Lyondellbasell Icorene 3545 Bue 5335 Polyethylene Linear Low Density

LyondellBasell Icorene 3545 BUE 5335 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 3545 BUE 5335 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 165142
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene
    Density 0.935 g/cm³
    Melt Index 190 C 2 16 Kg 4.5 g/10 min
    Melting Point 125 °C
    Vicat Softening Temperature 95 °C
    Tensile Strength At Yield 10.0 MPa
    Tensile Strength At Break 12.0 MPa
    Elongation At Break 700%
    Flexural Modulus 300 MPa
    Shore D Hardness 50
    Dart Drop Impact 100 g
    Elmendorf Tear Strength 200 g
    Haze 20%
    Gloss 50%
    Coefficient Of Friction 0.2

    As an accredited LyondellBasell Icorene 3545 BUE 5335 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 3545 BUE 5335 is typically supplied in 25 kg polyethylene-lined bags, palletized and stretch-wrapped for transport.
    Container Loading (20′ FCL) 20′ FCL loaded with palletized 25 kg bags of LyondellBasell Icorene 3545 BUE 5335 LLDPE, stretch-wrapped and secured for transport.
    Shipping LyondellBasell Icorene 3545 BUE 5335 is a non-hazardous linear low density polyethylene resin. It is not regulated for transport by DOT, IMDG, or IATA. Ship in original sealed bags, bulk bags, or bulk containers. Keep dry, avoid heat, sunlight, and contamination. Normal truck, rail, sea, or air freight applies.
    Storage Store polyethylene resin in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep containers tightly closed to prevent moisture and contamination. Avoid dust generation and static discharge; use grounding/bonding during handling. Do not store near food, drink, or incompatible materials. Follow manufacturer/SDS guidance and maintain spill containment.
    Shelf Life Shelf life is two years from production when stored in original unopened packaging, dry, below 50°C, and protected from sunlight.
    Application of LyondellBasell Icorene 3545 BUE 5335 Polyethylene, Linear Low Density

    In rotational molding of closed-top chemical containment units, LyondellBasell Icorene 3545 BUE 5335 is dry-blended as 100 parts by mass of base resin with 1.5–2.5 wt% of a polyethylene-carrier carbon black masterbatch where opacity and exterior UV resistance are specified. For units intended to hold aggressive aqueous chemical solutions, the molding resin is not diluted with filler or impact modifier; the butene linear low-density polyethylene matrix retains slow crack growth resistance under continuous internal pressure. Compliance for the molded shell is verified against AS/NZS 4766:2006 for polyethylene storage tanks for water and chemicals, and where the unit is supplied as an inner receptacle of a composite intermediate bulk container, UN 31A/Y certification under 49 CFR 178.509 and ADR 6.5.2 requires drop, hydraulic pressure, and stacking tests on the assembled pack. Laboratory qualification of each rotomolded lot includes environmental stress crack resistance under ASTM D1693-15e1 Condition B in 10% Igepal; failure before 1,000 h on 6-mm plaques is treated as a batch nonconformance. The production process on a shuttle-type rotational molding machine with arm ratio 4:1 begins with ambient-temperature charging of the powder blend into a fabricated steel or cast aluminium mold. The tool is rotated biaxially through an oven set at 260–295 °C until the internal air temperature reaches 190–205 °C, held at this peak internal air temperature for 2–5 minutes to sinter the powder into a void-free wall, then cooled by forced ambient air to 110 °C followed by water mist to 90 °C. Demolding is conducted at wall temperatures below 65 °C to avoid post-mold shrinkage exceeding 1.5%. Operating excursions above 215 °C peak internal air temperature accelerate oxidative embrittlement of the inner wall surface and are considered a process deviation. Terminal products in this segment include cone-bottom dosing tanks, 1,000-litre composite IBC inner bottles, and double-contained pallet tanks for chemical distribution.

    What Limits Peak Internal Air Temperature in Potable Water Tank Molding?

