Lyondellbasell Icorene 3545 Bue 5504 Polyethylene Linear Low Density

LyondellBasell Icorene 3545 BUE 5504 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 3545 BUE 5504 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 757306
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene
    Density 0.935 g/cm³
    Melt Mass Flow Rate 0.50 g/10 min
    Tensile Strength At Yield 16.0 MPa
    Tensile Strength At Break 31.0 MPa
    Tensile Elongation At Break 700%
    Flexural Modulus 0.700 GPa
    Shore D Hardness 55
    Vicat Softening Temperature 110 °C
    Melting Temperature 125 °C
    Thermal Conductivity 0.33 W/m·K
    Coefficient Of Linear Thermal Expansion 1.5E-4 cm/cm/°C
    Specific Heat 1.9 J/g·°C
    Dielectric Constant 2.3
    Dielectric Strength 20 kV/mm
    Volume Resistivity 1E15 ohm·cm
    Environmental Stress Crack Resistance >1000 h
    Water Absorption <0.01%
    Oxygen Index 17%
    Ul Flammability Rating HB

    As an accredited LyondellBasell Icorene 3545 BUE 5504 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 3545 BUE 5504 Polyethylene, Linear Low Density, is typically supplied in 25 kg bags, palletized and stretch-wrapped.
    Container Loading (20′ FCL) 20′ FCL loading for LyondellBasell Icorene 3545 BUE 5504 LLDPE: palletized bags, securely stowed, braced, and shrink-wrapped for ocean transport.
    Shipping LyondellBasell Icorene 3545 BUE 5504 Linear Low Density Polyethylene ships as non-hazardous resin pellets in 25 kg bags, octabins, or bulk trucks/railcars. Keep containers closed, dry, and away from heat, moisture, UV, and oxidizers. No special DOT/IMDG/IATA hazard classification; follow local regulations and use appropriate handling PPE.
    Storage Store LyondellBasell Icorene 3545 BUE 5504 Polyethylene, Linear Low Density in a cool, dry, well-ventilated warehouse at ambient temperature. Keep original containers sealed, off the floor on pallets, away from direct sunlight, heat, moisture, ignition sources, and strong oxidizers. Avoid prolonged UV exposure. Follow first-in, first-out rotation; prevent dust accumulation, control static, and maintain clean, dry conditions. Use proper grounding.
    Shelf Life LyondellBasell Icorene 3545 BUE 5504 LLDPE shelf life: typically 24 months unopened, stored cool, dry, protected from UV, heat, and moisture.
    Application of LyondellBasell Icorene 3545 BUE 5504 Polyethylene, Linear Low Density

    What Governs Bubble Stability in Butene-Grade LLDPE Film at Thin Gauges?

    On conventional blown-film equipment, direct substitution of a high-pressure LDPE with Icorene 3545 BUE 5504 changes the bubble stability envelope because butene LLDPE does not possess the same strain-hardening behaviour as autoclave LDPE. Production-scale work on 90 mm grooved-feed extruders with L/D 30:1 and dual-lip air rings indicates that a die gap of 1.8–2.4 mm, a blow-up ratio of 2.5:1–3.2:1, and a melt flat-temperature profile between 195 °C and 220 °C are required to keep a stable bubble at 15–25 µm gauge. Addition of erucamide slip at 0.05–0.15 wt% and synthetic silica antiblock at 0.10–0.30 wt% is tested under ASTM D1894; fluoropolymer processing aid at 0.02–0.08 wt% suppresses melt fracture at die shear rates above 500 s⁻¹. For agricultural exposure, hindered amine light stabilizer is compounded at 0.30–0.80 wt% and UV absorber at 0.10–0.30 wt%. Food-contact film is covered by FDA 21 CFR § 177.1520(c) 3.1a and 3.1b, and EU Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm². Terminal products obtained within this process envelope are agricultural silage bags, FIBC liner film, construction vapour barrier sheet, and heavy-duty industrial sacks.

    Compliance and test matrix for film applications
    StandardReferenceBoundary condition
    FDA 21 CFR § 177.1520(c)3.1a/3.1bFood-contact olefin polymer monolayer
    EU Regulation (EU) No 10/2011Article 12, overall migration limit10 mg/dm²
    ASTM D4976-12aStandard specification for PE extrusion materialsMaterial classification
    ISO 1133-1:2022Melt flow rate, 190 °C, 2.16 kgBatch release

