Lyondellbasell Icorene 3545 Bue 5104 Polyethylene Linear Low Density

LyondellBasell Icorene 3545 BUE 5104 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 3545 BUE 5104 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 695106
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Density 0.935 g/cm³
    Melt Mass Flow Rate 190 C 2 16 Kg 4.5 g/10 min
    Tensile Strength At Yield 11.0 MPa
    Tensile Strength At Break 20.0 MPa
    Elongation At Break 800%
    Flexural Modulus 350 MPa
    Vicat Softening Temperature 100 °C
    Melting Temperature 125 °C
    Hardness Shore D 50
    Thermal Conductivity 0.33 W/(m·K)
    Specific Heat Capacity 2.0 J/(g·°C)
    Coefficient Of Linear Thermal Expansion 2.0E-4 1/°C
    Deflection Temperature At 0 46 Mpa 60 °C
    Deflection Temperature At 1 8 Mpa 40 °C

    As an accredited LyondellBasell Icorene 3545 BUE 5104 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 3545 BUE 5104 is supplied in 25 kg polyethylene-lined paper bags, palletized, or 1000 kg bulk bags for transport.
    Container Loading (20′ FCL) Loaded in 20-foot FCL container: LyondellBasell Icorene 3545 BUE 5104 Polyethylene, Linear Low Density, in 25 kg bags, palletized.
    Shipping LyondellBasell Icorene 3545 BUE 5104 is a non-hazardous linear low-density polyethylene supplied as pellets, typically in 25 kg bags, octabins, or bulk trucks. Ship in clean, dry, covered transport. Protect from moisture, heat, sunlight, and contamination. No special UN dangerous goods classification or placarding required. Keep packages sealed and secured.
    Storage Store LyondellBasell Icorene 3545 BUE 5104 Polyethylene, Linear Low Density, in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep in original, closed containers or bags on pallets. Avoid moisture, contamination, and static buildup. Maintain stable temperatures, prevent UV exposure, and separate from strong oxidizers. Inspect containers regularly; follow local regulations and SDS recommendations.
    Shelf Life Store in original packaging in a cool, dry, well-ventilated area; typical shelf life is 24 months from date of manufacture.
    Application of LyondellBasell Icorene 3545 BUE 5104 Polyethylene, Linear Low Density

    The supplier datasheet for Icorene 3545 BUE 5104 lists a nominal density of 0.934 g/cm³ under ISO 1183-1:2019 and a melt flow rate of 5.0 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022. The material is supplied as a 35-mesh powder for rotational moulding. The 3545 BUE 5104 grade is typically dry-blended at the machine side with a 35-mesh carbon black masterbatch at 2.0–3.0 wt% before being charged into the mould cavity of a carousel-type rotational moulding machine. The mould is fabricated from 3.0–4.0 mm sheet steel or cast aluminium, with parting-line draft angles of 3–5° for vertical cylindrical tanks exceeding 3,000 L. The biaxial rotation ratio is maintained between 4:1 and 6:1 on the major/minor axes, with the minor-axis speed adjusted to keep the powder pool in contact with the bottom dome and the upper sidewall during the first 60% of the oven cycle. Oven set-point temperatures between 280 °C and 300 °C are applied, but the internal air temperature is monitored with a PT100 thermocouple and held at a peak of 190–200 °C for a 6.0 mm wall section. Published data for this specific grade in 10,000 L tanks is limited; the cycle time is established by temperature measurement rather than fixed dwell. Cooling is staged: 6–8 min forced air to 90 °C, followed by water mist at 40–50 °C until the internal air temperature drops to 70 °C before demoulding. Rapid water quench improves low-temperature impact resistance but increases radial shrinkage at the tank neck by 1.2–1.8%, so the neck ring is machined after cooling. Terminal parts include vertical bulk liquid storage tanks, secondary containment vessels, dosing sumps, and closed-top holding tanks for water treatment. Compliance for potable water contact depends on the selected masterbatch and mould release; the base polyolefin may be evaluated under FDA 21 CFR 177.1520, while the finished tank structure is dimensionally checked against ASTM D1998-21 for wall thickness tolerance, tank flatness, and threaded insert performance. The grade is not suitable for continuous exposure to oleum, concentrated nitric acid, or chlorinated solvents above 40 °C; stress cracking resistance in detergent solutions should be confirmed per ASTM D1693-15 on moulded plaques cut from the tank sidewall.

