Lyondellbasell Icorene 3545 Bue 5304 Polyethylene Linear Low Density

LyondellBasell Icorene 3545 BUE 5304 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 3545 BUE 5304 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 338320
    Density 0.935 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 3.5 g/10 min
    Tensile Strength At Yield 12 MPa
    Tensile Strength At Break 25 MPa
    Elongation At Break 600%
    Flexural Modulus 350 MPa
    Shore D Hardness 55
    Vicat Softening Temperature 105 °C
    Melting Temperature 125 °C
    Thermal Conductivity 0.33 W/m·K
    Specific Heat Capacity 1.90 J/g·°C
    Water Absorption <0.01%

    As an accredited LyondellBasell Icorene 3545 BUE 5304 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 3545 BUE 5304 LLDPE is packaged in 25 kg moisture-resistant polyethylene bags, palletized and shrink-wrapped for industrial delivery.
    Container Loading (20′ FCL) 20′ FCL loaded with LyondellBasell Icorene 3545 BUE 5304 LLDPE in 25 kg bags, palletized or floor-loaded, stowed for export.
    Shipping LyondellBasell Icorene 3545 BUE 5304 Linear Low Density Polyethylene is non-hazardous and not classified as dangerous goods for transport. It ships as solid pellets in 25 kg bags, palletized and stretch-wrapped, or in bulk containers. Keep dry, avoid excessive heat, and follow applicable transport regulations.
    Storage Store LyondellBasell Icorene 3545 BUE 5304 LLDPE in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and ignition sources. Keep bags or containers sealed, off the floor, and protect from moisture, dust, and UV exposure. Avoid excessive stacking and use first-in, first-out rotation. Keep separate from strong oxidizing agents and follow local regulations.
    Shelf Life Shelf life: 24 months from production when stored dry, in original packaging, at temperatures below 50°C, away from direct sunlight.
    Application of LyondellBasell Icorene 3545 BUE 5304 Polyethylene, Linear Low Density

    In blown-film conversion of butene-modified linear low density polyethylene, the processing window is set less by extruder back-pressure than by bubble sidewall stress distribution above the frost line. On a 75 mm grooved-feed extruder with a 30:1 L/D ratio and a 350 mm low-pressure spiral die, the melt stream is typically brought to 195–215 °C at the die lip, with a die gap of 1.8–2.4 mm and a blow-up ratio of 2.2:1–3.0:1 to balance machine-direction and transverse-direction tear propagation. Formulation addition ratio for machine stretch film is commonly 90–100 wt% Icorene 3545 BUE 5304, with 0–10 wt% autoclave LDPE added when bubble instability appears above 280 kg/h, and 1–3 wt% polyisobutylene cling masterbatch incorporated when the finished film must retain pallet-surface adhesion without migratory transfer to packaged goods. Compliance for food-contact structures requires the finished film to meet 21 CFR 177.1520(c) 3.2a and Commission Regulation (EU) No 10/2011 as amended, with verification by overall migration testing under the intended contact simulant; the converter must avoid amine-based antistatic additives in food-contact film unless the additive is explicitly listed in the relevant positive list, because amine migration can exceed the Union list limits. Downstream production uses single-layer or coextruded blown film lines with internal bubble cooling and automatic width control, running at a frost line height equivalent to 5–8 die diameters and a die-to-nip collapse distance calibrated to avoid blocked-film defects at thickness below 15 µm. The terminal product range covers 10–25 µm machine stretch film for prestretch ratios of 150–300 %, 15–23 µm hand stretch film, 25 µm agricultural silage wrap, and overwrap for secondary beverage packaging where tear toughness under ASTM D1922 and puncture resistance under ASTM D5748 are the decisive release criteria.

    What Limits Oven Residence Time in Rotational Molding of This Butene LLDPE Grade?

    When the same resin is dry-pulverized to a 35-mesh cut with an average particle size below 500 µm and a bulk density of 0.43–0.49 g/cm³, the controlling variable shifts from melt flow to oxidative induction time at the mold inner surface. Formulation addition ratio for closed-head agricultural tanks is 95–100 wt% Icorene 3545 BUE 5304, 0.5–2.0 wt% hindered amine light stabilizer masterbatch, 0.2–1.0 wt% pigment masterbatch, and 0.1–0.3 wt% antioxidant masterbatch when the part is exposed to sunlight for more than 1000 hours per year; published data for this specific configuration is limited, and the converter should verify the stabilizer masterbatch carrier resin compatibility before dry blending. Industry compliance standards include 21 CFR 177.1520(c) 3.2b for food-contact surfaces, EU No 10/2011 for overall migration, and NSF/ANSI/CAN 61 where the finished vessel is intended for storage of potable water or drinking-water treatment chemicals. Downstream production is conducted on a biaxial carousel or shuttle rotational molding machine with an oven setpoint of 285–315 °C, a peak internal air temperature of 185–200 °C, and a biaxial rotation ratio of 4:1; demolding occurs only after the mold surface cools to 75–85 °C, otherwise warpage in the rim flange exceeds tolerance. Continuous exposure to strong oxidizing acids at elevated temperature is outside the operational boundary for untreated LLDPE rotomolded components. Terminal product types include 100–10,000 L agricultural spray tanks, intermediate bulk container liners, secondary containment pallets, and outdoor play components where low-temperature impact below −20 °C is specified according to ISO 179-1.

