Lyondellbasell Icorene 3545 Bue 5101 Polyethylene Linear Low Density

LyondellBasell Icorene 3545 BUE 5101 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 3545 BUE 5101 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 453562
    Density 0.935 g/cm3
    Melt Index 3.5 g/10 min at 190°C/2.16 kg
    Hardness Shore D 55
    Tensile Strength At Yield 11 MPa
    Tensile Strength At Break 20 MPa
    Elongation At Break 800%
    Flexural Modulus 350 MPa
    Tensile Modulus 350 MPa
    Vicat Softening Point 100°C
    Melting Point 124°C
    Thermal Conductivity 0.33 W/m·K
    Coefficient Of Linear Thermal Expansion 1.5E-4 1/°C
    Specific Heat Capacity 2.3 J/g·°C
    Dielectric Constant 2.3
    Volume Resistivity 1.0E+15 ohm·cm
    Water Absorption <0.01%
    Mold Shrinkage 1.5-2.0%

    As an accredited LyondellBasell Icorene 3545 BUE 5101 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 3545 BUE 5101 linear low density polyethylene resin is supplied in 25 kg bags, typically palletized for shipping.
    Container Loading (20′ FCL) A 20-foot FCL container loaded with LyondellBasell Icorene 3545 BUE 5101 Linear Low Density Polyethylene bags, palletized, shrink-wrapped, and secured.
    Shipping LyondellBasell Icorene 3545 BUE 5101 Polyethylene, Linear Low Density is a non-hazardous thermoplastic resin. It is not DOT/IMDG/IATA regulated, requiring no UN number, class, or packing group. Ship in sealed bags, bulk bags, or bulk containers, palletized and dry, away from heat and ignition.
    Storage Store LyondellBasell Icorene 3545 BUE 5101 Polyethylene, Linear Low Density indoors in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original containers or bags closed and palletized to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and temperature extremes. Follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf life is typically 24 months when stored unopened in original packaging, cool, dry, well-ventilated, away from direct sunlight and heat.
    Application of LyondellBasell Icorene 3545 BUE 5101 Polyethylene, Linear Low Density

    LyondellBasell Icorene 3545 BUE 5101 is a UV-stabilised linear low-density polyethylene powder supplied for rotational molding. The typical nominal density is 0.934 g/cm³ per ISO 1183-1:2019, and the melt flow rate is 4.5 g/10 min at 190 °C/2.16 kg per ISO 1133-1:2022. The powder is ground to a controlled particle size distribution consistent with 35-mesh (500 µm) material used to fill mould ribs, undercuts, and back-drafted surfaces. Rotational molding processors generally specify peak internal air temperature from 190 °C to 210 °C depending on wall thickness, mould mass, and oven load, with oven set points between 280 °C and 320 °C. Prolonged internal air temperature above 220 °C can oxidise thick sections, increase gel formation, and reduce low-temperature impact performance.

    Potable water contact tanks are rotomoulded from 100 % virgin powder with a dry-blended LLDPE pigment masterbatch added at 2–4 wt% where colour coding is required. The dry blend is tumbled for 10–15 min before charging because a mismatch in masterbatch particle size can segregate during hopper transfer and produce localised colour streaking in thin corners and moulded-in fittings. The material is processed on biaxial rotational molding machines using a speed ratio of 3:1–4:1, with steel or cast aluminium moulds and sealed parting lines to limit internal air pressure variation. For a 6 mm nominal wall, oven cycle time is typically 25–40 min, with demoulding below 70 °C. Potable water contact compliance is evaluated under FDA 21 CFR §177.1520, food-contact migration under EU Regulation 10/2011, and system-level water contact under NSF/ANSI 61. Terminal products include rainwater harvesting tanks, potable water buffer vessels from 500 L to 10,000 L, and well-water storage tanks. Continuous exposure to chlorinated water above 3 ppm free chlorine at 60 °C may accelerate antioxidant depletion and shorten the service life of the moulded wall; published data for this specific configuration is limited.

    What Controls Chemical Permeation in Agricultural Sprayer and Fertiliser Tanks?

