| HS Code | 222470 |
| Productname | LyondellBasell Icorene 3545 BUE 5332 Polyethylene, Linear Low Density |
| Materialtype | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Density | 0.935 g/cm³ |
| Meltindex | 3.5 g/10 min at 190°C/2.16 kg |
| Tensilestrengthatyield | 10.3 MPa |
| Tensilestrengthatbreak | 20.7 MPa |
| Elongationatbreak | 800% |
| Flexuralmodulus | 310 MPa |
| Dartdropimpact | 120 g |
| Elmendorftearstrength | 200 g |
| Vicatsofteningpoint | 98 °C |
| Meltingpoint | 124 °C |
| Haze | 10% |
| Gloss | 80% |
| Coefficientoffriction | 0.15 |
| Processingmethod | Blown Film |
| Additives | Slip, Antiblock |
As an accredited LyondellBasell Icorene 3545 BUE 5332 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 3545 BUE 5332 Linear Low Density Polyethylene comes in 25 kg moisture-resistant bags, palletized for industrial handling. |
| Container Loading (20′ FCL) | 20′ FCL loaded with palletized, shrink-wrapped 25 kg bags of LyondellBasell Icorene 3545 BUE 5332 LLDPE, secured for transport. |
| Shipping | Shipping description: LyondellBasell Icorene 3545 BUE 5332 Polyethylene, Linear Low Density, solid, non-hazardous, not regulated for transport. Typically shipped in 25 kg polyethylene bags or bulk boxes on pallets. Store in a cool, dry, ventilated area away from ignition sources and direct sunlight. Handle with care to prevent package damage. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed and labeled. Avoid contact with strong oxidizers. Minimize dust generation and accumulation; use grounding/bonding if handling generates static. Maintain good housekeeping, protect from moisture and contamination, and follow local regulations and SDS guidance. |
| Shelf Life | Typically 24 months from production when stored in original unopened packaging, dry, below 40°C, protected from direct sunlight. |
Blown stretch-film extrusion with LyondellBasell Icorene 3545 BUE 5332 linear low-density polyethylene is concentrated on air-cooled monolayer and three-layer lines producing pre-stretch pallet film, hand stretch film and silage wrap in thickness bands from 12 µm to 35 µm. The butene comonomer architecture narrows the stable bubble window relative to hexene or octene LLDPE; gauge banding and edge instability are typically controlled by maintaining blow-up ratios between 2.2:1 and 3.0:1, with frost line height held at 4 to 8 die diameters. Formulation ratios used in industrial practice include 0.5–2.5 wt% polyisobutylene tackifier, 1,000–5,000 ppm silica-based antiblock and 200–1,000 ppm erucamide slip. Processing equipment for such film generally consists of a single-screw extruder with L/D 24:1–30:1, die gap 1.5–2.5 mm, melt temperature 190–230 °C, and high-speed centre winders fitted with pre-stretch capability of 100–300%. Compliance for food-contact packaging is assessed under FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011; mechanical conformance is tested under ASTM D882-18, ASTM D1922-15(2020), ASTM D5748-19 and ISO 527-3:2018. Terminal product forms include pallet wrap, agricultural silage film, stretch hood and collation bundling film. Downgauging below 10 µm requires verification of dart impact under ASTM D1709-16a because lower melt strength in butene LLDPE can produce film with lower puncture tolerance than octene LLDPE at equal thickness.