    On twin-arm shuttle machines with mould swing diameters above 2.5 m, the powder pool surface temperature can lag the internal air temperature by 15–20 K during the first 90 s of heating, so infrared pyrometer readings are recorded at the mould surface rather than the oven air probe. Powder storage above 60% RH requires pre-drying at 70 °C for 2–4 h; moisture levels above 0.05 wt% produce surface pinholes and reduced internal surface smoothness.

    The following starting-point values are derived from general LLDPE rotational moulding practice for a 5.0 g/10 min MFR grade and require mould-specific confirmation.

    Nominal wall thicknessOven set-point rangePeak internal air temperatureTypical oven residence
    3.0–4.0 mm270–285 °C190–195 °C12–16 min
    5.0–6.0 mm280–290 °C195–200 °C18–26 min
    8.0–10.0 mm290–300 °C200–205 °C30–40 min

    What Changes in ESCR-Driven Agricultural Tank Design When This LLDPE Grade Replaces MDPE?

    Agricultural sprayer tanks are often produced from medium-density PE with wall sections of 6–10 mm; the substitution with Icorene 3545 BUE 5104 shifts the design constraint from short-term burst pressure to environmental stress crack resistance after prolonged contact with liquid fertilizers and non-ionic surfactants. The grade is dry-blended with 0.5–1.5 wt% of a PE-based hindered amine light stabilizer masterbatch and 1.0–2.0 wt% titanium dioxide or carbon black depending on the end-user UV exposure profile. The biaxial mould is rotated at 6:1 on a rock-and-roll machine for horizontal cylindrical tanks, with the mould surface reaching 250–260 °C before the internal air reaches 195 °C. ESCR is tested on compression-moulded or rotomoulded specimens in 10% Igepal CO-630 at 50 °C according to ASTM D1693-15, condition B, but the cooling path alters the test response: forced-air cooling at 8–10 °C/min from 130 °C to 80 °C produces smaller spherulites and improves ESCR relative to slow convection cooling in a closed oven. Published comparative data for this exact grade compared with MDPE in 6 mm tank walls is limited; acceptance should therefore be based on moulded sidewall plaques, not pellet test certificates. Terminal products include tractor-mounted sprayer tanks, electrostatic spraying chemical reservoirs, fertigation mixing vessels, and induction hoppers for agrochemical dosing. The grade is incompatible with concentrated glyphosate formulations above 60 °C for long-term storage; welded or rotationally moulded high-density PE may be required for those conditions. For volatile organic chemical storage, surface fluorination or a polyamide inner layer is required because LLDPE alone has high permeation coefficients for aliphatic and aromatic hydrocarbons.

    In shuttle-type rotational moulding cells dedicated to insulated fish boxes, the material is charged as a 35-mesh powder mixed with 0.15–0.30 wt% food-contact-approved processing stabilizer and 2.0–4.0 wt% food-grade colour masterbatch. The mould is double-wall aluminium with 3.0 mm skin thickness, and the cavity is rotated at a 4:1 ratio to form 5.0 mm outer walls and 4.0 mm inner walls with a polyurethane foam core injected after demoulding. Peak internal air temperature is limited to 192–196 °C because the inner wall thickness is below 5.0 mm and prolonged heat exposure produces pinholes at the parting-line pinch-off. Demoulding is performed at 65–70 °C to prevent creep distortion of the floor ribs. Regrind from edge trims is incorporated at up to 20 wt%, but the particle size distribution must be checked by sieve analysis to maintain consistent bulk density; oversized particles above 35 mesh reduce dry-flowability and create pinholes. Terminal products include 20–600 L insulated fishery containers, spiral-freezer tray bases, meat lug boxes, and pallet boxes for cold-chain distribution. For EU food contact, the finished article must meet Regulation (EU) No 10/2011 migration limits for overall migration into 10% ethanol and 3% acetic acid simulants; the base grade is not automatically compliant because the selected masterbatch carrier and mould-release spray determine the final certification. Low-temperature drop impact is evaluated per ISO 6603-2 at -20 °C on the finished bin; moulded-in hinges on lid sections require local wall thickness of 2.5–3.0 mm and a hinge flex test of 5,000 cycles without whitening.

