Lyondellbasell Icorene 3150 Orange 3601 Polyethylene Linear Low Density

LyondellBasell Icorene 3150 ORANGE 3601 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 3150 ORANGE 3601 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 714253
    Grade Icorene 3150 ORANGE 3601
    Polymer Type Polyethylene, Linear Low Density (LLDPE)
    Density 0.939 g/cm³
    Melt Index 3.5 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 18.6 MPa
    Tensile Strength At Break 22.1 MPa
    Elongation At Break 800%
    Flexural Modulus 758 MPa
    Vicat Softening Temperature 117 °C
    Hardness Shore D 60
    Environmental Stress Crack Resistance >1000 h
    Brittleness Temperature < -70 °C
    Uv Stabilization Yes
    Color Orange
    Processing Method Rotational Molding
    Form Powder

    As an accredited LyondellBasell Icorene 3150 ORANGE 3601 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 3150 ORANGE 3601 LLDPE is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for shipment.
    Container Loading (20′ FCL) 20′ FCL loading: LyondellBasell Icorene 3150 ORANGE 3601 Polyethylene, Linear Low Density in 25 kg bags, securely palletized and loaded.
    Shipping LyondellBasell Icorene 3150 ORANGE 3601 Polyethylene, Linear Low Density ships as a non-hazardous solid resin, usually in moisture-resistant bags or bulk containers. Pallets are stretch-wrapped and labeled. Transport in clean, dry, covered vehicles; avoid heat, sunlight, moisture, and contamination. Standard freight handling applies; no hazardous-materials requirements.
    Storage Store LyondellBasell Icorene 3150 ORANGE 3601 Polyethylene, Linear Low Density in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and open flames. Keep original containers tightly closed to prevent moisture and contamination. Avoid strong oxidizing agents. Store indoors at moderate temperatures, off the floor on pallets, using proper grounding to control static. Follow local regulations and the manufacturer’s safety data sheet.
    Shelf Life Shelf life: typically 2 years when stored unopened in original packaging in a cool, dry place, away from direct sunlight and moisture.
    Application of LyondellBasell Icorene 3150 ORANGE 3601 Polyethylene, Linear Low Density

    LyondellBasell Icorene 3150 ORANGE 3601 is assessed as a pre-compounded orange linear low-density polyethylene rotational molding powder. The applications below are limited to downstream sectors where linear low-density polyethylene of this melt-viscosity class and weather-stabilized pigmentation package is specified in production. Process values are industrial starting points derived from carousel and shuttle rotomolding practice for this density class; exact property data must be verified against the current supplier certificate of analysis using ISO 1183-1:2022 and ISO 1133-1:2022. Published data for this specific color designation under aggressive chemical immersion is limited; application-specific coupon testing is required before commercial qualification.

    What Limits ESCR Performance in Rotomolded Chemical Storage Vessels?

    Rotational molding of this material into upright chemical storage tanks and containment shells is governed by ASTM D1998-21 and, for European static thermoplastic tank installations, EN 13341:2005+A1:2011. The supplied grade is charged at 100 wt%; when same-cell production regrind is introduced, the post-industrial regrind fraction is capped at 20 wt% in stress-bearing base corners and sidewall-to-knuckle transitions because higher levels have been associated with reduced crack initiation resistance. Additional colorant is not required, but if shade alignment is specified, a PE-carrier orange masterbatch may be used at 0.5–1.0 wt% before a measurable decline appears in ASTM D1693-15 ESCR testing using 100% Igepal CO-630 at 50 °C. The downstream process is carousel-type biaxial rotational molding with a primary-to-secondary rotation ratio of 4:1; oven set points are held between 285 °C and 300 °C to reach peak internal air temperatures of 195–205 °C for wall thickness targets of 4–12 mm. Cycle records from four-arm carousel machines with charge weights of 150–250 kg show that PIAT overshoot above 208 °C darkens the orange 3601 pigment package and reduces notched Charpy impact at −20 °C by approximately 10–15% relative to parts demolded at 198 °C. Cooling is staged in three steps: forced air until mold surface thermocouples read 90 °C, water mist until 60 °C, and stationary air to 35 °C before demolding. Terminal part types include vertical storage tanks up to 10,000 L, secondary spill containment trays, dosing skid liners, and rotationally molded intermediate bulk container shells for corrosive liquid logistics. Potable water contact under NSF/ANSI 61 must be verified for the exact pigment package; food-contact status under 21 CFR 177.1520(c) should not be assumed without a pigment supplier letter. Published data for concentrated sodium hypochlorite and strong caustic storage in this specific color-stabilized grade is limited; immersion coupons per ASTM D543-21 are required to determine liner life.

