Lyondellbasell Icorene 3545 Bue 5503 Polyethylene Linear Low Density

LyondellBasell Icorene 3545 BUE 5503 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 3545 BUE 5503 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 867134
    Density 0.935 g/cm³
    Melt Flow Rate 3.5 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 17 MPa
    Tensile Strength At Break 20 MPa
    Elongation At Break 800%
    Flexural Modulus 550 MPa
    Hardness Shore D 55
    Vicat Softening Temperature 110 °C
    Melting Point 125 °C
    Environmental Stress Crack Resistance >1000 hr
    Brittleness Temperature < -70 °C
    Impact Strength 20 kJ/m²

    As an accredited LyondellBasell Icorene 3545 BUE 5503 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 3545 BUE 5503 Polyethylene, Linear Low Density is supplied in 25 kg bags, 40 bags per 1,000 kg pallet.
    Container Loading (20′ FCL) 20′ FCL loaded with LyondellBasell Icorene 3545 BUE 5503 Polyethylene, Linear Low Density, 25 kg bags, palletized, shrink-wrapped, securely stowed.
    Shipping LyondellBasell Icorene 3545 BUE 5503 Polyethylene, Linear Low Density ships as a non-hazardous solid resin, typically in 25 kg bags, octabins, or bulk containers. Store cool and dry, away from sunlight and ignition sources. Transport in covered vehicles and comply with all applicable local, national, and international shipping regulations.
    Storage Store LyondellBasell Icorene 3545 BUE 5503 LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed to prevent moisture and contamination. Avoid strong oxidizing agents. Maintain ambient storage temperatures and practice first-in, first-out rotation. Protect bags from tearing, UV exposure, and excessive stacking.
    Shelf Life Typically 24 months from production when stored in original, unopened packaging under cool, dry, well-ventilated conditions, away from direct sunlight.
    Application of LyondellBasell Icorene 3545 BUE 5503 Polyethylene, Linear Low Density

    Industrial application data for LyondellBasell Icorene 3545 BUE 5503 linear low-density polyethylene are organized below according to established downstream processing routes. The material is supplied as a rotomoulding-grade powder with a butene-copolymer backbone and a stabilization package indicated by the BUE 5503 suffix; exact density and melt flow rate values for a given lot must be confirmed from the certificate of analysis because production lots are controlled within specification intervals. Processing windows shown in the following sections are industrial starting values for equipment-specific qualification and do not replace the manufacturer’s technical data sheet, regional food-contact approvals, or the safety data sheet.

    What Limits Wall Porosity in Rotomoulded Agricultural Water and Liquid Feed Tanks?

    Rotational moulding of agricultural water and liquid feed tanks with Icorene 3545 BUE 5503 starts with dry blending of 100 parts virgin powder, a rotomoulding-grade colour masterbatch at 0.2 wt% to 1.0 wt%, and clean internally generated regrind at ≤20 wt% of total feed; higher regrind fractions reduce low-temperature impact strength and increase the risk of pinhole formation in the upper tank wall. The loaded mould is heated in a forced-air carousel oven with an air setpoint of 260 °C to 300 °C until the internal air temperature reaches 190 °C to 220 °C. Rotation speed ratio is maintained between 1:4 and 1:8, with a primary-axis speed of 8 rpm to 12 rpm; the dwell time for a nominal 6 mm wall is typically 18 min to 28 min. The main process conflict is between densification and porosity: an oven setpoint above 300 °C accelerates melting but drives coalesced gas bubbles toward the inner wall and can create voids, while an internal air temperature below 180 °C leaves poorly densified corners and reduced environmental stress crack resistance under ASTM D1693-15b Condition B. Cooling is staged, with forced air to drop the part surface to 90 °C to 110 °C, followed by a water mist not exceeding 15 °C/min cooling rate; demoulding is performed only after the surface is below 70 °C. Pre-drying is not required because the powder is non-hygroscopic; if silo bags show condensation at relative humidity above 80%, a dry-air purge at 40 °C for 30 min is used before charging. Compliance for potable water contact is assessed under NSF/ANSI 61, FDA 21 CFR 177.1520(c) 3.2a, and EU Regulation No 10/2011; for liquid animal feed tanks, EU Regulation No 1935/2004 conditions of good manufacturing practice under EC 2023/2006 apply. Terminal products include cylindrical agricultural water storage tanks, rainwater harvesting tanks, and liquid feed tanks for livestock dosing.

