Lyondellbasell Icorene 3545 Ao Grn 6203 Polyethylene Linear Low Density

LyondellBasell Icorene 3545 AO+ GRN 6203 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 3545 AO+ GRN 6203 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 140016
    Density 0.935 g/cm³
    Melt Flow Rate 20 g/10 min
    Tensile Strength At Yield 11.0 MPa
    Tensile Strength At Break 10.0 MPa
    Elongation At Break 700 %
    Flexural Modulus 260 MPa
    Vicat Softening Point 93.0 °C
    Melting Point 124 °C
    Hardness Shore D 50
    Notched Izod Impact Strength 100 J/m
    Heat Deflection Temperature 50.0 °C
    Color Green

    As an accredited LyondellBasell Icorene 3545 AO+ GRN 6203 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 3545 AO+ GRN 6203 Polyethylene, Linear Low Density is supplied in 25 kg polyethylene-lined paper bags, palletized and stretch-wrapped.
    Container Loading (20′ FCL) 20′ FCL containing LyondellBasell Icorene 3545 AO+ GRN 6203 Polyethylene, Linear Low Density, packed in 25 kg bags, securely stowed.
    Shipping LyondellBasell Icorene 3545 AO+ GRN 6203 LLDPE ships as non-hazardous resin pellets, typically in 25 kg bags or 1,000 kg bulk bags on pallets, stretch-wrapped. Transport by covered truck, railcar, or container. Keep dry, clean, and protected from direct sunlight, heat, and contamination. No special dangerous-goods documentation required.
    Storage Store in a cool, dry, well-ventilated area at ambient temperature, preferably below 50°C, in original closed bags or containers. Keep pallets off the floor and away from direct sunlight, heat, ignition sources, moisture, dust, and strong oxidizers. Avoid excessive stacking, contamination, and static buildup. No smoking. Follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf life is 24 months from manufacture when stored in original, unopened packaging under cool, dry, well-ventilated conditions.
    Application of LyondellBasell Icorene 3545 AO+ GRN 6203 Polyethylene, Linear Low Density

    In liquid fertilizer storage, vertical-walled cylindrical tanks are rotomoulded from LyondellBasell Icorene 3545 AO+ GRN 6203 Polyethylene, Linear Low Density powder in a single-shot biaxial process. The oven set point is commonly held between 280 °C and 300 °C, with a mould rotational ratio of 4:1 on the major and minor axes. Powder charge mass is 1.05–1.15 times the finished shot weight to compensate for flash and vent losses. Peak internal air temperature, measured inside the rotating mould, is controlled at 190–200 °C for 8–15 min depending on nominal wall section. Insufficient internal air temperature leaves residual unmelted powder at the inner wall, while overshoot oxidizes the inner skin and can shift sidewall colour. The nominal wall thickness for aggressive agricultural adjuvants is specified at 5–9 mm, and the cooled tank is leak-tested under 0.3–0.5 bar internal air pressure. Threaded inserts are induction-heated and positioned before powder charging; post-mould drilling is avoided because it initiates stress cracking at the boss root. The green compound is supplied with its pigment package already dispersed, so additional dry-blend colorant is normally unnecessary for the base colour. If a carrier-based functional additive is dry-blended, the ratio is kept below 3 wt% to avoid changing the powder dry-flow profile. Chemical resistance is assessed against the specific stored formulation, not the generic polyethylene class, because ester-based adjuvants can plasticize the inner wall at elevated temperature. End products include vertical storage tanks from 200 L to 10,000 L, inductor tanks, and transport skids with integrally moulded fork pockets.

    Application zoneStandard / methodMeasured condition
    Upright polyethylene tanksASTM D1998-15Wall thickness, venting, hydrostatic test
    Dry food contactFDA 21 CFR 177.1520End-use migration testing
    Pigment heavy metalsEN 71-3Element migration from finished surface
    REACH SVHCRegulation (EC) 1907/2006Article-level declaration
    RoHS hazardous substancesDirective 2011/65/EU Annex IIPb, Cd, Hg, Cr(VI), PBB, PBDE

    What Internal Air Temperature Curve Limits Pinholing in Diesel Fuel Tanks for Off-Highway Vehicles?