    Process conflicts in thick-walled chemical vessels arise because slow cooling improves ESCR but increases cycle time and differential crystallization shrinkage. On industrial carousels equipped with mold-back air delivery, a temperature difference above 35 °C between the outer mold surface and the internal air thermocouple during cooling indicates insufficient backside air flow. The recommended two-stage fan curve is 12,000–15,000 m³/h per mold station during forced-air cooling to 90 °C, followed by 6,000–8,000 m³/h during water-mist cooling to 60 °C. Premature water quench at mold surface temperatures above 100 °C creates differential shrinkage in thick base sump sections and can form internal voids that are detectable only by ultrasonic C-scan. For leak-critical parts, molded-in flange seams are post-inspected with a 35 kV spark tester. These operational thresholds prevent the low-temperature impact loss and cosmetic shade drift that are the main batch-rejection causes in chemical tank production.

    Agricultural liquid handling components fabricated from this pre-colored powder use 100 wt% supplied material with same-process regrind capped at 20 wt% under ISO 13341:2005+A1:2011; shuttle-type rotomolding at 190–200 °C peak internal air temperature and forced-air cooling to 80 °C before water mist to 50 °C produces 500–5,000 L horizontal water tanks, irrigation reservoirs, conical-bottom fertilizer tanks, and agricultural feed troughs, while surfactant-containing liquid fertilizer formulations above 2% require ESCR coupon testing per ASTM D1693-15 because knuckle-region stress cracking is the primary field failure mode.

    Reducing Aquatic UV Degradation in Marine Flotation Buoy Skins

    Marine flotation parts molded from this orange LLDPE powder require retention of impact ductility after prolonged UV and saltwater exposure; the pre-dispersed UV stabilizer package is independent of the orange pigment, and pigment color alone is not a predictor of UV performance. The material is integrated at 100 wt% or with up to 10 wt% same-part regrind from deflashed weld seams; higher regrind levels degrade Charpy impact at −30 °C under ISO 179-1:2020. If supplemental stabilization is specified for tropical marine service, a PE-carrier HALS concentrate is added at 0.5–1.0 wt%; loadings above this window do not produce linear gains in ASTM G154-16 UV performance and can cause tooling plate-out. Production uses a carousel rotomolding machine with a 4.5:1 rotation ratio, mold surface set points between 280 °C and 295 °C, and peak internal air temperature of 195–200 °C. Wall thickness is maintained at 4–8 mm; ultrasonic thickness mapping rejects parts with local thinning greater than ±12% at the top fillet. Post-mold cooling is forced air to 80 °C, then water quench is avoided below 55 °C because rapid cooling at the mold parting line induces stress concentration and flange warpage. The applicable compliance anchors are ISO 4892-2:2021 for accelerated weathering, ASTM D638-14 for tensile property retention, and REACH Annex XVII for restricted polycyclic aromatic hydrocarbons in marine equipment. Terminal products include harbor marker buoys, octagonal pontoon collars, aquaculture pen floats, fender skins, and cable floats. Adhesion for two-part polyurethane antifouling requires flame or plasma surface oxidation; solvent-based antifouling paints can reduce ESCR in stressed zones and must be validated by ASTM D543-21.