| Test | Standard / Designation | Specimen Condition | Parameter under Verification |
|---|---|---|---|
| Tensile properties | ASTM D882-18 | Crosshead speed 500 mm/min | MD/TD tensile strength, elongation at break |
| Elmendorf tear | ASTM D1922-15(2020) | 25 µm film, 400 g pendulum | MD/TD tear resistance |
| Dart impact | ASTM D1709-16a | Method B | Puncture failure at 12–35 µm |
| Stretch film puncture | ASTM D5748-19 | Probe speed 250 mm/min | Protrusion puncture resistance |
| Kinetic coefficient of friction | ASTM D1894-14 | 23 °C, 50% RH | Slip-additive response |
In extrusion coating of liquid packaging board, adhesion of Icorene 3545 BUE 5332 below 20 g/m² is governed less by resin viscosity alone than by substrate moisture content, board surface energy, melt temperature uniformity and chill roll temperature control. The resin is commonly let down at 20–40 wt% into LDPE to reduce neck-in and edge weave on high-speed coating lines running 80–400 m/min. A typical laminate structure places a tie layer of maleic anhydride grafted polyethylene at 2–5 g/m² between the board and the LLDPE-based layer, with the LLDPE coating weight set at 12–25 g/m². Extruder configuration for such lines usually includes a barrier screw with L/D 26:1–32:1, die gap 0.5–0.8 mm, melt temperature 285–320 °C, air gap 150–250 mm and chill roll temperature 10–20 °C. Corona treatment to 38–42 dyn/cm is applied before subsequent laminating or printing. Compliance for paperboard food packaging is evaluated under FDA 21 CFR 176.170(c), Regulation (EU) No 10/2011, and melt mass-flow rate is verified by ISO 1133-1:2022. Barrier performance is measured by ASTM F1249-20 for water vapour transmission and TAPPI T 540 for bond strength. Terminal products include aseptic carton liners, paper cups, frozen food board, single-serve sachets and medical packaging lidding. Oxidation off-taste risk increases when melt temperature exceeds 320 °C for residence times beyond 20 min; the published data for this specific grade in neat high-speed extrusion coating is limited and should be confirmed on the target line before commercial qualification.
Vertical chemical storage tank production by rotational moulding with Icorene 3545 BUE 5332 requires the resin to be pulverized to a particle size distribution with 95% below 500 µm and dried at 70–80 °C for 2–4 h when ambient relative humidity exceeds 60%. The moulding cycle uses an oven temperature of 280–320 °C and a mould surface temperature of 190–220 °C; heating time for a 6 mm wall section is ordinarily 12–20 min, followed by forced-air cooling of 15–30 min. Rotation ratios of 4:1 are set on biaxial moulding machines to reduce wall thinning at the tank shoulder and along vertical ribs. The standard formulation is 96.5–97.5 wt% LLDPE powder, 2–3 wt% carbon black masterbatch for ultraviolet stabilization, 0.15–0.40 wt% hindered phenolic antioxidant and 0.10–0.30 wt% HALS. Compliance for chemical storage tanks is tested under ASTM D1998-21 for polyethylene upright storage tanks, FDA 21 CFR 177.1520 for food and water contact grades, NSF/ANSI/CAN 61 for potable water components and Regulation (EU) No 10/2011. Terminal product types include vertical chemical storage tanks, agricultural spray tanks, water storage tanks, insulated coolers and kayak hulls. The butene structure produces lower environmental stress-crack resistance than octene LLDPE; tanks intended for aggressive oxidizing agents or long-term stress require testing under ASTM D1693-15 and ASTM D5397-19 before specifying wall thickness.
Twin-screw compounding of Icorene 3545 BUE 5332 as a carrier resin for pigment and additive masterbatch is limited to formulations requiring lower processing temperatures and moderate melt strength. Co-rotating twin-screw extruders with L/D 40:1–52:1, screw speeds 300–800 rpm and specific energy input 0.18–0.24 kWh/kg are used, with melt temperature held at 180–230 °C to avoid gel formation in the die plate. Carrier loading is prescribed at 25–60 wt%, pigment or filler at 40–60 wt%, wax dispersant at 4–8 wt% and processing aid at 0.5–1.5 wt%. Strand pelletizing is preferred for highly filled grades; underwater pelletizing is used only when the melt viscosity and die-face temperature permit clean pellet separation. Compliance is governed by REACH (EC) No 1907/2006, RoHS Directive 2011/65/EU and, when the masterbatch contacts food, FDA 21 CFR 177.1520. Terminal product types are white masterbatch, carbon black masterbatch, antioxidant masterbatch and custom colour concentrates for downstream extrusion.
