Lyondellbasell Icorene 3150 Gry 7776 Polyethylene Linear Low Density

LyondellBasell Icorene 3150 GRY 7776 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 3150 GRY 7776 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 796078
    Density 0.935 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 3.5 g/10 min
    Tensile Strength At Yield 13.8 MPa
    Tensile Strength At Break 20.7 MPa
    Elongation At Break 800%
    Flexural Modulus 0.690 GPa
    Hardness Shore D 55
    Vicat Softening Point 108 °C
    Melting Point 125 °C
    Thermal Conductivity 0.33 W/m·K
    Specific Heat Capacity 1.9 J/g·°C
    Coefficient Of Linear Thermal Expansion 1.5E-4 cm/cm/°C

    As an accredited LyondellBasell Icorene 3150 GRY 7776 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 3150 GRY 7776 LLDPE is packaged in 25 kg polyethylene-lined bags, 40 bags per pallet (1,000 kg).
    Container Loading (20′ FCL) 20′ FCL loading of LyondellBasell Icorene 3150 GRY 7776 LLDPE, 25 kg bags, palletized and secured for safe ocean transport.
    Shipping LyondellBasell Icorene 3150 GRY 7776 Polyethylene, Linear Low Density, is a non-hazardous solid. It is shipped in bags, octabins, or bulk trucks/railcars. Not regulated by DOT, IMDG, or IATA. Keep dry, cool, clean, and away from heat, ignition, moisture, and contaminants. No special shipping labels required.
    Storage Store LyondellBasell Icorene 3150 GRY 7776 Polyethylene, Linear Low Density in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers sealed to prevent moisture and contamination. Do not stack excessively. Use grounding during bulk handling to control static. Maintain ambient storage temperatures, preferably below 50°C.
    Shelf Life Typically 24 months from date of manufacture when stored unopened in original packaging, in a cool, dry area away from direct sunlight.
    Application of LyondellBasell Icorene 3150 GRY 7776 Polyethylene, Linear Low Density

    Because the supplier datasheet for the grey precoloured configuration of Icorene 3150 GRY 7776 is not publicly available for every property input, the processing windows cited below are derived from standard industrial practice for linear low-density polyethylene rotomoulding powders of this class. Grade-specific certificates for melt flow rate, density, additive package, and pigment loading should be reviewed before tooling is cut or a production cycle is locked.

    For rotationally moulded vertical tanks intended for corrosive liquid containment, Icorene 3150 GRY 7776 is normally processed as a pulverised linear low-density polyethylene compound with a grey pigmentation package that alters infrared absorption in gas-fired ovens. The mould charge is calculated from the part surface area and a nominal wall thickness of 6 mm to 12 mm, using a standard rotomoulding weight formula with a powder bulk density in the range of 0.33 g/cm³ to 0.39 g/cm³; the actual bulk density must be verified from the certificate of analysis because fines content below 35 mesh influences material distribution in the cavity. In a carousel or shuttle-type machine, steel moulds are heated to an oven set-point of 280 °C to 300 °C while the arm rotates biaxially; a rotation speed ratio of approximately 4:1 is typical for cylinders with a diameter-to-height ratio near 1.0, although deep cylinders may require an adjusted ratio to prevent wall thinning at the shoulder. The internal air temperature is monitored with a thermocouple located at the mould centre, and the peak internal air temperature is held between 205 °C and 215 °C for a 6 mm wall section. A processing window of approximately ±5 °C is applied to this peak: below 200 °C, the inner surface remains insufficiently fused, producing microporosity at the outer gradient; above 220 °C, oxidation of the inner surface accelerates, visible as yellowing of the grey compound and a measurable reduction in oxidative induction time.