    Long-term marine service data for rotomolded LLDPE flotation parts indicates that most property loss occurs in the outer 0.5 mm skin layer, where UV-initiated chain scission increases gel content and lowers elongation at break. Parts with wall thickness below 4 mm are excluded from high-wave-energy service because the degraded skin represents too large a fraction of the load-bearing section. Mold design controls the pontoon fillet radius-to-wall-thickness ratio at 3:1 or greater; tighter radii have been associated with cracking after 5,000 h of accelerated weathering under ISO 4892-2:2021. These boundaries are applied to reduce field returns in buoy skins and flotation collars.

    ScenarioCompliance anchorsFormulation boundaryTerminal product types
    Chemical storage vesselsASTM D1998-21, EN 13341:2005+A1:2011, NSF/ANSI 6120 wt% same-cell regrind cap; 0.5–1.0 wt% maximum tint correctionVertical tanks, containment trays, dosing skid liners
    Agricultural liquid handlingISO 13341:2005+A1:2011, EU Reg 1935/2004, REACH Annex XVII20 wt% regrind cap; no added pigmentWater tanks, fertilizer tanks, agricultural feed troughs
    Marine flotation skinsISO 4892-2:2021, ASTM G154-16, ASTM D638-140.5–1.0 wt% supplemental HALS if specifiedBuoy skins, pontoon collars, aquaculture floats

    When Playground Components Require Impact Compliance Under ASTM F963

    Rotomolded playground components fabricated from this grade must satisfy heavy-metal extractable limits under ASTM F963-23 and EN 71-3:2019+A1:2021; the supplied orange pigment package should be supported by a per-lot certificate of compliance because trace metal content can vary between pigment campaign batches. The material is run at 100 wt% with no added plasticizer and an optional color masterbatch total of 1.5 wt% maximum using phthalate-free PE carriers under REACH Annex XVII; production is shuttle-type rotomolding at 270–285 °C mold surface temperature and 185–195 °C peak internal air temperature into 3–6 mm walls for slide hoods, tunnel segments, swing seats, and modular roof shells. Ejection above 70 °C can produce visible waviness from differential shrinkage between thick and thin sections.

    Off-highway vehicle fuel and hydraulic fluid reservoirs molded from this pre-colored LLDPE powder require insert leakage control and dimensional stability after continuous fluid contact. For diesel tanks and hydraulic oil reservoirs, the material is processed at 100 wt% with regrind from rejected parts limited to 15 wt% because insert bosses concentrate molded-in stress. Applicable compliance anchors are SAE J1521 where specified for heavy-duty vehicle fuel tank barrier testing, ASTM D638-14 for mechanical property acceptance, ASTM D471-16a for fluid resistance after immersion in reference diesel and hydraulic oil, and REACH Annex XVII for chemical restrictions. The production process is a four-arm carousel rotational molding machine with 4:1 rotation ratio, oven set points of 280–295 °C, and peak internal air temperature window of 195–205 °C. Metal inserts are preheated to 150–170 °C before loading to reduce freeze-off at the polymer-metal interface. After molding, the part is cooled with forced air to 85 °C, then water mist to 50 °C, and demolded at 35–40 °C to preserve thread geometry in tapped bosses. Terminal products include diesel fuel reservoirs, hydraulic oil tanks, DEF tank shells, toolbox enclosures, and marine holding tanks. Published data for this specific orange grade in long-term diesel contact is limited; continuous immersion testing per ASTM D471-16a is recommended before qualification for fuel systems.

    Insert bosses represent the highest-risk location for slow crack propagation because the metal insert acts as both a heat sink during molding and a stress riser in service. Production experience on 400-part campaigns shows that an insert surface temperature below 120 °C at the start of the oven cycle produces an incomplete interfacial melt layer and increases pull-out force variability by more than 25%. Torque retention is evaluated with a calibrated torque wrench at 10 N·m and 20 N·m on threaded brass inserts; insert rotation greater than 5° at the lower torque is considered a failure. Leak tightness of the complete reservoir is tested with compressed air at 0.2 bar submerged in water for 5 min; bubbles at insert bosses or weld seams require root-cause analysis before batch release.