    Potable-water contact imposes an upper bound on peak internal air temperature that is tighter than in industrial chemical tank production. For LyondellBasell Icorene 3545 BUE 5335, the recommended peak internal air temperature window for 6–8 mm nominal wall sections is 190–198 °C; excursions above 205 °C during oven residence produce organoleptic degradation products that are detectable as off-taste or odour after the tank is filled and conditioned. The formulation for drinking-water service is kept at 100 parts per hundred resin without slip agents, antiblock agents, or secondary lubricants; only a water-contact-approved white or blue masterbatch with polyethylene carrier is used, at 1.0–2.0 wt%, and regrind is restricted to 20 wt% maximum of identical potable-water-approved material with a documented contamination control procedure. Compliance is anchored to NSF/ANSI/CAN 61:2023 for North America, AS/NZS 4020:2018 for Australia and New Zealand, BS 6920-1:2014 where UK water fittings are specified, and EU Regulation (EU) No 10/2011 for plastic materials intended for food or water contact, with migration testing conducted using simulant A for aqueous foods under the time–temperature conditions of the tank’s intended use. The powder is stored below 70% relative humidity; preconditioning is not required unless surface condensation is observed. The process is run on carousel or shuttle rotational molding machines equipped with internal air thermocouples logged at 0.5 Hz; the mold is rotated at 5 rpm on the primary axis and 12 rpm on the secondary axis for a 1,500-litre cylindrical mold. Cooling starts only after the pyrometer confirms complete powder coalescence; forced-air cooling to 115 °C is followed by a fine water mist stage of no more than 5 °C/min to reduce thermal stress. Terminal products include 500–5,000-litre vertical water storage tanks, mobile water bowsers, and rectangular header tanks for drinking-water distribution in remote installations.

    Outdoor playground components rotationally molded from Icorene 3545 BUE 5335 require a different compliance set: EN 1176-1:2017 Clause 4.2.8 governs the absence of toxic substances in accessible surfaces, and ASTM F1487-21 addresses head and neck entrapment, protrusions, and impact attenuation of the assembled structure rather than the polymer alone. The dry powder formulation is based on 100 parts virgin rotational molding powder, 2.0–3.0 wt% high-opacity masterbatch, and a hindered amine light stabilizer top-up only when the molded part will be installed above 1,500 m elevation or in UV index zones above 11; no halogenated flame retardants are added because they introduce opacity instability and surface bloom after outdoor thermal cycling. Processing takes place on independent-arm machines with cast aluminium molds polished to a 4-μm surface finish; oven set points are 250–275 °C, peak internal air temperature is kept at 195–205 °C, and cooling is staged through air and mist to avoid differential shrinkage between thick and thin wall sections. Demolding is delayed until the wall temperature drops below 60 °C in high-gloss tooling to prevent surface deformation at the part extraction point. Terminal products in this sector include rotationally molded slide bodies, tunnel sections, climbing panels, and modular roof elements for play structures.

    When Regrind Loading Exceeds 25 wt% in Agricultural Tank Production

    Agricultural water and liquid fertilizer storage tanks are produced with regrind levels that can reach 20–30 wt% in cost-sensitive markets, but exceeding 25 wt% introduces a measurable conflict between melt flow stability, powder bulk density distribution, and wall thickness uniformity. The base formulation is 100 parts virgin Icorene 3545 BUE 5335 powder plus returned unpainted tank trim regrind; at 20 wt% regrind, the melt flow rate measured under ISO 1133-1:2022 at 190 °C/2.16 kg typically shifts by less than 0.7 g/10 min from the virgin value, while density under ISO 1183-1:2019 shifts by less than 0.002 g/cm³. At 30 wt% regrind, operators on shuttle machines with 3.2 m swing diameter have observed wall thickness coefficient of variation rising from 6–8% to 11–13% when the regrind powder contains fines below 106 μm in excess of 15 wt%. Published data for this exact grade at 30 wt% regrind in thin-wall agricultural tank molds is limited; the shift envelope described above derives from comparative trials on butene LLDPE rotational molding powders and should be confirmed per lot. Therefore, regrind above 25 wt% is air-classified before dry mixing and the final powder blend is screened through a 35-mesh sieve; if fines cannot be controlled, regrind loading is capped at 20 wt%. For agricultural service, chemical compatibility is assessed under AS/NZS 4766:2006 or national equivalent; liquid fertilizer tanks are additionally checked by oxidation induction time at 200 °C under ISO 11357-6:2018 to ensure regrind addition does not lower residual antioxidant protection below 15 minutes. The production process uses a biaxial rotational molder with oven temperature set at 260–280 °C; the molded part is cooled in forced air from 200 °C to 115 °C at 4–6 °C/min and then sprayed with water mist to 85 °C to lock in flat sidewall geometry. Terminal products are 2,000–20,000-litre agricultural water storage tanks, fertigation mixing tanks, and transportable liquid feed tanks for livestock operations.

