Lyondellbasell Icorene 3545 Bue 5005 Polyethylene Linear Low Density

LyondellBasell Icorene 3545 BUE 5005 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 3545 BUE 5005 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 580281
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Density 0.945 g/cm³
    Melt Index 190 C 2 16 Kg 3.5 g/10 min
    Melting Point 130 °C
    Vicat Softening Temperature 115 °C
    Tensile Strength At Yield 16 MPa
    Tensile Strength At Break 25 MPa
    Elongation At Break 800%
    Flexural Modulus 600 MPa
    Hardness Shore D 60
    Dart Drop Impact 100 g
    Thermal Conductivity 0.33 W/m·K
    Specific Heat 2.3 J/g·°C
    Coefficient Of Linear Thermal Expansion 200 µm/m·°C
    Brittleness Temperature < -70 °C

    As an accredited LyondellBasell Icorene 3545 BUE 5005 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 3545 BUE 5005 LLDPE is packaged in 25 kg bags, 55 bags per pallet (1,375 kg).
    Container Loading (20′ FCL) 20′ FCL loading: LyondellBasell Icorene 3545 BUE 5005 Polyethylene, Linear Low Density; 25 kg bags, palletized, approx. 18–20 MT net.
    Shipping LyondellBasell Icorene 3545 BUE 5005 Polyethylene, Linear Low Density is a non-hazardous polymer resin. It is typically shipped in 25 kg moisture-barrier bags or bulk sacks, palletized and stretch-wrapped. Transport in clean, dry trucks, railcars, or containers, protected from heat, sunlight, moisture, and contamination. Follow supplier SDS and local regulations.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed and labeled. Avoid contact with strong oxidizers. Protect from moisture, dust, and contamination. Use original packaging; maintain clean, dry handling conditions. Prevent static discharge by grounding equipment where dust may accumulate. Follow all local regulations and SDS recommendations.
    Shelf Life Typically 24 months when stored unopened in original packaging in a cool, dry, well-ventilated area away from sunlight and heat.
    Application of LyondellBasell Icorene 3545 BUE 5005 Polyethylene, Linear Low Density

    LyondellBasell Icorene 3545 BUE 5005 is a linear low density polyethylene powder supplied for rotational moulding of single-wall and double-wall parts. The nominal density is 0.934 g/cm³ evaluated under ISO 1183-1:2019, and the melt flow rate is 4.5 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022. The selected downstream scenarios below are limited to documented rotomoulded product categories where medium stiffness, stress-crack resistance, and stabilizer package performance define the application window. Blown film, injection moulding, and extrusion coating are outside the grade’s design scope.

    When Peak Internal Air Temperature Exceeds 205 °C in Vertical Tank Moulding

    Potable water storage tanks produced by biaxial rotational moulding use shot weights calculated from finished wall thickness between 4.0 mm and 9.0 mm and powder bulk density of 0.40 g/cm³ to 0.48 g/cm³. The mould is charged without pre-drying if ambient relative humidity is below 60%; above 60% RH, the powder is pre-dried at 70 °C for 2 h to limit steam-induced pinholes at the inner wall. Oven set point is held at 290 °C to 300 °C, and the mould internal air temperature measured by radio telemetry is brought to 190 °C to 205 °C, with the peak internal air temperature held for 3 min to 5 min to complete particle coalescence. Exceeding 205 °C by more than 3 °C accelerates oxidative degradation at the inner surface, producing yellowing and a measurable reduction in environmental stress crack resistance under ASTM D1693-24 Condition B, 100% Igepal CO-630.

    Compliance for potable water contact is evaluated against ASTM D1998-21 for polyethylene upright and moulded tanks, NSF/ANSI/CAN 61-2023 Section 5.1 for health effects, and FDA 21 CFR 177.1520(c)(2.1) for olefin polymer food-contact status. A completed 1,000 L tank is hydrostatically tested to 1.5 times rated head pressure and inspected for creep deformation after 24 h. Published data for long-term chlorine resistance of this specific grade at elevated water temperatures is limited, so accelerated service testing at 50 °C in 2 ppm free chlorine is required before field approval.