    Extrusion coating onto aluminium foil and paperboard subjects the LLDPE web to a 150–250 mm air gap before the pressure nip, and the decisive grade attribute is the neck-in ratio at the die edge, not melt strength alone. Formulation addition ratio in seal-layer coating is 100 wt% Icorene 3545 BUE 5304 or 10–30 wt% blended into autoclave LDPE to raise seal-initiation temperature tolerance on high-speed sachet lines; for low-slip surfaces, 0.05–0.2 wt% erucamide masterbatch is added, but this slip package must be omitted if the laminate is destined for subsequent metallization because surface energy loss above 2 dyn/cm hinders metal adhesion. Compliance obligations derive from 21 CFR 177.1520(c) 3.2a for direct food contact under low-moisture and aqueous-acidic conditions, and Commission Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² for the finished multi-material laminate. Downstream processing uses a single-screw extruder with a 30:1 L/D ratio, barrel profile rising to 300–325 °C at the T-slot die, a die-to-nip air gap of 150–250 mm, and a chill roll temperature of 10–20 °C to quench the melt before delamination can occur at the coating-substrate interface. Terminal product categories include liquid carton board for juice and dairy, paper-based laminate for dry food sachets, aluminium foil lamination for pharmaceutical strip packs, and release-liner outer layers where hot-tack strength is tested according to ASTM F1921.

    Cast Film Quenching Parameters and Film Flatness Control

    On polished chill rolls held at 12–25 °C, slot-die cast film production with this butene LLDPE grade operates with a die-to-chill roll gap of 25–50 mm and a vacuum box or air knife positioned to eliminate air entrapment at line speeds between 250 m/min and 500 m/min. Formulation addition ratio is 70–90 wt% Icorene 3545 BUE 5304 and 10–30 wt% LDPE, with 0.05–0.2 wt% erucamide slip masterbatch and 0.05–0.15 wt% synthetic silica antiblock masterbatch added when downstream unwinding requires coefficient of friction below 0.25 under ASTM D1894. The relevant compliance framework for packaging films includes 21 CFR 177.1520(c) 3.2a and EU No 10/2011, with specific migration testing for the chosen slip additive under the worst-case fatty simulant only where the film directly contacts free fat; overcooling below 10 °C is avoided because condensation at the roll surface causes melt puddling and increases gauge variation. Downstream production relies on a 90 mm extruder with barrier screw and piggyback screen changer, melt filtration at 80–120 µm, and a flexible-lip coathanger die with automatic gauge control; the corona treater set to 38–42 dyn/cm in-line ensures print and adhesive wetting without causing roll blocking. Terminal products include 15–50 µm cast stretch film for hood packaging, hygiene film backsheet lamination, tape winding film, and pre-stretched wrapping film where tensile elongation at break under ISO 527-3 exceeds 400 %.

    When Geomembrane Seam Strength Dictates the Welding Window

    Beneath a flex-lip sheet die operating at 210–240 °C, flat-die geomembrane extrusion runs at a lower specific energy input than blown film, typically 0.18–0.24 kWh/kg, because the melt exits through a 2000–3000 mm die onto a three-roll polishing stack held at 60–90 °C. Formulation addition ratio is 95–100 wt% Icorene 3545 BUE 5304, 2–3 wt% carbon black masterbatch to achieve 2.0–3.0 % carbon black content, and 0.1–0.3 wt% blended antioxidant masterbatch for oxidative resistance during high-temperature wedge welding; published data for this specific configuration is limited, so the processor must verify carbon black dispersion through ASTM D5596 before committing to a production lot. Industry compliance standards include GRI-GM17 for LLDPE geomembrane test properties, ASTM D6693 for tensile stress and strain after immersion, and ASTM D4833 for puncture resistance under static load. Downstream production uses a counter-rotating twin-screw extruder or a single-screw extruder with a gear pump, melt temperature at the die lip of 210–240 °C, line speed of 2–8 m/min, and a peel-trim winding station that limits gauge variation to ±5 % across the web width; field seaming above 450 °C at the wedge tip accelerates oxidative chain scission at the seam edge. Terminal product categories are 0.5–2.0 mm single-ply pond and canal liners, landfill leak-detection buffer layers, mining heap leach pad liners, and temporary containment sheets where field seams are welded at 300–450 °C and tested to ASTM D6392 under both peel and shear modes.