Replacing 1.5 mm HDPE with 2.0 mm Icorene 3545 BUE 5332 LLDPE in secondary containment alters tensile strain capacity, environmental stress-crack resistance margin and seaming temperature. Flat-die sheet extrusion and calendering are run with melt temperature 200–240 °C, die gap 2.5–3.5 mm, roll stack temperature 40–90 °C and line speed set to maintain thickness tolerance of ±5%. The compounding formula is 96.5–98.5 wt% LLDPE, 2.0–3.0 wt% carbon black, 0.3–0.7 wt% hindered phenolic antioxidant and 0.1–0.3 wt% HALS. Hot-wedge welding is performed at 350–400 °C and 1.0–2.0 m/min; extrusion fillet welding requires preheat at 60–80 °C for butene LLDPE to reduce stress concentration at the weld root. Compliance is verified by ASTM D5199-12 for nominal thickness, ASTM D638-14 for tensile properties at break, ASTM D4833-07(2020) for puncture resistance, ASTM D5397-19 for notch constant tensile load, ASTM D1693-15 for environmental stress-crack resistance and GRI-GM13 for geomembrane specification. Terminal products include landfill caps, pond liners, secondary containment basins, canal liners and mining heap leach pads. The lower ESCR of butene LLDPE relative to octene LLDPE requires either a thicker cross-section or reduced differential settlement when exposed to stress-cracking agents such as surfactants and hydrocarbon seepage.
| Test | Standard / Designation | Specimen or Condition | Parameter under Verification |
|---|---|---|---|
| Thickness | ASTM D5199-12 | Ten specimens per sheet | Average and minimum thickness |
| Tensile at break | ASTM D638-14 | Type IV dumbbell, 50 mm/min | Yield and break strength / elongation |
| Puncture resistance | ASTM D4833-07(2020) | 8 mm probe | Puncture resistance at failure |
| NCTL | ASTM D5397-19 | Notch at 30% yield stress | Stress-crack resistance |
| ESCR | ASTM D1693-15 | Surfactant environment | Failure time under bending stress |
| Carbon black content | ASTM D1603-20 | Combustion analysis | 2.0–3.0 wt% carbon black |
In thin-wall injection moulding of lids and containers, Icorene 3545 BUE 5332 is processed at melt temperatures 190–240 °C, mould temperatures 10–40 °C, injection velocities 80–150 mm/s and holding pressures 400–800 bar; clamp force for multi-cavity tools is usually 1,000–2,500 kN. The cooling time for a wall thickness of 0.8–1.8 mm is 5–15 s. Formulation is 90–100 wt% LLDPE, with 0–10 wt% LDPE as a flow modifier, 0.05–0.15 wt% nucleating agent and 1–3 wt% colour masterbatch. Shrinkage measured after 24 h at 23 °C under ASTM D955-08(2023) is dependent on flow direction, gate size and mould temperature; published data for this specific formulation configuration is limited and should be generated for each tool geometry. Compliance covers FDA 21 CFR 177.1520(c) for food contact, Regulation (EU) No 10/2011, EN 71-3:2019 + A1:2021 for migration from toy components and RoHS Directive 2011/65/EU. Terminal products include thin-wall storage containers, over-caps, lids, toy components and non-structural packaging inserts.
Competitive LyondellBasell Icorene 3545 BUE 5332 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
The material designated LyondellBasell Icorene 3545 BUE 5332 is a blue-pigmented, linear low-density polyethylene (LLDPE) in the supplier’s Icorene ethylene polymer series. The alphanumeric suffix is a commercial colour and stabilizer identifier rather than a comonomer descriptor; the extension 5332 denotes the registered shade. Specification control is obtained from the certificate of analysis and current technical data sheet issued for the purchased lot, not from the trade designation alone. In materials databases, representative values for this grade are commonly listed as a density of 0.938 g/cm³ and a melt mass-flow rate of 5.0 g/10 min at 190°C/2.16 kg. A tensile yield strength of approximately 17 MPa and flexural modulus near 550 MPa are frequently cited as single-point characterisation values under ASTM D638 and ASTM D790; these figures are not specification limits and must be re-verified for the incoming batch.
The grade is positioned for monolayer rotational-moulded parts where moderate stiffness, low-temperature ductility, and outdoor stabilisation are required. Potential applications include agricultural tanks, industrial containers, fluid reservoirs, and outdoor enclosures. The presence of a coloured stabiliser package means weathering behaviour is a function of pigment concentration and processing history, not solely the base polyethylene. Before production release, converters should confirm that the exact shade and ultraviolet package satisfy the exposure class of the finished article.
