Lyondellbasell Icorene 3545 Bue 5325 Polyethylene Linear Low Density

LyondellBasell Icorene 3545 BUE 5325 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 3545 BUE 5325 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 165686
    Product Name LyondellBasell Icorene 3545 BUE 5325 Polyethylene, Linear Low Density
    Manufacturer LyondellBasell
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene
    Density 0.935 g/cm³
    Melt Index 3.5 g/10 min (190°C/2.16 kg)
    Melting Point 124 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield 11 MPa
    Tensile Strength At Break 25 MPa
    Elongation At Break 700%
    Flexural Modulus 400 MPa
    Dart Drop Impact 120 g
    Haze 10%
    Gloss 70%
    Coefficient Of Friction 0.20
    Additives Slip and antiblock
    Form Pellets

    As an accredited LyondellBasell Icorene 3545 BUE 5325 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 3545 BUE 5325 LLDPE is supplied in 25 kg bags, typically palletized and shrink-wrapped for bulk shipment.
    Container Loading (20′ FCL) 20′ FCL loaded with LyondellBasell Icorene 3545 BUE 5325 Linear Low Density Polyethylene, securely stowed and lashed for ocean shipment.
    Shipping LyondellBasell Icorene 3545 BUE 5325 Polyethylene, Linear Low Density, is a non-hazardous, non-regulated solid resin supplied as pellets. Ship in original sealed bags, octabins, or bulk containers. Protect from moisture, contamination, direct sunlight, and excessive heat. No UN number, hazard class, or special transport labeling required.
    Storage Store LyondellBasell Icorene 3545 BUE 5325 Polyethylene, Linear Low Density in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original bags or containers closed to prevent moisture, dust, and contamination. Use grounding to control static. Avoid prolonged UV exposure and excessive stacking. Follow local regulations and SDS guidance.
    Shelf Life Typically 24 months from manufacture when stored unopened in a cool, dry, well-ventilated area, away from direct sunlight and heat.
    Application of LyondellBasell Icorene 3545 BUE 5325 Polyethylene, Linear Low Density

    Rotational moulding of vertical polyethylene tanks for potable water and mild chemical storage uses Icorene 3545 BUE 5325 as the primary virgin powder in a 100% base-resin formulation, with 0.10–0.25 wt% hindered phenolic antioxidant masterbatch and 2.0–4.0 wt% pigment masterbatch introduced by high-speed dry blending at 1,400–2,200 rpm for 5–8 min. The powder is charged into a carbon steel or cast aluminium mould, rotated biaxially at a 4:1 ratio, and heated in a forced-air oven at a set temperature of 260–300 °C until the internal air temperature reaches 180–200 °C; demoulding is delayed until the mould surface temperature falls below 70 °C to prevent warpage and impact-strength loss. Potable water contact compliance follows FDA 21 CFR 177.1520(c) for olefin polymers and NSF/ANSI 61 for drinking water system components; EU 10/2011 requires overall migration below 10 mg/dm². Terminal parts include conical-bottom dosing tanks, cylindrical open-top storage vessels, and horizontal transport tanks in capacities from 50 L to 30,000 L.

    Compliance checklist for rotationally moulded potable water storage vessels using Icorene 3545 BUE 5325
    StandardScopeRelevant requirementTest condition
    FDA 21 CFR 177.1520(c)Olefin polymers in food-contact articlesFinished article migration testing with food simulants21 CFR extraction protocols for aqueous, acidic, and fatty simulants
    NSF/ANSI 61Drinking water system componentsNormalised contaminant concentration limitspH 5 and pH 10 extraction waters
    EU 10/2011Plastic materials and articles intended to contact foodOverall migration ≤ 10 mg/dm²10 days at 40 °C
    ASTM D1998-21Polyethylene upright storage tanksHydrostatic pressure test and drop impact38 °C water fill, full-volume hydrostatic

    Published production-scale observations show that improper peak internal air temperature control is the dominant cause of non-fused inner-surface porosity in tank walls thicker than 8 mm. A temperature overshoot above 220 °C accelerates oxidative degradation of the UV package, while an undershoot below 170 °C produces pinholing along weld lines. Field measurements on shuttle-type rotational moulding machines indicate that wall-thickness variation in 5,000 L tanks can reach ±12% when the mould is not indexed through two rotational axes at constant ratio; this variation directly reduces ASTM D1998-21 hydrostatic test margin. The use of this grade in chemical storage requires compatibility testing with the specific service fluid because ketone- or chlorinated-solvent exposure can reduce environmental stress-crack resistance despite the high molecular weight.

