Lyondellbasell Icorene 3545 As Blk 9001 Polyethylene Linear Low Density

LyondellBasell Icorene 3545 AS BLK 9001 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 3545 AS BLK 9001 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 356645
    Density 0.935 g/cm³
    Meltflowrate 0.70 g/10 min (190°C/2.16 kg)
    Tensilestrengthatyield 10.3 MPa
    Tensilestrengthatbreak 17.2 MPa
    Elongationatbreak 700%
    Flexuralmodulus 0.310 GPa
    Hardnessshored 50
    Vicatsofteningtemperature 105 °C
    Brittlenesstemperature -70 °C
    Meltingtemperature 125 °C
    Dielectricconstant 2.30
    Dissipationfactor 0.00020
    Volumeresistivity 1.00e+15 ohm·cm
    Dielectricstrength 20.0 kV/mm
    Thermalconductivity 0.350 W/m·K
    Coefficientoflinearthermalexpansion 1.50e-4 1/°C
    Specificheat 1.90 J/g·°C

    As an accredited LyondellBasell Icorene 3545 AS BLK 9001 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 3545 AS BLK 9001 Polyethylene, Linear Low Density is supplied in 25 kg bags, 40 bags per pallet, shrink-wrapped.
    Container Loading (20′ FCL) 20′ FCL container loaded with LyondellBasell Icorene 3545 AS BLK 9001 Linear Low Density Polyethylene, securely stowed for ocean transport.
    Shipping LyondellBasell Icorene 3545 AS BLK 9001 Polyethylene, Linear Low Density is a non-hazardous thermoplastic resin. Ship in sealed bags, octabins, or bulk containers. Store dry, away from ignition sources and extreme heat. Not regulated for transport under DOT, IMDG, or IATA. No UN number, hazard class, or packing group required.
    Storage Store in a cool, dry, well-ventilated area away from heat, sparks, flames, and direct sunlight. Keep original containers closed to prevent moisture, dust, and contamination. Avoid strong oxidizers. Ground equipment to control static. Maintain clean handling areas and avoid physical damage. Do not store near food, feed, or drinking water. Follow SDS and local regulations. Use appropriate PPE. Inspect containers regularly.
    Shelf Life Shelf life is typically 24 months when stored cool, dry, ventilated, away from direct sunlight in unopened original packaging.
    Application of LyondellBasell Icorene 3545 AS BLK 9001 Polyethylene, Linear Low Density

    Continuous biaxial rotation of an aluminum mold charged with 100% LyondellBasell ICORENE 3545 AS BLK 9001 powder is the standard starting condition for rotomolded agricultural chemical storage vessels. In this application, the as-supplied black LLDPE powder is processed without additional carbon black or UV masterbatch; the built-in black pigmentation contributes to weathering resistance in outdoor exposure. The addition ratio is restricted to 0–15 wt% clean internal regrind from the identical grade, and regrind exceeding 15 wt% requires tensile and environmental stress-cracking resistance revalidation because the antioxidant and UV stabilizer residue in reclaimed powder differs from virgin feed. Oven setpoint is maintained between 290 °C and 315 °C, with peak internal air temperature typically between 190 °C and 210 °C; exceeding 220 °C peak internal air temperature for this LLDPE class produces inner-wall oxidation and measurable loss of low-temperature impact. Cooling is sequenced as forced air for the first 10–15 min, followed by water mist on the aluminum mold shell; localized cooling at mold corners is controlled to avoid differential shrinkage that causes warpage at the tank base. The governing product standard is ASTM D1998-21, which specifies minimum wall thickness, drop impact, and environmental stress-cracking resistance for polyethylene upright storage tanks; chemical resistance screening follows ASTM D543 immersion with the specific pesticide formulation or fertilizer salt solution, and secondary containment installations for listed hazardous agricultural chemicals reference 40 CFR 264.193. Terminal product types include sprayer tanks from 200 L to 2,500 L, nurse tanks, fertigation reservoirs, and secondary containment basins produced by carousel and shuttle rotational molding machines with cast aluminum or fabricated steel molds.