    Thin-wall closure molding sets a first-stage injection speed boundary at high LLDPE content

    At melt temperatures above 215 °C, thin-wall closure molding with LLDPE-rich compounds derives its process limit from shear heating generated during first-stage injection through 0.5–1.0 mm gate lands, where excessive velocity creates gate blush and weakens the hinge fold under repeated cyclic loading. Formulation addition ratio for snap-fit closures is 60–80 wt% Icorene 3545 BUE 5304 and 20–40 wt% injection-grade HDPE or LDPE, while for tamper-evident overcaps the LLDPE fraction may drop to 20–40 wt% as a toughening modifier to raise environmental stress crack resistance under ASTM D1693. Compliance for pharmaceutical and cosmetic closures requires 21 CFR 177.1520(c) 3.2a plus USP 661.1 plastic packaging extractables standards where the closure is specified for oral solid dosage packaging. Downstream processing is performed on a high-speed injection molding machine with a clamping force of 150–350 tonnes for 8–16 drop cavities, a mold temperature of 10–30 °C, first-stage injection velocity of 60–150 mm/s, and hold pressure limited to 40–70 % of peak injection pressure to avoid overfilling the gate and freezing excessive orientation into the hinge region. Terminal products include 22–38 mm snap-on lids for personal care jars, 28 mm tamper-evident beverage overcaps, 20 mm flip-top dispensing closures, and laboratory specimen container lids where dimensional stability is verified under ISO 1133-1:2022 melt-flow-rate lot release and ASTM D638-14 tensile yield tests.

    Free Quote

    Competitive LyondellBasell Icorene 3545 BUE 5304 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 3545 BUE 5304 is a pelletised polyethylene resin described in producer literature as a linear low-density grade, with a molecular architecture based on linear chains and short-chain branching rather than the long-chain branching typical of high-pressure tubular or autoclave low-density products. The grade designation can be separated into a melt-flow identifier and a suffix that denotes the comonomer/additive configuration; however, the producer’s lot-specific certificate of analysis remains the controlling reference for composition, melt flow rate, density, and additive levels. In the classification framework of ISO 17855-1:2014, the product is placed below the 0.930 g/cm³ density threshold, distinguishing it from medium-density and high-density resins while aligning it with the low-density polyethylene grouping used for injection moulding and masterbatch carrier applications. The short-chain branching topology obtained from alpha-olefin comonomer incorporation reduces crystallinity compared with HDPE and changes the elastic response during melt extension. These structural characteristics directly influence processing pressure, shrinkage, and solid-state toughness.

    What Melt Rheology and Density Values Define the Processing Window?

    The primary rheological specification is the melt flow rate of 45 g/10 min at 190 °C under a 2.16 kg load, determined in accordance with ISO 1133-1:2022. This value is high for a low-density resin and places the grade in a viscosity band suitable for thin-wall filling, masterbatch let-down, and injection moulding of closures with long flow paths relative to wall thickness. The nominal density of 0.923 g/cm³, measured under ISO 1183-1:2019, is moderate within the low-density spectrum and reflects a crystallinity level below that of unimodal HDPE. These two values define the processing window: at melt temperatures of 200 °C to 240 °C, the resin behaves as a low-viscosity melt under shear, but the linear short-chain branching may reduce melt strength in operations requiring bubble stability or parison uniformity. The shear viscosity at 100 s⁻¹ and 220 °C is not disclosed for this specific grade; published data for this specific configuration is limited, and the moulder must rely on nozzle pressure measurements and short-shot studies rather than generic viscosity curves.

    Rheological data beyond the MFR value is not provided in the public summary. Capillary rheometry under ISO 11443:2021 is recommended for determining apparent viscosity at the shear rates observed in the target process. For thin-wall injection moulding, apparent shear rates at the gate can exceed 10⁴ s⁻¹; at these rates, wall slip and melt compressibility effects become measurable. A single MFR point at 2.16 kg is insufficient to predict pressure drop through hot-runner tips, but the high MFR is generally accompanied by reduced cavity pressure loss. Hot-runner manifold sizes should not be reduced without performing pressure-drop simulations, because shear heating in a restricted manifold can raise the local melt temperature above 250 °C despite a nominal barrel setpoint of 220 °C.