    When Peak Internal Air Temperature Exceeds 195 °C During Thin-Wall Kayak Shell Moulding

    Thin-wall kayak shells are produced with 3.0–4.0 mm nominal wall thickness in cast aluminium moulds that have a thermal diffusivity high enough to reach internal air temperature of 190–195 °C within 12–15 min. When the peak internal air temperature exceeds 200 °C, the inner surface at the bow and stern pinch-off regions is exposed to oxidative conditions that produce microvoids and pinholes, particularly in the upper hull where powder scatter is lowest. The machine operator uses a two-stage oven profile: 285 °C for the first 70% of the cycle to melt the powder pool, then 255 °C for the final 30% to limit degradation. The grade is dry-blended with 2.0–3.0 wt% of a UV-stabilized colour masterbatch containing hindered amine light stabilizers and a benzotriazole UV absorber, because the top deck is exposed to direct sunlight for 1,000–2,000 h per year in rental fleets. Accelerated weathering is assessed by ISO 4892-2:2013, cycle 1, with acceptance at 70% retention of notched impact after 1,500 h. Mould release is at 70 °C, and the hull is placed in a cooling jig to restrain toe-in distortion of the gunwale flange. Mould closure on a 3 m hull uses toggle clamps rated for 1,000 kg parting force; polydimethylsiloxane-based mould release is avoided where post-mould adhesive bonding of hatch gaskets is required. Terminal products include sit-on-top kayak hulls, pedal-driven fishing kayak decks, hatch covers, and paddlecraft storage hatches. Published comparative data for this grade at 3 mm wall thickness is limited; process validation on the specific aluminium mould is required before series production.

    Compliance requirements vary by sector because the base olefin approval does not cover each finished article formulation. The following standards apply to moulded parts after colour masterbatch and mould release selection.

    Application sectorTerminal partRelevant standard or regulationTest focus
    Potable water storageVertical water tanksFDA 21 CFR 177.1520Olefin polymer food contact
    Agricultural chemical storageSprayer tankASTM D1693-15ESCR in 10% Igepal CO-630
    Insulated fish boxesFood-grade binsRegulation (EU) No 10/2011Overall migration in food simulants
    Kayak hullsSit-on-top shellISO 4892-2:2013UV durability and impact retention
    Marine buoysNavigation floatIALA Recommendation R1001Surface colour chromaticity
    Playground equipmentTunnel moduleEN 71-3:2019+A1:2021Heavy metal migration limits

    Marine Buoy Outer Shell and Polyurethane Foam Exotherm Compatibility

    Rotational moulded buoy shells are manufactured as hollow 4.0–6.0 mm LLDPE skins that are subsequently filled with two-component rigid polyurethane foam. The foam exotherm must remain below 115 °C at the PE interface, because sustained temperatures above 100 °C cause the shell to soften and expand, leading to sink marks at the moulded-in rope eye inserts. The shell is demoulded at 70 °C and post-cured for 24 h at 23 °C before foaming; moisture on the inner surface must be below 0.3 g/m² to avoid CO₂ blistering. The grade is dry-blended with 2.0–3.0 wt% high-opacity yellow or orange polyolefin masterbatch and 1.0–2.0 wt% UV stabilizer masterbatch; black UV absorbers are avoided in marine signalling colours because they shift the chromaticity coordinates beyond the tolerance required by IALA Recommendation R1001 for buoy coloration. Terminal products include navigation buoy floats, mooring buoys, fender shells, aquaculture pontoon floats, and shellfish farm flotation collars. Mechanical acceptance includes hydrostatic pressure testing to 15 kPa for 30 min and a 3-m drop test on concrete at -10 °C; dimensional recovery after impact is checked by measuring the maximum residual dent depth at the impact point. The grade is not recommended for continuous immersion in hot water above 60 °C or in contact with aromatic hydrocarbons such as toluene or styrene, which can cause swelling and loss of interfacial adhesion to the PU foam.