    How Does Rotational Molding Control Wall Thickness in Chemical IBC Liners?

    For intermediate bulk container bottles and industrial liquid liners, the primary process conflict is maintaining a dimensionless wall-thickness uniformity index above 0.85 across vertical sidewalls while meeting UN Model Regulations Chapter 6.5 drop-test and leak-test criteria. The mold is charged with a predetermined shot weight calculated from surface area multiplied by target wall thickness and powder bulk density; for a nominal 5.0 mm wall, the shot weight is fixed during mold qualification and is not adjusted by simple cycle-time compensation. The formulation is 100% ICORENE 3545 AS BLK 9001 for first-generation liners; addition of clean in-house regrind is allowed up to 20 wt% only when the reclaim is generated from the same grade and the bottle qualification has been repeated under ISO 16101:2010 chemical compatibility testing. The rotational molding cycle runs at an oven temperature of 270 °C to 300 °C with a rotation ratio of 4:1 primary-to-secondary axes; peak internal air temperature is held at 180 °C to 200 °C for densification, after which forced-air cooling at an average mold surface cooling rate of 0.5–1.0 °C/s reduces warpage and sink marks around the fill port. If the liner is intended for food-contact intermediate storage, the fabricated bottle qualifies under FDA 21 CFR 177.1520 for olefin polymers. Terminal product types include 1,000 L rotomolded IBC bottles, cylindrical process liners, mild acid and alkali dosing tanks, and bulk liquid containers for cosmetic and food intermediate transport.

    Saltwater immersion testing of rotomolded polyethylene floats under cyclic wave loading places a premium on low-temperature impact retention and resistance to stress cracking in continuously deflected shells. For black grade ICORENE 3545 AS BLK 9001, the material is processed as 100% as-supplied powder for buoyancy-critical parts; regrind is limited to 0–10 wt% and is excluded entirely for hollow units that are post-filled with rigid closed-cell polyurethane foam, because the foam exotherm and subsequent mechanical load can expose reclaim-induced inconsistencies at knit lines. The rotational molding cycle uses a rock-and-roll machine for long cylindrical pontoons or a shuttle machine for multi-cavity buoy floats; mold oven temperature is held between 275 °C and 305 °C, and the part is demolded below 60 °C to avoid permanent set in flat areas intended for mechanical fastening. Product-level acceptance testing is normally based on water absorption below 0.01% per ASTM D570, notched Izod impact at -20 °C per ASTM D256, and weathering resistance after 1,000 h of UV exposure per ASTM G154. Published data for this exact black marine float configuration is limited; qualification programs therefore combine laboratory aging with full-section compression and buoyancy-loss testing. Terminal product types include floating dock floats, wave attenuator segments, aquaculture pen floats, and channel marker buoys.

    Wall-Stock Integrity in Rainwater Harvesting Cisterns

    Potable and rainwater contact applications shift the qualification burden from mechanical strength alone to extraction and residual stress control. The resin is charged neat at 100 wt% for potable-water contact surfaces; if regrind is used at all, it is capped at 15 wt%, drawn only from the same NSF/ANSI 61-listed material, and excluded from surfaces above the water line where long-term UV exposure is greatest. Rotational molding of cistern shells from 500 L to 50,000 L uses cast aluminum molds with inserts for threaded fittings and inspection ports; peak internal air temperature is controlled to 185–205 °C, and the cooling rate is kept below 0.5 °C/s for large flat panels to avoid sink marks around inserts and to reduce residual hoop stress that can later initiate environmental stress cracking. The governing potable-water compliance standard is NSF/ANSI 61, with additional material qualification under ASTM D1998-21 for upright storage tanks and extraction limits under U.S. FDA 21 CFR 177.1520 where required. Terminal product types include above-ground and underground rainwater cisterns, potable water storage tanks, and fire suppression water buffer tanks, with wall thicknesses commonly between 6 mm and 20 mm depending on tank diameter and burial load.