    Cooling is staged in forced-air and water-spray modes to control shrinkage without inducing residual stress. For a 6 mm wall, forced air is applied for 10–14 min followed by water spray until the mould surface reaches 70–80 °C; demoulding above 90 °C causes warpage at flat tank heads, while demoulding below 60 °C increases the risk of brittle release and surface tearing at deep draw locations. The grey pigmentation raises surface temperature during heating but does not significantly alter the cooling rate; therefore the cooling time is still governed by wall thickness and mould thermal mass. Shrinkage in the mould is approximately 1.5% to 2.5% for LLDPE rotomoulding grades, depending on cooling rate, and is accommodated in the tank CAD model as a dimensional scale factor. Fittings are inserted either by post-moulding welding of the same polymer family or by moulded-in threaded inserts; for chemical service, post-moulding extrusion welding of polyethylene sockets is preferred because moulded-in metal inserts can create stress concentrations and initiate environmental stress-cracking at the thread root when exposed to polar liquids.

    Vertical cylindrical tanks manufactured from this grade are specified under ASTM D1998 where wall thickness tolerances and top-head design are defined; for outdoor installation, the tank is assessed for environmental stress-crack resistance per ASTM D1693, condition B, at 50 °C in a 100% Igepal CO-630 solution. Published data for this specific grey configuration is limited, so each production lot should be qualified with a supplier-provided ESCR certificate before chemical service. The resin is suitable for continuous contact with dilute inorganic acids, caustic solution up to 30% concentration, and neutral salt solutions at ambient temperature; continuous exposure to aromatic hydrocarbons, chlorinated solvents, or concentrated oxidising acids above 50 °C is outside the recommended service envelope because these environments accelerate solvent uptake and reduce the retained tensile elongation of LLDPE. Tanks above 5,000 L require structural support bands or external frames when installed unanchored, because the flexural modulus of LLDPE is lower than that of high-density polyethylene and the unsupported sidewall can deflect under hydrostatic load.

    In agricultural fertigation and pesticide dilution skids, Icorene 3150 GRY 7776 is converted into cone-bottom batch tanks, closed-top mixing vessels, and drain pans using aluminium moulds with integrally machined fitting bosses. The moulding cycle is shortened relative to chemical storage tanks because a wall thickness of 4 mm to 8 mm is sufficient for the lower hydrostatic load; the peak internal air temperature is reduced to 195–205 °C for the thinner sections, and the heating time is trimmed by 2–4 min per 1 mm reduction in nominal wall when compared with a 6 mm baseline. Grey pigmented LLDPE absorbs infrared energy more efficiently than natural resin, so a surface temperature probe on the mould is used to avoid over-curing the outer wall before the inner wall reaches fusion. In cone-bottom designs, the apex is the most difficult zone to densify due to powder bridging and reduced heat transfer; a common production countermeasure is to increase the biaxial rotation speed ratio to 5:1 during the last 30% of the heating stage, allowing more uniform coverage at the sloped lower section. Threaded bosses are formed by moulded-in inserts made of the same polyethylene family or by specially designed brass inserts with a thermal expansion mismatch that must be compensated by a recessed insert pocket depth of 1.5–2.0 mm. Fertiliser concentrates based on urea, potassium chloride, or ammonium phosphate are handled at ambient temperature; the LLDPE matrix resists these dilute salt solutions, but acidic formulations below pH 2 require a chemical compatibility review under ISO 175 exposure testing because prolonged contact can extract lower-molecular-weight fractions and cause surface microcracking at stress points.

    Outdoor agricultural tanks are positioned on compacted gravel or concrete pads, and the base design includes a drain sump to avoid residual liquid pooling. UV stabilisation in the grey compound is necessary for service life beyond 3 years; resistance is evaluated through accelerated weathering according to ISO 4892-2 method A with a black panel temperature of 65 °C, and the acceptance criterion is typically a retained elongation at break of not less than 50% after 3,000 h exposure. The grey colour package itself reduces photo-oxidative attack on the bulk polymer by absorbing UV radiation before it reaches deeper layers, but surface chalking still occurs over extended exposure; mechanical cleaning with abrasive pads is avoided because it removes the stabilised skin layer. Tank installations where the liquid is injected with air agitation show higher oxidative stress at the liquid line; this zone should be inspected at annual intervals for cracking using visual assessment after chemical exposure per ASTM D543, with dye penetrant inspection used as a supplementary check when surface grazing is suspected.