    For insulated cold-chain transport boxes manufactured from Icorene 3545 BUE 5503, the rotomoulding process uses a shuttle or carousel machine with a primary-arm rotation speed of 7 rpm to 10 rpm and a secondary axis at 1.5 rpm to 2.5 rpm. The powder is dry-blended from 100 parts base resin, 0.2 wt% to 0.8 wt% of a food-grade compatible pigment masterbatch, and 0.5 wt% to 1.0 wt% of an internal mould-release additive only when ejection force exceeds the machine demoulding limit. Oven temperature is set to 260 °C to 290 °C; the desired internal air peak is 190 °C to 220 °C, and cooling is controlled at 10 °C/min to 15 °C/min below 100 °C to prevent cold-chain impact failure under ISO 179-1:2017 notched Charpy evaluation at -20 °C. For food-contact boxes used in fish and fresh produce logistics, compliance is established through FDA 21 CFR 177.1520(c) 3.2a, EU Regulation No 10/2011 Annex I overall migration not exceeding 10 mg/dm², and good manufacturing practice under EC 2023/2006. Terminal products are insulated cold-chain transport boxes, fish landing and storage boxes, and ice bins for food service.

    Standard/RegulationClause or MethodMeasured ParameterControl Value
    FDA 21 CFR177.1520(c) 3.2aOlefin polymer food-contact statusConforms
    EU Regulation No 10/2011Annex IOverall migration10 mg/dm²
    EC 2023/2006Good manufacturing practiceFood-contact materialsDocumented GMP
    ISO 179-1:2017Charpy notched impactImpact at -20 °CNo brittle crack

    When Marine Buoys Demand Long-Term UV Ageing Resistance

    When a rotomoulded marine buoy is exposed to continuous seawater and UV radiation, the stabilization package of the BUE 5503 suffix is supplemented only for extended outdoor warranty conditions; otherwise the dry blend is 100 parts Icorene 3545 BUE 5503, 0.5 wt% to 1.5 wt% of an additional HALS masterbatch, and 0.2 wt% to 1.0 wt% of pigment masterbatch formulated without heavy-metal colorants. The part is processed on a rock-and-roll or carousel rotomoulding unit with a wall thickness of 5 mm to 12 mm; oven setpoint is 270 °C to 300 °C, and the internal air temperature is held between 200 °C and 220 °C for a densification plateau of 5 min to 10 min before cooling. Rotation ratio for buoy shapes with asymmetric draft sections is set at 1:5 to 1:8 to control wall distribution at the rope eyelet and ballast flange. Inserts, such as galvanized steel attachment points, are preheated to 80 °C to 120 °C before charging; a sharp thermal gradient above 40 °C between insert and powder is avoided because it produces a resin-starved interfacial region and early stress cracking under load. Compliance for marine equipment uses REACH Regulation (EC) No 1907/2006 Annex XVII, RoHS Directive 2011/65/EU for restricted substances, and ASTM G154-23 Cycle 1 accelerated UV exposure for performance testing; published data for this specific configuration is limited, so end-use qualification remains mandatory. Terminal products are marine buoys, floating fenders, and buoyancy modules for aquaculture installations.

    Rotomoulded Playground Panel and Outdoor Furniture Impact Requirements

    Playground panels and outdoor furniture shells manufactured from Icorene 3545 BUE 5503 are dry-blended with 0.5 wt% to 2.0 wt% of a heavy-metal-free colour masterbatch and 0.5 wt% to 1.0 wt% of a UV-stabilizer masterbatch; post-consumer recycled powder is limited to ≤15 wt% of total feed because higher fractions create inconsistent impact behaviour under ASTM F963-23 and EN 71-3:2019+A1:2021 heavy-metal migration testing. The part is rotomoulded on a carousel line at an oven setpoint of 280 °C to 300 °C and an internal air temperature of 200 °C to 215 °C; wall thickness is controlled between 6 mm and 10 mm for structural panels. The cooling phase is divided into a forced-air stage to 100 °C, a water-mist stage to 60 °C, and a final air-cool stage to ambient; rushing through the mist stage above 12 °C/min accelerates skin shrinkage and produces visible sink marks around bosses and mounting holes. After demoulding, panels are conditioned at 23 °C and 50% RH for 24 h before impact verification; failure is defined as full-thickness cracking or detachment of any metal insert, not as surface scuffing. Compliance for toy-like playground components in the EU includes EN 71-3:2019+A1:2021 and REACH Annex XVII; for the North American market, ASTM F963-23 and 16 CFR Part 1303 lead limits apply. Terminal products are rotomoulded playground panels, outdoor seating shells, and safety barrier components for public play areas.