Linear low-density polyethylene derives its mechanical profile from a polyethylene backbone carrying short-chain branches introduced by the comonomer. The branch length and distribution reduce crystallite thickness, lower spherulitic order, and increase the concentration of tie molecules between lamellae. These tie chains transmit stress across crystalline domains and suppress craze propagation under impact or slow crack growth. Consequently, LLDPE grades in the density interval 0.918–0.940 g/cm³ generally exhibit greater low-temperature penetration resistance than long-chain branched low-density polyethylene at equivalent melt flow.
For characterisation, tensile yield and elongation at break are measured under ISO 527-2 or ASTM D638-14; flexural modulus under ISO 178 or ASTM D790-17; and impact resistance under ISO 180, ISO 179-1, or ASTM D256. Environmental stress-crack resistance is typically assessed by ASTM D1693 in a surfactant such as Igepal CO-630, though rotational-moulded parts may also be evaluated by the longer-duration ASTM F1473 notched creep test. Low-temperature impact resistance is commonly screened by the ASTM D746 brittleness temperature or by instrumented impact tests on full-scale parts.
The density of 0.938 g/cm³ cited for Icorene 3545 BUE 5332 places the material in the higher-crystallinity portion of the LLDPE class. The two-phase density model using a crystalline-phase density of 1.000 g/cm³ and an amorphous-phase density of 0.855 g/cm³ gives a mass crystallinity of approximately 61%. This level of crystallinity supports moderate stiffness while retaining enough amorphous tie-chain population for ductility. Differential scanning calorimetry under ISO 11357-3 typically records a melting peak in the 120–135°C interval for such LLDPE materials; the exact peak shape and enthalpy depend on comonomer type, comonomer distribution, and thermal history.
In rotational moulding, melt quality is developed by heating the mould surface and monitoring the peak internal air temperature rather than by a barrel set point. The powder or micropellet charge densifies through tackifying, sintering, and bubble-dissolution stages. For LLDPE formulations with a melt mass-flow rate near 5.0 g/10 min, typical oven set points fall between 260°C and 300°C, while the peak internal air temperature required for bubble removal commonly ranges from 190°C to 220°C. These values are equipment-dependent; cast steel tools, aluminium moulds, and fabricated sheet-metal moulds differ in heat transfer, and the optimum cycle must be established on the production machine.
On a single-arm biaxial machine with a steel mould, cycle-time adjustments of 2–4 min can shift the inner-surface bubble count and the residual pigment dispersion. Clam-shell ovens with high-velocity air recirculation produce faster heat transfer than static ovens and can reduce the processing window for dark blue grades. Because pigmented Icorene 3545 BUE 5332 absorbs infrared more efficiently than natural resin, excessive oven temperature or prolonged heating may consume the hindered phenolic antioxidant package and generate surface oxidation before full densification is achieved. Processors often reduce oven temperature by 10–20°C relative to natural LLDPE when running saturated colours and compensate with a modest extension of rotational time. Batch-to-batch variation in pigment dispersion can shift the bubble-dissolution window by 5–10°C; this is a production-scale variable that cannot be fully corrected by trading specifications alone.
Cooling rate controls shrinkage, warpage, and impact strength. Slow air cooling in the mould improves impact resistance but increases cycle time and can raise total mould shrinkage. Water-mist cooling accelerates production and improves dimensional reproducibility but may quench the outer surface and introduce residual stresses. Sudden water quench while the part is above 70°C can cause warpage in large panels. No pre-drying is normally required for fresh bags; storage in high-humidity conditions above 90% relative humidity may introduce surface moisture that should be removed by warming the resin to 60°C for 4 h before charging.
Selection against LDPE is usually governed by low-temperature impact, environmental stress-crack resistance, and stiffness. LDPE carries long-chain branching; LLDPE carries short-chain branching. The higher linearity of LLDPE gives higher tensile and flexural modulus at equal density, while its spherulitic structure is less brittle than HDPE in many impact and slow crack growth conditions. HDPE selected at 0.941–0.970 g/cm³ provides higher compressive and flexural stiffness but generally lower environmental stress-crack resistance and reduced low-temperature ductility compared with LLDPE rotational-moulding grades. The following class-level comparison illustrates the design envelope; values are generic for polyethylene classes and not Icorene lot specifications.