    Marine Buoyancy and Dock Float Shells

    For modular floating docks and mooring buoys, the rotational moulding process utilises the same LLDPE matrix but shifts the critical performance requirement from chemical resistance to impact toughness at sub-zero temperatures and resistance to water absorption over long immersion periods. The shell is rotationally moulded as a hollow enclosure with a nominal wall thickness of 6 mm to 10 mm; after demoulding, the cavity is filled with closed-cell expanded polystyrene or injected polyurethane foam, depending on the required buoyancy reserve. Icorene 3150 GRY 7776 provides a low-temperature impact response that is evaluated by ASTM D5276 drop testing of the complete rotationally moulded shell from 1.5 m at -20 °C, with no visible crack on the inner surface. Because the grey compound contains a pigment package that increases surface temperature under direct sunlight, black or dark grey float shells in tropical installations reach surface temperatures above 70 °C; this condition accelerates oxidative degradation at the waterline unless the material contains a hindered amine light stabiliser package and the moulding cycle does not exceed the prescribed peak internal air temperature.

    The process conflict in marine parts arises from the need to achieve complete powder coalescence at the deep draft corners while avoiding excessive internal air temperature that can degrade the foaming interface. A low peak internal air temperature of 190–200 °C is often used for foam-filled floats, but this narrows the processing window because any drop below 185 °C leaves partially sintered powder at the lower mould extremities. To compensate, the oven set-point is raised to 290–310 °C and the heating time is extended by 5–8 min compared with an unfilled tank of similar wall thickness. The resulting outer skin is fully fused, while the inner surface remains at a lower temperature that reduces adhesion to the subsequent PU foam pour; this interfacial control is monitored by measuring the mould surface temperature at demoulding, which is held at 65–75 °C. Marine floats manufactured for dock systems are also checked for dimensional stability after a 24 h water immersion at 23 °C, using ISO 62 to confirm that water absorption is below 0.1% by mass; higher values indicate wall microporosity and are cause for rejection of the shell before foam filling.

    Because the grey colour package shifts surface heat absorption during oven residence, injection moulders do not dominate heavy-gauge industrial containers; instead, fabricators use Icorene 3150 GRY 7776 for rotationally moulded pallet boxes, dunnage trays, and scrap hoppers with a nominal wall thickness of 8 mm to 12 mm. These parts are produced in fabricated steel moulds with integral stand-off feet and reinforcement ribs; the long oven cycle, typically 28–40 min for a 10 mm wall at a peak internal air temperature of 205–215 °C, is balanced against the high material consumption per part. The LLDPE grade offers superior resistance to repetitive impact and abrasion from metal parts compared with high-density polyethylene of the same wall thickness, but its lower modulus requires additional structural ribbing to maintain fork pocket stability under rated loads. A pallet box with a 10 mm sidewall and 12 mm base is commonly rated for a static load of 1,000 kg when the base is supported on a flat floor; dynamic lifting with fork pockets reduces the safe load to 400–600 kg due to flexural deformation at the unsupported span. Production lines use mould release agents based on polydimethylsiloxane or semi-permanent polymer films; overtreatment beyond the supplier’s recommended film weight of 2–4 g/m² causes surface streaks and inconsistent cooling on the grey surface, which is particularly visible in parts with large flat panels.

