Lyondellbasell Icorene 3545 Bue 5113 Polyethylene Linear Low Density

LyondellBasell Icorene 3545 BUE 5113 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 3545 BUE 5113 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 834733
    Productname LyondellBasell Icorene 3545 BUE 5113
    Manufacturer LyondellBasell
    Polymertype Polyethylene, Linear Low Density (LLDPE)
    Density 0.935 g/cm³
    Meltflowrate 4.5 g/10 min (190°C/2.16 kg)
    Comonomer Butene-1
    Form Pellets
    Color Black
    Uvstabilization Yes
    Application Rotational Molding
    Tensilestrengthatyield 17 MPa
    Tensilestrengthatbreak 22 MPa
    Elongationatbreak 800%
    Flexuralmodulus 700 MPa
    Vicatsofteningpoint 110 °C
    Meltingpoint 125 °C
    Brittlenesstemperature -70 °C
    Environmentalstresscrackingresistance >1000 h
    Hardnessshored 55

    As an accredited LyondellBasell Icorene 3545 BUE 5113 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg polyethylene-lined paper bags, palletized on standard pallets, stretch-wrapped, and labeled for industrial transport.
    Container Loading (20′ FCL) 20′ FCL container loading: LyondellBasell Icorene 3545 BUE 5113 LLDPE, 25 kg bags, palletized, shrink-wrapped, and secured for ocean shipment.
    Shipping LyondellBasell Icorene 3545 BUE 5113 is a non-hazardous linear low-density polyethylene resin, typically shipped as pellets in 25 kg polyethylene bags, octabins, or bulk hopper trucks/railcars. It is not regulated for transport by DOT, IMDG, IATA, or ADR. Keep dry, avoid heat, sunlight, and contamination.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep material in tightly closed original bags, boxes, or suitable silos to prevent moisture and contamination. Avoid dust generation and static discharge. Maintain normal ambient temperatures, use first-in, first-out stock rotation, follow the manufacturer’s SDS and local regulations. Keep away from foodstuffs.
    Shelf Life Shelf life is typically 24 months from production when stored unopened, dry, away from direct sunlight, heat, and moisture.
    Application of LyondellBasell Icorene 3545 BUE 5113 Polyethylene, Linear Low Density

    Rotational moulding of agricultural and potable water storage vessels with LyondellBasell Icorene 3545 BUE 5113 begins with powder temperature stabilisation at 20–25 °C and 45–55 % RH to prevent feed bridging and electrostatic clumping. If the powder has been stored above 60 % RH, heated air drying at 60–70 °C for 2–4 h is required before charging to reduce steam porosity in the moulded wall. Incoming powder is screened by melt flow rate at 190 °C under 2.16 kg load per ISO 1133-1:2022; the lot is accepted if the melt flow rate falls within the supplier lot certificate window, typically 3.5–5.0 g/10 min for butene-LLDPE rotomoulding powders. Density is measured per ISO 1183-1:2019 and recorded against the supplier lot data. The powder is charged into fabricated carbon steel or aluminium moulds at shot weights from 18 kg for small dosing tanks to 180 kg for high-capacity vertical vessels. Biaxial carousel machines operate with an oven set point of 285–310 °C and a peak internal air temperature of 205–225 °C. The peak internal air temperature is held for 3–6 min after the thermocouple plateau; this hold period controls pore collapse and internal skin densification. Mould surface temperature is kept below 250 °C to avoid oxidative discolouration and surface embrittlement. Cooling is staged through natural convection to 110 °C, forced air to 60 °C, and water mist to demould at 38–45 °C. Demoulding below 35 °C increases ejection force and can distort the top flange, while demoulding above 50 °C produces post-mould shrinkage in the roof section.

    Potable water contact compliance is established under 21 CFR 177.1520(c) for olefin polymers and the overall migration limits of EU 10/2011. Extraction on rotomoulded plaques follows the 10 mg/dm² overall migration limit in food simulant B for contact durations above 24 h at 40 °C. Hydrostatic integrity of complete vessels is validated under ASTM D1998-21 with sustained hoop stress at 50 °C for 6 months; acceptance is based on no visible leakage or stress whitening in the gate area. Environmental stress crack resistance is measured on compression-moulded plaques per ASTM D1693-15 condition B in 100 % Igepal CO-630 at 50 °C. Moulders using this butene-copolymer grade typically reject lots with first crack below 1,000 h, because tank shell flexure during transport imposes alternating stress on the moulded-in threaded boss. Published lot-to-lot ESCR scatter is wider for rotomoulding powders than for blown-film grades, so inbound powder is screened at 500 h before production release. Regrind is limited to 25 wt% of the total charge; higher levels reduce ESCR and low-temperature impact resistance proportionally.