    Compliance checklist for moulded potable water tanks
    RequirementStandard designationAcceptance criterion
    Density verificationISO 1183-1:20190.934 g/cm³ ± 0.003
    Melt flow rateISO 1133-1:20224.5 g/10 min at 190 °C/2.16 kg
    Food contactFDA 21 CFR 177.1520(c)(2.1)No migration above titre threshold
    Drinking water health effectsNSF/ANSI/CAN 61-2023Pass Section 5.1 extraction
    Tank constructionASTM D1998-21Hydrostatic 1.5 × rated head

    Formulation for outdoor potable water tanks blends 100 parts Icorene 3545 BUE 5005 with 0.25–0.50 parts HALS-based UV stabilizer masterbatch, 0.05–0.10 parts phenolic antioxidant, and 1.0–2.0 parts white or black pigment masterbatch carried in FDA-compliant polyolefin resin. The blend is dry-tumbled in a ribbon mixer at 40 rpm for 20 min before loading into a cast aluminium mould. The mould is rotated with a primary-to-secondary axis ratio of 4:1 and heated in a forced-air oven until the peak internal air temperature reaches 195 °C. Cooling is staged: forced air at 30 °C to 40 °C lowers the part surface to 120 °C, followed by water mist at 15 °C to 20 °C until demoulding at 70 °C. Direct water quenching from 120 °C produces differential shrinkage at the floor-to-wall junction; the air-to-water transition must occur after the crystalline plateau near 110 °C is crossed.

    Terminal finished product types include vertical cylindrical water storage tanks from 500 L to 20,000 L, rectangular transport tanks, and low-profile underground cistern liners. Bulkhead flanges, drain ports, and vented lids are either moulded as inserts or spin-welded after demoulding. Each tank is inspected under ASTM D1998-21 wall-thickness and weld sections, with ultrasonic checks at seam and corner regions.

    For agrochemical transport tanks moulded as single-piece shells, the formulation is adjusted for UV and chemical exposure by dry blending 100 parts Icorene 3545 BUE 5005 with 2.0–3.0 parts carbon black masterbatch, 0.50–1.0 parts HALS stabilizer masterbatch, and 0.05–0.10 parts phenolic antioxidant. Carbon black loading is limited to 3.0 wt% because higher loadings reduce impact strength and increase melt viscosity during particle coalescence. Rotational moulding equipment used is a three-arm independent turret machine with a swing diameter of 2.6 m; oven set point is 280 °C to 290 °C, and the part is removed after the internal air temperature has remained between 190 °C and 200 °C for 4 min. Fast water quenching is avoided because it lowers environmental stress crack resistance under ASTM D1693-24 Condition B from more than 1,000 h to below 300 h in the wall-to-base radius. Regulatory compliance for agrochemical service follows UN 31H1 intermediate bulk container testing under UN Model Regulations Chapter 6.5, supplemented by ADR packing group III requirements. The moulded shell is subject to a drop test at 1.2 m at -18 °C, a hydrostatic pressure test of 20 kPa for 10 min, and chemical compatibility immersion testing with the intended formulation. Terminal finished product types include 200 L to 10,000 L horizontal cylindrical tanks, conical bottom induction tanks, and bunded secondary containment assemblies.

    Does Polyurethane Foam Exotherm Warp the LLDPE Liner Below 95 °C?

    Insulated cooler shells are produced as two separate single-wall LLDPE liners rotomoulded on shuttle machines with steel moulds polished to SPI A-2 surface finish. The formulation for the food-contact liner uses 100 parts Icorene 3545 BUE 5005, 0.20–0.40 parts zinc stearate mould release, 0.05–0.10 parts antioxidant, and 1.0–2.0 parts white masterbatch. Wall thickness is held to 3.0 mm to 4.0 mm by shot-weight control, and the oven set point is 275 °C to 285 °C with a peak internal air temperature of 185 °C to 195 °C. After demoulding at 65 °C, the outer and inner shells are assembled into a fixture and rigid polyurethane foam with a free-rise density of 32 kg/m³ to 40 kg/m³ is injected into the cavity. The exothermic foam temperature must remain below 95 °C to prevent liner distortion; when exceeded, the inner shell collapses at the sidewall radii and the assembly is rejected for wall-thickness nonconformance. Compliance includes FDA 21 CFR 177.1520 for the LLDPE shell and EU 10/2011 migration testing where the liner contacts chilled food or beverage. Terminal finished product types are 20 L to 100 L insulated coolers, medical cold-chain shippers, and ice storage bins.

    Where returnable bulk bins are rotomoulded as one-piece boxes with stacking lugs and fork pockets, the formulation is 100 parts Icorene 3545 BUE 5005 with 0.10–0.20 parts antioxidant and 2.0–4.0 parts pigment masterbatch; the resin is processed on a 4-arm independent turret rotomoulding machine at an oven set point of 280 °C and a peak internal air temperature of 190 °C, with air cooling to 110 °C before demoulding, and the finished products are 250 kg to 1,200 kg capacity returnable bins, intermediate bulk containers, and slip-sheeted pallet boxes; compliance relies on EU 10/2011 and FDA 21 CFR 177.1520 where food ingredients are stored, and mechanical integrity is verified by ASTM D638-14 tensile yield of 15 MPa to 18 MPa and ASTM D790-17 flexural modulus of 550 MPa to 650 MPa.

