| HS Code | 435599 |
| Density | 0.935 g/cm³ |
| Melt Flow Rate | 3.5 g/10 min (190°C/2.16 kg) |
| Melting Point | 125 °C |
| Vicat Softening Point | 108 °C |
| Tensile Strength At Yield | 12.1 MPa |
| Tensile Strength At Break | 20.0 MPa |
| Elongation At Break | 800% |
| Flexural Modulus | 310 MPa |
| Hardness Shore D | 55 |
| Tear Strength | 200 g/mil |
| Dart Drop Impact | 120 g |
| Haze | 10% |
| Gloss | 80% |
As an accredited LyondellBasell Icorene 3545 BEI 2142 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 3545 BEI 2142 LLDPE is supplied in 25 kg polyethylene-lined paper bags, palletized, or 1,000 kg bulk bags. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with LyondellBasell Icorene 3545 BEI 2142 Linear Low Density Polyethylene, securely stowed and sealed for shipment. |
| Shipping | LyondellBasell Icorene 3545 BEI 2142 Polyethylene, Linear Low Density is shipped as a non-hazardous plastic resin in 25-kg bags, octabins, or bulk containers. It should be kept dry and away from heat, sunlight, and moisture. Transport is not regulated by DOT, IMDG, or IATA; standard cargo handling applies. |
| Storage | Store in a cool, dry, well-ventilated warehouse at ambient temperature, away from direct sunlight, heat, ignition sources, and strong oxidizing agents. Keep original containers or bags closed, off the floor on pallets, protecting from moisture, contamination, and physical damage. Avoid excessive stacking. Maintain good housekeeping to prevent dust accumulation and slipping. Follow local regulations, SDS, and first-in, first-out stock rotation. |
| Shelf Life | Shelf life is typically 12 months from production date when stored unopened in original packaging in cool, dry conditions away from direct sunlight. |
Rotational moulding converts this linear low-density polyethylene powder only after particle size distribution is controlled to 35–65 mesh (500–250 µm) with dry flow measured at 28–32 s/100 g under ISO 6186:1998. The dry-blend formulation for outdoor storage articles consists of 100 parts Icorene 3545 BEI 2142 powder, 0.05–0.15 phr hindered phenolic antioxidant, 0.05–0.20 phr HALS stabiliser, and 0.5–2.0 phr colour concentrate; no processing aid is added because fluoropolymer-based aids reduce inter-particle sintering and create microvoids at the inner surface. Compliance for potable-water tanks is assessed under FDA 21 CFR 177.1520 extractables limits, EU Regulation No 10/2011 overall migration limit of 10 mg/dm², NSF/ANSI 61 for cold-water contact, and ASTM D1998-15 for upright polyethylene storage tanks. Agricultural chemical tanks require UN dangerous goods compatibility testing according to ADR 6.1.5.2.4 or equivalent. On a four-arm carousel machine with aluminium moulds, the mould is charged to a shot weight calculated to give 6–8 mm nominal wall, then rotated at 4:1 primary and 2:1 secondary gear ratios. Oven air temperature is held at 280–300 °C with forced-air velocity 1.5–3.0 m/s; peak internal air temperature must reach 190–205 °C for complete sintering, while exposure beyond 210 °C causes oxidative embrittlement at the inner surface. The cooling track follows a two-step sequence: forced air at 8–12 °C/min to 70–80 °C, then water mist or ambient cooling to mould release. Terminal articles produced under this regime include vertical chemical storage tanks, water contact tanks, agricultural sprayer tanks, playground components, and enclosures for water treatment equipment.