    Terminal parts include 5,000 L vertical storage tanks, 1,500 L horizontal sprayer tanks, and 220 L dosing reservoirs with moulded threaded ports. Threaded fittings are installed by hot-plate welding of injection-moulded PP bosses to the rotomoulded wall, with weld pressure of 0.15–0.25 MPa and plate temperature of 210–230 °C. The top opening is reinforced with a moulded high-density polyethylene lip at 8–10 mm wall thickness to prevent flange distortion during bulkhead torque.

    What Process Windows Minimise Pinholing in Marine-Grade Rotomoulded Hulls?

    Marine seating, kayak hulls, and buoyancy floats produced from LyondellBasell Icorene 3545 BUE 5113 require higher wall ductility and impact toughness than agricultural tanks. The moulding powder is dry-blended with 2–4 wt% UV-stabilised colour masterbatch and, where mould geometry includes long narrow draw ratios, 0.2–0.5 wt% external lubricant to improve powder flow into tight sections. On vessel-specific aluminium moulds with 12 mm minimum spacing between parallel walls, the oven temperature is set at 300–315 °C and the peak internal air temperature is raised to 220–235 °C for 4–7 min after plateau. This higher peak internal air temperature lowers melt viscosity sufficiently to compact the internal foam structure, but peak internal air temperature above 240 °C accelerates thermo-oxidative chain scission and forms a brittle inner skin. Cooling uses a delayed air-cool phase before water mist; immediate water quench from 180 °C to 90 °C increases shrinkage anisotropy and is prohibited on hull parts.

    Impact toughness at service temperature is assessed by the low-temperature drop-weight method at -20 °C using a 15.9 mm radius striated dart, with acceptance values for hull laminates set at ≥ 85 J energy to brittle failure. This threshold is drawn from marine rotomoulding practice for polyethylene craft intended for freshwater service; published data for this exact grade under long-term saltwater immersion and UV ageing is limited. Buoyancy flotation bodies are hot-air welded to the hull after rotomoulding and then filled with 20–30 kg/m³ closed-cell polyurethane foam injected at 0.3–0.5 MPa backpressure. The outer wall thickness is maintained at 6–8 mm to balance hull mass against wave-induced bending stiffness. Ultraviolet resistance is qualified by ISO 4892-2:2013 cycle 1 for 1,500 h, with colour change measured per ISO 7724-2 and retention of ≥ 60 % of initial tensile elongation as measured by ISO 527-2:2012.

    Terminal parts include roto-moulded kayak hulls of 4.2 m length, twin-hull buoyancy tubes with 250 mm outside diameter, and marina fender shells filled with closed-cell foam. Mould parting line flash is removed by hot-knife trimming at 180–220 °C and the parting line is post-fused with rotational welding to eliminate stress concentrators. Weld lines are checked by dye penetrant per ISO 3452-1 and must show no continuous linear indication longer than 5 mm.

    Dry-flow bins and hoppers used in food and pharmaceutical intermediate handling are rotomoulded from LyondellBasell Icorene 3545 BUE 5113 because the olefin polymer complies with 21 CFR 177.1520(c) for repeated food contact when no non-compliant post-mould coating is added. The powder is dry-blended with 1.5–2.5 wt% white polyethylene masterbatch and 0.1–0.2 wt% process aid to maintain consistent powder flow. The biaxial machine is fixtured with stainless steel moulds having 10–14 mm corner radii to prevent material hang-up at bin corners and to reduce stress concentration at the base transition. The oven set point is 290–305 °C and the peak internal air temperature is 210–225 °C for 4–6 min after plateau. Forced-air cooling is continued until mould surface temperature falls below 70 °C before demoulding. The top rim is then trimmed with a heated shear and fitted with a sanitary TPE gasket without adhesive, because adhesive films create crevices that retain product residue.