    Exterior Furniture Components: HALS Loading and Cooling Fixture Design

    Exterior furniture components such as benches, planter shells, and play equipment panels are rotomoulded with a formulation that must pass accelerated UV aging without surface frosting. The blend contains 100 parts Icorene 3545 BUE 5005, 1.5–3.0 parts HALS stabilizer masterbatch, 0.05–0.10 parts antioxidant, and 2.0–4.0 parts pigment masterbatch; the exact ratio depends on the L*a*b* color target and the required 3,000 h xenon-arc exposure according to ASTM D2565-23 with no more than ΔE 3.0. Processing on an 3-arm carousel machine with a swing diameter of 2.4 m uses a 270 °C oven set point and a peak internal air temperature of 185 °C to 195 °C. Large flat panels warp if demoulded without restraint, so parts are transferred to water-cooled aluminium jigs that hold the rim within ±1.0 mm until the surface temperature drops below 80 °C. Compliance standards include EN 1176-1:2017 for playground equipment, ASTM F1487-21 for public play equipment, and REACH (EC) No 1907/2006 Annex XVII for polycyclic aromatic hydrocarbons; the grade itself does not contain intentionally added phthalates, but pigment masterbatches must be selected from REACH-compliant carriers. Terminal products are modular seating units, durable planters, outdoor playground panels, and equipment enclosures.

    In submersible flotation elements moulded from Icorene 3545 BUE 5005, the parts are produced as hollow single-wall shells with a wall thickness of 5.0 mm to 8.0 mm and closed-cell polyurethane fill. The rotational moulding formulation uses 100 parts resin, 0.20–0.50 parts antioxidant, and 1.0–2.0 parts UV stabilizer masterbatch; pigment masterbatch is limited to 1.0 part to avoid reducing long-term weld strength. The part is moulded on an independent-arm shuttle machine at an oven set point of 285 °C and a peak internal air temperature of 190 °C to 200 °C. After cooling and demoulding, the cavity is injected with two-component polyurethane foam to a density of 40 kg/m³ to 48 kg/m³. Compliance is assessed by ISO 4892-2:2013 for UV exposure and ASTM D638-14 for weld tensile strength; published data for this specific configuration is limited, so each batch requires a weld pull test on a moulded tag. Terminal finished product types include mooring buoys, aquaculture floats, and dredge pipeline flotation collars.

    Free Quote

    Competitive LyondellBasell Icorene 3545 BUE 5005 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 3545 BUE 5005 is classified as a linear low-density polyethylene resin supplied as a rotational-moulding powder. The product is an ethylene–butene copolymer carrying a stabilization package identified by the 5005 suffix. Nominal density is 0.934 g/cm³ and melt mass-flow rate is 5.0 g/10 min at 190 °C under 2.16 kg, determined according to ISO 1133-1:2022 and ISO 1183-1:2019. The resin is intended for low-shear rotational moulding of hollow articles in which uniform wall distribution, environmental stress-crack resistance, and low-temperature ductility are specified.

    The material is supplied as a powder rather than as pellets because dry-flow and bulk-density behaviour control how uniformly the resin distributes against the mould surface during biaxial rotation. Lot-to-lot evaluation therefore includes apparent bulk density, dry flow, and particle-size distribution. These powder characteristics are commonly screened using ASTM D1895-17 for apparent density and pourability and ASTM D1921-18 for sieve analysis. The grade is used in agricultural tanks, water-storage tanks, intermediate bulk containers, tool boxes, playground components, and general-purpose hollow parts with wall sections typically above 3 mm.

    Incoming powder control matrix
    ParameterMethodPurpose in lot qualification
    Melt mass-flow rateISO 1133-1:2022Confirms viscosity and sintering behaviour
    DensityISO 1183-1:2019Confirms crystallinity and stiffness baseline
    Apparent bulk densityASTM D1895-17 Method ADetects storage compaction or particle-shape variation
    Dry flowASTM D1895-17 Method BPredicts mould fill in narrow cavities
    Particle-size distributionASTM D1921-18Controls oversize and fine-particle defects

    What Rotational Moulding Variables Govern Wall-Thickness Uniformity and Porosity?

