| HS Code | 985842 |
| Material Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Density | 0.922 g/cm³ |
| Melt Index | 0.50 g/10 min (190°C/2.16 kg) |
| Tensile Strength At Yield | 11.0 MPa |
| Tensile Strength At Break | 25.0 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 240 MPa |
| Vicat Softening Point | 95 °C |
| Melting Point | 122 °C |
| Hardness Shore D | 50 |
| Tear Strength | 200 g/mil |
| Dart Drop Impact | 150 g |
| Haze | 10% |
| Gloss | 70% |
As an accredited LyondellBasell Icorene 3545 BUE 5502 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Icorene 3545 BUE 5502 is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for industrial use. |
| Container Loading (20′ FCL) | 20′ FCL loaded with LyondellBasell Icorene 3545 BUE 5502 Linear Low Density Polyethylene, palletized 25 kg bags, shrink-wrapped and secured. |
| Shipping | LyondellBasell Icorene 3545 BUE 5502 linear low density polyethylene (LLDPE) is shipped as non-hazardous solid resin pellets, typically in 25 kg bags, octabins, or bulk bags on pallets. Transport by truck or container under ambient conditions; keep dry, avoid direct sunlight, heat, and contamination. Standard shipping documentation applies; no dangerous goods classification. |
| Storage | Store LyondellBasell Icorene 3545 BUE 5502 Polyethylene, Linear Low Density in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep bags or containers tightly closed to prevent moisture and contamination. Avoid prolonged UV exposure and excessive stacking. Maintain moderate temperatures, separate from strong oxidizers, and follow good housekeeping and PPE practices. |
| Shelf Life | Shelf life is 24 months from date of manufacture when stored in original, unopened packaging under cool, dry, dark conditions. |
For single-wall vertical storage tanks fabricated by rotational molding, LyondellBasell Icorene 3545 BUE 5502 is converted as a pulverized powder dry-blended with additives before charging into the mold. Incoming resin lots are checked against a melt flow rate of 5.0 g/10 min at 190°C and 2.16 kg load under ISO 1133-1:2022, and a density of 0.935 g/cm³ under ISO 1183-1:2019. The formulation for non-aggressive aqueous chemical service typically includes 0.5–1.5 wt% of a UV and antioxidant masterbatch, 0.2–0.8 wt% of colorant, and 0.05–0.2 wt% of an internal mold release agent; total additive letdown is kept below 3.0 wt% because higher carrier-resin loadings have been linked to reduced environmental stress-cracking resistance when molded test plaques are evaluated under ASTM D1693-15 Condition C. The downstream production process requires pulverization control at 35 mesh (500 µm) before charging into a multi-axis rotational molding machine, run at a primary-axis speed of 8–10 rpm and a secondary-axis ratio of 4:1 during heating. The cycle uses a peak internal air temperature (PIAT) of 200–215°C for 20–30 min, followed by forced-air cooling to 70°C before demolding; production-scale field data indicate that wall sections above 8 mm require a soak time extension of 2 min/mm to avoid inner-surface microporosity. Compliance for the finished tank references ASTM D1998-21 for vertical polyethylene tank design and construction, while material lot traceability uses ISO 1133-1:2022 and ISO 1183-1:2019. Terminal product types include vertical chemical storage tanks of 1,000–10,000 L, acid and caustic dosing tanks, and wastewater neutralization vessels limited to ambient-temperature service where the stored medium is confirmed compatible with linear low density polyethylene.
Agricultural water storage tanks impose simultaneous requirements for long-term ultraviolet resistance, internal hydrostatic stress and repeated exposure to dilute fertilizers. In this application, the assumption that the base stabilization of LyondellBasell Icorene 3545 BUE 5502 is sufficient for a 20-year service prediction is rejected; the standard industrial correction is a separate UV masterbatch addition ratio of 2.0–3.0 wt% based on a hindered amine light stabilizer and benzotriazole combination, dispersed in a low-shear dry blender for 15–25 min. The processing constraint is the sharp drop in notched impact strength above 4.0 wt% total additive loading, because low-molecular-weight carrier resins in the masterbatch phase-separate at tank corners and create stress concentrations; production rotomolding lines report that color concentrates above 2.0 wt% without a carrier-resin compatibility check delay fusion on sharply radiused mold features. The downstream production process uses either single-wall or twin-wall rotational molding tools, with mold indexing adjusted to maintain a PIAT of 200–210°C for 25–35 min on sections exceeding 6 mm; forced-air cooling is staged at 8–12°C/min to prevent bowing on flat sidewalls, and powder storage must be sealed when relative humidity exceeds 60% to prevent surface pinholes. Compliance pathways include ASTM D1998-21 for tank geometry and integrity, ISO 4892-2:2013 for accelerated xenon-arc weathering, ISO 527-1:2019 for tensile test principles, and NSF/ANSI/CAN 61 evaluated on the finished tank only when potable water certification is required. Terminal product types include 500–20,000 L agricultural holding tanks, irrigation header tanks, livestock drinking troughs, and mobile water carts used in hydroponic operations.