    Insulated Fish Tub Double-Wall Processing and Hot-Water Cleaning Limits

    Double-wall rotational molding for insulated fish tubs and food-processing bins uses Icorene 3545 BUE 5335 as the outer and inner polyethylene shells, with the cavity between the walls injected later with rigid polyurethane foam to provide 25–40 kg/m³ density insulation. The food-contact side must comply with 21 CFR 177.1520(c) for olefin polymers in contact with food, and the complete tub is verified under EU Regulation (EU) No 10/2011 for migration where export documentation requires European conformity. The formulation for the inner shell is 100 parts natural resin with no pigmentation; the outer shell may contain 1.5–2.0 wt% color masterbatch, but no fillers are used because calcium carbonate at even 5 wt% reduces impact strength under ISO 6603-2 puncture testing at 2 °C. Processing requires a two-shot rotational molding sequence: the outer shell is molded to a wall thickness of 5–7 mm, cooled to 70 °C, then the inner shell is charged and molded inside the outer shell on a multi-axis machine with internal air temperature not exceeding 205 °C. The polyurethane foam is injected through pre-formed fill ports at 20–25 °C and allowed to expand under mold confinement to a core density of 35–45 kg/m³. Repeated hot-water cleaning at 80 °C requires slow-cooled inner walls with minimal molded-in stress; rapid demolding or uneven water-mist cooling can produce craze lines under subsequent alkaline detergent contact. Terminal products include insulated fish boxes, ice storage containers, and dairy processing bin liners where washdown cycles are applied at ambient to 80 °C.

    Free Quote

    Competitive LyondellBasell Icorene 3545 BUE 5335 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 3545 BUE 5335 Polyethylene, Linear Low Density is a rotational moulding grade of ethylene–α-olefin copolymer supplied as a free-flowing black powder. The 3545 designation places the material in the 0.934 g/cm³ density class and the 5.0 g/10 min melt flow index class; the BUE 5335 suffix denotes an integral black ultraviolet-stabilizer package rather than a dry-blended pigment added at the moulding machine. The grade is used for biaxial rotational moulding of hollow articles such as agricultural storage tanks, outdoor seat components, playground panels, marine buoys, and industrial bins. Because the stabilizer and carbon black are compounded into the polymer matrix, the powder avoids the segregation, static-charge separation, and surface-defect risks associated with post-added masterbatch.

    Typical powder-handling values for this product class are a bulk density of 0.36–0.42 g/cm³ and a 500 g dry-flow time of 25–35 s when measured by a funnel method adapted from ASTM D1895-17. Particle-size distribution is controlled to retain the majority of the powder between 150 µm and 500 µm; excessive fines below 106 µm may reduce hopper flow, increase dust generation during grinding, and promote non-uniform wall-thickness distribution in deep-draw tools. Melt flow index is ordinarily determined under ASTM D1238-20 or ISO 1133-1:2022 at 190°C with a 2.16 kg mass. Density is measured by ASTM D1505-18 or ISO 1183-1:2019 on compression-moulded plaques after conditioning at 23°C ± 2°C and 50% ± 5% relative humidity.

    Measured responseReference methodTypical use in grade qualification
    DensityASTM D1505-18 / ISO 1183-1:2019Controls stiffness, warpage, permeation resistance
    Melt flow indexASTM D1238-20 / ISO 1133-1:2022Controls melt deposition, bubble escape, thin-section fill
    Tensile yield strength and elongation at breakASTM D638-22Qualifies load-bearing walls and ductility
    Flexural modulusASTM D790-17Predicts part stiffness and creep resistance
    Notched Izod impactASTM D256-23Assesses crack propagation resistance in moulded walls
    Environmental stress cracking resistanceASTM D1693-21Evaluates resistance to detergent and chemical stress cracking
    Accelerated weatheringISO 4892-2:2013 / ASTM D2565-21Verifies retention of the UV-stabilizer package

    What limits the processing window in a 0.934 g/cm³ LLDPE rotational moulding powder?