    PropertyTypical valueTest method
    Melt flow rate45 g/10 minISO 1133-1:2022
    Density0.923 g/cm³ISO 1183-1:2019
    Tensile stress at yield11 MPaISO 527-2:2012
    Tensile strain at break500 %ISO 527-2:2012
    Flexural modulus200 MPaISO 178:2019
    Vicat softening temperature90 °CISO 306:2022

    The values in the table are representative producer-published data; batch-to-batch variation in additive levels and comonomer distribution can shift tensile elongation and Vicat softening by a few percentage points. Such variation is not a specification failure unless the producer’s certificate of analysis establishes a narrower release range. For precision components, shrinkage measurements should be conducted under ISO 294-4:2018 after a minimum stabilisation period of 24 h at 23 °C and 50 % relative humidity.

    Typical conversion routes for this melt-flow band are injection moulding of thin-wall housewares, high-flow masterbatch carrier resin, compounded concentrates, and closures where long-flow characteristics are required. The grade is not typically used for blown film because high MFR and low melt strength complicate bubble stability, unless blended with a film-grade LDPE or LLDPE. Blown-film operators who attempt to run this grade at neat concentrations commonly observe bubble instability because the high melt flow rate and linear architecture lower melt strength. A film-grade LDPE with a melt flow rate below 2 g/10 min is frequently added at 10 % to 20 % to restore bubble stability, though the exact addition level depends on die diameter and frost-line height.

    Thermal and mechanical characterisation under ISO 527 and ISO 306 methods.

    Tensile stress at yield is reported at 11 MPa following ISO 527-2:2012, with tensile strain at break of 500 % and flexural modulus of 200 MPa under ISO 178:2019. The Vicat softening temperature of 90 °C under ISO 306:2022 method A50 indicates that the material should not be used as a rigidity-critical or high-temperature load-bearing resin. These values place the grade in the flexible polyethylene range, suitable for snap-fit closures, squeezable containers, and masterbatch carriers where stiffness is secondary to melt flow and low-temperature flexibility. The elongation-at-break value is direction-dependent in injection moulded plaques due to flow-induced orientation; transverse-direction values are typically lower than longitudinal values, and published data for this specific grade is limited.

    Because tensile elongation values measured on standard ISO multi-purpose test specimens may not translate directly to thin-wall parts, weld-line efficiency should be assessed on the production tool. Flow fronts that converge around core pins in closures and spouts reduce tensile elongation, with the reduction being a function of melt temperature, mould temperature, and holding pressure. Weld-line efficiency can be measured under ISO 527-2:2012 using double-gated specimens; published values for this grade are limited. Environmental stress crack resistance is not specified in the public data sheet, but it is inversely related to melt flow rate because lower molecular weight reduces tie-chain density. When the moulded part is exposed to surfactants, detergents, or fatty hydrocarbons, the resistance of the compound should be verified under ASTM D1693 condition B or equivalent test conditions. The resin is not a solvent-resistant barrier polymer; permeation properties must be tested according to ASTM D3985 or ISO 15105-2 when oxygen or water-vapour transmission is a design requirement.

    Production-scale conversion of high-flow low-density polyethylenes with this melt-flow band is documented on injection moulding machines with general-purpose screws of 20:1 to 25:1 L/D and compression ratios between 2.0:1 and 2.5:1. Barrel temperature profiles are typically set from 180 °C in the feed zone to 220 °C or 240 °C at the nozzle, while mould temperatures are maintained between 20 °C and 50 °C. Back pressure on the plastication stroke is held in the region of 0.5 MPa to 1.0 MPa to avoid excessive shear heating while maintaining melt homogeneity. The high melt flow rate reduces injection-pressure demand, but the low viscosity also increases the tendency to flash if clamp force is inadequate for the projected area. In thin-wall packaging with wall sections below 1.0 mm, gate freeze-off time becomes the primary cycle-limiting factor rather than cavity filling; because the high flow rate prolongs the filling window, nozzle drool can occur if decompression is not correctly set. No pre-drying is required at relative humidity below 60 %. If surface condensation is visible, drying at 60 °C to 70 °C for 2 h in a desiccant or hot-air hopper is sufficient.

    Thermal residence is the limiting processing variable. Extended exposure at melt temperatures above 250 °C consumes the antioxidant package and can release aldehyde and acid species that alter organoleptic properties. Melt temperatures above 280 °C should be avoided, and recycle content above 30 % should be qualified if the final part is subject to food-contact or high-clarity specifications. In cold-runner injection tools, the screw retraction and decompression distance should be set to prevent melt starvation at the nozzle tip, which is a documented source of flow lines in high-flow polyethylene grades.