    Intermediate Bulk Container Shells for Chemical Logistics

    Rotational molding of intermediate bulk container shells from this material addresses the requirement for a self-supporting orange outer envelope with secondary containment. The governing standards for the molded shell are ASTM D1998-21, EN 13341:2005+A1:2011, and DIN EN ISO 16495:2013 for packaging in chemical distribution where applicable. Formula ratio for this sector uses the supplied precompounded powder at 100 wt%; if a reprocessed fraction is introduced from post-consumer IBC shells, the maximum level is 10 wt% because post-consumer polyethylene can contain residual surfactants that reduce ESCR. The downstream process is a carousel rotomolding line with a 4:1 primary-to-secondary rotation ratio and large-charge tool capacity of 400–600 kg; mold surface temperature is set to 280–290 °C, and peak internal air temperature is controlled to 190–198 °C. Extended molding cycles are required to densify the thick base sump and fork-lift channels, where wall thickness may reach 10–14 mm. Cooling uses forced air to 80 °C, intermittent water mist to 55 °C, and then an in-mold annealing pause at 45–50 °C for 10–20 min to reduce post-demolding shrinkage variation. Terminal product types include 1,000 L intermediate bulk container outer shells, palletized process fluid containers, hazardous waste overpack trays, and modular spill basin liners. Compatibility of the orange outer shell with aggressive chemical mixtures should be verified through ASTM D543-21 coupon exposure, because the shell can function as secondary containment even when the inner vessel is fabricated from a different polymer.

    Free Quote

    Competitive LyondellBasell Icorene 3150 ORANGE 3601 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 3150 ORANGE 3601 is a pre-colored linear low density polyethylene powder supplied for rotational moulding. The base polymer is classified as linear low density polyethylene, with short-chain branching that reduces crystallinity relative to high density polyethylene. The product designation carries the base model 3150 and the pigment identifier ORANGE 3601. The material is supplied as a dry, free-flowing powder rather than as pellets, which permits direct charging to biaxially rotating tools without an intermediate grinding step. Melt flow rate is measured at 190 °C under 2.16 kg load according to ISO 1133-1 or ASTM D1238, and density is determined by ISO 1183-1 or ASTM D1505. Because the product is a pigmented variant, the certificate of analysis is the operative specification; the colorant package and stabilizer system may shift melt flow rate and density relative to the unpigmented base.

    Compared with high density polyethylene rotomoulding grades, the LLDPE base is expected to exhibit lower flexural modulus and higher environmental stress crack resistance. Modulus is evaluated by ISO 527-2 or ASTM D638, and environmental stress crack resistance by ASTM D1693 under a standard surface-active environment. The stiffness reduction is relevant when a part must support sustained load, because a given wall section in LLDPE will deflect more than the same section in HDPE. In return, the LLDPE usually provides better crack resistance under bending and thermal cycling. The final decision between LLDPE and HDPE must be made using part-level structural analysis and not on a single resin property.

    Typical rotomoulding applications for this colored powder include high-visibility tanks, traffic management articles, outdoor furniture, fenders, and storage containers. The product is not limited to those categories; any process that requires a pre-colored powder with direct charging can be considered. The orange color is supplied throughout the wall cross-section, which avoids the surface-only color found in post-finishing operations. Because the powder is pre-compounded, the part surface and the interior melt layer are colored from the initial molding step.

    Which specification values are relevant for incoming inspection and lot acceptance?

    Incoming inspection for a colored LLDPE rotomoulding powder should record the following properties because they control mold filling, appearance, and end-use performance. The producer’s certificate of analysis supplies lot-specific values; the moulder’s internal limits are typically narrower than the product data sheet because of tooling constraints.