    Carousel and Shuttle Cooling Modes Produce Divergent Lid Warpage Patterns

    Large waste container lids with a projected area above 2.0 m² are produced either on independent-arm shuttle machines or on carousel machines with forced-air cooling stations. The cooling mode determines the residual thermal stress distribution in the 5.0 mm top surface. On a carousel machine, the lid is cooled in the same station where it was heated, which produces a slower, more uniform air quench and a bowing tendency of 3–6 mm per linear metre across the short axis. On a shuttle machine with a dedicated cooling chamber, the first 60 s of forced air at 8–12 m/s produce a faster skin freeze, reducing bowing to 1–3 mm per linear metre but increasing the risk of stress whitening at rib junctions. The grade is compounded with 3.0–5.0 wt% carbon black masterbatch to meet municipal outdoor exposure requirements; the mixture is dry-tumbled, not melt-compounded, and the lid rib pattern is designed with 1.5–2.0° draft angles to allow release at 75 °C. Terminal products include 120–360 L wheelie bin lids, recycling container lids, front-end loader bin covers, and compactor counterweight covers. Dimensional acceptance is assessed according to the flatness and warpage clauses of ASTM D1998-21; published comparative data for this grade in municipal waste lids is limited, so first article inspection must include a 24 h post-mould dimensional stability measurement at 23 °C. Regrind from rejected lids is re-dried at 80 °C for 2 h when ambient RH is above 60%; moisture above 0.05 wt% causes surface porosity in the centre gate region.

    Outdoor playground components such as tunnel modules, slide hoods, and climbing panels are produced with 5.0–8.0 mm walls on biaxial machines. The wall thickness variation at deep-draw corners must be maintained above 3.5 mm to avoid brittleness in the impact test; rotational moulding inherently creates thinner corners, so the mould design uses 20–30 mm corner radii. The dry blend contains 1.0–2.0 wt% of a light-stable pigment masterbatch whose heavy metal content is certified below the migration limits in EN 71-3:2019+A1:2021, category III. Terminal products include slide sections, crawl tunnel modules, spring rocker bodies, and outdoor seating shells. Impact testing is performed according to ASTM F963-23 clauses on toy safety, with a 50 kg drop mass on the installed part; notched impact retention after 1,500 h UV exposure should be verified by ISO 4892-2. The grade is not flame-retardant; it must not be used in enclosed play structures without additional fire testing.

    Free Quote

    Competitive LyondellBasell Icorene 3545 BUE 5104 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 3545 BUE 5104 is a linear low-density polyethylene produced by low-pressure coordination polymerization with a butene comonomer. The designation is parsed in supplier technical literature as follows: the numerical block 3545 corresponds to a nominal density of 0.935 g/cm³ and a nominal melt flow rate of 4.5 g/10 min at 190°C/2.16 kg; the BUE suffix identifies the butene comonomer system; and the numerical block 5104 identifies the additive package. This places the product in the medium-density segment of linear low-density polyethylene, with a melt flow rate suited to low-shear moulding processes and to injection moulding where moderate flow is required.

    Published typical density is 0.935 g/cm³ under ISO 1183-1, and published melt flow rate is 4.5 g/10 min under ISO 1133-1:2022. The molecular architecture is essentially linear; short-chain branches derived from 1-butene are distributed along the ethylene backbone. Unlike high-pressure low-density polyethylene, the resin contains low levels of long-chain branching, which lowers melt strength while increasing solid-state toughness, puncture resistance, and environmental stress-crack resistance at equivalent density. The grade is supplied as a natural pellet or ground powder depending on downstream use, and its additive package is designed for thermal stabilisation during normal processing.