    Why Does Oven Residence Time Control Impact Strength in Large-Diameter Agricultural Silos?

    Agricultural feed silos and liquid supplement tanks made from Icorene 3545 BUE 5325 are processed as a 100% virgin powder or with 0.5–1.5 wt% colour concentrate; black formulations intended for outdoor UV resistance use 2.0–3.0 wt% carbon black masterbatch. Compliance for dry animal feed contact is based on EU Regulation 1935/2004 and Commission Regulation 2023/2006 GMP; for silage leachate and liquid molasses, service-specific migration testing under EU 10/2011 is required. The downstream process is rotational moulding in multi-arm independent-arm machines with oven setpoints of 270–300 °C; peak internal air temperature is held at 190–210 °C for 8–15 min depending on wall thickness, because LLDPE crystallises rapidly and residence time below the plateau does not fully coalesce powder particles. Terminal products include feed hoppers, molasses lick tubs, calf hutches, and silo cones.

    On production-scale four-station carousel moulding lines, agricultural silo bodies above 10,000 L exhibit a documented process sensitivity: oven residence time increments of 60 s at 290 °C can shift the outside-to-inside temperature gradient from 25 °C to 45 °C, causing the inner wall to remain below fusion temperature while the outer wall begins to degrade. The resulting parts show reduced Izod impact strength under ISO 180/A and lower drop impact failure height during field-handling tests. Process engineers typically set a minimum mould internal air temperature of 180 °C and a maximum of 205 °C; demoulding below 70 °C prevents thermal shrinkage. Published data for this specific large-diameter silo configuration is limited; verified field failures more commonly track to venting deficiencies that cause pressure-driven pinholes than to base resin failure.

    When Marine Buoyage Demands a UV-Stabilised LLDPE Powder with High Environmental Stress-Crack Resistance

    For marine navigation buoys, mooring buoys, and aquaculture collars, Icorene 3545 BUE 5325 is processed as a 100% base resin with 3–5 wt% UV-stabilised pigment masterbatch only when colour is not included in the pre-compounded BUE 5325 package; many converters rely on the as-supplied stabiliser package and add 0–2 wt% processing aid to reduce pinhole formation. Compliance for marine service is not covered by a single resin standard; raw-material quality is controlled through ISO 1133-1:2022 melt index and ISO 1183-1:2019 density measurements, while finished float shells are inspected under ISO 11673 or client-specific drop and weld-integrity standards. Rotational moulding of double-wall buoy hulls uses forced-air oven setpoints of 265–290 °C; the powder must maintain a particle-size distribution of 80–35 mesh with no more than 5 wt% below 100 mesh to prevent bridging in feed tubes. Terminal products include navigation buoys, mooring buoys, fish farm floats, and floating fenders.

    The operational boundary is seawater fatigue loading combined with ultraviolet exposure at latitudes above 40°. A stabiliser package designed for general outdoor exposure does not automatically protect against chlorinated-pool water or constant immersion in diesel-contaminated harbour water. Swelling from absorbed hydrocarbons can reduce the effective modulus and create stress concentrations at moulded-in tie-rod bosses. Fabricators testing cold-weather impact resistance should condition specimens at −20 °C for 24 h before ISO 179-1/1eA Charpy testing because LLDPE ductile-to-brittle behaviour is strongly cooling-rate dependent.

    High-density polyethylene food-processing tubs and transport lugs are rotationally moulded using 70–80 wt% Icorene 3545 BUE 5325 and 20–30 wt% clean in-house regrind from the same grade, a ratio that preserves food-contact suitability only if the regrind is used under the same food-contact conditions. The dry blend is prepared in a low-shear ribbon blender at 80–120 rpm for 10–15 min to avoid fines generation; the addition of regrind above 30 wt% raises melt viscosity and can shift peak internal air temperature requirements upward by 5–10 °C. Contact compliance is established under FDA 21 CFR 177.1520(c) and EU 10/2011; migration testing of the finished article is required for fatty, acidic, or alcoholic food types because LLDPE is not a universal barrier. Terminal products include 50–1,000 L fish tubs, meat lug containers, cheese vats, and insulated bulk food carriers.