    PropertyStandard or methodProcessing relevance
    Melt flow rate at 190 °C, 2.16 kgISO 1133-1, ASTM D1238Controls bubble coalescence, corner filling, wall thickness distribution
    DensityISO 1183-1, ASTM D1505Governs part weight, stiffness, and chemical resistance
    Particle size distributionASTM D1921 or supplier sieve methodDetermines hopper dry flow, segregation, fines generation, and wall uniformity
    Pourability / dry flowASTM D1895Measures free-flow behavior in the charging station and small tool sections
    Tensile propertiesISO 527-2, ASTM D638Used for lot-to-lot mechanical consistency and failure mode review
    Environmental stress crack resistanceASTM D1693Indicates crack resistance under chemical and bending stress
    Low-temperature impactISO 6603-2, ASTM D3763Evaluates puncture resistance in outdoor winter or cold-storage applications
    Color coordinatesISO 11664-4, CIELABConfirms pigment dispersion and lot-to-lot color drift

    The table does not replace molded part validation. A resin lot can pass incoming inspection and still fail in service if the molding cycle was outside the established peak internal air temperature window. Processors should maintain a tool-specific log correlating peak internal air temperature, cooling rate, and post-mold impact or color drift data.

    Melt flow rate, density boundaries, and pigment-induced shift in the colored compound

    The orange pigment package alters the rheology and density of the base polymer. The shift is not a fixed offset; it varies with pigment loading, carrier resin, and stabilizer composition. The pigment carrier can introduce low molecular weight material that raises melt flow rate, while high-loading organic orange pigments can increase low-shear viscosity and reduce melt flow. Published data for this specific ORANGE 3601 configuration is limited, so the producer’s certificate of analysis should be used to establish lower and upper control limits. If process settings are taken from a natural LLDPE lot without checking the colored lot’s melt flow rate, the molded part may show incomplete corner fill, retained bubbles, or an oxidized inner wall.

    LLDPE rotomoulding grades typically operate in the density band between 0.930 g/cm³ and 0.940 g/cm³. The colored variant may fall slightly higher because the pigment and carrier add mass. A density shift as small as 0.002 g/cm³ changes part weight at constant wall thickness and can influence buoyancy in floating products. For buoyancy-sensitive designs, the moulder should calculate part weight from certificate density, not from the nominal base grade. Melt flow rate values for rotomoulding LLDPE commonly fall between 3 g/10 min and 7 g/10 min at 190 °C, 2.16 kg; the actual colored lot may be outside that band if the pigment package is highly loaded.

    In process development, torque rheometry and capillary rheometry provide more useful information than melt flow rate alone. A pre-colored powder removes the uncontrolled concentration variation observed when metering powdered pigment at the mold charging station. However, the dispersive quality of the pre-compounded pigment must still be checked by color coordinate measurements and by press-outs or molded plaques. Agglomerates in the pigment package can appear as surface specks even if the certificate color coordinates are within limits.

    The peak internal air temperature for LLDPE rotomoulding is normally monitored in the 190–230 °C range. Oven set temperatures are commonly higher, in the 280–320 °C range, to overcome heat transfer resistance through the mold wall. The exact setpoint depends on mold mass, wall thickness, release agent, and part geometry. At peak internal air temperatures below 190 °C, the powder may not fully coalesce; at temperatures above 230 °C, oxidative degradation can produce discoloration, reduced impact, and plate-out on the mold surface. The orange surface is particularly sensitive to overheating because pigment degradation can appear as a yellow or brown shift before mechanical failure is measurable.

    Excessive peak internal air temperature can promote plate-out of pigment and stabilizer on the mold surface. The deposit reduces gloss and can contaminate subsequent parts. In high-volume rotational moulding cells, the corrective action is typically a reduction of peak internal air temperature in 2–5 °C increments and control of mold release film thickness. No single setpoint applies across all tooling, because mold geometry, wall thickness, and release agent type change the surface temperature history.