    In rotational moulding, the material undergoes a sintering sequence instead of screw plastication. The powder is loaded into a mould, heated in an oven, and rotated on two axes until a densified layer forms at the mould wall. Oven air temperatures for linear low-density polyethylene powders of this melt index are typically set between 280 °C and 320 °C. The more critical control variable is peak internal air temperature, commonly held between 220 °C and 260 °C depending on part mass and tooling. Published data for this specific product is limited, so transfer of these ranges to production should be validated with in-mould thermocouples and a temperature recorder mounted on the rotating arm.

    Wall-thickness distribution is governed by rotation ratio, mould surface finish, and powder dry-flow. On a carousel machine with biaxial rotation, the primary-axis speed and secondary-axis speed are frequently set at a ratio near 4:1 or 5:1, depending on part geometry. Cylindrical tanks tolerate lower secondary-axis speed, while box-shaped parts with deep draw require a higher secondary-axis ratio to prevent thin corners. If the powder exhibits low dry flow, it can accumulate in pockets or narrow ribs and produce sections below 3 mm even when nominal wall thickness is above 6 mm. When the supplier’s dry-flow value falls outside the range established for a given tool, the lot should not be used for complex moulds without a production trial.

    Porosity formation has three practical sources in this grade class: incomplete sintering, moisture or volatile entrapment, and bubble generation from polymer degradation. Incomplete sintering is corrected by increasing internal air temperature or oven residence time. Moisture entrapment is addressed by conditioning the powder and avoiding low-temperature condensation. If the powder is moved from a cold warehouse into a warm humid plant, surface moisture can generate steam during heating and form pinholes. Pre-drying is not normally required for polyethylene, but the resin should be conditioned to plant temperature and protected from relative humidity above 60% during open storage.

    Cooling rate creates a process conflict between cycle time and part quality. Slow air cooling produces lower residual stress and better dimensional stability but increases cycle time and may allow warpage in flat panels. Forced-air cooling shortens cycle time but may increase through-thickness crystallinity gradients and dimensional instability. Water-mist cooling provides the fastest solidification but can induce localised shrinkage in thick bosses and around inserts. Because butene-containing linear low-density polyethylene has lower crystallinity and slower crystallisation than high-density polyethylene, the cooling stage should not be shortened below the point at which the part can be demoulded without distortion. Mould release agents should be selected for compatibility with polyethylene; silicone-based releases may reduce surface gloss and interfere with post-mould trimming or welding.

    Differentiation against high-density and medium-density rotational-moulding grades is based on the relationship among density, stiffness, environmental stress-crack resistance, and low-temperature impact. High-density rotational-moulding polyethylene with density above 0.940 g/cm³ provides higher flexural modulus and surface hardness but lower environmental stress-crack resistance and lower impact at sub-zero temperatures. Medium-density grades in the range 0.935–0.940 g/cm³ occupy an intermediate position. The 0.934 g/cm³ nominal density of Icorene 3545 BUE 5005 therefore shifts selection toward parts in which sustained ductility and stress-crack resistance are more important than maximum rigidity. Tensile yield stress can be screened using ISO 527-2:2012, environmental stress-crack resistance using ASTM D1693-21 or ISO 16770:2019, and low-temperature brittleness using ASTM D746-20. Class-level data for butene-copolymer rotational-moulding powders at this density show tensile yield stress in the approximate range of 14–18 MPa and flexural modulus in the approximate range of 500–600 MPa, but the current supplier datasheet should be consulted for grade-specific values.

    Comonomer type also differentiates the grade from hexene- and octene-copolymer linear low-density polyethylene. Butene short-chain branching is less efficient at forming tie molecules, so at equal density and melt index a butene-copolymer resin may show lower puncture impact and environmental stress-crack resistance than a hexene- or octene-copolymer grade. For general-purpose rotational moulding at moderate wall thickness, the butene level in this product is balanced against processability and cost. Differences from pelletized injection-moulding linear low-density polyethylene are more pronounced: injection-moulding grades typically have melt mass-flow rates above 20 g/10 min and are not suitable for rotational moulding because they cannot form a stable powder layer under low-shear rotation. A rotational-moulding grade with 5.0 g/10 min melt mass-flow rate has higher molecular weight, longer relaxation time, and better bubble expulsion during low-shear sintering.

    Within the Icorene family, grade selection follows melt index and additive package. Lower-melt-index rotational-moulding grades may provide better toughness but require longer oven residence. Higher-melt-index grades fill fine detail more easily but may lose environmental stress-crack resistance and low-temperature impact. The BUE 5005 suffix identifies a specific butene-based stabilization package; users comparing this product to another Icorene grade should not assume identical ultraviolet resistance or thermal stability. If outdoor weathering is required, accelerated testing under ASTM G154-23 or ISO 4892-3:2016 should be performed on moulded plaques, and the results compared against the intended service life in the target climate. Published data for this specific package is limited in public databases, so qualification should rely on the supplier’s current technical data sheet and weathering certificate.