    Batch-to-batch variation in the pulverised powder directly affects the flow behaviour in these deep-draw tools. A powder with excessive fines content may fuse at the mould surface before tumbling completes, causing pinholes at the corner intersections; a powder with an excessively broad particle size distribution can segregate during the biaxial rotation, producing thin sections at the upper walls. Sieve analysis is performed per ASTM D1921 with a target of less than 5% retained on a 35 mesh screen and less than 15% passing a 200 mesh screen; these limits are common for LLDPE rotomoulding powders and are verified on incoming lots. If the powder fails the sieve specification, the processing correction is not simply longer heating but a reduction in oven set-point and an increase in rotation speed to limit early fusion. The fabricated steel moulds are coated with a thermal insulation layer on the outer flat surfaces to direct heat into the corner ribs; this practice, combined with internal air temperature monitoring, reduces the wall-thickness variation from ±1.5 mm to ±0.5 mm on 10 mm nominal sections.

    When Potable Water Contact Parts Require Grade-Specific NSF/ANSI 61 Verification

    Potable water tanks and distribution system components moulded from Icorene 3150 GRY 7776 cannot be placed into drinking water service solely on the basis of the base polymer type. Certification under NSF/ANSI 61 or NSF/ANSI 372 is formulation-specific and must be confirmed with the supplier for the exact grey colour package because pigments and process stabilisers contribute to extraction profiles. For parts intended for cold water storage at 23 °C, the polymer is converted in the same rotational moulding process as industrial tanks, but the mould surface is cleaned between colour changes, and no external mould release containing phthalates or amine-based additives is used because these substances can migrate into the contact surface during the long heating cycle. The extraction test is performed according to NSF/ANSI 61 Section 6 for multiple exposure water types at pH 5 and pH 10, with total organic carbon and specific contaminant monitoring; results are evaluated against the pass/fail criteria in the standard. If the grade is not listed for the relevant temperature and surface-to-volume ratio, it is not acceptable for the intended installation, regardless of the base resin compliance with FDA 21 CFR 177.1520 for food-contact olefin polymers.

    The operational boundary for potable water tanks is more conservative than for chemical service. Continuous exposure to hot water above 60 °C reduces the permissible hoop stress and increases the extraction rate of lower-molecular-weight species, so rotomoulded tanks are typically limited to cold and ambient service. Surfaces are not flame-treated or exposed to solvent wipe cleaning after moulding because oxidation of the contact layer can alter the organoleptic properties and introduce low-molecular-weight oxygenated fragments that may fail the standard’s taste and odour threshold. Fibreglass reinforcement or metal bands are not used in direct contact, and any external reinforcement is isolated from the water path. For tank liners installed inside concrete cisterns, the moulded shell is dimensioned with a minimum thickness of 4 mm, and the liner is hydrostatically tested for 24 h at the maximum operating water level to detect pinholes before backfilling.

    Playground and Recreational Structures Demand a Different Failure Envelope

    Rotational moulding is used for slides, tunnel sections, climbing domes, and playhouse panels made from Icorene 3150 GRY 7776 because the process yields a one-piece hollow shell without weld lines that can become crack initiation sites under cyclic child-loading. The grey grade is specified where the playground owner requires a neutral colour that disguises surface abrasion, but the same colour complicates oven control because it absorbs more infrared radiation than light-coloured LLDPE; processors compensate by setting the oven dial 10–15 °C lower than for a natural grade of equivalent melt flow. A slide shell with a nominal thickness of 5 mm to 8 mm is moulded in a highly polished aluminium tool; the peak internal air temperature is held at 195–205 °C to maintain surface gloss measured by ASTM D523 at a 60° specular angle, which influences slide speed but is not the only acceptance criterion. Static load tests on playground equipment are conducted according to ASTM F1487 and EN 1176; the moulded shell must resist a point load of 1.0 kN on the slide bed without visible cracking or permanent deformation, and the edge radius checks are integrated into the tooling design rather than achieved by secondary trimming.