Powder storage before moulding requires closed hoppers at 60% RH maximum; if moisture uptake exceeds 300 ppm, pre-drying at 60–70 °C for 2–3 h is required to prevent pinholes. Batch-to-batch variance in dry flow larger than 2 s/100 g has been observed to increase wall thickness variation to more than 8% on 6 mm walls. In-plant scrap regrind is limited to 15 wt% because higher levels increase melt flow instability and puncture impact variance under ISO 6603-1:2000.
| Rotational moulding variable | Lower bound | Upper bound | Failure mode outside the band |
|---|---|---|---|
| Oven air temperature | 280 °C | 300 °C | incomplete sintering below; inner-surface oxidation above |
| Peak internal air temperature | 190 °C | 205 °C | inter-particle porosity; oxidative embrittlement |
| Cooling rate | 8 °C/min | 12 °C/min | warpage; excessive crystallinity development |
| Demoulding temperature | 70 °C | 80 °C | part distortion; forced release marks |
Injection moulding thin-wall food-contact containers and distribution closures
Because thin-wall packaging requires a balance between low-temperature ductility and processability, injection moulding of Icorene 3545 BEI 2142 is configured around a blend ratio of 85–95 wt% Icorene 3545 BEI 2142 with 5–15 wt% high-pressure LDPE to reduce shear heating and improve surface gloss; slip and antiblock additives are incorporated at 800–1,500 ppm each, while a clarifying/nucleating package is limited to 0.10–0.25 wt% because higher levels lower haze-free impact. Regulatory compliance for food-contact containers and caps is evaluated under FDA 21 CFR 177.1520, EU Regulation No 10/2011 with an overall migration limit of 10 mg/dm², and EN 71-3 when the article may be handled by children. The downstream process runs on a hydraulic toggle injection moulding machine with clamp force of 120–250 t, a general-purpose 40 mm screw with 20:1 L/D, check-ring tip 3 mm stroke, and rectangular gate dimensions of 0.8–1.2 mm thickness. Melt temperature is kept at 200–230 °C; mould temperature is set to 10–30 °C to minimize crystallinity-induced shrinkage without producing sink marks. Injection speed is set at 80–120 mm/s, followed by holding pressure of 40–60 MPa for 6–10 s per 1.0 mm nominal wall, and cooling time of 8–15 s for a 1.5 mm wall. Terminal finished products include thin-wall circular lids, stackable food storage containers, caps for non-carbonated beverages, housewares, and toy components requiring ductile failure.
When this linear low-density polyethylene is run alone on continuous extrusion blow moulding equipment, severe parison sag occurs; therefore, the material is formulated as 75–85 wt% Icorene 3545 BEI 2142 and 15–25 wt% high-density polyethylene with a melt index of 0.3–1.0 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022. Colour or UV protection is supplied through 1–3 wt% masterbatch; for black articles, carbon black content in the final article is held below 2.5 wt% to avoid loss of impact strength. Regulatory compliance is established under FDA 21 CFR 177.1520 for food-contact appearances, EU Regulation No 10/2011 for overall migration testing using EN 1186-1:2002, and EN 71-3 for hollow articles intended for children. The downstream process uses a shuttle blow moulding machine with a 65 mm extruder 24:1 L/D, accumulator head volume 1.0–1.5 L, die head temperature 190–210 °C, die gap 0.8–1.4 mm, parison drop time less than 3.5 s, blow pressure 0.60–0.75 MPa, and mould temperature 10–25 °C. Terminal outputs include collapsible containers, industrial bellows, hollow insulated panels, and light-load dunnage bladders.
Masterbatch carrier resin for pigment and additive concentrates
As a carrier for polyolefin masterbatches, Icorene 3545 BEI 2142 is used at 65–80 wt% with 20–35 wt% pigment or additive; high-carbon-black formulations may load to 35–40 wt% only when a twin-screw side feeder and a long distributive mixing section are available. Regulatory compliance follows REACH (EC) No 1907/2006 registration/notification duties and RoHS Directive 2011/65/EU where electrical or electronic goods may be involved; no food-contact claim is conferred by the masterbatch itself. The downstream compounding process uses a co-rotating twin-screw extruder with 40:1 L/D, side-feeder at 28–32 L/D, screw speed 300–500 rpm, melt temperature 190–220 °C, vacuum venting at -0.08 MPa, and underwater pelletizing to 3–4 mm nominal diameter. Terminal finished products are colour concentrates and additive masterbatches for let-down in rotational moulding, blow moulding, injection moulding, and film extrusion. The material is not recommended as a sole carrier for hydrolytically sensitive additives requiring pre-dried polar resins.