    For additive and colour concentrate producers, Icorene 3545 BUE 5503 functions as a carrier powder in masterbatch and compound production. The resin is incorporated at 30 wt% to 70 wt% of the formulation, with organic or inorganic pigment or filler at 20 wt% to 60 wt%, a low-molecular-weight polyethylene wax dispersant at 5 wt% to 15 wt%, and a hindered phenolic antioxidant at 0.1 wt% to 0.5 wt%. Compounding is performed on a co-rotating twin-screw extruder with 40:1 to 52:1 L/D ratio, segmented screws, melt temperature 180 °C to 210 °C, specific mechanical energy of 0.15 kWh/kg to 0.25 kWh/kg, and continuous melt filtration through a 200-mesh screen pack before strand pelletizing. The terminal product is a colour or additive masterbatch in pellet form, subsequently let down at 2 wt% to 6 wt% into rotomoulding, blow-moulding, or film-grade polyethylene. Compliance for the masterbatch mixture is governed by REACH Annex XVII and RoHS Directive 2011/65/EU; where the masterbatch is intended for food-contact end articles, EU Regulation No 10/2011 Annex I and FDA 21 CFR 177.1520(c) status of the carrier resin are part of the supply documentation.

    Large industrial waste containers and curbside bins manufactured from Icorene 3545 BUE 5503 are rotomoulded on independent-arm or shuttle machines with wall thickness specified at 6 mm to 12 mm for the lower body and 4 mm to 8 mm for the upper rim. The powder is dry-blended with 0.2 wt% to 0.6 wt% black pigment masterbatch and 0.3 wt% to 0.7 wt% UV-stabilizer masterbatch for outdoor storage. Processing uses an oven setpoint of 270 °C to 300 °C and an internal air temperature peak of 200 °C to 215 °C; demoulding is delayed until the part surface drops below 70 °C to prevent distortion at wheel slots and lid retainers. Terminal products are municipal waste bins, industrial hazardous-waste containers, and recycling collection containers. Compliance includes REACH Annex XVII, RoHS Directive 2011/65/EU, and EN 840-1:2020 for mobile waste containers.

    Free Quote

    Competitive LyondellBasell Icorene 3545 BUE 5503 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 3545 BUE 5503 Polyethylene, Linear Low Density is a butene-comonomer linear low density polyethylene powder supplied for rotational molding of hollow parts. The product combines a nominal density of 0.935 g/cm³ (ISO 1183-1) with a melt flow rate of 5.0 g/10 min at 190 °C/2.16 kg (ISO 1133-1). The powder carries a UV stabilization package identified by the 5503 designation, which is intended for outdoor components such as storage tanks, agricultural hoppers, and access covers. The powder form permits dry blending with pigment masterbatches or foaming agents before charging to the mold, provided the additive particle size remains within the sieve tolerance of the base resin.

    Compared with high-density polyethylene rotomolding powders above 0.940 g/cm³, this grade trades modulus for higher environmental stress-crack resistance and greater elongation. Compared with octene-based LLDPE grades, the butene comonomer produces shorter side branches and a less efficient tie-molecule network at equivalent density, which generally lowers low-temperature dart impact but reduces raw-material cost and improves processability on carousel lines. The material is not a metallocene-catalyzed grade; its molecular architecture is therefore more heterogeneous in short-chain branching distribution than single-site resins of similar density. That heterogeneity produces a broader melting range and can reduce warpage in thick-walled parts, but it also requires tighter control of oven residence time to avoid low-crystallinity fusion defects at the inner wall.