    In carousel, shuttle, and open-flame rock-and-roll machines, the dominant process variable is internal air temperature, not oven set point. For a linear low-density polyethylene powder of this density and melt-flow class, the peak internal air temperature is commonly controlled between 190°C and 220°C. The lower bound is set by sintering completion: insufficient peak internal air temperature leaves partially fused powder particles, pinholes, and poor bubble elimination at the inner surface. The upper bound is set by thermo-oxidative degradation: excursions above approximately 230°C accelerate chain scission, reduce notched Izod impact, and increase inner-surface discoloration, particularly in the presence of residual oxygen in the mould cavity. Oven set points from 280°C to 320°C are generally required to achieve the target internal air temperature, depending on part mass, mould thickness, and machine type.

    On production-scale carousel machines, internal air temperature ramp rates of 8–12°C/min are common when the mould enters the oven at ambient temperature. The rotation speed ratio is typically maintained between 3:1 and 5:1, with primary-arm speeds of 6–10 min⁻¹ and secondary-arm speeds of 1.5–2.0 min⁻¹. A 4:1 ratio is often applied for moulds with deep draw or offset cavities because it improves powder flow into the lower extremities and reduces bridging at narrow radii. The cooling sequence is equally critical: forced-air cooling to approximately 120°C followed by natural cooling reduces warpage, while abrupt water-mist cooling below 95°C can increase residual stress in thick walls and may promote dimensional instability after demoulding. Demoulding temperatures between 80°C and 100°C are commonly used to balance cycle time against creep distortion.

    Published grade-specific process data should be obtained from the current LyondellBasell technical datasheet because the values stated here represent the broader LLDPE rotomoulding envelope, not a lot-specific process guarantee. Peak internal air temperature must be verified with an air-probe thermocouple inserted through the mould vent; surface temperature measured by infrared pyrometer is a supplementary control, not a substitute for internal air temperature. Batch-to-batch variation in melt flow index of up to 0.5 g/10 min may shift the required peak internal air temperature by several degrees, and a change in particle-size distribution below 150 µm can alter the heating rate in thin-wall sections.

    In outdoor service, the BUE 5335 designator is associated with an integrated black stabilizer system. Carbon black acts as a light screen and free-radical scavenger, while hindered amine light stabilizers and phenolic antioxidants are typically present to control photo-oxidative chain scission. The carbon black particle size and dispersion are controlled because undispersed agglomerates act as crack-initiation sites under impact loading. For black polyethylene formulations, accelerated weathering qualification is usually conducted under ISO 4892-2:2013 Method A at a black-panel temperature of 65°C ± 3°C and an irradiance of 60 W/m² in the 300–400 nm band. Retention of tensile elongation and notched impact after exposure is monitored; a common acceptance criterion for black LLDPE outdoor grades is retention of at least 75% of initial elongation at break after 2000 h of xenon-arc exposure, although the exact criterion for this grade must be confirmed against the manufacturer’s control specification.

    Mechanical performance and environmental stress cracking resistance in moulded walls

    Published qualification data for this class are generated on compression-moulded plaques because the rotomoulding process itself introduces internal voids, fusion lines, and variable wall thickness that can affect apparent mechanical response. For a 0.934 g/cm³ LLDPE rotomoulding grade with a 5.0 g/10 min melt flow index, flexural modulus is typically in the 450–700 MPa range, tensile yield strength is commonly 15–18 MPa, and elongation at break generally exceeds 700%. Notched Izod impact at 23°C is usually above 500 J/m, and low-temperature impact at -40°C is substantially higher than that of a comparable HDPE rotomoulding grade because the lower density and linear architecture increase tie-molecule concentration. Environmental stress cracking resistance measured by ASTM D1693-21 under 10% Igepal CO-630 at 50°C is often reported in the hundreds of hours for similar LLDPE grades; the exact value for Icorene 3545 BUE 5335 must be taken from the current product datasheet rather than extrapolated from generic LLDPE data.