    Cast pallet wrap produced from Icorene 3545 BUE 5504 is run as the core layer in three-layer A/B/A structures because the butene LLDPE provides puncture resistance while the skin layers carry cling additives. The core is set at 70–80 wt%, the skin layers at 10–15 wt% each, and polyisobutylene is metered into the skin at 1.0–2.5 wt%; erucamide is omitted or limited to 0.05–0.10 wt% to prevent over-migration. The slot-die gap is 0.5–0.8 mm, the chill-roll temperature is held at 18–28 °C, and line speeds of 300–600 m/min produce film at 12–30 µm. Peel cling is tested according to ASTM D5458, puncture resistance according to ASTM D5748, and tensile properties according to ASTM D882-18. Food-contact grades fall under FDA 21 CFR § 177.1520 and EU Regulation (EU) No 10/2011. Terminal formats are hand stretch wrap, machine pallet wrap, vented or pre-stretched film, and agricultural bale wrap where UV stabilisation is introduced at 0.30–0.60 wt%. At warehouse temperatures below 10 °C, polyisobutylene-based cling force can decline because migration is diffusion-controlled; cold-cling grades require ethylene-vinyl acetate-based tackifiers instead of PIB.

    Rotomoulded IBC Liners: Peak Internal Air Temperature and Wall Porosity Management

    When rotomoulding Icorene 3545 BUE 5504 into IBC liners, pellet grinding to powder with a maximum particle size of 500 µm precedes dry blending with hindered amine light stabiliser at 0.30–0.60 wt%, phosphite/antioxidant synergist at 0.05–0.10 wt%, and pigment masterbatch at 1.0–3.0 wt%. The mould is rotated biaxially at a 4:1 major-to-minor speed ratio in an oven set at 250–300 °C; the peak internal air temperature is held at 190–200 °C for 8–12 min to consolidate powder into a void-free wall of 3–8 mm. Wall porosity is controlled by forced-air cooling at 8–15 °C/min after the curing plateau; rapid cooling of thick sections can induce warpage while slow cooling can leave voids detectable by ASTM D2842. Dangerous goods containers are assessed as rigid plastic IBCs under UN 31H1, and tank-grade polyethylene is specified under ASTM D1998-06. Terminal products are vertical chemical dosing tanks, IBC inner liners, and water-treatment holding vessels. The main boundary for butene LLDPE is lower environmental stress-cracking resistance than octene-1 LLDPE under sustained hydrostatic pressure at 40–60 °C; published data for Icorene 3545 BUE 5504 in this specific configuration is limited, so design should avoid continuous contact with polar solvents and use a minimum wall thickness of 6 mm.

    Because the sealant layer must develop oxidative adhesion against primed foil and corona-treated paper, extrusion coating with Icorene 3545 BUE 5504 is run at melt temperatures from 260 °C to 300 °C through a slot die gap of 0.5–0.7 mm. The resin is let down at 20–40 wt% into an LDPE-rich coating compound to reduce draw resonance; maleic anhydride-grafted LLDPE is added at 0.5–1.5 wt% when bond strength tested under ASTM F904-16 must exceed 1.5–2.0 N/15 mm. Coating weight is maintained between 15 g/m² and 50 g/m², with line speed controlled by chill-roll contact length rather than by melt strength alone. Food-contact laminate layers are governed by FDA 21 CFR § 177.1520(c) 3.1a and EU Regulation (EU) No 10/2011. Terminal flexible structures include aseptic carton sealants, paperboard barrier liners, sachet webs, and medical pouch interlayers. Retortable pouches above 121 °C are outside the recommended sealant performance window because sealant reflow can reduce bond strength and create channel leaks.

    When Thin-Wall Injection Moulding Replaces Flexible PVC in Lid and Closure Applications

    Icorene 3545 BUE 5504 is moulded at 100 wt% or let down at 10–30 wt% with LDPE for pail lids and overcaps on machines with clamp forces from 150 tonnes to 350 tonnes. Barrel zones are set from 190 °C at the feed throat to 230 °C at the nozzle, with injection speed of 60–120 mm/s and holding pressure at 40–70% of peak injection pressure; tool temperatures are kept at 15–35 °C for 1.2–2.0 mm wall sections. Melt flow rate is controlled under ISO 1133-1:2022, density under ISO 1183-2:2019, tensile properties under ASTM D638-14, flexural modulus under ISO 178:2019, and food-contact suitability under FDA 21 CFR § 177.1520. Terminal products are snap-on pail lids, industrial container overcaps, and tamper-evident covers where the lower flexural modulus of butene LLDPE relative to high-density polyethylene requires ribbing or deep-draw design to avoid oil-canning. Published data for this specific injection-moulding grade configuration is limited; mould-filling simulation should use viscosity data from the batch certificate rather than a nominal melt-flow index.