In multi-material flexible packaging, extrusion lamination and coating of this resin onto paperboard and aluminium foil is carried out with a formulation of 70–85 wt% Icorene 3545 BEI 2142 and 15–30 wt% autoclave LDPE to reduce neck-in and improve melt draw; when foil adhesion is required, a separate tie layer of ethylene-vinyl acetate or ethylene-acrylic acid containing 8–12 wt% comonomer is coextruded at 10–15 wt% of total coating weight. Compliance for food-contact paperboard and aluminium laminates is assessed under FDA 21 CFR 176.170(c) for paper components, EU Regulation No 10/2011, and EN 1186-1:2002 migration testing; converters must verify that the final laminate meets specific food type and temperature conditions. The downstream process uses a tandem extrusion laminating line with a 90 mm extruder 28:1 L/D, T-die gap 0.7–1.0 mm, melt temperature 265–295 °C, and line speed 80–220 m/min; corona or ozone pretreatment must raise the substrate surface energy to 42–48 mN/m immediately before the nip. Terminal finished products include coated paperboard trays, multi-material sachets, aluminium-foil laminates, and industrial wrapping substrates requiring low-temperature flex crack resistance.
| Application zone | Primary standard | Test method / clause | Typical acceptance criterion |
|---|---|---|---|
| Rotational moulded tanks | ASTM D1998-15 | wall thickness and low-temperature impact | nominal wall ± 10%; no brittle failure below -18 °C |
| Injection moulded food contact | FDA 21 CFR 177.1520 / EU 10/2011 | overall migration method EN 1186-1:2002 | 10 mg/dm² |
| Extrusion blow moulded hollow parts | EN 71-3 | element migration from toy materials | limits by element category |
| Masterbatch carrier | REACH (EC) No 1907/2006 | substance registration / notification | SVHC content < 0.1 wt% where applicable |
| Extrusion lamination | FDA 21 CFR 176.170(c) | paper/paperboard component migration | food-type and temperature conditions |
Competitive LyondellBasell Icorene 3545 BEI 2142 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 3545 BEI 2142 Polyethylene, Linear Low Density is identified in supplier documentation as a linear low density polyethylene resin. The grade designation alone does not convey the complete thermal, rheological, or stabilisation profile, and lot-specific values must be obtained from the certificate of analysis before material is transferred into production silos. Incoming inspection for this resin class typically includes density by ISO 1183-1:2019, melt mass-flow rate by ISO 1133-1:2022 at 190 °C/2.16 kg, and tensile properties by ISO 527-2:2012. The suffix BEI 2142 is interpreted as a supplier-specific additive or stabilisation variant, not as a public specification; the product technical bulletin should be consulted for antioxidant, processing-aid, and antiblock loadings. Because linear low density polyethylene differs from high-pressure low density polyethylene in shear-thinning behaviour, extrusion settings derived from LDPE campaigns cannot be transferred directly to this grade without pressure and motor-load verification.
On coextrusion lines producing three-layer or five-layer barrier film, high-pressure LDPE is often included for melt strength and bubble stability. The LLDPE class represented by Icorene 3545 BEI 2142 supplies higher tensile strength and elongation at equivalent film thickness, but the melt tension is lower if long-chain branching is absent. This trade-off is observed at the die exit: the LDPE-rich bubble resists neck-in and draw resonance, while the LLDPE-rich film requires a lower frost-line position or higher blow-up ratio to maintain gauge uniformity. Processors may compensate by blending the LLDPE with LDPE at addition levels of 10 % to 30 % by mass, but the blend ratio must be validated for seal initiation temperature and haze according to ASTM D1003-13.