    The failure envelope for playground components is dominated by weathering and puncture from vandalism, not by chemical attack. UV stabilisation is verified under ISO 4892-2 as in agricultural service, but the acceptance criterion includes colour change and impact retention after 3,000 h. In temperate climates, the shell surface can reach 70 °C on a sunny day; the touch-temperature requirement is not controlled by the polymer alone, so shade structures or perforated panels are often added above open slide sections. Fasteners and metal posts are isolated from the moulded shell with polyethylene or rubber grommets; direct metal-to-polymer contact creates a difference in thermal expansion that can lead to fretting wear at cyclic load points. After 5 years of service, the stabilised skin may show chalking, which is a surface phenomenon rather than a loss of bulk mechanical integrity; retained impact toughness should be checked by cutting test coupons from replacement parts and subjecting them to a -20 °C drop dart test per ASTM D5276, with acceptance tied to the original moulded value.

    Free Quote

    Competitive LyondellBasell Icorene 3150 GRY 7776 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 3150 GRY 7776 is a linear low density polyethylene (LLDPE) rotational moulding powder. The base code 3150 identifies the resin grade within the Icorene family; the suffix GRY 7776 identifies a controlled grey pigment package. The material is supplied as a free-flowing powder rather than as pellets because rotational moulding requires a controlled particle size distribution, not a pellet feed. Under ISO 1043-1 the material is classified as PE-LLD. Melt flow rate and density are batch-controlled and shall be read from the certificate of analysis against ISO 1133-1:2022 and ISO 1183-1:2019 respectively. The manufacturer’s technical data sheet remains the controlling specification for any lot-specific value.

    Intended uses include single-layer rotomoulded tanks, containers, agricultural hoppers, and exterior panels where a balance of stiffness, impact, and environmental stress crack resistance is required. Because the base resin and the grey colour package may be produced in separate operations, the incoming lot should be compared with the previous approved lot. A shift in dry flow or sieve profile can occur without a shift in melt flow rate and should be monitored by statistical process control. The powder is often handled in bulk boxes or silos; transfer systems should be grounded because polyethylene powder can generate static charge. Conveying lines should not introduce metal fines or glass fibre residues.

    Polyethylene is not hygroscopic, but condensation on cold powder or silo walls at high relative humidity can create agglomerates that survive into the mould and appear as unmelted inclusions. At relative humidity above 60 %, dry air conveying or conditioned storage may be required. Contamination with polypropylene, PVC, or other polymer fines should be excluded. Even 0.5 wt% of a foreign semi-crystalline polymer can disrupt melt fusion and produce visual defects or weak boundary layers in the finished wall.

    What distinguishes the linear low density backbone from high-pressure LDPE in rotomoulding?

    LLDPE is produced by low-pressure coordination polymerisation with an α-olefin comonomer, giving chains with a linear backbone and short-chain branches. High-pressure LDPE, by contrast, contains long-chain branches from free-radical chemistry. This difference changes melt rheology and solid-state properties. At comparable melt flow rate under ASTM D1238, an LLDPE rotomoulding powder frequently demonstrates higher tensile elongation, greater puncture resistance, and longer environmental stress crack resistance measured by ASTM D1693 than an LDPE of similar density. The lower level of long-chain branching, however, can reduce strain-hardening behaviour in the melt. The grade must therefore be formulated with controlled molecular weight and comonomer distribution to resist sag while the powder densifies on the rotating mould surface.

    Compared with high-density polyethylene, an LLDPE grade such as Icorene 3150 GRY 7776 has lower flexural modulus under ASTM D790 and lower softening point under ASTM D1525. It may provide better low-temperature impact performance and better resistance to slow crack growth in thick-walled parts. The product is therefore used where toughness and ESCR are more important than maximum rigidity: storage tanks, waste containers, agricultural hoppers, and outdoor enclosures. The 3150 designation should not be assumed to match another Icorene grade of different melt index; each base code has a separate melt flow range and stabiliser package.