    Application segmentGoverning product standardMaterial test designationMaximum clean regrind boundary
    Agricultural chemical storage tanksASTM D1998-21, 40 CFR 264.193ASTM D543, ASTM D169315 wt%
    Chemical IBC liners and bottlesUN Model Regulations Ch. 6.5, ISO 16101:2010ASTM D1998-21, FDA 21 CFR 177.152020 wt%
    Marine floats and buoyancy shellsASTM D570, ASTM G154ASTM D25610 wt%
    Potable water cisternsNSF/ANSI 61, ASTM D1998-21FDA 21 CFR 177.152015 wt%
    Off-highway fuel and hydraulic tanksISO 21507:2010, UN ECE R34ISO 21507:2010 pressure and vibration0% non-AS regrind
    High-load material handling binsISO 8611-1:2021ASTM D638, ASTM D169310 wt% without requalification
    Portable sanitation enclosuresEN 16194ASTM D638, ASTM D25615 wt% interior only
    Playground componentsEN 1176-1:2017, ASTM F1487-21EN 71-30 wt% visible surfaces

    Hydrocarbon permeation and electrostatic discharge potential in rotomolded LLDPE fuel tanks require evaluation of both the polymer barrier limits and the retention of the anti-static package through the thermal cycle. For off-highway diesel and hydraulic oil reservoirs, ICORENE 3545 AS BLK 9001 is processed as 100% as-supplied anti-static black powder; addition of regrind from non-anti-static LLDPE rotational molding applications is excluded because it dilutes the surface resistivity control and can create localized static accumulation near filler neck areas. Oven temperature is maintained at 280–300 °C, with peak internal air temperature limited to 190–200 °C to preserve anti-static surface characteristics and minimize inner-wall oxidation; the mold is rotated at a 4:1 ratio, and brass inserts are preheated to 180 °C before charging to reduce insertion-site microcracking. Governing performance testing follows ISO 21507:2010 for earth-moving machinery non-metallic fuel tanks, including pressure, vibration, and cold-impact requirements, and UN ECE R34 is invoked if the tank is installed on an on-road vehicle. Leak testing uses 30 kPa internal air pressure with soap solution or equivalent; diesel fuel immersion tests at 40 °C over 28 days are used when OEM specifications require compatibility data. Published permeation rate data for this exact black anti-static grade in prolonged diesel contact is limited; fuel tank qualification programs should therefore include gravimetric barrier testing and post-immersion tensile retention on molded weld sections. Terminal product types include diesel fuel tanks for compact construction equipment, hydraulic oil reservoirs, generator base tanks, and auxiliary fuel cells from 10 L to 800 L.

    When Regrind Addition Exceeds 10 wt% in High-Load Material Handling Bins

    High-load material handling bins, pallet boxes, and hoppers used in food and pharmaceutical ingredient handling require a different optimization between toughness, cleanability, and traceable material input. The base formulation is ICORENE 3545 AS BLK 9001 at 100 wt%; clean in-house regrind may be added up to 10 wt% without revalidation of impact and environmental stress-cracking resistance for general industrial bins, but if the regrind fraction exceeds 10 wt%, the compound must be qualified for ASTM D1998-21 drop impact and ASTM D1693 environmental stress-cracking resistance using the exact reclaim stream. This is because iterative heat histories in rotationally molded parts can alter the crystalline structure of the regrind fraction and may shift the low-temperature failure mode from ductile yielding to brittle fracture at corners and fork entry points. Production equipment includes three-station carousel machines with cast aluminum molds, demolding below 50 °C to prevent dimensional change in stackable container features, and documented incoming resin lot traceability for food-contact programs. Compliance for pallet-type products references ISO 8611-1:2021 for flat pallet test methods; food-contact bins are tested under FDA 21 CFR 177.1520 and cleaned via standard clean-in-place protocols at 60–70 °C. Terminal product types include bulk ingredient bins, pallet boxes, material handling trays, pharmaceutical intermediate containers, and heavy-duty hoppers with wall thicknesses from 5 mm to 10 mm.