    Rotational moulding of diesel fuel tanks from Icorene 3545 AO+ GRN 6203 requires a narrower internal air temperature band than agricultural tanks because diesel contact and drop-load certification dominate the specification. Diesel tanks are moulded to a wall thickness of 6–10 mm, with the thickest sections at the filler neck and mounting bosses. Wall distribution below 4 mm at a boss root has been observed to initiate stress whitening during low-temperature impact testing at -20 °C. The mould is heated to 290–310 °C in a forced-air rock-and-roll machine, and the internal air temperature is ramped at 4–6 °C/min to a plateau of 195–205 °C. A plateau duration below 6 min leaves residual unmelted powder at the inner surface and creates microporosity that is detected only after prolonged diesel contact. A plateau above 210 °C produces surface oxidation and increases low-molecular-weight wax formation, which can contaminate fuel filters. For monolayer construction, hydrocarbon permeation is the primary regulatory constraint; published data for the specific green 6203 monolayer permeability to diesel under UN ECE R34 or EPA evaporative emission cycles is limited, so off-highway original equipment manufacturers often specify post-mould fluorination or an internal barrier layer. The powder charge ratio is adjusted upward at the double-wall bung and metal insert zones. Mould release is not applied to weld areas because contamination prevents a homogeneous melt front. Final articles include 20–120 L diesel tanks for compact excavators, skid-steer loaders, and mobile generators.

    Material Handling Bins, Hoppers, and Light-Abrasion Liners

    Rotomoulded bins and hoppers from the green powder are used for granular food ingredients, seed, and non-abrasive polymer pellets. The mould is fabricated with external angle-iron reinforcements, and the powder charge is calculated by the projected surface area multiplied by a wall-thickness factor of 4.5–6.0 mm. Foam-filled and double-wall hoppers are produced by sequential charging: the outer skin is moulded first, then the cavity is vented and a second powder charge or rigid polyurethane foam is introduced. The process uses an oven temperature of 270–295 °C and forced-air cooling to a demoulding temperature below 70 °C; demoulding above this temperature can induce rim shrinkage and warpage. Part design avoids internal sharp corners, and a minimum radius of 6 mm is maintained at the sidewall-to-base transition to reduce stress concentration. Thread inserts for lid clamps are moulded-in rather than screwed after processing. The material is not recommended for dry mineral abrasion such as sand or metal swarf; high-molecular-weight or crosslinked polyethylene grades demonstrate greater abrasion resistance under those conditions. When used for dry food contact, the finished bin must be evaluated under FDA 21 CFR 177.1520 and applicable overall migration requirements. Terminal parts are typically 100–1,500 L bins with forklift guides, stacking lugs, and removable lids.

    For marine buoyancy applications, closed-cell floatation devices and dock fenders are moulded from a single charge of Icorene 3545 AO+ GRN 6203 into aluminium or steel shells at wall thicknesses between 6 mm and 12 mm. The powder is dried in shallow trays below 60 °C for 4–6 h if storage humidity has exceeded 70 % relative humidity; trapped moisture creates surface pits and weakens the weld line at the mould parting line. For long-term marine exposure, the base green compound is generally insufficient for UV stabilization by itself; a hindered amine light stabilizer masterbatch is dry-blended at 1–3 wt% or the article is coated with a marine polyurethane. Low-temperature toughness is evaluated by dropping a hemispherical striker onto a flat section conditioned at -30 °C, with failure criteria defined by ISO 6603-1 or an original equipment manufacturer-specific multi-axial impact method. When structural foam is introduced, the internal air temperature plateau is deliberately held at 185–195 °C to reduce foam decomposition at the interface. Common terminal parts include cylindrical marker buoys, pontoon floats for dredge lines, aquaculture collars, and dock edge bumpers; each part is leak-tested before assembly, often at 0.2–0.4 bar.