    Published typical property values for LyondellBasell Icorene 3545 BUE 5503
    PropertyTest methodTypical value
    Melt flow rateISO 1133-1:2022, 190 °C/2.16 kg5.0 g/10 min
    DensityISO 1183-1:20190.935 g/cm³
    Tensile yield stressISO 527-2/1A18 MPa
    Tensile modulusISO 527-2/1A550 MPa
    Elongation at breakISO 527-2/1A>800%
    Vicat softening temperatureISO 306/A50118 °C
    Brittleness temperatureASTM D746-20-70 °C
    Environmental stress-crack resistanceASTM D1693-15, condition B, 100% Igepal>1000 h

    The tabulated values are supplier-published typical values, not release limits. Lot-to-lot variation in ESCR and brittleness temperature can be significant when regrind or pigment masterbatch is added; incoming resin certificates should be retained for traceability. Published data for the specific configured formulation is limited for extended weathering beyond 5000 h in xenon-arc or 3000 h in fluorescent UV apparatus; therefore, outdoor service in high-UV environments must be validated on finished parts.

    What Operating Boundaries Emerge on Production-Scale Rotomolding Lines?

    On shuttle and carousel machines, the product is typically brought to a peak internal air temperature of 210 °C to 240 °C. Oven set points between 280 °C and 320 °C are common, with residence time adjusted to mold metal mass and wall thickness. Peak internal air temperatures below 200 °C leave residual powder grains at the mold surface, causing porosity and low tensile strength in fusion tests. Temperatures above 250 °C accelerate oxidative degradation of the polymer and the UV stabilizer, producing yellowing at the inner surface and a measurable loss of elongation at break.

    Because the grade is a powder, moisture uptake in humid storage can introduce steam bubbles during densification. Pre-drying at 60 °C to 70 °C for 2 h to 4 h is recommended when bulk powder has been exposed to relative humidity above 60% or when pinholes are observed in first-shot parts. Agitated dryers or fluid-bed dryers are preferred over static tray dryers to avoid particle fusing. On twin-screw compounding lines used to precompound the powder with color concentrates, barrel set temperatures should remain below 220 °C to preserve the stabilization package; higher melt temperatures can deactivate hindered amine light stabilizers before the molding operation.

    The melt flow rate of 5.0 g/10 min supports filling of long, narrow cavities that high-molecular-weight HDPE powders cannot reach before mold skin tackifying. The trade-off appears when molding very thin walls below 3 mm, where the low melt viscosity permits early drainage from vertical surfaces and produces thick rims with thin center sections. In such cases, a lower-melt-flow grade or a modified rotation ratio may be required to maintain wall thickness tolerance.

    Powder dry-flow and bulk density are monitored by ASTM D1895 Method A and Method B. A dry-flow drift outside the supplier acceptance range can indicate accumulated fines from grinding, recycled powder, or moisture. Bulk density below the nominal value for the grade can produce insufficient powder mass in deep mold cores, resulting in thin sidewalls at the bottom of vertical tank ribs. On aluminum molds with internal ribs, the powder must flow into rib cavities before the mold skin reaches the tackifying temperature; otherwise, bridging occurs and the rib remains hollow. Sieve analysis to ASTM D1921 is used to detect particle-size shift; excessive fines below 125 µm can segregate during mold rotation and produce localized pinholes in the part corners.

    Fusion testing should be performed on prototype parts by cutting a cross-section and examining the melt lines. Residual powder at the inner surface appears as a granular layer under 20× magnification and indicates insufficient peak internal air temperature. Dynamic mechanical analysis in torsion or flexure can detect a lower storage modulus at 60 °C if the wall is undercured; this is more sensitive than tensile yield for detecting processing defects in parts with complex ribs.

    Thermal Degradation and Stabilizer Consumption in Long-Cycle Molding

    For parts with wall thickness above 10 mm, oven cycle time becomes the principal degradation risk. The inner surface remains above 180 °C for extended periods while the outer wall cools, consuming antioxidant and UV stabilizer at different rates. Oxidative induction time measured by differential scanning calorimetry to ISO 11357-6 can be used to compare molded parts against virgin powder. A reduction below 20 min at 200 °C in the final part indicates significant stabilizer depletion and should trigger cycle reduction or lower oven set point.