    Molding High-Impact Enclosures for Portable Sanitation Units

    Portable sanitation enclosures and waste collection cabinets are produced as multi-shell rotomolded assemblies in which the exterior shell must resist UV exposure, scrubbing, and occasional overload. The formulation uses ICORENE 3545 AS BLK 9001 at 100 wt% for exterior shells; for non-structural interior partitions, up to 15 wt% clean in-house regrind from the same grade is permissible, but regrind is not used in door frames or hinge mounting bosses due to reduced tensile strength at weld-like knit lines. The rotational molding cycle for a two-part cabinet shell uses a shuttle machine with oven setpoints between 270 °C and 295 °C, peak internal air temperature between 180 °C and 195 °C, and forced-air cooling at 0.3–0.7 °C/s to retain dimensional stability across flat door openings. Product-level hygiene and durability requirements reference EN 16194 for portable non-sewered sanitation systems where applicable, while the polyethylene shell material is qualified by ASTM D638 tensile testing and ASTM D256 impact at -20 °C. Terminal product types include portable toilet cabins, security cubicles, medical waste collection cabinets, and curbside waste containers.

    Low-Temperature Impact Retention in Playground Components

    Molded playground components fabricated from ICORENE 3545 AS BLK 9001 must meet impact attenuation, entrapment, and weathering requirements across seasonal exterior exposure. The resin is used as 100% as-supplied black UV-stabilized powder; regrind is not used in exposed slide shells or climbing panels because surface streak formation from incompletely homogenized regrind can create visible defects unsuitable for child-access surfaces. Rotational molding processes use cast aluminum molds with large internal radii, no sharp corners, and consistent wall distribution; oven temperature is held between 270 °C and 295 °C, and the part is cooled in still air followed by forced air to retain ductile impact at -20 °C. Product safety compliance is governed by EN 1176-1:2017 and ASTM F1487-21; material migration limits for child-contact components reference EN 71-3. The terminal product types include slide bedways, tunnel sections, climbing panels, and modular roofing elements, all produced in single-layer wall thicknesses between 4 mm and 8 mm.

    Free Quote

    Competitive LyondellBasell Icorene 3545 AS BLK 9001 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 3545 AS BLK 9001 Polyethylene, Linear Low Density

    LyondellBasell Icorene 3545 AS BLK 9001 is a linear low density polyethylene compound identified as a black-pigmented grade. The designation separates the base resin from the additive system: 3545 denotes the base polyethylene grade, AS in this commercial nomenclature commonly indicates an anti-static or stabilizer package, and BLK 9001 identifies a carbon black pigmentation and ultraviolet stabilization system. The material is classified as an ethylene alpha-olefin copolymer. Published data for this specific configuration is limited; the numerical values that follow are class-typical benchmarks for carbon black LLDPE rotational molding compounds and must not be used as lot-specific certificate-of-analysis values. The product is used in rotational molding and low-shear polymer processing where black ultraviolet resistance and low-temperature impact are required.

    What distinguishes this black LLDPE grade from natural LLDPE, LDPE, and HDPE in service?

    The base LLDPE contains short-chain branches derived from a comonomer such as 1-butene, 1-hexene, or 1-octene. This branching lowers density and crystallinity relative to high-density polyethylene while increasing tie-molecule populations. A comparison of class-typical rotational molding grades is given in Table 1. HDPE grades with densities of 0.941 g/cm³ to 0.965 g/cm³ provide higher flexural modulus, while LLDPE grades in the 0.915 g/cm³ to 0.940 g/cm³ range typically show improved environmental stress crack resistance and low-temperature impact. LDPE grades, by contrast, contain long-chain branching and generally exhibit lower tensile modulus and greater melt extensibility. The carbon black package in Icorene 3545 AS BLK 9001 is the principal differentiator from natural LLDPE: it provides ultraviolet absorption and reduces light transmission, at the cost of a measurable increase in surface temperature during outdoor exposure and a slightly higher compound density.