    On production lines with single-shot charging, regrind above 30 wt% increases the incidence of bubble entrapment at mould parting lines because the lower bulk density of regrind flakes delays heat transfer to the polymer mass. Some processors compensate by increasing the mould internal air temperature from 190–195 °C to 200–210 °C, but this narrows the oxidative degradation margin of the UV package. ASTM D1998-21 hydrostatic and drop tests are not required for food tubs; however, many converters apply internal standards derived from ASTM D638-14 tensile specimen production and ASTM D256-10 Izod conditioning to reject parts with visible weld-line porosity.

    Underground Septic Tank and Utility Vault ESCR Thresholds

    Icorene 3545 BUE 5325 is used in rotational moulding of underground septic tanks, cisterns, and utility vaults where soil loading and aggressive leachate expose moulded walls to continuous stress. The formulation is typically 100% virgin powder or 90–95 wt% virgin with 5–10 wt% regrind; addition above 10 wt% regrind is limited because field inspections show faster loss in environmental stress-crack resistance under wetting-agent exposure. Structural compliance follows EN 12566-1 for small wastewater treatment systems, while environmental stress-crack resistance is characterised by ASTM D1693-15 under wetting-agent immersion. The downstream process is rotational moulding of ribbed single-wall or double-wall tanks; oven setpoints range from 280–310 °C, peak internal air temperature is held at 195–215 °C, and cooling proceeds by water mist followed by forced air until demould surface temperature falls below 65 °C. Terminal products include septic tanks, pump chambers, utility vaults, and stormwater retention chambers.

    Representative rotational moulding process envelope for Icorene 3545 BUE 5325
    Parameter6 mm wall thickness12 mm wall thickness
    Oven setpoint270–290 °C280–305 °C
    Peak internal air temperature180–195 °C190–205 °C
    Post-fusion hold at peak internal air temperature4–7 min8–15 min
    Demould surface temperature≤ 70 °C≤ 65 °C

    The process conflict is that the same high molecular weight that raises ESCR also lowers powder flowability in large moulds with deep ribs. Converters using 100% virgin Icorene 3545 BUE 5325 report that rib filling at the bottom of a 1,500 mm deep vault requires a peak internal air temperature of at least 200 °C; below this, incompletely fused powder leaves surface porosity that reduces wall stiffness under accelerated soil-load deflection tests referenced in EN 12566-1 Annex C. Published data for this specific configuration is limited; however, the operational boundary is clear: regrind content above 10 wt% should be qualified by lot-specific ASTM D1693-15 testing because recycled powder particle geometry changes the heat-up rate and increases the probability of radial cold spots.

    Outdoor Urban Furniture Extends Service Life Only When Cooling Rates Are Controlled

    Rotational moulding of urban litter bins, seating shells, bollards, and playground climbing panels uses Icorene 3545 BUE 5325 at 100% virgin powder with 3–5 wt% colour masterbatch; light colours are pre-dried at 60–70 °C for 2–4 h when relative humidity exceeds 60% because surface moisture increases pinholing. Outdoor weathering compliance is evaluated through ISO 4892-2:2013 method A accelerated xenon-arc exposure; visual colour change is specified as ΔE ≤ 3 after 3,000 h, and impact retention is checked by ISO 6603-2 instrumented puncture tests on 6 mm plaques. The production process uses rock-and-roll or shuttle rotational moulding machines with oven setpoints of 250–290 °C; moulded parts are cooled in forced air to 60 °C before ejection to avoid post-mould distortion. Terminal products include park benches, bollard shells, waste receptacles, and playground tunnel sections.

    The main inline failure mode in urban furniture is not UV embrittlement but cold-temperature impact fracture caused by improper cooling rate. When parts are cooled too quickly from 200 °C to ambient with high-velocity water mist, shrinkage stresses remain frozen at inner bosses and insert bosses; these stress concentrations can reduce instrumented puncture peak force, but published data for this specific configuration is limited. Moulding trials show that a 3–4 °C/min cooling rate between 120 °C and 70 °C reduces warpage in flat seating slats without lowering crystallinity below the level needed for stiffness. The BUE 5325 stabiliser package must not be combined with metallic stearate levels above 0.1 wt% because excessive acid scavenger can deactivate the hindered amine light stabilizer in long-term UV service.