    The notched Izod test is not always representative of rotomoulded parts because the inner surface is rough and the outer surface is in contact with the mould; drop-weight impact testing on moulded panels under ASTM D5276-19 is therefore used to evaluate actual part toughness. On a 3 mm moulded wall, a typical LLDPE rotomoulding formulation may exhibit ductile puncture with extensive plastic deformation rather than brittle fracture at 23°C. At -20°C, the same material may show a transition to more localized cracking, but retained impact energy remains higher than for a 0.945 g/cm³ HDPE rotomoulding powder of similar wall thickness. This behavior is relevant for agricultural tanks and marine buoys that experience impact during installation and service in cold environments.

    The material is not a high-temperature engineering resin. Continuous load-bearing service above 60–70°C should be avoided because creep and loss of dimensional stability become significant. For applications requiring continuous exposure to hot chemicals or steam, a high-density rotomoulding grade or a crosslinked polyethylene grade should be evaluated instead. Chemical exposure should be reviewed against ASTM D543-21 or ISO 175:2010 practice, particularly for storage of surfactants, agricultural adjuvants, or aliphatic hydrocarbons, because environmental stress cracking response is formulation-specific.

    When a 5.0 g/10 min melt index grade displaces a 1.9 g/10 min HDPE rotomoulding formulation

    A 0.934 g/cm³ LLDPE powder with a 5.0 g/10 min melt index occupies a middle position between low-density polyethylene and high-density polyethylene rotomoulding grades. Compared with an LDPE rotomoulding powder of similar melt index, the linear low-density material offers higher flexural stiffness, higher tensile yield strength, and significantly better environmental stress cracking resistance because the short-chain branching distribution produces a greater number of load-bearing tie molecules. Compared with an HDPE rotomoulding powder of 0.945 g/cm³ density and 1.9 g/10 min melt index, the Icorene 3545 class provides lower flexural modulus, lower heat-deflection temperature, and less creep resistance, but it cycles faster and retains better low-temperature impact. The higher melt index also improves melt deposition and bubble elimination in medium-thickness walls, reducing the formation of internal voids at sharp corners and around metal inserts.

    Material classDensity range (g/cm³)Melt flow index range (g/10 min)Flexural modulus range (MPa)Typical rotomoulding limitation
    LDPE rotomoulding0.915–0.9253.0–10150–300Lower stiffness, lower ESCR, higher permeation
    LLDPE rotomoulding, this class0.930–0.9404.0–6.0450–700Greater warpage than HDPE, lower continuous-use temperature
    HDPE rotomoulding0.940–0.9551.0–4.0700–1200Longer cycles, lower low-temperature impact

    Within the Icorene portfolio, the BUE 5335 suffix distinguishes the black UV-stabilized variant from natural, non-stabilized, or differently stabilized versions of the same base polymer. This distinction is operationally significant because natural grades may require separate letdown of UV masterbatch, which can be difficult to disperse uniformly in low-shear rotomoulding equipment. The integrated package reduces batching error and gives more reproducible weathering performance. However, the carbon black loading also reduces the available peak internal air temperature window because black surfaces absorb infrared radiation more rapidly than natural powders; processors may need to lower oven set points by 10–20°C relative to natural grades to avoid overshoot above 220°C.

    On multiple-cavity moulds with deep draw, internal wall-thickness variation below ±10% is generally achievable with this powder class when particle-size distribution is stable and rotation ratio is optimized. Areas around kiss-off ribs and metal inserts are critical because powder bridging and stagnant regions can produce thin spots that fail under environmental stress cracking before the surrounding wall. Production-scale experience indicates that venting must be sufficient to prevent backpressure from degrading the antioxidant package; a vent diameter of 10–15 mm per 0.25 m³ of mould volume is commonly used for LLDPE rotomoulding powders, but tool-specific venting must be validated by measuring internal air pressure during the heating cycle. Regulatory compliance for the grade should be confirmed against the current manufacturer’s declaration for FDA 21 CFR 177.1520, REACH Regulation (EC) No 1907/2006, and RoHS Directive 2011/65/EU; specific compliance of the BUE 5335 stabilizer package must be verified for food-contact and potable-water applications.

    Top