| Property / test basis | LDPE | LLDPE class | HDPE |
|---|---|---|---|
| Density under ASTM D1505 | 0.912–0.928 g/cm³ | 0.918–0.940 g/cm³ | 0.941–0.970 g/cm³ |
| Flexural modulus ISO 178 | 200–400 MPa | 250–700 MPa | 700–1500 MPa |
| Tensile yield ASTM D638-14 | 7–12 MPa | 10–20 MPa | 18–28 MPa |
| ESCR ASTM D1693 response | low to moderate | moderate to high | moderate to high, density-dependent |
| Low-temperature impact | moderate | high | moderate to low |
Because Icorene 3545 BUE 5332 is coloured, its stiffness and impact values may shift relative to the natural base resin. Pigment concentrates act as rigid fillers at low loading but can nucleate or disrupt crystallisation depending on particle size and dispersion. The processor should therefore compare compound properties rather than neat resin data when substituting away from a coloured LDPE or HDPE grade.
Because the material is sold as a pigmented compound, regulatory compliance for food-contact and outdoor use is not automatically identical to that of natural polyethylene. In the United States, the base olefin polymer is generally covered by 21 CFR 177.1520(c), but the final coloured article may require separate assessment of the pigment under 21 CFR 178.3297 or a food-contact notification. In the European Union, plastic food-contact materials fall under Regulation (EU) No 10/2011; the overall migration limit of 10 mg/dm² applies for general food-contact plastics, but specific migration limits for the pigment and light stabiliser must be obtained from the supplier’s declaration of compliance.
For heavy-metal restrictions, RoHS 2011/65/EU and packaging Directive 94/62/EC set concentration limits for lead, cadmium, mercury, and hexavalent chromium. A blue shade is not free of regulatory risk simply because it is non-black; the converter must request full heavy-metal data for the exact 5332 colour. REACH registration duties are supplier-side; downstream users should confirm that the grade and its stabiliser package are registered for the intended application.
Outdoor weathering is assessed by accelerated methods such as ASTM G154, ASTM D2565, or ISO 4892-2. Coloured LLDPE can exhibit surface chalking, colour fade, and loss of impact after extended ultraviolet exposure; performance is strongly influenced by part thickness, geographic location, and surface orientation. The stabiliser package in Icorene 3545 BUE 5332 should be regarded as process and service protection, not as an unlimited ultraviolet barrier. Published data for this specific configuration is limited under long-term coastal or desert exposure, so outdoor validation is recommended when the part is load-bearing or contains potable water.
The table below lists the principal standardised methods applicable to incoming inspection and process validation. These methods do not by themselves define a specification; the purchaser should establish upper or lower control limits from the Icorene 3545 BUE 5332 certificate of analysis and process-capability studies.
| Standard / method | Measured parameter | Use in specification or process audit |
|---|---|---|
| ISO 1133-1:2022 / ASTM D1238 | melt mass-flow rate at 190°C/2.16 kg | incoming lot control; rotational moulding processability |
| ISO 1183-1 / ASTM D1505 | density of solid polyethylene | stiffness and crystallinity proxy |
| ISO 527-2 / ASTM D638-14 | tensile yield strength and elongation | mechanical acceptance |
| ISO 178 / ASTM D790-17 | flexural modulus | part deflection analysis |
| ISO 179-1 / ASTM D256 | impact resistance | low-temperature ductility acceptance |
| ASTM D1693 / ASTM F1473 | environmental stress-crack resistance | chemical-contact part validation |
| ISO 4892-2 / ASTM G154 | accelerated weathering | outdoor colour and impact retention |
At the converting line, the material should be purged with a transition resin when changing from an engineering polymer or from a highly filled compound. Accumulated degraded polyethylene can form gels and specks in rotational-moulded surfaces. The use of reground pigmented parts is common but should be controlled by melt-flow shift, not by input weight alone. If the melt mass-flow rate of the finished compound shifts by more than 1.0 g/10 min or if the low-temperature impact falls below the application limit, the regrind fraction should be reduced. Contact with strong oxidising acids, aromatic hydrocarbons, and chlorinated solvents at elevated temperature should be avoided because these agents accelerate oxidative degradation and environmental stress-cracking of linear low-density polyethylene.