    Agricultural sprayer tanks require simultaneous resistance to environmental stress cracking and permeation from polar and nonpolar active ingredients. Icorene 3545 BUE 5101 is used in this application because the LLDPE architecture provides a broader interlamellar tie-molecule population than higher-density polyethylene grades, which delays crack propagation in contact with surfactant and ester solvent systems. The typical charge consists of resin plus 3–5 wt% carbon black or pigment masterbatch and, where release is required, 0.1–0.3 wt% of a polyolefin-compatible internal mould release. Exceeding 0.3 wt% is not recommended because additive migration can lower long-term environmental stress-crack resistance. Tanks are rotomoulded to wall thicknesses of 6–12 mm using a peak internal air temperature of 195–205 °C, with oven temperatures above 300 °C limited to the early heating phase to avoid thermal oxidation at sharp corners and drain bosses. Chemical resistance of the moulded parts is assessed by ASTM D543-21 and ISO 175:2010, while transport containers for agricultural chemicals may require UN certification under UN 1H1 or 31H1. Finished product types include tractor-mounted spray tanks from 600 L to 2,000 L, nurse tanks, and fertiliser hoppers. Continuous exposure to concentrated aromatic solvents above 40 °C is outside the operating boundary for this single-layer LLDPE configuration.

    When Diesel Fuel Contact Requires Vapour Pressure Management in Rotomoulded Tanks

    Diesel and hydraulic oil storage tanks rotomoulded from Icorene 3545 BUE 5101 are produced with wall thicknesses from 8 mm to 15 mm to meet creep and hydrostatic loading requirements. The formulation is generally 100 % resin with 2–3 wt% UV masterbatch and 0.2 wt% maximum internal mould release. In service, the tank wall is exposed to diesel vapour and condensate; oxygen diffusion through the amorphous phase and fuel absorption are controlled by wall thickness and crystallinity, with the density of 0.934 g/cm³ producing lower permeation than lower-density PE but not the barrier performance of PA- or EVOH-based multilayer structures. Process parameters for a 12 mm wall include an internal air temperature of 200–215 °C, forced air cooling to 85 °C, and water mist cooling to demould. Moulded-in inserts, baffles, and threaded fittings are placed before charging and are encapsulated during the melt densification phase. Standards include AS/NZS 4766 for polyethylene storage tanks, UN 31H1 for intermediate bulk containers, and ASTM D1998 for polyethylene upright storage tanks. Terminal products include auxiliary diesel tanks, hydraulic oil reservoirs, waste oil containers, and generator day tanks. This material is not recommended for continuous petrol or high-aromatic fuel exposure above 40 °C because wall softening and permeation increase rapidly beyond that threshold; published data for this specific configuration is limited.

    Outdoor playground panels and furniture shells are moulded with a dry-blend addition of 2–5 wt% weather-resistant masterbatch in an LLDPE carrier. The base resin already contains a hindered amine light stabilizer, so additional liquid UV absorbers are generally unnecessary unless the part is specified for high-altitude continuous sun exposure. The charge is processed in closed moulds with undercuts and return surfaces that require powder flow into cavities with depth-to-width ratios up to 1:3; the 35-mesh powder size distribution supports corner filling on shuttle and carousel machines. Rotational molding uses a peak internal air temperature of 185–200 °C for relatively thin 4–6 mm walls to avoid impact loss from over-cure. Compliance for heavy metal migration is evaluated under EN 71-3 and ASTM F963, structural safety of equipment under EN 1176 or ASTM F1487, and accelerated weathering under ISO 4892-2 cycle 1. Terminal product types include swing seats, tunnel sections, activity panels, and outdoor seating shells. Low-temperature impact tests are conducted under ISO 6603-2 because cracking at sub-zero temperatures is a known failure mode in constrained panels when wall thickness uniformity deviates by more than ±10 %.

    Outdoor Electrical Enclosures Demand Controlled Cooling Rates to Preserve Dimensional Stability

    Telecommunication and utility enclosures produced from Icorene 3545 BUE 5101 require flat mounting surfaces and moulded-in bosses that remain dimensionally stable after demoulding. The rotational molding charge includes 3–5 wt% carbon black masterbatch for UV opacity and, where electrostatic dissipation is specified, a conductive additive masterbatch at 8–12 wt%; however, the base grade is an insulating polyolefin and cannot be converted into a flame-retardant UL 94 V-0 system by dry blending. The process uses biaxial rotation ratios from 2:1 to 4:1, a peak internal air temperature of 195–205 °C, and a two-stage cooling profile: forced air from 205 °C to 95 °C at 3–5 °C/min, then water mist to 65 °C demoulding. Rapid water quenching is avoided because differential shrinkage across metal inserts and thick bosses induces warpage and can initiate microvoids around encapsulated hardware. Enclosures are evaluated for ingress protection under IEC 60529 to IP65, impact resistance under IEC 62262, and UV weathering under ISO 4892-2. Terminal products include base station shrouds, solar battery cabinets, and utility junction boxes. Published data for this specific configuration is limited with respect to internal heat release from electronics above 60 °C; continuous service above this temperature is outside the rated operating window.