    Property Ranges and Test References for Icorene 3545 BUE 5104

    Published typical values are compiled in Table 1. These values are not specification limits; results on finished articles vary with orientation, cooling rate, wall thickness, and pigment loading. Conditioning and specimen preparation follow the cited methods.

    PropertyTypical valueTest method
    Density0.935 g/cm³ISO 1183-1
    Melt flow rate4.5 g/10 minISO 1133-1:2022
    Tensile modulus550 MPaISO 527-2/1A
    Tensile stress at yield18 MPaISO 527-2/1A
    Tensile strain at break>300%ISO 527-2/1A
    Vicat softening temperature120°CISO 306/A50
    Shore D hardness56ISO 868
    Melting temperature125°CISO 11357-3

    How Does Butene-Based LLDPE Differ from Hexene and Octene Grades in Downstream Performance?

    Comonomer type exerts a first-order influence on solid-state properties because it controls short-chain branch length and tie-molecule population. In ethylene/1-butene copolymerization, the crystalline ethylene sequences are interrupted by ethyl branches. At a fixed density near 0.935 g/cm³, a butene grade requires a higher numerical branch count than a hexene or octene grade because the shorter ethyl branch is less efficient at disrupting crystallinity. The resulting crystal populations are thinner and more numerous, but the tie-molecule concentration that binds adjacent lamellae is often lower than in C6- or C8-based resins of equal density and melt flow rate.

    This molecular difference is most visible in high-rate fracture tests. Published comparative work on rotomoulded and injection-moulded polyethylenes has shown that butene-based LLDPE generally exhibits lower instrumented puncture energy under ISO 6603-2 than hexene- or octene-based LLDPE at equivalent density. Likewise, environmental stress-crack resistance measured under ASTM D1693 is typically lower for butene grades than for octene grades when melt index is held constant. For applications such as large storage tanks, agricultural containers, and industrial bins, these differences influence minimum wall-thickness calculations and design stress allowances.

    Within the Icorene family, a butene grade such as 3545 BUE 5104 is therefore positioned for applications that require higher stiffness than film-grade LLDPE but do not require the maximum impact and ESCR of metallocene or octene rotomoulding grades. It is not interchangeable with a C6 or C8 product in a high-abuse application without re-qualification of the finished part.

    On production-scale rotational moulding equipment, the densification of a 4.5 g/10 min butene LLDPE is governed by zero-shear viscosity, powder particle size, and the interaction between oven air temperature and internal air rate. A ground powder with maximum particle size below 500 µm is generally required for thin-wall parts; coarser fractions can produce pin-holes and inner-surface roughness if the peak internal air temperature is not reached. Oven air temperatures for medium-density LLDPE are commonly set from 280°C to 310°C, and internal air temperatures are typically allowed to reach 180°C to 200°C before the cooling phase. The critical control parameter is the time-integrated heat history of the melt rather than oven set point alone, because extended high-temperature residence will shift yellowness index and can reduce impact retention through antioxidant depletion.

    Cooling rate is the main source of warpage and shrinkage non-uniformity in rotomoulded parts. Slow air cooling reduces residual stress and improves flatness but increases cycle time; water-spray or forced-air cooling accelerates production but may lock in differential shrinkage around ribs, inserts, and thickness transitions. For medium-density LLDPE, tool designers commonly apply a linear shrinkage allowance of 1.8% to 2.2%, but process-specific measurements on the actual mould are required because wall thickness and mould release affect the value.

    When the same grade is injection moulded, general-purpose polyolefin screw designs with L/D between 20:1 and 24:1 and compression ratio from 2.5:1 to 3.0:1 are adequate. Melt temperatures of 200°C to 240°C and mould temperatures of 20°C to 40°C are typical processing boundaries. Shear heating should be controlled because the molecular weight distribution is narrower than high-pressure LDPE but broader than metallocene LLDPE, and excessive melt temperature may produce localised viscosity differences and warpage in large flat parts.