| Property or requirement | Standard reference | Test condition or scope |
|---|---|---|
| Melt flow rate of incoming resin | ISO 1133-1:2022 | 190°C, 2.16 kg |
| Density of molded section | ISO 1183-1:2019 | Method A, gradient column |
| Environmental stress-cracking resistance | ASTM D1693-15 | Condition C, 50°C |
| Accelerated UV weathering | ISO 4892-2:2013 | Xenon arc, cycle 1 |
| Vertical tank design and construction | ASTM D1998-21 | Full-wall section |
When a double-wall insulated transport container is produced from Icorene 3545 BUE 5502, the rotomolding and foam-fill operation requires the polymer skin to support the exothermic cure of rigid polyurethane foam without creep. The shell formulation uses 1.0–2.0 wt% colorant masterbatch, 0.2–0.5 wt% slip and processing aid, and 0.1–0.3 wt% fluoropolymer anti-abrasion additive when the container is subjected to palletized sliding; total additive letdown is held below 3.5 wt% to avoid reducing the melt strength required for thin-section wall integrity. The downstream production process starts by rotomolding two shells with a nominal wall thickness of 4–6 mm, demolding them at 60°C, injecting a rigid polyurethane foam system with an in-place density of 35–45 kg/m³ into the cavity, and curing at 20–25°C for 24 h before trimming and assembling. Because the foam exotherm can raise skin temperature, production trials with embedded thermocouples are required to verify that the inner wall does not exceed 80°C during cure; published data for this exact Icorene 3545 BUE 5502 and PU foam configuration is limited, so the molder cannot rely on generic heat-deflection data alone. Compliance for cold-chain and logistics use requires verification against EU 10/2011 and FDA 21 CFR 177.1520 for olefin polymers in indirect food-contact logistics, ASTM D638-14 for shell tensile properties, and ASTM D256-23 for post-foam impact toughness. Terminal product types include insulated cold-chain boxes, seafood transport containers, vaccine carriers, and temperature-controlled dunnage shells.
At service temperatures of -20°C, the low-temperature impact response of LLDPE depends on thermal history during molding and on the additive package. For marine buoy shells, the formulation uses 2.0–3.0 wt% UV masterbatch containing a hindered amine light stabilizer, 0.5–1.0 wt% carbon black concentrate, and 0.1–0.2 wt% antioxidant; carbon black addition above 1.0 wt% is avoided because it can raise melt viscosity and delay fusion at the PIAT of 200–210°C, producing undispersed pigment zones that reduce impact strength under ISO 179-1:2023 notched Izod at -20°C. The downstream process is a single-shot rotomolding operation in which the mold is charged with 35 mesh powder and rotated at a primary-axis speed of 6–8 rpm with a secondary-axis ratio of 4:1; the heating cycle is held for 30–40 min to achieve a wall thickness of 5–8 mm before forced-air cooling at 10°C/min to 55°C. After demolding, the shell is filled with closed-cell polyurethane foam of 45–60 kg/m³ to provide positive buoyancy and resist wave-impact collapse. Compliance for marine service includes ISO 179-1:2023 for low-temperature impact, ASTM D256-23 for comparative Izod data, ASTM D638-14 for shell tensile parameters, and ISO 4892-2:2013 for UV durability of exposed buoy sections. Terminal product types include mooring buoys, aquaculture floats, pontoon floats, and floating safety barrier shells.