    Specification and certification test method matrix

    PropertyReference methodReported unit
    Melt flow rate, 190 °C/2.16 kgASTM D1238 / ISO 1133-1:2022g/10 min
    DensityASTM D1505 / ISO 1183-1:2019g/cm³
    Tensile yield stress and elongationASTM D638 / ISO 527-2MPa, %
    Flexural modulusASTM D790 / ISO 178MPa
    Environmental stress crack resistanceASTM D1693, 100 % Igepal CO-630h, F50
    Low-temperature brittlenessASTM D746 / ISO 974°C
    Falling dart impactASTM D5628 / ISO 6603-2J or J/mm
    Powder dry flowASTM D1895 Method A / ISO 6186s
    Particle size distributionASTM D1921 / ISO 4610% retained
    Colour differenceASTM D2244 / ISO 11664-4ΔE*

    The table identifies the standard test matrix used to verify incoming material. It does not state that any single batch meets every listed method; the certificate of analysis controls the results for the lot. Published data for this specific GRY 7776 configuration are limited in public documents. Substitution decisions should rely on the manufacturer’s current technical data sheet and a trial on the intended mould, not on generic LLDPE class averages.

    Internal air temperature, not oven temperature, controls part densification.

    On carousel and shuttle rotational moulding machines, oven air temperature may be set between 260 °C and 320 °C, but that external condition is only a heat source. The process variable that correlates with part densification is the internal air temperature inside the rotating mould. The powder bed absorbs heat from the tool, melts, and fuses into a continuous layer. If the internal air temperature remains below a grade-dependent threshold, the inside surface retains pinholes and microvoids. Removing the part too early reduces low-temperature impact strength and ESCR. Internal air temperature is typically measured with an in-mould thermocouple or an IR pyrometer with emissivity correction for the grey surface. Published rotational moulding process literature for LLDPE indicates that full densification occurs within a temperature range above the crystalline melting point, but the exact plateau for Icorene 3150 GRY 7776 must be established on the intended tooling because wall thickness, mould geometry, and oven heat transfer rate change the response.

    Thick sections require longer internal air holds. An increase in wall thickness from 3 mm to 6 mm can extend the internal air plateau time significantly because the powder bed must densify through a larger thermal mass. The exact time depends on oven set point, tool material, and pigment absorptivity. The powder bed must also spread evenly before melting. On a carousel or shuttle machine with a 4:1 or 5:1 biaxial arm ratio, poor dry flow can produce angular thickness variation. Dry flow measured by ASTM D1895 Method A or ISO 6186 is a useful incoming inspection parameter. Particle size distribution by ASTM D1921 or ISO 4610 affects bubble disappearance; a distribution skewed to excessive fines can increase dust and reduce dry flow, while coarse particles can settle and reduce surface smoothness. The grey pigment package may modify bulk density relative to natural powder and should be checked after colour blending. For pigmented LLDPE, tool-surface temperature control within ±5 °C is often necessary to prevent visible colour differences caused by nonuniform cooling histories.

    In-oven failure modes observed on production lines include uneven pigmentation at sharp corners and local thinning around inserts. A colour package with a different melt viscosity or particle size distribution from the base powder may not remain uniformly distributed during rotation. Corner thickness should be checked after prototype runs with an ultrasonic gauge or a ball micrometer. External mould release agents should not be applied until a clean mould surface has been tested; residual release agent can reduce adhesion of the powder layer and create surface defects.

    After demoulding, cooling rate changes the crystalline structure. Quenching with water spray or compressed air reduces crystallinity and can lower flexural modulus, while slow cooling increases crystallinity and shrinkage. For LLDPE rotomoulding powders, mould shrinkage is process-dependent and may fall between 1.5 % and 3.5 %. A prototype tool should be used to measure actual shrinkage for the part geometry. Internal stress generated by rapid cooling can reduce ESCR; if the application requires long-term chemical exposure, slower cooling or post-mould annealing below the crystalline melting point should be evaluated.