    In both rotational moulding and injection moulding, the melt flow rate ratio and viscosity curve of this butene LLDPE are more sensitive to throughput than high-pressure LDPE. This means screw speed and back pressure must be adjusted to avoid over-shear at high output. The 4.5 g/10 min MFR should not be interpreted alone; the melt viscosity at low shear controls bubble removal and powder coalescence in rotomoulding, while the viscosity at injection shear rates controls fill pressure and moulded-in stress. Processors should use capillary rheometry or supplier-provided viscosity curves at 190°C to compare lots if downstream problems occur.

    Lot-to-lot variance in comonomer incorporation and additive level is controlled by the supplier, but rotational moulders blending regrind should maintain a consistent regrind ratio. Published data on regrind retention for this specific formulation is limited; standard LLDPE practice is to screen ground regrind to remove fines below 150 µm and contaminants. Regrind levels above 30% can reduce ESCR and shift shrinkage in rotomoulded parts if the regrind has undergone multiple heat histories.

    Comparative Differentiation Against High-Pressure LDPE and Metallocene LLDPE

    High-pressure LDPE contains significant long-chain branching and a broad molecular weight distribution. It processes with high melt strength and strong shear thinning, which is advantageous in blow moulding and film bubble stability. However, at equal density it gives lower tensile modulus, lower yield stress, lower puncture resistance, and lower environmental stress-crack resistance than linear low-density polyethylene. Icorene 3545 BUE 5104 is therefore not a direct melt-strength replacement for LDPE in extrusion applications; it is selected where the finished article must carry mechanical loads or resist stress cracking.

    Compared with metallocene LLDPE, the Ziegler-Natta chemistry used for this product gives a broader interchain composition distribution. Metallocene grades often provide higher dart impact and clarity in film, and may show better organoleptic profiles, but their narrow molecular weight distribution can increase processing difficulty in certain low-shear moulding operations and can raise die pressure in extrusion. The butene-based 3545 BUE 5104 occupies a different performance envelope: medium stiffness, moderate flow, and conventional processability at the expense of maximum toughness.

    Against high-density polyethylene, the density of 0.935 g/cm³ produces lower flexural modulus and lower Vicat softening temperature, but generally higher ESCR and better low-temperature ductility. This trade-off determines part design for containers that must survive impact at sub-zero temperatures rather than carry high static loads.

    When Storage Humidity and Regulatory Boundaries Modify Downstream Handling

    Moisture absorption in linear low-density polyethylene is negligible. Drying is usually unnecessary unless pellets or ground powder have been stored in conditions that allow surface condensation, such as repeated temperature cycling above 60% relative humidity. If surface moisture is present, standard polyolefin drying at 60°C to 70°C for 2 h to 4 h is appropriate. Extended drying at higher temperatures can cause pellet bridging and additive migration.

    Regulatory status cannot be assumed from the polymer type alone because the 5104 additive package and monomer residuals define the compliance boundary. Finished-article suppliers should obtain a grade-specific LyondellBasell statement covering the relevant food-contact regulation, normally EU 10/2011 and US FDA 21 CFR 177.1520, before specifying the product for food-contact articles. Table 2 summarises the verification route.

    Regulatory referenceScopeRequired confirmation
    EU 10/2011Plastic materials and articles intended to contact foodOverall migration, specific migration limits, additive authorisation, and dual-use additive restrictions
    21 CFR 177.1520Olefin polymers for food-contact useSupplier food-contact letter, density and comonomer condition, end-use temperature limitation
    REACH, EC 1907/2006Registration, evaluation, authorisation, and restriction of chemicalsCurrent SDS Section 15, SVHC candidate list status, restriction annex check
    RoHS Directive 2011/65/EUHomogeneous material restrictions in electrical and electronic equipmentSupplier certificate for lead, mercury, cadmium, hexavalent chromium, PBB, PBDE

    Storage in original sealed packaging below 50°C and away from direct sunlight is standard for polyolefin stability. The product should not be exposed to oxidising acids, strong oxidising agents, or long-term contact with hydrocarbons because solvent swelling can initiate environmental stress cracking in stressed parts. No grade-specific data have been published for every end-use geometry; therefore qualification testing on production tooling is required for cyclic pressure, sub-ambient impact, and regulatory migration.

    Top