Compared with an HDPE grade of similar melt flow, the lower density of this linear low density product reduces flexural modulus and increases environmental stress-cracking resistance in finished articles. That distinction is relevant for flexible packaging and lamination structures where sealing force, puncture resistance, and ESCR are jointly specified. However, published data for this specific Icorene 3545 BEI 2142 formulation is limited; comparative lot testing under ASTM D1693-21 should be performed before replacing an HDPE or MDPE grade in a load-bearing package or laminated pouch.
Single-screw conveying of Icorene 3545 BEI 2142 depends on the confirmed melt mass-flow rate, not on the grade number. Barrier-flighted screws with 30:1 to 36:1 L/D ratios and Maddock mixing sections are used to complete additive dispersion and to flatten melt-temperature gradients. Barrel temperature profiles are set with a hopper zone near 180 °C and a die temperature of 220 °C to 230 °C. If melt pressure measured before the screen pack shows variation greater than 0.5 MPa over a 2-minute interval, screw-induced surging or inconsistent feed is indicated. The resin’s viscosity-shear curve is flatter than that of LDPE, so screw-speed increases do not reduce viscosity as rapidly; motor torque and melt temperature must be monitored rather than assuming LDPE-like behaviour.
For cast film lines using slot dies and chill-roll haul-offs, die gaps are normally set between 0.5 mm and 1.0 mm. Melt temperature at the die exit is kept below 240 °C to reduce gel formation. Because LLDPE crystallises rapidly after contact with a chill roll, roll temperature and web tension control film flatness and blocking. For blown film, a blow-up ratio of 2.2:1 to 2.8:1 is a common starting point, with frost-line height adjusted to stabilise the bubble. These parameters are not grade-specific and must be refined with the supplier’s processing guide and lot-specific melt index.
If screw speed is increased to raise output without corresponding adjustment of barrel temperatures, shear heating can elevate melt temperature above 230 °C. In stabilised LLDPE, oxidative degradation may not be immediately visible, but gel counts and odour levels can drift upward over a shift. Operators should measure melt temperature immediately after the screw tip and compare it with the die setpoint; a difference greater than 8 °C to 12 °C indicates excessive viscous dissipation. At that point, a reduction in screw speed or a change to a lower-compression screw is more effective than lowering die temperature. The onset of shark-skin melt fracture on the film surface is not corrected by die-temperature manipulation alone; it requires a die-lip shear-rate reduction or the addition of a fluoropolymer process aid if approved by the supplier.
The stabilisation package indicated by the BEI 2142 suffix influences oxidative resistance but not the intrinsic rheology of the polyethylene backbone. During long runs on blown film lines, annular dies or fixed-lip dies may accumulate low-molecular-weight species and stabiliser decomposition products. Cleaning frequency is therefore a function of both the additive package and the extrusion temperature history. A documented purging procedure using a commercial polyethylene purge compound is recommended before colour changes or shutdowns. Since exact additive loading is not publicly disclosed, the safety data sheet and product technical bulletin control storage and handling practices.
Tensile testing of film produced from Icorene 3545 BEI 2142 is performed according to ISO 527-2:2012 using 15 mm-wide strip specimens or Type 1B dumbbells. Machine-direction and transverse-direction specimens are conditioned at 23 °C ± 2 °C and 50 % ± 5 % relative humidity for at least 40 h before testing. A loss of machine-direction yield stress exceeding two standard deviations from the control-lot average indicates orientation imbalance or thermal degradation. Puncture resistance is evaluated under ASTM D5748-19 or ISO 7765-1; because published data for this specific configuration is limited, converters must establish internal control ranges before converting this grade into high-speed packaging lines.