    Vehicle and marine impact components manufactured from Icorene 3545 BUE 5101 use a single-layer wall with a dry-blend addition of 2–4 wt% carbon black or pigment masterbatch. For double-walled kayak hulls and buoyancy chambers, the outer layer is charged first and moulded to 6–9 mm, followed by a second powder charge for the inner skin at 3–5 mm; the interlayer is demoulded only after both skins have reached 190–205 °C internal air temperature. The process is run on shuttle or carousel machines with moulds rotated on two axes at non-integer speed ratios such as 3.3:1 to avoid repetitive powder paths. Low-temperature ductility is assessed by ASTM D638-14 tensile tests at −40 °C and by multi-axial impact under ISO 6603-2. Marine component compliance may include ISO 12215 for small craft structural evaluation, while automotive wheel arch liners and fender shells are specified to OEM material standards rather than a single public regulation. Terminal product types include kayak hulls, marine fenders, wheel arch liners, and heavy-duty toolbox shells. Wall thickness uniformity is governed by mould charging weight, oven time, and rotational speed, not by post-mould trimming, so operators must monitor bulk density variation between incoming powder lots under ASTM D1895 to maintain consistent shot weights.

    Free Quote

    Competitive LyondellBasell Icorene 3545 BUE 5101 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 3545 BUE 5101 is a butene-comonomer linear low-density polyethylene powder engineered for rotational moulding of hollow, double-walled, and complex-radius parts. The material is supplied as a free-flowing powder with a nominal density of 0.935 g/cm³ determined by ISO 1183-1 and a nominal melt mass-flow rate of 4.5 g/10 min at 190°C under 2.16 kg load according to ISO 1133-1:2022. These values place the grade in the low-density segment of the LLDPE rotomoulding range, where low-temperature ductility and environmental stress crack resistance are weighted more heavily than short-term stiffness. The BUE 5101 designation identifies a specific butene-based formulation and stabiliser package; it is not a generic polyolefin designation.

    Representative datasheet values for initial part design
    PropertyMethodValueUnit
    DensityISO 1183-10.935g/cm³
    Melt mass-flow rateISO 1133-1:2022, 190°C/2.16 kg4.5g/10 min
    Tensile stress at yieldISO 527-217MPa
    Tensile elongation at breakISO 527-2>600%
    Flexural modulusISO 178600MPa
    Environmental stress crack resistance, 10% IgepalASTM D1693 Condition A>1000h
    Vicat softening temperature, A50ISO 306116°C
    Melting temperature, DSCISO 11357-3127°C

    The representative values in the table are suitable for first-pass wall thickness and cycle time calculations; lot-specific certificates of analysis should be obtained for silicone-free food-contact or high-temperature service. Where a value is governed by a national regulatory certification, the certificate number takes precedence over the generic datasheet range.

    During powder charging, hopper flow uniformity is more important than pellet flow. Particle-size distribution for rotomoulding grades in this class is normally controlled from 250 µm to 710 µm, with fines below 150 µm limited to avoid dusting and electrostatic segregation. Dry flow is frequently measured on a funnel-type device under ASTM D1895; typical values of 25–35 s/100 g are expected for free-flowing powder, although each lot must be checked against the certificate of analysis because bulk density and particle-size distribution can shift during silo transport. Pneumatic conveying should be operated in dense phase below 10 m/s where possible; dilute-phase air velocities above 20 m/s can create fines and melt streamers in sections charged to a heated mould. When the powder is loaded into narrow ribs or high-detail mould areas, delayering and coarse segregation can occur if the powder is not dry-blended uniformly.

    In production-scale carousel, shuttle, and rock-and-roll machines, the powder is charged into fabricated steel or cast aluminium moulds rotating about two axes. The biaxial speed ratio is typically set between 2:1 and 4:1, with arm speed in the range 4–8 min⁻¹ depending on part diameter and wall thickness. Oven air temperatures of 270–310°C are common for single-layer parts of 4–10 mm nominal wall thickness. The peak internal air temperature is held at 190–210°C; this value is a more reliable indicator of the melt-state condition than oven setpoint because it reflects the actual heat accumulated by the mould and powder bed. During densification, the inner melt surface reaches approximately 220–250°C, and the powder sinters into a bubble-free layer under low-shear rotation. Cooling in forced air at 5–15 K/min is used to reduce warpage and to set dimensional stability; ejection should be delayed until the inner surface temperature has fallen below 80°C to limit shrinkage marks and part distortion.