    The 5503 stabilization package is intended for outdoor UV service. In rotomolded parts exposed to sunlight, UV degradation is dominated by surface crazing and loss of elongation at break; tensile impact alone may remain acceptable for a longer period. Long-term outdoor performance should be evaluated using ASTM D2565 xenon-arc exposure or ASTM G154 fluorescent UV exposure on rotomolded test panels, with tensile elongation retention as the primary failure criterion. Measurement of gloss loss without confirming elongation retention is not sufficient for load-bearing tank walls.

    Regrind addition above 20% by weight can reduce ESCR and low-temperature impact because the regrind has undergone one or more thermal histories and may contain oxidized outer skin from shredded parts. A drop in ESCR below 500 h under ASTM D1693 condition B or a brittleness temperature increase above -60 °C indicates excessive regrind or contamination. Production facilities that return unpigmented fall-back powder directly to the virgin stream should screen at 500 µm to remove melt skin flakes.

    In chemical tank service, the material is evaluated according to ASTM D1693 for environmental stress-crack resistance, but chemical compatibility must be confirmed by immersion testing in the actual stored fluid at the maximum service temperature. The lower density and butene comonomer content improve resistance to slow crack growth in mild detergents and aqueous acids compared with HDPE grades of equal melt flow rate. It is not recommended for continuous contact with strong oxidizing acids, aromatic hydrocarbons, or chlorinated solvents at elevated temperature unless tank wall stress and fluid absorption have been calculated. Compared with crosslinked polyethylene, the grade remains thermoplastic and therefore cannot sustain the same sustained internal pressure at elevated temperature; creep rupture and environmental stress cracking govern long-term failure.

    Because the grade is stabilized for weathering, the outer skin contains hindered amine light stabilizers and phenolic antioxidants that migrate at different rates. Extraction by nonpolar solvents can remove surface stabilizers and reduce the UV resistance of the finished part. For tanks storing fatty or oily substances, the wetted inner wall may lose antioxidant protection faster than the outside; this is a known limitation for rotational-molded polyolefin tanks.

    When Regulatory Compliance for Food-Contact and Outdoor Articles Is Required

    Regulatory conformity for the grade depends on the additive package and the final article construction. The following matrix summarizes the principal compliance instruments that a fabricator should request from the resin supplier or verify on the finished component. Because the powder is intended for industrial processing and not for consumer use as a formulated compound, final food-contact status is determined by the complete formulation, including colorants and processing aids.

    Compliance checklist for LyondellBasell Icorene 3545 BUE 5503
    Regulation or standardScopeVerification requirement
    FDA 21 CFR 177.1520Olefin polymers for direct food contactConfirm finished article meets extractive and end-use condition of food type specified by the article fabricator
    EU 10/2011Plastic materials intended for food contactOverall migration limit 10 mg/dm²; verify specific migration of additives against original supplier declaration
    REACH EC 1907/2006Registration, evaluation, authorization of chemical substancesConfirm grade is registered and no SVHC above 0.1% w/w
    RoHS 2011/65/EURestriction of hazardous substances in electrical and electronic equipmentSupplier must confirm lead, cadmium, mercury, hexavalent chromium, PBB and PBDE are not added

    Because the grade is supplied as a powder, dust control is required. The product should be stored in sealed containers below 30 °C and away from direct sunlight to preserve the UV stabilizer before processing. Combustible dust precautions apply during conveying and dry blending; equipment grounding and explosion venting must follow local regulations. For processing facilities with high dust loading, a maximum dust concentration below the lower explosion limit, typically 30 g/m³ for polyethylene, is a conservative engineering control.

    Agricultural tank bodies and flat-bottom hoppers are the dominant application envelope. The grade’s melt flow rate supports filling of long, narrow flat cavities, but rotation ratio, internal air flow, and cooling rate must be revalidated when changing from cylindrical to rectangular molds. Warpage at parting lines and shrinkage pull-in around metal inserts remain the primary defects observed on production lines; these are controlled by cooling sequence and mold release rather than by polymer properties alone. Slow air cooling inside the mold reduces residual stress but increases cycle time, while water mist cooling shortens cycle time but raises warpage risk at mold parting lines; for critical tank openings, forced-air cooling with directed fans at 0.5 m/s to 1.5 m/s is preferable.

    Top