before demoulding reduces cycle time but increases through-thickness crystallinity gradients in thick sections and can raise warpage. Slow ambient cooling produces lower moulding stress but extends the cycle. Mould shrinkage for Icorene 3545 is typically in the range of 1.5–2.0%, depending on pigment content and mould restraint. The powder does not require pre-drying at ambient humidity below 50% RH; storage above 60% RH can promote surface moisture adsorption, poor dry flow, and pinhole formation.

    Nominal mechanical and thermal values for the unfilled Icorene 3545 series are consolidated in the following table. These values are typical single-point data from LyondellBasell technical literature and are not specification limits. The BUE 5513 colour package may shift tensile and impact values slightly with pigment loading, part wall thickness, and cooling history.

    PropertyTest methodNominal valueUnit
    DensityISO 1183-1:20190.934g/cm³
    Melt flow rate, 190 °C/2.16 kgISO 1133-1:20224.5g/10 min
    Tensile strength at yieldISO 527-2/1B18MPa
    Tensile elongation at breakISO 527-2/1B>800%
    Flexural modulusISO 178550MPa
    Vicat softening temperature, A50ISO 306118°C
    Melting peak temperatureISO 11357-3127°C
    Environmental stress crack resistance, F50, Condition BASTM D1693-15>1000h

    The property profile shown in the table places the grade in the intermediate stiffness class among rotomoulding polyethylenes. The flexural modulus of 550 MPa is lower than that of high-density rotomoulding grades of 0.945 g/cm³ density, which often exceed 900 MPa; however, the linear low-density architecture returns environmental stress crack resistance and low-temperature ductility values that are difficult to obtain in a high-density homopolymer without compromising processability. Elongation at break above 800% indicates a highly ductile failure mode in short-term tensile deformation; it does not by itself predict long-term creep or slow crack growth behaviour under continuous load.

    When long-term UV exposure and chemical resistance drive specification of BUE 5513 grades

    Outdoor tanks, agricultural hoppers, and marine buoys are the most common application classes for UV-stabilised LLDPE rotomoulding powders. The BUE 5513 designation signals the presence of a hindered amine light stabiliser and a pigment package, although the exact additive loading is not disclosed in standard technical literature. This package is intended to retain tensile elongation and surface gloss after prolonged weathering; acceptance testing generally follows ISO 4892-2 Xenon-arc exposure or ISO 4892-3 QUV fluorescent exposure with end-user-defined retention criteria. Chemical resistance of the base resin follows conventional polyolefin behaviour: it is resistant to dilute acids, aqueous salt solutions, and many alkaline solutions at ambient temperature, but it is swollen by aromatic hydrocarbons, chlorinated solvents, and some mineral oils at elevated temperature.

    For potable-water tanks, the finished article must meet migration limits under EU Regulation 10/2011 and, where applicable, NSF/ANSI 61; the BUE 5513 package may require separate testing because pigment additives are not automatically covered by base-resin food-contact status. Under FDA 21 CFR 177.1520, the base olefin polymer is generally recognized for food-contact use provided the finished article meets end-use extraction conditions, but colourants and stabilisers remain subject to additive clearance and use limitations. The base resin is not recommended for continuous service above 60 °C under sustained internal pressure without a time-dependent hydrostatic strength assessment such as ISO 9080. Short-term tensile and flexural data do not replace long-term creep or slow crack growth testing for pressure vessels. Halogenated flame-retardant additives and certain peroxide crosslinking systems may interfere with the BUE 5513 stabiliser package and should be evaluated for radical scavenging and colour shift before production lot approval.

    The following compliance matrix summarises regulatory positions commonly relevant to rotomoulded articles made from this grade. Final conformity must be established on the finished article, because conversion conditions, pigment loading, and wall thickness affect extraction and migration behaviour.

    Standard or regulationScopeTypical status
    FDA 21 CFR 177.1520Olefin polymers for food contactBase resin recognised; finished-article extraction must be confirmed
    EU Regulation 10/2011Plastic food-contact materialsBase resin complies; BUE 5513 package requires lot confirmation
    NSF/ANSI 61Drinking water system componentsNot automatically covered; formulation-specific testing required
    RoHS Directive 2011/65/EUHazardous substance restrictionsMeets typical limits for lead, mercury, cadmium, hexavalent chromium, PBB, PBDE
    REACH Regulation (EC) 1907/2006Chemical registration and authorisationPolymer and monomer registration obligations apply at import of finished article
    ISO 4892-2Xenon-arc weatheringTest condition used for UV retention; end-user criteria apply

    Processing-property trade-offs against HDPE and metallocene LLDPE

    When compared with a high-density polyethylene rotomoulding powder of similar melt flow rate, Icorene 3545 BUE 5513 gives up stiffness and heat deflection capability in exchange for greater slow crack resistance and better low-temperature ductility. The density difference of approximately 0.010–0.015 g/cm³ between the 0.934 g/cm³ LLDPE and conventional 0.945–0.950 g/cm³ HDPE grades is sufficient to lower flexural modulus by roughly 30–40%. For a geometrically complex tank that must tolerate repeated external impact at low temperature, the LLDPE architecture is often selected over HDPE because the failure mode is more ductile. Against metallocene-catalysed LLDPE rotomoulding powders, the butene-catalysed Icorene 3545 series may exhibit lower dart impact and tensile toughness at equivalent density but generally has a wider processing plateau and lower gel sensitivity. The broad molecular weight distribution supports a slower, more forgiving sintering and bubble-removal stage; metallocene powders can demould earlier but are more sensitive to peak internal air temperature overshoot and mould release variation.

    On production lines, the powder is not compounded before charging. Dry-blending with pulverised colour masterbatch at 2–4 wt% is common; loadings above 5 wt% can increase melt viscosity, reduce impact strength, and produce pinholes at thin corners. Static charge on powder bins can lead to uneven cavity filling; grounding of the mould, vent, and powder-handling equipment is required in dry winter conditions. Aluminium moulds provide faster heat transfer than steel moulds and can shorten cycle time, but differential thermal expansion between mould and polymer increases warpage risk in thick ribs and flat panels. Mould release agents may be used to reduce demoulding force, but silicone-based external releases can interfere with post-mould surface treatment and should be validated before production. Processors working outside these boundaries should generate lot-specific tensile and impact data before mould fabrication.

    Top