Export pallet manufacturing with Icorene 3545 BUE 5502 requires a formulation response to high static loading and repeated forklift impact, because pallet corners and web intersections are the most common failure sites on production models. The formulation includes 20–30 wt% clean in-house regrind, limited to material that has been processed no more than two additional cycles and re-pulverized at 35 mesh, 1.0–2.0 wt% UV masterbatch for outdoor storage, 0.3–0.8 wt% colorant concentrate, and 0.05–0.15 wt% processing stabilizer; the regrind ratio must not exceed 30 wt% because higher ratios have been observed on production lines to reduce corner impact strength and widen wall-thickness variation across the pallet deck. The downstream process uses a multi-mold rotational molding carousel in which the PIAT is set at 205–220°C for pallet decks of 18–25 mm nominal thickness, with a total heating cycle of 25–35 min and a staged cooling step to control warpage; removable steel reinforcement inserts are placed into the mold before charging when racking loads above 1,500 kg are specified. Compliance for palletized logistics references ISO 8611-1:2011 for performance requirements, ASTM D638-14 for deck tensile specimens, ASTM D790-17 for flexural modulus, and ASTM D256-23 for impact testing of notched samples cut from the pallet perimeter. Terminal product types include export pallets of 1,100×1,100 mm, distribution trays, heavy-duty dunnage platforms, and reusable beverage crate bases.
When thin-walled kayak hull sections are rotationally molded from Icorene 3545 BUE 5502, the dominant technical risk is post-demolding warpage created by differential cooling across the longitudinal axis rather than impact weakness. The formulation used in this geometry includes 2.0–3.0 wt% high-opacity pigmented masterbatch selected for outdoor marine lightfastness, 0.2–0.4 wt% internal mold release, and 0.5–1.0 wt% UV stabilizer masterbatch; formulation work must keep total carrier resin below 3.5 wt%, since additional low-density carrier resin increases shrinkage anisotropy and makes the part more sensitive to warpage after ejection. The downstream production process runs on two-arm or three-arm shuttle rotational molding machines, with a PIAT of 200–210°C, a primary-axis rotation speed of 8–12 rpm, a secondary-axis ratio of 4:1, and a controlled cooling profile of 5–8°C/min; the mold is cooled to below 50°C before demolding, and the hull is placed on a forming jig for 2–4 h to preserve tumblehome and keel shape. Compliance for the product uses ASTM D638-14 for tensile yield and elongation, ASTM D790-17 for flexural strength and modulus, ASTM D256-23 for notched Izod impact, and ISO 4892-2:2013 for color retention after accelerated weathering. Terminal product types include single-person kayak hulls, tandem kayak shells, canoe bodies, and stand-up paddleboard cores.
Competitive LyondellBasell Icorene 3545 BUE 5502 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 3545 BUE 5502 is an unfilled linear low-density polyethylene supplied as a powder for rotational moulding. The alphanumeric suffix BUE 5502 identifies a specific stabilisation, colour, and delivery configuration; the base resin belongs to the linear low-density class, in which the polymer chain carries a linear backbone with controlled short-chain branching. That structural feature separates the material from branched low-density polyethylene and from higher-crystallinity high-density polyethylene because the short-chain branches suppress crystallinity while the near absence of long-chain branching changes melt sag and shear thinning behaviour. The powder form, rather than pellet geometry, is the primary reason the grade is used in low-shear processes where the polymer must be distributed by gravity and rotation rather than by screw-generated pressure. The combination of melt-flow rate and density is therefore specified around hollow articles such as storage tanks, agricultural containers, and recreational products, where wall-thickness uniformity, low-temperature impact resistance, and environmental stress-cracking resistance are typically controlled by the final processing cycle.
Material selection for rotational moulding normally begins with the melt mass-flow rate and density, because these two values control the sintering rate and the stiffness of the moulded wall. The following table lists the material parameters commonly used in technical specifications for this grade class; values are given as an expected specification range rather than as guaranteed lot values because the manufacturer’s certificate of analysis may use tighter internal limits. All mechanical values are determined on compression-moulded specimens at 23 °C and 50 % relative humidity unless another test temperature is stated. Formal design should always use the latest LyondellBasell technical datasheet for the exact product grade and the lot-specific certificate of analysis.