    Free Quote

    Competitive LyondellBasell Icorene 3545 BUE 5325 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 3545 BUE 5325 is supplied as a linear low density polyethylene powder intended for closed-mould rotational moulding of hollow parts. The grade identifier separates the base ethylene-alpha-olefin copolymer, 3545, from the BUE 5325 formulation suffix, which denotes a specific light-stabilized and pigmented package for exterior service. The base resin belongs to the LLDPE class whose density generally falls between 0.930 g/cm³ and 0.940 g/cm³ at 23 °C when tested according to ISO 1183-1:2019. Melt flow rate is reported at 190 °C under 2.16 kg load using ISO 1133-1:2022; commercial rotational moulding powders in this mid-flow band are often supplied between 3.0 g/10 min and 7.0 g/10 min. The exact release range for this grade must be confirmed against the certificate of analysis because the 5325 formulation package can influence final melt viscosity and weathering reserve.

    How Does the BUE 5325 Stabilizer Package Extend Outdoor Service Life?

    The BUE 5325 suffix designates a compounded additive system rather than a separate masterbatch. In rotational moulding, a pre-stabilized powder reduces the need to dry blend a separate UV masterbatch, which can segregate during powder handling and create uneven surface concentrations of stabilizer. Weathering resistance is assessed by accelerated laboratory exposure under ISO 4892-2:2013 or ISO 4892-3:2016 methods; the primary acceptance criterion is usually retention of elongation at break after UV exposure. For LLDPE tanks exposed to sunlight, stabilizer performance is commonly reported as the UV exposure time required to reduce elongation to 50% of the unexposed value. The additive system typically includes a hindered amine light stabilizer and a UV absorber, although the exact ratio is proprietary. Published product-specific weathering data for this configuration is limited; outdoor service life must be validated on the finished part at the intended wall thickness, colour, and exposure orientation.

    In closed-mould rotational moulding, the powder is charged into a metal cavity, biaxially rotated, and heated by forced-air convection. The process is governed by peak internal air temperature rather than oven set point alone. For mid-flow LLDPE powders of this density class, process programmes commonly target a peak internal air temperature between 185 °C and 205 °C. Oven set points between 260 °C and 300 °C are typical on production shuttle machines, but oven temperature is insufficient evidence of cure because mould gauge, wall thickness, and powder particle size alter heat transfer. Undercure appears as pinholes at mould corners or a granular internal surface when the inner wall remains below the crystalline melting region for insufficient time. Overcure caused by operation above the acceptable peak internal air temperature for more than 10–15 min can raise crystallinity during cooling and increase flexural modulus while reducing low-temperature impact. The processing window is therefore narrow: peak internal air temperature should be held within ±5 °C of the grade-specific target to limit bubble defects and property drift. Portable data loggers mounted through the mould vent are used to record internal air temperature continuously on shuttle and rock-and-roll machines.

    Sintering, Bubble Collapse, and Peak Internal Air Temperature Control

    During oven residence, the powder undergoes densification by sintering, followed by bubble dissolution in the melt. LLDPE powders with a density near 0.936 g/cm³ require higher internal air temperatures and longer cure than LDPE powders at the same oven set point. Differential scanning calorimetry conducted under ISO 11357-3:2018 shows peak melting for this material class between 120 °C and 130 °C, with crystallinity typically between 35% and 50%. The zero-shear viscosity of the molten LLDPE controls bubble removal; at 190 °C, mid-flow rotational moulding grades commonly display complex viscosity in the range of 1,000 Pa·s to 5,000 Pa·s at low frequency. If peak internal air temperature is reached too quickly without sufficient hold time, residual air bubbles are frozen into the wall as pinholes. Slow cooling between 5 °C/min and 10 °C/min is used to control shrinkage and warpage; forced-air or water-mist cooling may be applied after the mould surface temperature approaches 90 °C. Abrupt cooling of thick sections can introduce differential crystallinity gradients that increase warpage at the parting line. Oxidative induction time determined according to ISO 11357-6:2018 is a useful stabilizer dispersion check on rotomoulded panels.

    When liquid containment is designed from LLDPE, short-term tensile values should not be used as long-term design allowables without creep derating. Tensile yield for rotational moulding LLDPE in this density class is typically between 14 MPa and 20 MPa when tested to ASTM D638-14 at 50 mm/min. Flexural modulus falls generally between 600 MPa and 900 MPa under ASTM D790-17 Procedure A. Environmental stress crack resistance is measured under ASTM D1693, condition A or B, in 100% Igepal CO-630; LLDPE rotational moulding grades normally exceed 500 h without failure, which is higher than many high-pressure LDPE rotomoulding powders. Low-temperature impact is assessed by ISO 6603-2:2023 or ASTM D3763; the linear backbone and short-chain branching provide higher puncture resistance than conventional LDPE. Mould shrinkage after demoulding measured by ASTM D955-21 is commonly between 1.5% and 2.5% for LLDPE rotomoulding powders; warpage increases when the cooling rate differential across the section exceeds 10 °C/min. Design calculations for storage tanks should use the hydrostatic creep rupture envelope and apply a minimum service factor of 1.5 on hoop stress when chemical attack is absent.