    When In-House Regrind Exceeds 20 wt% in Closed-Mould Cooling Stations

    In rotomoulding plants, the green powder is frequently blended with post-industrial regrind from trimmed flash and rejected parts. The dry-blend ratio is commonly limited to 15–20 wt% for cosmetic surfaces and up to 30 wt% for non-cosmetic agricultural parts, but the particle size distribution shifts because granulator regrind creates elongated flakes rather than spherical powder. A sieve stack with mesh openings of 500 µm, 300 µm, and 150 µm is used as a production control. An increase in the 150 µm fines fraction above 10 % of the total charge has been correlated with uneven melt-out and inner-surface roughness. Bulk density of the dry blend is measured by a funnel method equivalent to ASTM D1895; a drop below 0.28 g/cm³ indicates excessive fines and requires re-balancing with virgin powder. Moisture is a separate constraint: regrind stored outdoors or in unheated silos absorbs surface water, and the dry blend should be exposed to dehumidified air below 45 % relative humidity for at least 6 h before charging. The cooling station is operated with variable-speed fans rather than water mist because rapid mist cooling on regrind-rich blends causes differential shrinkage at metal insert bosses. Final article integrity in regrind-containing formulations is verified by sectioning a sacrificial part and measuring wall thickness distribution; sections below 80 % of nominal wall are rejectable for structural loads.

    In public-access playground equipment, contoured panels and site furniture components are manufactured from the green LLDPE powder when a colour-matched green article is required without post-mould painting. The mould surface is polished or chemically etched to a roughness average below 1.6 µm Ra to improve pigment transfer and gloss consistency. The charge is calculated to produce a wall thickness of 4–7 mm; thick sections at connection points are reinforced with internal ribs or moulded-in steel washers. The oven set point is reduced to 260–280 °C for thin-walled panels to minimise warpage during forced-air cooling, and demoulding is delayed until the part core temperature is below 55 °C. Compliance for public-access playground equipment requires that the pigmented surface meets heavy metal migration limits under EN 71-3; the raw material supplier may provide a compliance statement for the green pigment package, but the finished article remains subject to whole-product testing. For outdoor service, the base antioxidant-plus stabilization does not provide multi-year weathering; a UV masterbatch is dry-blended at 2–4 wt%, and the moulded component may be exposed to 1,500 h of UV-A accelerated ageing if a colour-fastness target is specified. Terminal products include tunnel slides, roof panels, bicycle racks, and park bench seats.

    Thermal Dimensional Stability in Double-Wall Insulated Panels

    At skins below 5 mm, double-wall panels for cold-chain boxes and thermal packaging are formed in a two-step process. The inner and outer skins are rotomoulded from the green powder, then the cavity is filled with rigid polyurethane foam. The LLDPE layer is typically 3–5 mm thick on each face; at these thin sections, the internal air temperature must be raised to only 180–190 °C to avoid burn-through, while the mould shell is kept at 250–270 °C. The powder charge is based on a skin-thickness factor of 0.35–0.45 kg/m² per millimetre of wall, with adjustment for mould release and corner geometry. Differential cooling between the outer and inner skins causes panel bowing if the forced-air stream impinges on one face before the other; the cooling station therefore uses reversing airflow or rotating fixtures. Polyurethane foam injection pressure must remain below 0.5 bar to prevent inner-wall collapse, and foam density exceeding 60 kg/m³ can produce print-through at the injection point. Final panels are tested for flatness using a 1,000 mm straightedge and a feeler gauge; deviation above 3 mm per metre is rejected for automated assembly lines. End uses include insulated food transport boxes, pharmaceutical cold-chain shippers, and temperature-controlled fishing bins.

    Free Quote

    Competitive LyondellBasell Icorene 3545 AO+ GRN 6203 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 3545 AO+ GRN 6203 is a linear low density polyethylene supplied as a pigmented rotational moulding powder. The identifier combines the Icorene 3545 metallocene-catalysed LLDPE base resin, an AO+ thermal stabiliser package, and GRN 6203 green colouration. It is intended for closed-mould rotational moulding of hollow parts requiring a controlled balance of low-temperature impact resistance, environmental stress-crack resistance, and consistent melt densification at moderate peak internal air temperature.

