| HS Code | 237327 |
| Density | 0.935 g/cm³ |
| Melt Mass Flow Rate Mfr | 4.5 g/10 min (190°C/2.16 kg) |
| Tensile Strength At Yield | 12 MPa |
| Tensile Strength At Break | 25 MPa |
| Elongation At Break | 800% |
| Flexural Modulus | 300 MPa |
| Vicat Softening Point | 100°C |
| Melting Point | 125°C |
| Haze | 10% |
| Gloss | 80% |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength | 200 g |
As an accredited LyondellBasell Icorene 3545 BUE 5116 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 3545 BUE 5116 Polyethylene, Linear Low Density is packaged in 25 kg polyethylene-lined bags, palletized for shipment. |
| Container Loading (20′ FCL) | Loading of 20-foot FCL container with LyondellBasell Icorene 3545 BUE 5116 Linear Low Density Polyethylene in 25 kg bags. |
| Shipping | LyondellBasell Icorene 3545 BUE 5116 Polyethylene, Linear Low Density is typically shipped as non-hazardous polymer pellets in 25 kg bags, octabins, or bulk trucks/railcars. It is not UN-regulated for DOT, IMDG, or IATA transport. Store dry, away from ignition sources and excessive heat; avoid dust generation and environmental release. |
| Storage | Store this LLDPE resin in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed, protecting contents from moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Maintain ambient temperatures, use good housekeeping, and keep away from incompatible materials. Ensure adequate ventilation to control dust. Use appropriate PPE during handling. |
| Shelf Life | Shelf life is typically 24 months from manufacture when stored unopened in original packaging, cool, dry, away from direct sunlight. |
In carousel-type rotational moulding cells producing agricultural fertigation tanks, Icorene 3545 BUE 5116 is dry-blended with a carbon black LLDPE-carrier masterbatch at 0.5–0.8 wt% to obtain wall opacity and ultraviolet resistance sufficient for extended exterior service. Compliance for upright storage is anchored to ASTM D1998-21, with water and chemical containment assessed under AS/NZS 4766:2020; potable-water variants require certification under NSF/ANSI 61-2023 for the monolayer wall. Processing on a drop-arm biaxial rotational moulding machine uses a rotation ratio of 4:1, oven air temperature 280–310 °C, and peak internal air temperature 195–205 °C. Demoulding is delayed until the part skin temperature is below 70 °C to reduce flat-panel warpage. Finished components include horizontal saddle tanks, sprayer sumps, fertigation dosing cubes, and batch mixing vessels with nominal wall thickness from 5 mm to 20 mm. A recurrent field failure is surface pinholes at the parting line when silicone mould-release agent is applied above 5 g/m²; the non-hygroscopic character of the powder does not require pre-drying unless condensation has formed on cold silo walls during outdoor storage.
Rotational moulding of agitated chemical storage vessels in Icorene 3545 BUE 5116 is specified for aqueous acids, alkalis, and hypochlorite solutions only when continuous service temperature does not exceed 40 °C and the specific chemical resistance chart for butene LLDPE is verified against molar concentration; published data for this specific grade in aggressive organic solvents is limited. Compliance is established through ASTM D1998-21 for upright tank geometry, with outer-shell intermediate bulk containers certified to UN 31A/Y under the relevant dangerous goods test sequence and the tank wall verified by ASTM D1693-15b environmental stress-crack resistance at 50 °C in 10% Igepal CO-630 solution. The charge formulation is maintained at 100% virgin powder or up to 10 wt% clean in-house regrind from the same tank class; carbon black LLDPE masterbatch is added at 0.3–0.5 wt% for opacity, while conductive black loadings above 1.5 wt% are not used because they lower melt flow and increase surface porosity at weld lines. The production sequence on a shuttle moulding machine uses oven air 290–310 °C, peak internal air temperature 200–210 °C, forced-air cooling to 80 °C, and water mist through the vent tube down to 35 °C. Ultrasonic wall-thickness checks are taken at 12 measurement points on each shell. Terminal product types include cylindrical caustic dosing tanks, containment pallets, agitation troughs, and IBC outer bodies; pinholes at knife-edge radii below 3 mm are a field signature when powder bridges in the mould during the first 2 min of rotation.