Heat seal initiation temperature is another critical difference among LLDPE grades. The seal initiation temperature depends on comonomer type and density; lower density shifts seal initiation lower but reduces stiffness. If this grade is used on form-fill-seal lines, the seal bar temperature setpoint must be optimised using a heat-seal range test such as ASTM F2029-16 to map seal strength against temperature. The supplier may disclose the comonomer type for this grade; if not, thermal fractionation or GPC-FTIR can characterise the short-chain branching distribution. Additive-package interactions can alter seal strength through bloom, so seal testing should be performed on actual production film, not on compression-moulded plaques.
Regulatory status must be confirmed with the manufacturer. If the grade is supplied as compliant with EU 10/2011, overall migration testing must meet the limit of 10 mg/dm² in food-contact applications, and specific migration limits for additives must be reviewed. For United States food-contact use, FDA 21 CFR 177.1520 covers olefin polymers under specified conditions of use, but the product name alone does not constitute approval. REACH and RoHS declarations should be requested as part of supplier documentation for electrical or electronic components.
Incoming inspection and reference test methods for this LLDPE grade are summarised below. These methods represent common specification points; more restrictive internal methods may be required for critical film or packaging structures.
| Property | Test Standard | Conditioning or Test Condition | Reported Unit |
|---|---|---|---|
| Density | ISO 1183-1:2019 | Gradient column at 23 °C | kg/m³ |
| Melt mass-flow rate | ISO 1133-1:2022 | 190 °C, 2.16 kg | g/10 min |
| Tensile stress at yield | ISO 527-2:2012 | Type 1B, 50 mm/min | MPa |
| Elongation at break | ISO 527-2:2012 | Type 1B, 50 mm/min | % |
| Haze | ASTM D1003-13 | 50 µm film specimen | % |
| Puncture resistance | ASTM D5748-19 | Conditioned at 23 °C ± 2 °C | N or mJ/µm |
Certificate-of-analysis parameters for Icorene 3545 BEI 2142 should include lot number, production date, density, melt mass-flow rate, and any additive dispersion indicator. Batch-to-batch variance in LLDPE can arise from comonomer distribution shifts even when the average density remains constant; film toughness and seal temperature may therefore move before density or melt flow move outside control limits. For this reason, converter specifications should include a reference lot for thermal analysis by differential scanning calorimetry using ISO 11357-3.
If the LLDPE contains only short-chain branches from butene, hexene, or octene, its melt relaxation behaviour differs from LDPE containing long-chain branches. This difference is visible in the onset of draw resonance during extrusion coating and in the melt strength during blow moulding. Thermal stability can be assessed by differential scanning calorimetry according to ISO 11357-3, but oxidative induction time by ISO 11357-6 gives a better indication of additive-package performance. Published data for this specific formulation is limited; laboratories must run identical reference resins before setting release criteria.
Polyethylene pellets should be stored in closed silos or hoppers protected from direct UV exposure and condensation. Pre-drying is generally not required for LLDPE unless surface moisture is visible or the material has been stored at relative humidity above 60 % in unheated warehouses. Avoid combining this grade with amine-based additives that are not approved by the supplier, because unexpected catalytic residues can interact with stabiliser packages. Equipment purging and screw removal procedures should follow the resin manufacturer’s processing guide.
The numeric portion 3545 is a series descriptor and is not a replacement for melt-flow data. Processors must not assume a specific melt-flow index or density without the certificate of analysis. When changing from an existing LLDPE grade, the first tests should be density and MFR, followed by melt rheology with a capillary rheometer under ISO 11443:2021. Viscosity curves at representative shear rates from 100 s⁻¹ to 1000 s⁻¹ reveal whether screw speed and die pressure will remain within acceptable limits. If the viscosity at 1000 s⁻¹ is more than 10 % below or above the existing grade, screw and die settings may require adjustment before startup.
If this grade is directed to injection moulding, the processing window differs from film extrusion. Melt temperature may be set between 200 °C and 230 °C, but hold pressure and cooling time are adjusted for the lower crystallinity of LLDPE. Published data for this specific Icorene grade in injection moulding is limited; trials should verify shrinkage, warpage, and ESCR before production release.