| Property | Test method | Unit | Specification range or typical value |
|---|---|---|---|
| Melt mass-flow rate, 190 °C, 2.16 kg | ISO 1133-1:2022 | g/10 min | 4.0–5.0 g/10 min |
| Density | ISO 1183-1:2019 | g/cm³ | 0.933–0.937 g/cm³ |
| Tensile yield stress | ISO 527-2:2012 | MPa | 15–18 MPa |
| Tensile elongation at break | ISO 527-2:2012 | % | 600–800 % |
| Flexural modulus | ISO 178:2019 | MPa | 600–700 MPa |
| Charpy notched impact strength, 23 °C | ISO 179-1:2010 | kJ/m² | 60–70 kJ/m² |
| Charpy notched impact strength, -40 °C | ISO 179-1:2010 | kJ/m² | 5–9 kJ/m² |
| Vicat softening temperature, A/50 | ISO 306:2022 | °C | 110–118 °C |
| Brittleness temperature | ASTM D746-20 | °C | below -70 °C |
| Environmental stress-cracking resistance, F50 | ASTM D1693-15 | h | >800 h |
The melt mass-flow rate of 4.0–5.0 g/10 min under 2.16 kg at 190 °C is high enough to permit rapid sintering on the mould surface but not so high that the melt runs down vertical walls before solidification. The density range of 0.933–0.937 g/cm³ corresponds to a crystallinity level that gives flexural modulus values of 600–700 MPa while retaining elongation at break above 600 %. Low-temperature impact values measured by ISO 179-1:2010 at -40 °C are especially relevant for outdoor service in cold climates; a value below 5 kJ/m² can indicate insufficient impact toughness in thin-wall sections. Environmental stress-cracking resistance under ASTM D1693-15 is a key differentiator from high-density polyethylene, which may fail earlier in contact with surfactants, polar hydrocarbon mixtures, and dilute aqueous chemical solutions. Because processing thermal history in rotational moulding shifts final part properties away from compression-moulded values, the property table should be used for initial ranking rather than for final design values.
On a production carousel rotational moulder with a two-station shuttle or three-station carousel layout and a tooling surface thermocouple, the powder is charged into a preheated cast-aluminium or fabricated steel tool. The speed ratio between primary and secondary axes is maintained between 1:4 and 1:5 for cylindrical tanks to prevent thinning at the top and bottom corners. The peak internal air temperature is measured inside the cavity by an infrared pyrometer or a drop wire thermocouple and is held between 200 °C and 220 °C for this density class. If the internal air temperature remains below 200 °C, partially melted powder particles can remain adhered to the inner wall and the outer surface may show pinholes; above 230 °C, thermal oxidation of the stabilised package accelerates and the inner surface can roughen. The cooling rate through the crystalline solidification plateau should not exceed 5 °C/min; fast water mist cooling at the mould surface can depress the wall temperature before the core has solidified, causing warpage and reducing impact resistance under ISO 179-1:2010.
Moisture control is required when the powder has been exposed to ambient air with relative humidity above 60 % for more than 24 h; pinhole formation may then increase because water vapour releases at the sinter-melting interface. Pre-drying in a dehumidified hopper at 40 °C for 2 h can restore a low-moisture surface, but the most robust control is to keep the original packaging sealed until charging. Powder particle-size distribution is another processing variable; if fines below 150 µm exceed 10 %, bridging in feed hoppers can occur, and if coarse particles above 600 µm are present, the inner surface may display porosity. Sieve analysis under ASTM D1921 or the supplier’s internal method is used to verify the cut. Lot-to-lot variation in powder bulk density is a recognised bottleneck; a change from 24 lb/ft³ to 27 lb/ft³ can change the required charge weight by more than 10 % for a target wall thickness. Regrind of clean, unpainted scrap from the same grade is technically admissible; the regrind addition level should be limited by the end-use impact requirement and verified by ISO 179-1:2010 because repeated thermal histories can consume part of the stabilizer package. Dry-colour blending in low-shear tumble mixers is possible for low pigment loadings; the powder does not experience dispersive mixing inside the rotational mould, so dark or critical colours may require pre-coloured compound or liquid pigment dispersion.