Marine buoy hulls moulded from Icorene 3545 BUE 5116 are produced on independent-arm rotational machines with a foaming-agent-free formulation because closed-cell polyurethane foam is injected after demoulding rather than foamed in situ; the polymer shell therefore retains a uniform 5–10 mm wall without gas-blown density gradients. Ageing compliance for tropical marine exposure applies ASTM G154-23 Cycle 1 accelerated weathering until colour change is below 3.0 ΔE after 2,000 h and ASTM D256-23 Izod impact at -20 °C above 600 J/m; salt-spray resistance is evaluated under ASTM B117-19 for 1,000 h. The formulation uses 0.8–1.2 wt% of an LLDPE-carrier pigment masterbatch containing carbon black or titanium dioxide, and secondary hindered amine light stabilizer at 0.2 wt% is added only where direct tropical sunlight exceeds 5 years of continuous service; independent published weathering data for this exact UV package beyond that interval is limited. Processing on a rock-and-roll machine for cylindrical fenders uses oven temperature 270–300 °C, peak internal air temperature 195–205 °C, and a two-stage forced-air cool with internal air purge at 15–20 kPa to hold part dimensions. Finished parts include navigation buoys, dock fenders, floating dredge floats, and foam-filled pontoon shells; the principal moulding defect is gas entrapment at the foam-injection port when the shell is demoulded above 60 °C and the inner surface remains tacky.
For below-grade utility enclosures and above-ground road barriers, Icorene 3545 BUE 5116 is processed at a wall thickness of 8–25 mm on shuttle machines with internal air injection through the vent tube at 10–25 kPa. Compliance for polymer replacement covers in pedestrian areas follows EN 124-1:2015 load classes A15–B125, while material classification uses ASTM D4976-21 as a polyethylene rotomoulding compound; ballast-filled temporary traffic barrier shells are tested under MASH 2016 TL-2 when specified. The charge formulation is 100% as-supplied powder with carbon black masterbatch at 0.2–0.4 wt% for outdoor stability; regrind from rejected enclosures is limited to 15 wt% because higher recycled content raises notched Izod failure rates at impact zones below -10 °C. The moulding cycle holds oven air at 285–310 °C, peak internal air temperature 198–208 °C, and a cooling ramp not exceeding 3 °C/min between 100 °C and 50 °C. Uncontrolled water quenching creates residual stress at rib roots and lowers the ASTM D1693-15b ESCR F50 value to under 100 h. Terminal products are utility pull boxes, meter pits, cable vault bases, and water-filled road barriers; in production audits the dominant defect is warpage of flat lids when demoulding temperature exceeds 75 °C or when only one side of the mould is cooled by floor fans.
Food-handling containers produced from Icorene 3545 BUE 5116 are specified for refrigerated and frozen service rather than hot-fill operations, because migration testing under EU Regulation 10/2011 requires an overall migration limit below 10 mg/dm² and increased comonomer content may raise extractable fractions in prolonged fatty-food contact above 40 °C. Compliance is anchored to FDA 21 CFR §177.1520(c) paragraphs 3.1a and 3.2a, with food equipment surface approval under NSF/ANSI 51-2023 only after the inner skin is found free of visible defects. The dry-blend formulation uses 100% virgin natural powder or up to 20 wt% clean in-house regrind from the same food-contact part family; external pigment masterbatch is limited to 0.2–0.5 wt% and must itself be food-compliant, while slip and antistatic additives are excluded because they alter organoleptic properties of the contact surface. Processing on an independent-arm carousel maintains oven air at 280–300 °C, peak internal air temperature 195–205 °C, and internal air pressure 10–15 kPa during cooling, with demoulding at a skin temperature below 60 °C to prevent surface peeling at the contact face. Terminal product types include insulated coolers, fish boxes, meat lugs, brine tanks, and bakery dough troughs; recurrent moulding faults are inner-surface blistering when the powder contains condensed moisture and flow lines when the mould rotates at less than 4 rpm on the secondary axis.