    The base resin of Icorene 3545 is typically characterised by a density of 0.935 g/cm³ according to ISO 1183-1 and a melt flow rate of 4.5 g/10 min at 190 °C/2.16 kg according to ISO 1133-1. The compounded GRN 6203 material may show a density increase of 0.001–0.003 g/cm³ and a minor melt-flow-rate shift relative to the natural base resin. The certificate of analysis for each production lot should be consulted for release-level values.

    Why Does the 3545 Grade Differ from Conventional Ziegler-Natta LLDPE Rotomoulding Powders?

    The principal difference originates in the metallocene catalyst chemistry. Icorene 3545 exhibits a narrower molecular weight distribution and a more homogeneous short-chain branching distribution than a conventional Ziegler-Natta LLDPE of comparable density and melt flow rate. The narrower distribution reduces the fraction of very high molecular weight chains that resist shear during powder coalescence and the fraction of very low molecular weight chains that contribute to extractables and odour. The practical effect is a different balance between impact strength and stiffness at equivalent nominal wall thickness, and generally lower residual warpage after forced-air cooling because crystallisation shrinkage is distributed more uniformly across the part.

    Compared with high-density polyethylene rotomoulding grades, the density of 0.935 g/cm³ reduces flexural stiffness but improves stress-crack resistance and sub-zero impact. This grade is therefore better matched to large thin-walled parts subjected to flexural fatigue and outdoor thermal movement than to rigid load-bearing structures. Compared with non-stabilised Icorene 3545 natural powder, the AO+ package extends the tolerable oven residence time before pronounced chain scission and colour shift occur. The GRN 6203 pigment is pre-dispersed at the supplier level, eliminating the hopper segregation and concentrate let-down variation that can occur with machine-side dry colour mixing.

    Rotational moulding powders in this viscosity class are screened for dry flow, bulk density, and particle-size distribution before charging to the mould. The values below are representative property envelopes for an LLDPE rotomoulding powder of the Icorene 3545 class. They are not release limits and do not replace the supplier certificate of analysis for the GRN 6203 compounded material.

    PropertyStandard/Test methodRepresentative range/value
    Melt flow rate, 190 °C/2.16 kgISO 1133-13.5–5.5 g/10 min
    Density, compounded materialISO 1183-10.932–0.940 g/cm³
    Bulk density, powderASTM D18950.34–0.42 g/cm³
    Particle size, powderSieve analysis95 wt% through 500 µm
    Tensile stress at yield, moulded plaqueISO 527-214–18 MPa
    Tensile strain at break, moulded plaqueISO 527-2>800%
    Charpy notched impact, 23 °CISO 179-1/1eANo break or >40 kJ/m²
    Environmental stress-crack resistance, 10% IgepalASTM D1693>1000 h

    When Icorene 3545 AO+ GRN 6203 Is Processed in a 3.2 m Shuttle Rotational Mould

    On shuttle-type rotational moulding equipment with a 3.2 m swing arm and moulds for 6–10 mm nominal wall thickness, oven set-points are commonly maintained at 280–310 °C. The cycle is not controlled by oven residence time alone. Peak internal air temperature provides the more reproducible indicator of powder coalescence, bubble removal, and densification. For Icorene 3545 AO+, a peak internal air temperature of 193–204 °C is typical. Sustained internal air temperature above 215 °C accelerates antioxidant depletion, promotes yellowing of the stabiliser package, and increases the probability of void formation at sharp corners and deep draws.

    Cooling rate is the primary warpage-control variable. Forced-air cooling at 6–12 K/min through the crystallisation plateau, followed by water mist only after the part has developed sufficient crystallinity, limits differential shrinkage in large flat panels. Demoulding is normally performed below 70 °C to prevent post-demoulding distortion. If the powder has been stored at relative humidity above 60%, or if visible moisture is present, pre-drying at 40 °C for 2–4 h in dehumidified air is required to reduce steam-generated pinholes and internal porosity.