    Free Quote

    Competitive LyondellBasell Icorene 3545 BUE 5504 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 3545 BUE 5504 is a linear low density polyethylene, rotational moulding powder based on a butene-comonomer ethylene copolymer. The model designation carries a nominal density of 0.935 g/cm³ and a nominal melt flow rate of 5.5 g/10 min at 190 °C under a 2.16 kg load determined by ASTM D1238 or ISO 1133-1. The BUE suffix indicates an ultraviolet-stabilized formulation supplied as a free-flowing powder for dry blending, grinding, and rotational moulding. Typical applications include agricultural tanks, outdoor furniture, industrial bins, recreational enclosures, and medium-to-large hollow parts requiring low-temperature ductility. In comparison with blown-film or injection-moulding LLDPE grades of equivalent density, the molecular weight distribution, additive package, and powder morphology are tailored to oven sintering and biaxial wall-thickness development rather than film bubble strength or screw recovery.

    Comonomer Distribution, Rheology, and the 0.935-Density Specification Window

    The grade belongs to the short-chain branched LLDPE family. Butene incorporation introduces ethyl branches along the polyethylene backbone, restricting lamellar thickness and reducing crystalline fraction relative to high-density polyethylene homopolymers. Density measured by ASTM D1505 or ISO 1183-1 therefore remains below the 0.940 g/cm³ threshold separating typical LLDPE from medium-density or high-density polyethylene products. A melt flow rate of 5.5 g/10 min at 190 °C and 2.16 kg is comparatively high among rotomoulding powders; it enables penetration into ribs, kiss-off features, and undercuts during low-shear biaxial rotation, but it also places an upper limit on zero-shear viscosity. In rotational moulding, bubble removal, particle coalescence, and wall-thickness uniformity are governed primarily by powder surface area, melt surface tension, and time-dependent viscosity after sintering. The 0.935 g/cm³ density combined with the 5.5 g/10 min melt flow rate produces a stiffness-impact balance typically selected when nominal wall thickness is in the 4–8 mm range and low-ambient-temperature ductility is a design requirement.

    Powder dry-flow behaviour and particle-size distribution directly influence mould wall-thickness consistency. Rotational moulding powders of this type are generally ground or pulverized to a median particle size between 300 µm and 500 µm, with fines below 150 µm controlled to avoid agglomeration and irregular fluidization within the rotating cavity. Bulk density measured by ASTM D1895 or ISO 60 is used to monitor lot-to-lot uniformity; sieve retention and hopper settings are adjusted at the compounding step rather than by the moulder. On production-scale carousel machines with independent arm speed ratios between 4:1 and 5:1, uneven wall distribution is observed when the powder contains excessive fines or when shot weight is below the specified cavity fill range. Published data for this specific grade’s particle-size distribution is limited; lot-specific certificates from LyondellBasell should be consulted before setting oven cycle timers and mould-position dwell periods.

    How Does Icorene 3545 BUE 5504 Process in Rotational Moulding Relative to High-Density Polyethylene?

    Relative to HDPE rotomoulding grades with densities of 0.945–0.955 g/cm³, the 0.935 g/cm³ LLDPE exhibits a lower melting peak, a broader melting range, and a lower flexural modulus. These differences affect oven-cycle design. The lower crystalline fraction reduces the heat of fusion that must be supplied before sintering and densification, which can allow shorter oven dwell periods or lower peak internal air temperature in thick sections. However, the lower modulus also increases the risk of warpage and dimensional movement during cooling of large flat panels. Moulders typically compensate by increasing wall thickness or by employing controlled cooling air-to-water-mist sequences after demoulding. For parts requiring stacking strength in hot environments, HDPE grades with higher density and higher Vicat softening points may be preferred. For parts subjected to repeated impact at temperatures below −20 °C, this LLDPE class retains ductility more effectively than many high-density homopolymers when evaluated by ASTM D638 or ISO 527-2 tensile yield and instrumented puncture procedures such as ISO 6603-2. Formulated parts of this class are also characterized by environmental stress crack resistance exceeding 1000 h under ASTM D1693 Condition B in 100% Igepal CO-630, whereas HDPE homopolymers can show wider lot-to-lot variation depending on molecular weight and comonomer content.

    Ultraviolet stabilization in the BUE package is intended for outdoor exposure, but actual service life depends on irradiation dose, part thickness, pigmentation, and local temperature cycling. Accelerated weathering of rotationally moulded LLDPE is commonly evaluated by ASTM D2565 or ISO 4892-3 using UVA-340 or UVB-313 lamps; retention of tensile elongation at break is a more sensitive indicator of chain scission than tensile strength. The present grade is not a cross-linked polyethylene and does not develop a thermoset network; it remains melt-reprocessable. In black or heavily pigmented variants, carbon black may provide supplementary ultraviolet screening, but dispersion and concentration must be confirmed by lot-specific documentation. The thermo-oxidative stabilizer package is designed to withstand repeated oven cycles only within the declared processing-temperature envelope. Prolonged excursions above 300 °C can consume hindered phenol or phosphite antioxidants and generate aldehyde or ketone degradation by-products, producing surface tack, gas bubbles, or discolouration. Published accelerated-weathering data for this specific BUE configuration is limited; end-use service life should be validated on the finished article.