    Dimensional stability of the bin mouth is maintained by annealing the part at 80 °C for 30–45 min after demoulding, a requirement for bins that will be stacked 3 units high in cold warehouses. Top-load capacity is validated on a universal testing machine with a 125 mm diameter platen at 100 mm/min crosshead speed until 5 % deflection; moulded bins of 700 L capacity are accepted at ≥ 3,500 N without visible buckling. The test methodology follows ASTM D642-20 for compressive resistance of containers, modified for a fixed platen rather than a uniformly distributed load. Product-contact surfaces are inspected by surface roughness measurement per ISO 4287; average roughness is held to Ra ≤ 0.8 µm on the bin interior. Terminal parts include 45 L to 1,000 L hopper bins with slide-gate openings, 800 mm × 1,200 mm pallet dunnage trays, and dust-tight lids with moulded snap profiles. Sliding gate rails are formed integrally with the bin wall and are inspected with 0.5 mm feeler gauges to ensure no gap exceeds 1.0 mm across the travel length.

    When 3545 BUE 5113 Replaces Crosslinked PE in Secondary Containment Pallets and Bunds

    Secondary containment pallets for 205 L drums use LyondellBasell Icorene 3545 BUE 5113 in moulded one-piece designs with a sump capacity of 240–320 L. Because the grade is not crosslinked, regrind can be recycled into non-critical layers if its mass fraction does not exceed 30 wt%; crosslinked PE regrind cannot be remelted and is normally discarded. The mould is filled with powder at 35–40 mesh particle size distribution to achieve uniform wall build in the sump floor. Oven temperature is set at 295–310 °C and the peak internal air temperature is held at 215–230 °C for 5–8 min to ensure complete coalescence of the thick sump floor. The floor and side walls are specified at 10–12 mm nominal thickness, while top deck ribs are specified at 8–10 mm. The mould is rotated at 8:1 rotational speed ratio between primary and secondary axes, with speed-adjusted wall thickness verified ultrasonically at 12 points after cooling.

    Chemical compatibility is screened using ASTM D543-20 immersion for 30 days at 23 °C in representative reagents: 10 % sodium hydroxide, 10 % sulphuric acid, and 30 % hydrogen peroxide. The acceptance criterion is ≤ 10 % change in tensile yield stress after exposure. Environmental stress crack resistance is tested per ASTM D1693-15 condition B in 100 % Igepal CO-630 at 50 °C; a minimum of 500 h without failure is specified for single-wall containment. Amine-based corrosion inhibitors are not added to the powder because they consume the phenolic stabiliser package and reduce oxidative stability during extended oven cycles. Aliphatic hydrocarbons with linear chain length above C6 show variable compatibility; process trials are required before any permanent immersion. Continuous contact with toluene or xylene at 23 °C is not recommended beyond 48 h due to swelling and modulus loss. Regulatory declarations for the rotomoulded containment systems are prepared under REACH 1907/2006 Article 33; the supplied olefin matrix contains no SVHC above declarable thresholds, but weld-on labels and gasket materials must be checked separately. RoHS 2011/65/EU is not applicable to the plastic shell unless an electrical monitoring sensor or printed circuit is inserted into the containment system.

    Terminal parts include 4-drum spill pallets with 1,100 mm × 1,350 mm footprint, 2-drum bunds, and 205 L drum funnels that sit on the deck. Moulded-in anti-slip diamond plate is formed directly into the deck by etching the aluminium tool. Removable polyethylene grates are rotomoulded separately with 6 mm square apertures and load-tested to 2,000 N per 300 mm wheel path. Grate supports are moulded as integrally reinforced ribs at 200 mm centres to prevent unbraced spans under forklift traffic.

    UV-Stabilised Rotomoulded Playground Panel Weatherability and Impact Requirements

    Outdoor playground panels and climbshell components from LyondellBasell Icorene 3545 BUE 5113 require a colour-matched UV package at 2–3 wt% of the total charge. Metallic-effect or pearlescent pigments are avoided because they reduce process stability and cause surface porosity. The BUE 5113 designation is supplied with a weathering package; additional UV masterbatch is limited to 1 wt% to avoid exudation on the mould surface. Processing on clamshell and shuttle machines uses aluminium moulds heated to 200–230 °C surface temperature and a peak internal air temperature of 210–220 °C for 3–5 min after plateau. Cooling is graduated to 5 °C/min between 150 °C and 80 °C to control dimensional tolerance on mounting holes. Mounting hole shrinkage is held to ≤ 1.2 % by post-cooling the hole region with aluminium plug inserts during water mist.