    What Separates a Linear Low Density Rotomoulding Powder from LDPE and HDPE?

    Compared with high-pressure LDPE, the linear copolymer contains short-chain branches from butene, hexene, or octene. The resulting molecular architecture raises tensile strength, puncture resistance, and stress crack resistance while maintaining processability in low-shear rotational moulding. Compared with HDPE, the lower crystallinity of LLDPE reduces flexural modulus and high-temperature stiffness but improves environmental stress crack resistance and low-temperature impact. Icorene 3545 BUE 5325 is therefore positioned for parts requiring a combination of low-temperature toughness and weathering resistance rather than maximum rigidity. In injection moulding, LLDPE would typically be selected for high-speed filling at lower melt temperatures; in rotational moulding, the same resin must be reduced to a controlled powder sieve profile to ensure uniform wall thickness.

    Property/Test MethodLLDPE Rotomoulding PowderLDPE Rotomoulding PowderHDPE Rotomoulding Powder
    Density (ISO 1183-1:2019)0.930–0.940 g/cm³0.918–0.925 g/cm³0.945–0.960 g/cm³
    Melt flow rate (ISO 1133-1:2022, 190 °C/2.16 kg)3.0–7.0 g/10 min3.0–8.0 g/10 min2.0–6.0 g/10 min
    Flexural modulus (ASTM D790-17)600–900 MPa200–400 MPa900–1,300 MPa
    ESCR (ASTM D1693, 100% Igepal CO-630)>500 h>100 hGrade-dependent; unmodified grades often lower than LLDPE
    Low-temperature impact (ISO 6603-2)High puncture resistance at -20 °CModerateLower than LLDPE unless impact-modified

    Batch-to-batch variance in powder pourability and sieve profile can alter mould-filling behaviour on automatic shuttle lines. For LLDPE powders, a typical sieve specification retains less than 1% on 500 µm and passes less than 10% through 150 µm, but this is grade-specific. Powder pourability determined according to ISO 6186:2023 is generally acceptable for automated hopper systems at values below 35 s/100 g; higher values may require hopper vibration or feed screws. The powder should not be dried at temperatures above 60 °C because thermal agglomeration can fuse fine particles. Storage above 40 °C or under direct ultraviolet exposure can reduce the stabilizer reserve, and moisture condensation at relative humidity above 60% should be prevented because surface water can create steam-induced porosity.

    ParameterMeasurement method / equipmentControl band / critical limit
    Oven set pointForced-air shuttle or rock-and-roll oven260–300 °C
    Peak internal air temperatureThermocouple / Rotolog data logger185–205 °C, hold within ±5 °C
    Cooling rate after demouldingTemperature logging in mould5–10 °C/min
    Powder pourabilityISO 6186:2023Usually below 35 s/100 g
    Storage relative humidityWarehouse hygrometerBelow 60%

    When a Compliance Decision Depends on Migration Limits

    For food-contact articles, the grade must comply with FDA 21 CFR 177.1520 for olefin polymers and, where applicable, Regulation (EU) No 10/2011. The overall migration limit under EU No 10/2011 is 10 mg/dm² of surface area for plastic food-contact materials. Specific migration of additives used in the BUE 5325 package must be assessed against EU No 10/2011 Annex II if the part is sold in the European Union. For potable water contact in North America, the finished tank must be evaluated to NSF/ANSI 61; resin compliance does not automatically certify a rotomoulded article. Documentation for restriction of hazardous substances can be requested from the supplier where the part enters electrical or industrial equipment supply chains under RoHS 2011/65/EU.

    The material should be processed in accordance with the manufacturer’s processing guide, but published data for this specific configuration is limited for aggressive chemical exposure cases. The polymer is not a universal corrosion barrier; oxidising acids, aromatic hydrocarbons, and halogens can attack the matrix and reduce long-term strength. Compatibility testing under ASTM D543-20 should be performed when the contained fluid is not water or a simple aqueous solution. Prolonged contact with hydrocarbon solvents above 60 °C should be avoided because environmental stress cracking can initiate in localised stressed zones. No later performance claim should be based solely on resin brand; wall thickness, moulded-in stress, cooling rate, and stabilizer consumption all govern the part’s service life.