    When Stored Above 60% Relative Humidity, Drying and Conveying Constraints Apply

    Although polyethylene is considered non-hygroscopic, rotational moulding powders are susceptible to surface moisture adsorption, particularly when ambient dew point exceeds 15 °C and storage relative humidity exceeds 60%. Surface moisture is a known source of pinholes, porosity, and inconsistent internal surface finish in rotomoulded parts. Pre-drying at 60–70 °C for 1–2 h in a desiccant or circulating-air dryer is typical for powders exposed to humid air before processing; the exact drying profile is established from inventory age, silo ventilation, and transfer-line temperature. Pneumatic conveying systems should be grounded and operated below the minimum ignition energy threshold for polyethylene dust; dust extraction and housekeeping follow NFPA 654 or equivalent local fire-protection codes. Incompatibility with strong oxidizers, chlorinating agents, and aromatic hydrocarbons is relevant during cleaning and maintenance. Contact with these materials can generate swelling, surface hardening, or oxidative degradation. Fine powder accumulations should be removed from hot surfaces, electrical panels, and unventilated hoppers to reduce smouldering ignition risk.

    Regulatory conformance remains application-dependent. The base olefin polymer may be manufactured to meet FDA 21 CFR 177.1520 for repeat-contact food applications when the finished article is tested for end-use extractives; however, the ultraviolet stabilizer and pigment package in this specific grade must be verified against the intended food-contact condition because not all BUE variants are automatically food-contact compliant. European Regulation (EU) No 10/2011 similarly requires migration testing of the finished article under its intended time–temperature exposure profile. RoHS Directive 2011/65/EU restrictions on lead, cadmium, mercury, hexavalent chromium, PBB, and PBDE are relevant only if the final article is sold into electrical and electronic equipment markets; the moulder is responsible for verifying that the supplied powder lot contains no restricted substance above the maximum concentration values. For potable water tanks, NSF/ANSI 61 or equivalent national standards must be evaluated on the produced article, not on the raw powder alone. The grade is not intended for medical devices requiring USP Class VI or ISO 10993 biocompatibility unless explicitly validated by the manufacturer.

    Property Benchmarks Separate LLDPE Rotomoulding Grades from Film and Injection Moulding Resins

    The table below summarizes class-typical property values for a 0.935 g/cm³ butene-based LLDPE rotational moulding powder. The manufacturer’s certificate of analysis remains the normative source for the specific grade, particularly where pigment and UV-stabilizer loading alter mechanical properties.

    Class-typical property ranges for Icorene 3545 BUE 5504 and comparable 0.935-density butene-based LLDPE rotomoulding powders
    Property Test method Class-typical range Engineering significance
    Density ASTM D1505 / ISO 1183-1 0.932–0.938 g/cm³ Controls crystallinity, stiffness, permeation, and low-temperature impact
    Melt flow rate ASTM D1238 / ISO 1133-1, 190 °C, 2.16 kg 5.0–6.0 g/10 min Defines sintering rate and rib-fill capability under low shear
    Tensile yield strength ASTM D638 / ISO 527-2 17–20 MPa Short-term load-bearing capacity at ambient temperature
    Elongation at break ASTM D638 / ISO 527-2 >800% Ductility and resistance to brittle failure
    Flexural modulus ASTM D790 / ISO 178 600–750 MPa Bending stiffness and panel rigidity
    Environmental stress crack resistance ASTM D1693 Condition B, 100% Igepal >1000 h Resistance to slow crack growth in detergent or chemical contact
    Vicat softening point ASTM D1525 / ISO 306 A50 112–120 °C Indicates softening under heated point contact
    Melting peak temperature ASTM D3418 122–127 °C Differential scanning calorimetry peak used for oven setpoint calibration

    The same melt flow rate in blown-film LLDPE would be considered relatively viscous for thin-gauge film processing, while injection moulding LLDPE grades in this melt-flow band are usually formulated with higher melt flow or lower density for thin-wall cavity filling. The rotomoulding powder’s high elongation and environmental stress crack resistance separate it from high-density injection grades, which rely on fast nucleation and short cooling times and often sacrifice low-temperature impact. Compared with metallocene-catalysed LLDPE rotomoulding powders, the butene-based architecture of this class may exhibit a broader molecular weight distribution and lower dart impact, but it can provide a wider sintering window and greater tolerance to oven-temperature overshoot. Published data for direct substitution of Icorene 3545 BUE 5504 with metallocene-based rotomoulding grades is limited; production trials on the target mould remain necessary when changing resin families.