    When This Grade Is Benchmarked Against High-Pressure LDPE and C6/C8 LLDPE

    The most significant structural distinction is the absence of long-chain branching. High-pressure LDPE grades rely on long-chain branches for melt strength, which stabilises blown-film bubbles and extrusion coating curtains. The linear short-chain branched architecture of Icorene 3545 BUE 5304 provides less shear thinning under typical extrusion conditions and lower extensional viscosity at the die exit. Consequently, a converter moving from an equivalent-density LDPE may observe a difference in melt curtain stability and may need to reduce the die gap or adjust the air ring. In injection moulding, the opposite effect is beneficial: the high melt flow rate improves cavity filling at lower pressure than a melt-flow-equivalent LDPE with long-chain branching.

    Against a C6/C8 hexene- or octene-based LLDPE, a butene-based grade of similar density and melt flow typically exhibits lower dart impact and lower Elmendorf tear resistance. Those differences are measured under ASTM D1709 and ASTM D1922 respectively. Compared with HDPE with density above 0.940 g/cm³, the grade has lower flexural modulus, lower Vicat softening, and lower density; however, it may offer improved low-temperature flexibility and easier filling of long-flow thin-wall geometry. This trade-off should not be interpreted as a universal replacement rule. The specific additive package and comonomer sequence distribution must be confirmed from the producer’s analytical certificate before substituting the resin into a stabilised film or injection moulding formulation.

    Substitution into an existing tool designed for 20 g/10 min LDPE may cause flashing at the parting line unless the clamp force is increased or the injection velocity profile is modified. Conversely, using this grade in a tool designed for 10 g/10 min HDPE can reduce fill pressure but also reduce stiffness and heat deflection of the part; such substitution requires verification of end-use mechanical loads under ISO 527-2:2012 or ASTM D638.

    Regulatory Compliance and Food-Contact Verification Matrix

    Compliance claims for plastics are end-use dependent. This product is typically evaluated under EU Regulation (EU) No 10/2011 for plastic materials intended to come into contact with food, and under FDA 21 CFR 177.1520(c) for olefin polymers, subject to the conditions of use assigned by the producer. European REACH compliance should be verified through the safety data sheet under EC No 1907/2006; substances of very high concern are not expected above the 0.1 % w/w reporting threshold. The RoHS-limited substances are below the maximum concentration values of EU Directive 2011/65/EU in typical formulations. The following matrix summarises the instruments used in commercial documentation.

    Regulatory instrumentTypical requirement or statusVerification basis
    EU Regulation (EU) No 10/2011Overall migration ≤ 10 mg/dm²Producer food-contact statement
    FDA 21 CFR 177.1520(c)Olefin polymer clause; conditions of use A–HProducer certification
    REACH (EC) No 1907/2006SVHC content < 0.1 % w/wSafety data sheet
    EU Directive 2011/65/EURoHS-limited substances below MCVSupplier declaration

    The 5304 suffix identifies a stabilisation and processing-aid system, not a food-contact or medical approval. For medical, potable-water, or pharmaceutical applications, the specific migration limits and biocompatibility requirements are outside the published data for this grade. Users should request a product compliance declaration from the producer and should not rely on generic summaries when national food-contact legislation imposes additional restrictions on specific monomers or additives.

    The overall migration limit under EU Regulation (EU) No 10/2011 is 10 mg/dm² for plastics intended for general food contact; however, this is a finished-article test and not a resin property. If the converted article is subjected to hot fill or pasteurisation, the food-contact compliance of the finished part must be tested under the intended temperature and duration conditions. High-density closures made from this resin may be used in contact with aqueous foods at ambient temperatures, but fatty food simulants may extract low-molecular-weight fractions. Migration testing under EN 1186-1:2002 or equivalent should be performed on the final part.

    Ambient storage is recommended at temperatures below 40 °C and away from ultraviolet light, ozone, and open flame. High-flow polyethylene is not hygroscopic in the manner of engineering resins, but surface moisture can generate splay in injection moulded parts if the pellets are stored under condensing conditions. Regrind can be incorporated in low proportions, but the particle-size distribution should be controlled to avoid bridge formation in the hopper. A regrind fraction above 30 % may widen residence-time distribution and alter melt-temperature uniformity on single-screw plasticating units. Peroxide-based purging or scavenging masterbatches should be evaluated for interaction with the stabiliser package before trial use on production tooling.

    Top