    Mechanical performance values for rotomoulded LLDPE are meaningful only when the specimen preparation route is identified. The manufacturer’s typical physical properties are usually generated on rotomoulded or compression-moulded plaques, not on injection-moulded specimens. A user comparing Icorene 3150 GRY 7776 with another rotomoulding powder should request the same specimen preparation and conditioning history. Properties generated under ISO 291 and ASTM D618 can differ from those measured on parts taken directly from the mould floor. Cross-comparisons between rotomoulded plaques and injection-moulded test bars are invalid because the thermal history and molecular orientation differ.

    For demanding rigidity applications with a flexural modulus target above 1,000 MPa, a high-density or mineral-filled rotomoulding powder may be more appropriate, but that substitution can reduce ESCR and low-temperature impact. For parts requiring moderate stiffness and high toughness, the 3150 LLDPE base is positioned toward the lower-density end of the polyolefin rotomoulding range. Comparative selection should use a full test battery under ASTM D638, ASTM D790, ASTM D1693, and ASTM D5628. Differences from other Icorene grades become visible in melt flow and density. A higher-melt-index grade may fill deep cavities more easily but can sacrifice ESCR and long-term creep resistance. A lower-melt-index grade can improve toughness and chemical resistance but may require longer oven cycles and may show poorer surface replication. Direct substitution should not be made without comparing the certificate of analysis and completing a mould trial because the pigment package can shift melt rheology and cooling shrinkage.

    If the 7776 grey colour package is specified for outdoor service, accelerated weathering should not be inferred from the colour code alone.

    A grey pigment package may contribute to ultraviolet screening, but weathering performance depends primarily on the base resin’s stabiliser system. The suffix GRY 7776 denotes colour, not a specific UV-stability rating. Accelerated weathering is evaluated by ISO 4892-2 or ASTM D2565 using xenon arc exposure with water spray. ASTM G154 is a supplementary screening method but may overrepresent the effect of certain UV-B wavelengths. Post-exposure retention of tensile elongation under ISO 527-2 or ASTM D638 is more informative than visual colour change alone. Colour difference is reported as ΔE* under ASTM D2244 or ISO 11664-4 with a defined illuminant and observer. Gloss loss is measured by ASTM D523 or ISO 2813; chalking and cracking are recorded according to the relevant surface evaluation methods.

    For long-term exterior tanks, cladding, and outdoor enclosures, the converter should obtain the manufacturer’s weatherability statement and, where possible, results from naturally weathered test panels. Published data for this specific grey configuration are limited. The pigment system may change thermal absorption or nucleation. The maximum service temperature and cumulative UV exposure limit are operational boundaries that shall be defined by the manufacturer’s test data, not by general LLDPE class values. If a natural or black UV-stabilised grade is approved for an application, the grey version should be revalidated because the pigment package can interact with stabiliser activation and surface oxidation.

    Assessing chemical compatibility in liquid-contact rotomoulded parts

    LLDPE has broad resistance to aqueous, alkaline, and polar solvent environments, but no unfilled polyethylene is universally resistant. Chemical containers, agricultural tanks, and industrial liners should be tested in the intended contact fluid under ASTM D543 at 23 °C and at the maximum service temperature. Aromatic hydrocarbons, chlorinated solvents, and strong oxidising acids can soften or stress-crack LLDPE. Environmental stress crack resistance measured by ASTM D1693 does not guarantee compatibility with every fluid; it is a slow crack growth test in a specific surfactant environment and is not a substitute for immersion testing in the target chemical.

    If food-contact or drinking-water compliance is required, the base polyethylene may be evaluated under 21 CFR 177.1520 or Regulation (EU) No 10/2011, but the grey pigment package must also meet the applicable positive list and migration limits. The converter should request a compliance statement for the finished colour-matched powder and should not assume that natural-grade approvals apply automatically to the GRY 7776 version. For toys, relevant regional standards such as EN 71-3 may apply to accessible material migration. No conclusion regarding food-contact status can be drawn from the product name alone.

    Top