Competitive LyondellBasell Icorene 3545 BUE 5116 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 3545 BUE 5116 is a linear low density polyethylene supplied as a rotomoulding powder. The designation combines the Icorene 3545 base resin with a specific BUE 5116 additive, stabiliser, or colour formulation; the exact additive loading is not disclosed in public datasheets and must be confirmed against a lot-specific certificate of analysis. The base resin is an ethylene–alpha-olefin copolymer produced with a linear backbone and short-chain branching. Typical published values for the Icorene 3545 family include a melt flow rate of 4.5 g/10 min at 190°C under a 2.16 kg load when tested in accordance with ASTM D1238, and a density of approximately 0.935 g/cm³ when measured by ASTM D1505. The product is specified for rotationally moulded tanks, containers, and industrial parts requiring low-temperature ductility and resistance to environmental stress cracking. Because the BUE 5116 suffix can alter stabiliser loading, the generic property values are indicative only; batch-specific conformance limits are obtained from the certificate of analysis.
For rotationally moulded LLDPE, the combination of a melt flow rate near 4.5 g/10 min and density near 0.935 g/cm³ places the product in a medium-toughness LLDPE envelope. A melt index in this range permits flow into complex mould cores at typical oven set points between 260°C and 315°C. Linear low density polyethylene of this density class ordinarily exhibits mould shrinkage between 2.5% and 3.5% when cooled on aluminium tooling. Sintering proceeds by particle coalescence on the hot mould surface, but the final mechanical integrity depends more on peak internal air temperature than on oven set point alone. Parts sintered below a peak internal air temperature of approximately 190°C can retain interparticle boundaries and lose impact strength. Temperatures above 230°C accelerate oxidative chain scission, producing yellowing, surface embrittlement, or internal voids from decomposition gases. The practical operating window for this density class is therefore maintained at 200°C to 225°C internal air temperature, with the exact value adjusted for wall section, part thickness, and mould material.
Machine configuration influences the processing window. On a three-axis closed-loop rotomoulding machine with forced-air circulation and a 4:1 arm ratio, typical rotation speeds for LLDPE tanks are 4–8 rpm on the primary axis and 1–2 rpm on the secondary axis; the speed ratio is adjusted to prevent powder pooling in corners and ribs. The powder should have an apparent bulk density in the range 0.32–0.40 g/cm³ when tested by ASTM D1895, and a dry flow time below 35 s/100 g for uniform filling of narrow ribs. Coarse particles above 500 µm can reduce sintering and leave pinholing at the inner surface, while fines below 150 µm can impair dry flow and produce dusty charging conditions. The mould surface temperature during cooling should drop from a demoulding-relevant plateau of 90–110°C to below 50°C before part ejection. Forced cooling by air or a fine water mist is used only after dimensional measurements confirm that warpage remains within the drawing tolerance. Condensation on a cold mould surface is an operational boundary: charging powder into a mould below the dew point introduces water films that vaporise during heating and create pinholes. Pre-drying at 60–75°C for 2–4 h is applied only when powder has been stored at relative humidity above 60%; otherwise, unnecessary drying can oxidise powder surfaces and increase yellowing.
Compared with high-pressure LDPE, the linear backbone of Icorene 3545 BUE 5116 contains short-chain branches distributed along the polymer chain rather than long-chain branching. The difference produces higher tensile yield strength, higher flexural modulus, and substantially better environmental stress crack resistance at equivalent density. Typical LLDPE tensile yield strength values for this product family are reported near 14 MPa under ASTM D638, while an LDPE rotomoulding grade of similar density may yield at 10–12 MPa. The difference is more pronounced in environmental stress crack resistance: LLDPE grades of this type often exceed 1000 h in ASTM D1693 Condition B with 100% Igepal at 50°C, whereas many LDPE rotomoulding grades fail within 24–100 h under the same test conditions. This makes LLDPE preferred for tanks holding surfactants, agricultural chemicals, or mild alkaline solutions, provided that specific chemical compatibility is confirmed by immersion testing under ASTM D543 or ISO 175.