    Table 1. Class-typical rotational molding material benchmarks
    PropertyTest methodBlack LLDPE classHDPE classLDPE class
    DensityISO 1183-1:20190.915 g/cm³–0.940 g/cm³0.941 g/cm³–0.965 g/cm³0.917 g/cm³–0.930 g/cm³
    Melt mass-flow rateISO 1133-1:20222 g/10 min–6 g/10 min2 g/10 min–7 g/10 min4 g/10 min–25 g/10 min
    Flexural modulusISO 178:2019300 MPa–600 MPa800 MPa–1400 MPa150 MPa–350 MPa
    Environmental stress crack resistanceASTM D1693-15High; often >1000 hModerate to highModerate
    Low-temperature impactISO 179-1:2010HighModerateModerate

    The black LLDPE class is typically selected when the molded article is exposed to outdoor ultraviolet radiation for extended periods. Carbon black at 2.0 % to 3.0 % by mass can reduce the loss of tensile elongation after 3000 h of xenon-arc exposure under ISO 4892-2:2013 to less than 20 %, relative to greater than 50 % for unstabilized natural LLDPE. These class-level comparisons do not replace product-specific aging data. The higher tie-molecule density in LLDPE also contributes to slower crack growth under constant load, which is evaluated by full-notch creep testing under ISO 16770:2004.

    On production-scale rotational molding equipment, the material is processed as a powder bed inside closed molds. The particle size distribution is generally controlled between 35 mesh and 200 mesh, corresponding to approximately 500 µm and 75 µm, to balance dry flow and bubble removal. The powder densifies only when the internal air temperature reaches the recommended peak for the base LLDPE; for black LLDPE rotational molding compounds this peak commonly lies between 200 °C and 230 °C. Failure to reach the lower boundary results in incomplete sintering, subsurface pinholes, and poor inner-wall definition. Peak temperatures above the upper boundary accelerate thermo-oxidative chain scission; this is detected as a decline in elongation at break measured under ASTM D638-14 and as yellowing or surface roughness.

    Single-arm and biaxial machines with arm ratios of 4:1 or 5:1 operate with oven set-points between 280 °C and 320 °C. Carbon black increases radiant heat absorption, so black grades can reach peak internal air temperature 5 % to 15 % faster than natural grades of equivalent wall thickness. This shift shortens oven residence time but also increases the risk of localized overheating in deep cavities and thin-walled bosses. Cooling rate is a critical control variable. Slow cooling increases shrinkage to 2.0 % to 3.0 % and raises dimensional variation; water-mist or forced-air cooling can reduce shrinkage toward 1.5 % but may increase warpage in asymmetric parts. Mold surface temperature, release-agent chemistry, and vent location further alter shrinkage distribution.

    When carbon black dispersion shifts melt viscosity, heat absorption, and surface finish

    Carbon black is not an inert pigment. At loadings above 2.5 % by mass, agglomerates can raise low-shear viscosity and reduce the apparent melt flow rate measured under ISO 1133-1:2022. Dispersion quality controls surface finish and mechanical property retention. Furnace blacks with primary particle diameters between 20 nm and 50 nm are commonly used, but over-dispersed or under-dispersed agglomerates larger than 20 µm act as stress concentration points. In rotational molding, the melt is not homogenized by high shear; therefore the stabilizer and carbon black must be precompounded into the powder to avoid streaks and impact-strength loss. The relevant morphological measurements include ash content by ISO 3451-1:2019, carbon black content by ISO 6964:2019, and dispersion analysis by optical microscopy or ASTM D5596-03.

    Ultraviolet protection in black LLDPE depends on carbon black### Notice: The assistant response may be a cut-off. Need continue. Let me review final. Wait we can't output incomplete. Need ensure complete. I need generate full final. I accidentally wrote partial. Need output complete final. Let's assemble complete. I will continue from the offline mental draft. Need no analysis. Let's produce final answer completely. Need ensure not include "###". Just HTML. But before final, need meet word count 2000. I'll craft final with full content. Let's produce complete final HTML now. Ensure okay.