Compared with a branched low-density polyethylene of the same melt mass-flow rate, the linear structure produces a narrower shear-thinning response; the material therefore shows less sag on heated vertical walls but may require more careful adjustment of peak internal air temperature to obtain full sintering. In a direct comparison with a high-density polyethylene rotational-moulding powder, the lower density and lower crystallinity of this grade reduce flexural modulus and increase elongation at break, which can improve impact-loaded tanks and promote ductile failure modes. Against a butene-based linear low-density polyethylene of similar density, the use of a different short-chain branch length or broader molecular-weight distribution can raise low-temperature impact strength and environmental stress-cracking resistance; however, the specific comonomer identity of this product should be confirmed from the manufacturer’s document because it is not always distinguished in the product coding.
The material also differs from crosslinked polyethylene in that it remains a thermoplastic; no peroxide or silane crosslinking is required. It can therefore be reground and remoulded, but it does not provide the same high-temperature creep resistance as crosslinked rotomoulded parts. Where designers compare this product to ethylene-vinyl acetate or polyolefin plastomers, the distinction is that the modulus remains in the hundreds of megapascals range, so the product is structurally rigid rather than elastomeric. When replacing a low-density polyethylene grade in an existing tool, the processor may need to increase peak internal air temperature by 5–10 °C because linear chains require more thermal energy to reach full sintering. The exact adjustment is tool-specific and should be mapped by running a series of shot trials with internal air temperature logging and wall-thickness measurement.
For potable-water and food-contact tanks, the rotomoulder cannot rely only on raw-powder compliance. The thermal-oxidative conditions during the rotational moulding cycle can modify the inner surface, and the finished article must be assessed under migration test conditions appropriate for the intended contact time and temperature. For European applications, the final plastic article falls under Regulation EU 10/2011, and migration testing is normally carried out on the moulded article, not on the powder alone. For United States submissions, the olefin polymer base may be evaluated under 21 CFR 177.1520, but the conditions of use and any colourant or processing aid must also be considered. Outdoor weathering claims require accelerated ageing data, normally generated by xenon-arc weathering under ISO 4892-2 or ASTM D2565; the BUE 5502 suffix may denote a stabiliser package, but the exact UV and thermal stabilisation should be confirmed on the product data sheet. The following matrix summarises the typical regulatory checks required at the article level.
| Application area | Standard or regulation | Typical end-use verification |
|---|---|---|
| EU plastic food-contact articles | Regulation (EU) 10/2011 | Overall migration and specific migration on finished moulded article |
| US olefin food-contact materials | FDA 21 CFR 177.1520 | Conditions of use, additive compliance, food-type limitations |
| EU hazardous substances restriction | Directive 2011/65/EU as amended | Supplier declaration for RoHS-restricted substances |
| EU chemical regulation | REACH EC 1907/2006 | SVHC content and article safety assessment |
| Accelerated outdoor weathering | ISO 4892-2 or ASTM D2565 | Xenon-arc exposure, colour change, impact retention |
| North American potable-water contact | NSF/ANSI 61 where required | Extraction testing on finished tank or fitting |
The use of regrind, mineral fillers, or colour masterbatch may alter the migration profile and weathering response; therefore, each moulding plant should maintain a change control procedure that records the exact additive lot and regrind fraction used in every production batch. For repeated outdoor exposure, the stabilised package should be evaluated by following the colour and impact retention after the number of xenon-arc exposure hours specified by the end-use standard, not after a single arbitrary exposure time. If the final article is used in contact with fatty foods or aggressive simulants, the migration limit values apply to the finished surface, not to the bulk plaque used in the property table.
Thin-walled tanks for secondary containment and transport of low-hazard liquids are a common application for this grade when the part is rotomoulded in a single-shot steel tool. The powder charge weight is derived from the target wall thickness and the measured bulk density; because bulk density can vary by several percent between production lots, the moulding sheet should be recalculated after each delivery. On a typical two-station shuttle machine, the outer wall thickness is measured by ultrasonic gauge at the tank top, bottom, and sidewall after demoulding to detect thickness asymmetry caused by improper speed ratio or insufficient powder flow. For diesel tanks, the material must pass the end-use impact and environmental stress-cracking resistance tests specified by the tank standard; short-term tensile data alone do not predict long-term crack growth resistance. In contact with concentrated oxidising acids, aromatic solvents, or aggressive surfactants, compatibility testing is required because no unfilled polyolefin is universally resistant to all chemical environments. The final wall-thickness design for buried or externally loaded vessels should use long-term creep modulus and service temperature rather than the room-temperature flexural modulus shown in the property table.