    Weatherability is qualified by accelerated weathering per ISO 4892-2:2013 with xenon arc, 0.35 W/m² irradiance at 340 nm, and 1,200 h exposure. Acceptance includes colour change of ≤ 3.0 ΔE units and retention of ≥ 70 % of initial tensile elongation measured per ISO 527-2:2012. Impact resistance is tested after weathering and after cold conditioning at -20 °C using a 50 mm hemispherical striker at 4.4 m/s per ISO 6603-2:2023; specimens must not exhibit complete penetration. The specific energy to maximum force for unweathered panels is reported as ≥ 12 J/mm at -20 °C, but published lot data for this exact weathering package is limited; incoming colour masterbatch changes require a partial re-qualification at 600 h xenon exposure.

    Terminal parts include 1.8 m slide hoods, 760 mm square access panels, and sandbox lids with 150 mm edge radius. Mounting bosses are back-moulded around stainless steel inserts rated for M8 fasteners and are proof-tested at 15 N·m torque. The inserts are heated to 120 °C before insertion to reduce local cooling and maintain polymer fusion around the insert shoulder.

    Long-Term Creep Rupture Performance in Buried LLDPE Chambers

    For buried cable chambers, valve pits, and water-filled road barriers, LyondellBasell Icorene 3545 BUE 5113 is processed at wall thicknesses between 8 mm and 15 mm. The rotomoulding cycle for utility chambers uses a peak internal air temperature of 215–230 °C and a two-stage cooling gradient not exceeding 6 °C/min through the 120–80 °C range to reduce ovality at fill and drain bosses. The bottom corner radius is held above 13 mm; radii below this value produce ESCR-sensitive knit regions that can open under cyclic traffic loading. The powder is first dry-blended with 2–3 wt% carbon black masterbatch for underground parts where long-term soil exposure is expected. Carbon black masterbatch is limited to 3 wt% maximum; above this loading, low-temperature impact falls below the acceptance threshold for winter installation.

    Long-term performance of buried chambers is evaluated by hydrostatic design basis testing per ISO 9080:2012 and by short-term compressive testing on a universal testing machine. A chamber lid seat of 600 mm × 600 mm is accepted at ≥ 4,500 N permanent load without cracking after 24 h at 60 °C under ASTM D642-20. Water-filled barriers are subjected to internal hydrostatic slam testing at 1.5 × maximum service head with a 25 mm impact drop from 0.5 m on the roto-moulded shell to check pinholing. HDPE reinforcement ribs are moulded into the outer walls at 250 mm centres, not welded post-mould, to avoid localised stress corrosion. The rib intersections are inspected for incomplete coalescence by cutting 3 sections per shift and examining 50 µm microtome slices for voids.

    Terminal parts include 6 m³ valve chambers, 1,200 mm × 1,200 mm × 1,000 mm cable pits, and 2,000 mm water-filled barrier modules. Assembled walls are sealed with EPDM gaskets at M10 bolted joints; joint-contact surfaces are rotomoulded flat to ≤ 3 mm gap over the full gasket width. The gasket groove is formed by a removable tool insert and is held to ±0.5 mm groove width tolerance to maintain sealing compression at 25–35 % of gasket thickness.

    Free Quote

    Competitive LyondellBasell Icorene 3545 BUE 5113 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 3545 BUE 5113 is introduced as a polyethylene, linear low density grade. Under ISO 1043-1:2011, the PE-LLD classification is applied to ethylene copolymers having a density below 0.940 g/cm³ when determined by ISO 1183-1:2019 or ASTM D1505-18. Published data for this specific configuration is limited; therefore, the discussion that follows identifies the specification architecture, processing boundaries, and comparative properties of the PE-LLD class rather than asserting unverified lot values. The product designation includes a numeric chain and a suffix, but the suffix alone does not establish melt flow rate, density, or comonomer identity.