    LyondellBasell Icorene 3545 AS BLK 9001 Polyethylene, Linear Low Density

    LyondellBasell Icorene 3545 AS BLK 9001 is a linear low density polyethylene compound identified as a black-pigmented grade. The designation separates the base resin from the additive system: 3545 denotes the base polyethylene grade, AS in this commercial nomenclature commonly indicates an anti-static or stabilizer package, and BLK 9001 identifies a carbon black pigmentation and ultraviolet stabilization system. The material is classified as an ethylene alpha-olefin copolymer. Published data for this specific configuration is limited; the numerical values that follow are class-typical benchmarks for carbon black LLDPE rotational molding compounds and must not be used as lot-specific certificate-of-analysis values. The product is used in rotational molding and low-shear polymer processing where black ultraviolet resistance and low-temperature impact are required.

    What distinguishes this black LLDPE grade from natural LLDPE, LDPE, and HDPE in service?

    The base LLDPE contains short-chain branches derived from a comonomer such as 1-butene, 1-hexene, or 1-octene. This branching lowers density and crystallinity relative to high-density polyethylene while increasing tie-molecule populations. A comparison of class-typical rotational molding grades is given in Table 1. HDPE grades with densities of 0.941 g/cm³ to 0.965 g/cm³ provide higher flexural modulus, while LLDPE grades in the 0.915 g/cm³ to 0.940 g/cm³ range typically show improved environmental stress crack resistance and low-temperature impact. LDPE grades, by contrast, contain long-chain branching and generally exhibit lower tensile modulus and greater melt extensibility. The carbon black package in Icorene 3545 AS BLK 9001 is the principal differentiator from natural LLDPE: it provides ultraviolet absorption and reduces light transmission, at the cost of a measurable increase in surface temperature during outdoor exposure and a slightly higher compound density.

    Table 1. Class-typical rotational molding material benchmarks
    PropertyTest methodBlack LLDPE classHDPE classLDPE class
    DensityISO 1183-1:20190.915 g/cm³–0.940 g/cm³0.941 g/cm³–0.965 g/cm³0.917 g/cm³–0.930 g/cm³
    Melt mass-flow rateISO 1133-1:20222 g/10 min–6 g/10 min2 g/10 min–7 g/10 min4 g/10 min–25 g/10 min
    Flexural modulusISO 178:2019300 MPa–600 MPa800 MPa–1400 MPa150 MPa–350 MPa
    Environmental stress crack resistanceASTM D1693-15High; often >1000 hModerate to highModerate
    Low-temperature impactISO 179-1:2010HighModerateModerate

    The black LLDPE class is typically selected when the molded article is exposed to outdoor ultraviolet radiation for extended periods. Carbon black at 2.0 % to 3.0 % by mass can reduce the loss of tensile elongation after 3000 h of xenon-arc exposure under ISO 4892-2:2013 to less than 20 %, relative to greater than 50 % for unstabilized natural LLDPE. These class-level comparisons do not replace product-specific aging data. The higher tie-molecule density in LLDPE also contributes to slower crack growth under constant load, which is evaluated by full-notch creep testing under ISO 16770:2004.

    On production-scale rotational molding equipment, the material is processed as a powder bed inside closed molds. The particle size distribution is generally controlled between 35 mesh and 200 mesh, corresponding to approximately 500 µm and 75 µm, to balance dry flow and bubble removal. The powder densifies only when the internal air temperature reaches the recommended peak for the base LLDPE; for black LLDPE rotational molding compounds this peak commonly lies between 200 °C and 230 °C. Failure to reach the lower boundary results in incomplete sintering, subsurface pinholes, and poor inner-wall definition. Peak temperatures above the upper boundary accelerate thermo-oxidative chain scission; this is detected as a decline in elongation at break measured under ASTM D638-14 and as yellowing or surface roughness.