    When Regulatory Compliance and Chemical Resistance Both Constrain Compound Selection

    The base polyethylene belongs to the polyolefin class addressed by US FDA 21 CFR 177.1520 and by European Union Regulation 10/2011 for food-contact plastics. A food-contact statement is not automatically transferred to the finished article: the final part must be evaluated for migration under the intended food type, contact time, temperature, and regrind content. For US conditions, the article should meet the specifications and extractive limitations of 21 CFR 177.1520(c) for olefin polymers where applicable. For EU conditions, overall migration and specific migration limits under Regulation 10/2011 apply. REACH compliance under Regulation 1907/2006 and RoHS compliance under Directive 2011/65/EU are generally addressed by the supplier for the unpigmented base powder, but colourants, processing aids, and post-mould additives can alter the final regulatory status.

    Chemical resistance is concentration- and stress-dependent. Polyethylenes of this density absorb little water and resist many aqueous acids, bases, and polar solvents at ambient temperature, but aliphatic and aromatic hydrocarbons cause swelling and loss of tensile properties. For storage tanks exposed to aggressive liquids, the product should not be qualified by immersion alone; stress-crack resistance under the actual chemical and temperature is required. ASTM D1693-21 uses a bent strip and a surfactant to rank environmental stress-crack resistance, while ISO 16770:2019 provides a full-notch creep test that is more sensitive for higher-density and medium-density materials. Published data for Icorene 3545 BUE 5005 in aggressive fluids is limited; qualification should therefore be performed on moulded plaques or prototype bottles at the maximum service temperature and stress.

    Thermal stabilizer retention is measured by oxidation induction time. The relevant method is ISO 11357-6:2018 under oxygen at 200 °C or another agreed temperature. Rotational moulding consumes antioxidant because the polymer is held at high internal air temperature for extended periods. Repeated recycling of regrind can reduce oxidation induction time and should be controlled by the moulder. The 5005 package is intended to provide weathering resistance, but ultraviolet protection is not indefinite. For outdoor products, accelerated weathering testing should be performed under ASTM G154-23 using UVA-340 or UVB-313 lamps, or ISO 4892-3:2016 with fluorescent ultraviolet sources. The change in tensile elongation should be monitored by ISO 527-2:2012. If the part is coloured with an external masterbatch, the pigment and carrier resin may change weathering and food-contact status.

    At the incoming-quality-control stage, the rotational moulder should measure melt mass-flow rate and density on each lot, but these two values alone do not capture powder behaviour. Bulk density and dry flow can differ between production campaigns even when melt index and density remain within specification. A lot with acceptable nominal density and melt mass-flow rate but poor dry flow can generate thin walls, porosity, and poor surface detail on moulds with narrow ribs. When parts with wall sections below 3 mm are produced, an incoming powder sieve analysis can be used to set an upper limit on fines below 150 µm. Excess fines can reduce dry flow and may increase dust exposure during mould charging. If such a limit is not provided by the supplier, the moulder should establish it by production trial.

    Storage and handling boundaries also affect processing. The powder should be kept in sealed containers away from direct sunlight and stored below 50 °C. Open storage in a high-humidity plant should be avoided; if condensation forms on the powder surface, the steam generated during heating produces pinholes and rough internal surfaces. The product is not compatible with strong oxidizing agents at elevated temperature, and it should not be dry-blended with additives that decompose below the peak internal air temperature used in rotational moulding. If a colour masterbatch is added, it should be selected for rotational moulding and should not increase viscosity to the point that bubble removal is compromised. Addition level should be kept within the masterbatch supplier’s recommended range, typically below 5% by weight; higher loadings may alter dry flow and reduce impact properties.

    For equipment qualification, carousel machines with multiple arms allow the same mould to be processed at different heating and cooling stations. The temperature profile should be recorded on the rotating arm because internal air temperature can differ from the oven set point by more than 20 °C depending on oven efficiency and mould mass. A production trial should evaluate at least three peak internal air temperatures to identify the lower boundary for complete sintering and the upper boundary for oxidation. Moulded parts should be sectioned for wall-thickness uniformity and tested at the minimum service temperature. For flat plaques, multiaxial impact resistance can be measured using ISO 6603-2 or ASTM D3763. Published data for this specific product under those methods is limited, so test conditions should be fixed by the end-use specification rather than taken from general polyethylene literature.

    Top