    At process shear rates below 1 s⁻¹, the melt exhibits high-viscosity, low-elasticity flow that is not reflected by melt flow rate alone. Bubble removal in rotomoulding is controlled by this low-shear viscosity, not by the capillary viscosity at 100–1000 s⁻¹. In a rotating mould, air bubbles are rounded and compressed at the melt-vacuum interface; if the melt is too stiff at 190–210°C, the bubbles remain as spherical voids. The 4.5 g/10 min melt mass-flow rate of this grade gives a lower low-shear viscosity than a 2.0 g/10 min HDPE, which reduces the peak internal air temperature required for dense, pinhole-free skins. That lower peak internal air temperature also shortens cooling demand and reduces total cycle time by a limited amount; published data for this specific configuration is limited because cycle time depends primarily on metal mass and oven capacity.

    What Distinguishes Low-Density LLDPE from HDPE Rotational Moulding Powders?

    At the molecular level, the short-chain branching introduced by butene comonomer disrupts chain packing and reduces lamellar thickness relative to a homopolymer HDPE. The practical result is that the 0.935 g/cm³ grade has a flexural modulus of approximately 600 MPa by ISO 178, versus 800–1000 MPa for many 0.940–0.946 g/cm³ HDPE rotomoulding powders. The reduction in stiffness must be compensated in flat panels or tall tanks by ribbing, thicker walls, or a metal cradle; an unsupported flat wall of 4 mm will deflect more under hydrostatic pressure than the same wall in HDPE. The benefit is a strong increase in environmental stress crack resistance and low-temperature ductility. Notched constant-strain testing under ASTM D1693 Condition A in 10% Igepal shows greater than 1000 h, and the failure mode in sidewall impact testing is generally ductile rather than brittle at temperatures below -20°C. For moulders whose current HDPE tanks crack at moulded-in inserts or sharp weld lines, the switch to this lower-density grade often moves the failure location from a crack to a stretched zone; the part may yield but does not release its contents.

    Against conventional Ziegler-Natta butene LLDPE powders of similar density and melt flow, the formulation may have a different catalyst residue and stabiliser package, but the main performance difference is lot-to-lot consistency rather than a single physical property. Users should not interchange grades without checking dry flow, particle size distribution, and UV stabiliser content, because the same nominal density and melt flow rate can produce different sintering time in thin-wall parts. When a stiffer part is required, the usual substitution is not a different LLDPE but a 0.940–0.946 g/cm³ HDPE powder, with an accompanying increase in oven air temperature of 10–20 K and a longer cooling stage to control shrinkage.

    When Peak Internal Air Temperature Exceeds 210°C in Thick-Walled Parts

    Overheating the melt surface is the main process conflict in thick-walled rotomoulding. Sections above 12 mm require longer oven dwell to conduct heat into the powder bed, but the inner surface remains molten while the outer surface has already reached the degradation threshold. In open-flame or poorly circulated ovens, local air temperatures above 310°C can generate carbonyl species and odour; material degradation is detected as a rise in melt flow rate above 5.0 g/10 min by ISO 1133-1:2022 and a reduction in tensile elongation below 400% by ISO 527-2. Baffled hot-air ovens with a temperature spread of less than ±5 K across the mould are preferred. Nitrogen purging is not required when the grade is processed within the normal peak internal air temperature range, but venting at the parting line must be maintained to allow decomposition vapours to escape. If dark specks appear at the inner surface, the oven temperature should be reduced before cycle time is adjusted.

    For food-contact articles, the grade is represented by the supplier as suitable for evaluation under FDA 21 CFR 177.1520 and EU 10/2011. Because the finished rotomoulded part has low surface-to-volume ratios and may contain regrind layers, the converter is responsible for migration testing on the actual moulding. For chemically aggressive service, laboratory immersion in the intended fluid under ASTM D543 is used to determine whether the wall thickness is sufficient. Oxidising media, strong mineral acids, and low-molecular-weight aromatic hydrocarbons can plasticise or oxidise the material; continuous service above 60°C in such fluids is not recommended without long-term vessel testing. Outdoor weatherability is stabilised in the formulation; however, black or strongly pigmented dry-blend colours can alter heat absorption during heating and should be validated for each masterbatch level.

    Regrind of clean rotationally moulded parts can be incorporated up to 20 wt% when the particles are re-ground below 710 µm and dry-flow remains within lot limits. Higher levels of regrind, or regrind that has been subjected to repeated thermal cycles, can increase melt viscosity and produce pinholes at the inner surface. In double-wall parts with foam between skins, the grade is used as the structural skin layer; the core material must be selected so that its decomposition gases do not exceed the venting capacity of the mould. For marine buoyancy components and underground sumps, the part should be tested at the lowest service temperature, not at ambient laboratory conditions, because impact resistance decreases as temperature falls even if the material remains ductile well below -20°C.

    Top