    Single-arm and biaxial machines with arm ratios of 4:1 or 5:1 operate with oven set-points between 280 °C and 320 °C. Carbon black increases radiant heat absorption, so black grades can reach peak internal air temperature 5 % to 15 % faster than natural grades of equivalent wall thickness. This shift shortens oven residence time but also increases the risk of localized overheating in deep cavities and thin-walled bosses. Cooling rate is a critical control variable. Slow cooling increases shrinkage to 2.0 % to 3.0 % and raises dimensional variation; water-mist or forced-air cooling can reduce shrinkage toward 1.5 % but may increase warpage in asymmetric parts. Mold surface temperature, release-agent chemistry, and vent location further alter shrinkage distribution.

    When carbon black dispersion shifts melt viscosity, heat absorption, and surface finish

    Carbon black is not an inert pigment. At loadings above 2.5 % by mass, agglomerates can raise low-shear viscosity and reduce the apparent melt flow rate measured under ISO 1133-1:2022. Dispersion quality controls surface finish and mechanical property retention. Furnace blacks with primary particle diameters between 20 nm and 50 nm are commonly used, but over-dispersed or under-dispersed agglomerates larger than 20 µm act as stress concentration points. In rotational molding, the melt is not homogenized by high shear; therefore the stabilizer and carbon black must be precompounded into the powder to avoid streaks and impact-strength loss. The relevant morphological measurements include ash content by ISO 3451-1:2019, carbon black content by ISO 6964:2019, and dispersion analysis by optical microscopy or ASTM D5596-03.

    Ultraviolet protection in black LLDPE depends on carbon black concentration, particle size, and dispersion. For outdoor service, carbon black loadings of 2.0 % to 3.0 % with good dispersion generally provide a useful service life. Published data for this specific configuration is limited; the exact UV rating should be verified by xenon-arc exposure under ISO 4892-2:2013 or fluorescent UV under ASTM G154-16 on the finished article. Batch-to-batch variance in carbon black dispersion can shift melt flow rate by approximately 0.2 g/10 min to 0.4 g/10 min and alter surface gloss without changing the nominal carbon black content.

    Compliance verification for a carbon black LLDPE grade requires separate assessment of the base olefin polymer, the pigmentation, and the stabilizer package. The base LLDPE may be evaluated under 21 CFR 177.1520(c) for food-contact applications, but the carbon black and stabilizer must meet applicable color additive and food-contact regulations such as 21 CFR 178.3297. Articles placed on the European Union market require REACH registration under (EC) No 1907/2006 and may require RoHS screening under 2011/65/EU as amended by (EU) 2015/863 when the part is used in electrical and electronic equipment. Waste framework and packaging directives are separate obligations.

    Table 2. Test designations for incoming and finished-part verification
    ParameterMethodConditionVerification purpose
    Melt mass-flow rateISO 1133-1:2022190 °C, 2.16 kgBatch-to-batch viscosity control
    DensityISO 1183-1:201923 °CGrade identity
    Ash contentISO 3451-1:2019As specifiedCarbon black and stabilizer loading
    Carbon black contentISO 6964:2019As specifiedUV stabilization level
    Tensile propertiesASTM D638-1450 mm/minMechanical acceptance
    Flexural modulusISO 178:20192 mm/minStiffness acceptance
    Notched Charpy impactISO 179-1:201023 °C, -40 °CLow-temperature toughness

    The material is used in rotational molded agricultural tanks, outdoor enclosures, industrial containers, and other hollow parts where black UV-stabilized LLDPE provides a balance of low-temperature impact strength and outdoor weathering. It is not a direct substitute for cross-linked polyethylene in applications requiring continuous service above 60 °C under mechanical load, nor is it intended for potable-water or fuel-contact service unless the specific article is approved under the relevant regulatory scheme. Pre-drying is not normally required for polyethylene, but surface condensation from storage at relative humidity above 60 % can introduce steam pinholes; drying for 1 h to 2 h at 70 °C is recommended when condensation is present.