Against HDPE, the 0.935 g/cm³ density of Icorene 3545 BUE 5116 produces lower flexural modulus and hardness but improves low-temperature impact. Brittleness temperature by ASTM D746 is typically below -70°C, allowing service in cold-room or Arctic conditions where an HDPE rotomoulding grade may embrittle. However, HDPE retains greater stiffness and higher heat deflection temperature; the choice between HDPE and LLDPE in industrial tanks therefore balances stiffness and creep resistance against low-temperature ductility and environmental stress crack resistance. Metallocene LLDPE grades can offer narrower molecular weight distribution and higher dart impact in film applications, but in rotomoulding they may have a narrower sintering window and lower melt strength. The Icorene 3545 BUE 5116 family, produced by conventional Ziegler-Natta catalysis, retains a broader molecular weight distribution that supports particle coalescence and reduces pinholing in sharp radii. Published molecular weight distribution data for the exact BUE 5116 formulation are limited, so processors should request melt elasticity or rheology data when wall sections below 3 mm are planned.
Rotomoulding creates weld lines at the layering of successive powder charges and at the interface between the molten wall and the internal air. For LLDPE, insufficient heat history at the inner surface prevents complete wet-out of the powder, producing a sponge-like inner layer and reduced tensile elongation at break under ASTM D638. Internal air pressure in a sealed rotomoulding mould is generally low, but volatile species from antioxidant decomposition or residual moisture evolve at elevated peak internal air temperature. Venting of the mould or the use of a temperature-compensated pressurisation system maintains inner surface pressure below 0.1 MPa. In thick sections above 8 mm, the cooling rate is sufficiently slow that crystallinity and shrinkage differ through the wall; differential cooling produces residual stress and can initiate cracks at bosses or metal inserts. Normalisation of part dimensions is performed by annealing at 70–80°C for 1 h only after dimensional checks, because annealing can release moulded-in stress and alter flatness. Published residual stress data for Icorene 3545 BUE 5116 in specific rotomoulded configurations are limited; mould-filling simulations based on LLDPE heat capacity and thermal conductivity are used to estimate cycle time and thermal gradients.
Production-scale failure modes associated with rotomoulding LLDPE include powder bridging in narrow ribs, powder densification at the mould surface before the bulk reaches melt temperature, and uneven wall thickness at outer corners. Aluminium moulds with wall thickness between 6 mm and 10 mm transfer heat faster than stainless steel and therefore shift the optimum heating time. For an aluminium tool, oven residence time may be 15–25 min for 4–6 mm wall sections; stainless steel tools require longer residence because of lower thermal conductivity. The use of a release agent can reduce demoulding force, but excessive silicone release agent can migrate into the polymer and reduce weld line adhesion. When a release agent is used, the applied film thickness should remain below 5 µm; thicker films leave surface defects and can reduce post-moulding paint adhesion. Designed minimum inside radii of 3–6 mm, rib width-to-depth ratios of at least 1:1, and draft angles above 3° improve demoulding and reduce cracking at sharp intersections.
Because the BUE 5116 suffix identifies a specific additive or colour package, the weathering stability of the product is not equivalent to that of an unpigmented, non-UV-stabilised LLDPE. Outdoor performance claims require accelerated weathering data under ASTM D2565 or ISO 4892-2 on the exact BUE 5116 formulation; the base resin datasheet alone cannot support a warranty against surface chalking or loss of impact after prolonged UV exposure. Additive compatibility limits apply to active halogen-based or peroxide-based concentrates: direct combination with peroxides can crosslink the polymer and reduce melt flow, while high levels of acidic flame-retardant additives can deplete hindered amine stabiliser activity. Food-contact status, when relevant, must be verified against FDA 21 CFR 177.1520 or EU Regulation 10/2011 for the finished article, because migration limits depend on wall thickness, contact area, and shelf life. For potable water tanks, NSF/ANSI 61 or KTW recommendations may be required; the BUE 5116 suffix does not by itself confer such approvals. The product should not be melt-compounded into pellets for rotomoulding; pelletising destroys the required powder particle size distribution and dry-flow character. Storage of the powder should avoid direct sunlight and sustained temperatures above 40°C, and the product should be consumed within the supplier’s stated shelf life to preserve antioxidant activity.