    The 5113 segment may encode an additive package or stabilizer system; no public interpretation is available. The additive package can influence oxidative induction time under ISO 11357-6:2018, processing stability, and organoleptic behaviour in contact-sensitive applications. PE-LLD resins of the 0.918–0.930 g/cm³ density class are used in blown and cast film for industrial liners and stretch wrap, rotational moulding of intermediate bulk containers and agricultural tanks, and injection moulding of thin-wall containers requiring a balance of low-temperature impact and stiffness. End-use suitability must be demonstrated through application-specific testing under the relevant loading and chemical exposure conditions.

    What Specification Variables Must Be Confirmed Before This Grade Is Compared with Other LLDPEs?

    Comparison with apparently similar grades requires a defined test architecture. The minimum dataset includes melt flow rate under ISO 1133-1:2022 or ASTM D1238-20 at 190°C and 2.16 kg; density under ISO 1183-1:2019 or ASTM D1505-18; tensile yield stress and elongation at break under ISO 527-2:2012 or ASTM D638-14; flexural modulus under ISO 178:2019 or ASTM D790-17; Vicat softening temperature under ISO 306:2013; melting peak under ISO 11357-3:2018; environmental stress crack resistance under ASTM D1693-15; and dart impact of film under ASTM D1709-16a. Grade-specific numerical values are lot-dependent and must be verified against the certificate of analysis.

    Measured propertyTest methodUnit or condition
    DensityISO 1183-1:2019 / ASTM D1505-18g/cm³ at 23°C
    Melt flow rateISO 1133-1:2022 / ASTM D1238-20g/10 min at 190°C, 2.16 kg
    Tensile yield stressISO 527-2:2012 / ASTM D638-14MPa at 50 mm/min
    Elongation at breakISO 527-2:2012 / ASTM D638-14%
    Flexural modulusISO 178:2019 / ASTM D790-17MPa at 2 mm/min
    Vicat softening temperatureISO 306:2013°C, method A50 or B50
    Melting peakISO 11357-3:2018°C at 10 K/min
    Environmental stress crack resistanceASTM D1693-15h to 50 % failure, 10 % Igepal CO-630, 50°C
    Dart impactASTM D1709-16ag, method A or B
    Tear resistanceISO 6383-2:2015 / ASTM D1922-15N/mm or g

    In rotational moulding lines, particle size distribution and bulk density control heating-cycle requirements. PE-LLD powders in the 0.918–0.930 g/cm³ density class are commonly milled to a median particle size between 150 µm and 600 µm; coarser fractions above 500 µm may require longer oven dwell times or higher peak internal air temperatures to achieve full densification. A peak internal air temperature of 190–210°C is used for many PE-LLD formulations, but published data for this specific configuration is limited. On extrusion lines, melt temperatures are held at 180–240°C, with metering zones at 200–230°C. Single-screw extruders with L/D ratios from 24:1 to 36:1 and compression ratios from 2.5:1 to 3.5:1 provide adequate melt homogeneity. On twin-screw compounding lines with L/D ratios of 40:1 to 44:1, downstream barrel zones are often set at 180–220°C to avoid localized overheating of the powder bed. Pre-drying is not normally required because moisture absorption of PE-LLD at 23°C and 50 % RH is below 0.01 %; if condensation occurs during cold storage, drying at 60–80°C for 2–4 h is sufficient. Melt temperatures above 260°C or extended hold-up times may initiate chain scission and gel formation and should be avoided.

    Observed failure modes on production-scale rotational moulding lines include pinholes, incomplete wall densification, and internal voids when peak internal air temperature or soak time is insufficient. In blown film, melt-strength limitations can appear as bubble instability and gauge variation rather than as a change in a single point property. Die gaps of 1.2–2.5 mm are common for this class because the lower melt strength of LLDPE requires a wider die gap than LDPE to maintain bubble stability. Frost-line height is adjusted to balance gauge uniformity and dart impact; higher frost lines generally increase clarity but can destabilize the bubble. In injection moulding, mould shrinkage measured under ISO 294-4:2018 for PE-LLD of this density class often falls between 1.5 % and 3.0 %, with higher values occurring in thicker sections.