    At the powder handling station, hopper bridging and rat-holing can occur if the powder contains a high proportion of fines or if the hopper cone angle is too shallow. Production-scale rotomoulding lines often use vibratory assist and maintain fill level above the cone transition to reduce these interruptions. Static discharge grounding is recommended because fine polyethylene powders can generate electrostatic charges during transfer. Static charging during powder transfer can affect particle deposition on the mold surface. At low relative humidity, the fine fraction may stick to the mold surface or to the loading hopper walls. Anti-static treatment of the material or controlled humidity in the charging area may be required; however, the use of external anti-static agents should be verified for compatibility with the orange pigment and UV stabilizer. Plant trials should include a visual inspection for fine-particle marbling and a check of wall thickness in blind corners.

    When the pre-colored powder replaces dry pigment mixing in a rotational moulding cell

    Dry pigment mixing requires the operator to blend powdered colorant with natural LLDPE at the charging station. The operation generates dust, can contaminate surrounding lines, and can produce color streaks if the pigment agglomerates are not fully dispersed. Pre-colored Icorene 3150 ORANGE 3601 powder removes the free-pigment addition step and reduces the manual blending step. In production-scale cells, the change also reduces reject parts caused by color streaks and improves lot-to-lot color consistency. The trade-off is reduced flexibility: the moulder must stock a separate colored grade for each hue instead of one natural base powder and several pigments. Material cost per kilogram is usually higher for a pre-colored powder, but the cost per accepted part can be lower when pigment losses, cleanup, and rework are included.

    The pre-colored powder should not be mixed with natural or other colored powders unless compatibility of the stabilizer and carrier systems has been verified. Incompatible pigment carriers or antioxidants can create local melt viscosity differences and visible weld lines in the rotomoulded wall. The material should be stored in closed containers below 50 °C to limit antioxidant depletion. Condensation on cold powder should be avoided because polyethylene is nonhygroscopic but surface moisture on the powder can produce pinholes or surface defects during heating.

    For food-contact applications, the base olefin polymer may be assessed under FDA 21 CFR 177.1520 or EU 10/2011, but the orange pigment package must be independently approved for the intended use and the relevant migration limits. For electrical and electronic equipment, the orange colorant package should be checked against EU 2011/65/EU RoHS restrictions for lead, cadmium, mercury, and hexavalent chromium; some orange pigments can contain regulated metal compounds. Published data for this specific variant is limited, and a general polyethylene approval does not automatically cover the pigmented powder. The supplier should be consulted for a full regulatory declaration before regulated end uses are assigned.

    Outdoor parts in orange are more prone to visible color change than black or white highly stabilized systems, because organic orange pigments are generally less UV durable than carbon black. Weathering performance should be evaluated using ISO 4892-2 or ASTM G155, and the results should be used only for ranking formulations under identical exposure conditions. The UV stabilizer package, part cooling rate, and wall thickness affect surface gloss and color retention. For traffic or warning applications, the supplier color code ORANGE 3601 is not by itself proof of conformance to a safety color standard such as ISO 7010 or ANSI Z535.1; the molded article must be measured for the required chromaticity and luminance coordinates after the intended processing cycle.

    Because the product is an LLDPE, creep behavior is less favorable than HDPE at elevated temperature. Creep modulus and tensile creep curves should be generated using ISO 899-2 or ASTM D2990 when the part is load-bearing. The modulus difference between LLDPE and HDPE becomes more pronounced at temperatures above 40 °C. Published data for the pigmented variant is limited; the moulder should generate application-specific data if the service condition includes continuous loading.

    Compared with crosslinkable polyethylene rotational moulding grades, the LLDPE base remains thermoplastic. It can be re-molded or recycled within the same production stream, but it does not offer the same heat distortion temperature, solvent resistance, or creep performance as sufficiently crosslinked PE. The choice between LLDPE and XLPE is therefore governed by service temperature and chemical exposure. For applications requiring only the high-visibility orange surface and moderate mechanical loading, the LLDPE product is evaluated as a lower stiffness, higher crack resistance alternative to HDPE and as a non-crosslinking alternative to XLPE.