    Mechanical performance targets for moulded parts

    Mechanical acceptance criteria for rotomoulded parts made from this material are usually derived from test specimens cut from flat panels moulded on the same cycle as the production article. Tensile yield values for LLDPE of this density class fall between 14 MPa and 18 MPa when tested according to ISO 527-2. The green pigment and AO+ package do not change the tensile-yield mechanism, but high pigment loading may reduce elongation at break by as much as 10% relative to natural Icorene 3545.

    Low-temperature impact is better assessed by instrumented falling-weight impact according to ISO 6603-2 or ASTM D3763. For a 6 mm plaque moulded from a 0.935 g/cm³ LLDPE rotomoulding powder, the ductile-brittle transition is commonly below -20 °C. This transition is strongly influenced by cooling rate, part thickness, and pigment dispersion. A rapid water-mist quench lowers impact resistance if the part is not allowed to complete crystallisation uniformly; a slow air cool may improve impact but increase cycle time and warpage risk.

    For food-contact service, the base polyethylene falls within the scope of FDA 21 CFR 177.1520 when used under the prescribed conditions of food type and temperature. Compliance of the finished article must be established by migration testing under EU 10/2011 because the green pigment and the antioxidant package are part of the final composition. The GRN 6203 pigment should be checked for heavy-metal migration if the part is intended for toy or potable-water contact under EN 71-3 or BS 6920.

    Regulation/standardScopeQualification condition
    FDA 21 CFR 177.1520Olefin polymers for food contactDepends on food type and use temperature
    EU 10/2011Plastic materials and articles in contact with foodOverall migration limit 10 mg/dm²
    EN 71-3Migration of certain elements from toysRequired where toy contact is intended
    ISO 4892-2Accelerated weathering, xenon-arc exposureRequired qualification for outdoor use

    What Limitations Apply to Recycle Content and High-Clarity or UV-Critical Parts?

    The green pigmentation precludes transparent applications and limits colour sorting in mixed polyethylene recycling streams. In closed-loop post-industrial regrind, additions above 20 wt% regrind may reduce low-temperature impact and increase pinhole rate unless regrind particle-size distribution, moisture content, and residual stabiliser levels are controlled. Regrind should be blended only from the same compound to avoid additive incompatibility and colour shift.

    For outdoor service, the green colour is not a substitute for a full UV-stabiliser package. Sunlight exposure causes carbonyl formation and surface embrittlement unless the part has been qualified with a weathering programme. Xenon-arc testing according to ISO 4892-2 should define the acceptance limits for colour change and retained elongation. Published data for the specific GRN 6203 configuration under multi-year outdoor exposure is limited; the processor shall validate end-use performance for the intended climate and wall thickness.

    The AO+ package is optimised for rotational moulding residence times. It should not be assumed to protect against repeated hot-fill or hot-oil service above 60 °C without end-use testing. Exposure to oxidising chemicals, strong acids, or long-term contact with hydrocarbon fuels requires specific chemical-resistance testing because the green pigment and antioxidant package may interact with the permeant.

    Applications for Icorene 3545 AO+ GRN 6203 include rotationally moulded agricultural tanks, water-treatment housings, outdoor enclosures, playground components, and other hollow articles requiring a moulded-in green colour and moderate wall thickness. Part design must follow rotomoulding-specific requirements: generous radii, draft angles above 3°, and uniform wall thickness to prevent internal air entrapment and uneven sinter-melting. Compared with natural Icorene 3545, the GRN 6203 grade removes the need for machine-side colour mixing and reduces worker exposure to pigment dust. Compared with a black UV-stabilised LLDPE rotomoulding powder, the green compound may have lower heat build-up in sunlight but also lower opacity to ultraviolet radiation. Compared with medium-density polyethylene rotomoulding grades, it offers lower stiffness and better stress-crack resistance, making it more appropriate for flexible thin-walled parts than for structural load-bearing frames.

    Top