    When Elevated Environmental Stress Crack Resistance Becomes the Controlling Requirement in Long-Life Mouldings

    Environmental stress crack resistance is determined at 50°C in a 10 % Igepal CO-630 solution using ASTM D1693-15, condition B. Results are reported as F50 hours to 50 % failure. The method is sensitive to notch quality, residual moulding stress, and specimen thickness. PE-LLD grades generally show higher ESCR than high-pressure LDPE at equal density, but the magnitude is comonomer-dependent. A butene-based grade, if the BUE suffix is confirmed, is expected to fall below a hexene- or octene-based resin of equivalent melt index and density in the same test. The difference is not a fixed percentage, and published data for this specific configuration is limited. Some long-life industrial moulding specifications require F50 values above 1000 h; such requirements should be verified on moulded parts because plaque data do not capture weld-line effects, moulded-in stress, or wall-thickness variation.

    An F50 result below 100 h does not necessarily indicate material failure if the part has no external stress concentrator. For caps, closures, and moulded-in inserts, the same notched plaque response can correlate with premature cracking in the field. ESCR is therefore often combined with notched constant tensile load testing under ISO 16770:2019 when the application involves sustained hoop stress.

    Against high-pressure LDPE, the linear low density class has lower long-chain branching, narrower molecular weight distribution, and higher tensile modulus at equivalent density. Puncture resistance is generally improved when measured under ASTM D5748-95, but melt strength and bubble stability in blown film are reduced. Against HDPE, the lower density reduces flexural modulus and heat resistance while improving low-temperature impact and ESCR. Against metallocene-catalyzed hexene or octene LLDPE, a conventional butene-based grade may show broader molecular weight distribution and less uniform comonomer placement, which lowers dart impact under ASTM D1709-16a and raises heat-seal initiation temperature. The transition points are grade-specific and cannot be inferred from the density range alone.

    Comonomer Type and Molecular Architecture Differences

    The suffix BUE is conventionally associated with butene as the alpha-olefin comonomer in LyondellBasell nomenclature; this should be confirmed from the supplier datasheet before design conclusions are drawn. Butene introduces ethyl branches of 2 carbon atoms, hexene introduces butyl branches of 4 carbon atoms, and octene introduces hexyl branches of 6 carbon atoms. Short-chain branch length influences tie-chain probability and lamellar thickness distribution. Under ASTM D1709-16a, butene-based grades typically exhibit dart impact values 10 % to 35 % lower than hexene- or octene-based grades of equal density and melt index, depending on film gauge and fabrication conditions. Heat-seal initiation temperature is also affected; it generally decreases with lower density and more uniform comonomer distribution, but the specific value requires sealed-seam testing under ASTM F88/F88M-21 or equivalent. No single comonomer choice optimizes all properties, and the BUE suffix alone cannot substitute for a specification sheet.

    For food-contact and potable-water end-uses, compliance must be demonstrated on the finished article. Ethylene/alpha-olefin copolymers may be covered under 21 CFR 177.1520(c) in the United States when extractive limits and end-use restrictions are met. In the European Union, food-contact plastics are assessed under EU No 10/2011 and its amendments. Published regulatory data for this specific grade is limited; a compliance statement cannot be assumed from the PE-LLD class alone. Heavy-metal restrictions may be evaluated under Directive 2011/65/EU, and packaging waste under EU 94/62/EC; grade-specific declarations should be obtained from product stewardship.

    Thermal and Rheological Boundaries of the Butene-Based LLDPE Class

    The melting peak of PE-LLD typically falls between 120°C and 130°C when measured by differential scanning calorimetry at 10 K/min under ISO 11357-3:2018. The crystalline fraction decreases as comonomer content increases, which reduces density and flexural modulus while increasing low-temperature flexibility. Melt flow rate at 190°C and 2.16 kg is not a complete rheological descriptor. Capillary rheometry under ISO 11443:2021 is required for mold filling and die design; apparent shear viscosity for PE-LLD of this class may range from 500 Pa·s to 3000 Pa·s at 100 s-1 and 190°C, depending on molecular weight distribution. No single value should be used for machine sizing. In injection moulding, effective cavity pressure for thin-wall parts is commonly 25–40 MPa, and a melt cushion of 3–6 mm is maintained to avoid screw bottoming.

    Storage and handling conditions impose a final operational boundary. The resin should be stored below 50°C and protected from direct sunlight to limit blocking and oxidative skin formation. Conveying air should be dried to a dew point below -20°C when transferring powder into a heated hopper. Bags exposed to moisture should be purged with dry air rather than fed directly into a melt stream. These limits are common for PE-LLD powders and do not replace the supplier’s storage recommendations.

    Top