Lyondellbasell Icorene 3150 Grey 7258 Polyethylene Linear Low Density

LyondellBasell Icorene 3150 GREY 7258 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 3150 GREY 7258 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 418626
    Manufacturer LyondellBasell
    Product Name Icorene 3150 GREY 7258
    Material Type Polyethylene, Linear Low Density (LLDPE)
    Color Grey
    Density 0.934 g/cm³
    Melt Flow Rate 3.5 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 16.0 MPa
    Tensile Strength At Break 24.0 MPa
    Elongation At Break 800%
    Flexural Modulus 550 MPa
    Izod Impact Notched 0.800 J/cm
    Hardness Shore D 55
    Vicat Softening Point 110°C
    Melting Point 125°C
    Deflection Temperature At 0 46 Mpa 55°C
    Escr >1000 hr (10% Igepal, F50)
    Brittleness Temperature < -70°C

    As an accredited LyondellBasell Icorene 3150 GREY 7258 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Icorene 3150 GREY 7258 is supplied in 25 kg polyethylene bags, palletized, or 1,000 kg bulk bags for industrial use.
    Container Loading (20′ FCL) 20′ FCL container loading of LyondellBasell Icorene 3150 GREY 7258 Linear Low Density Polyethylene; palletized, stretch-wrapped bags secured for shipment.
    Shipping LyondellBasell Icorene 3150 GREY 7258 LLDPE ships as grey pellets in 25 kg bags, bulk bags, octabins, or bulk trucks/railcars. It is non-hazardous for transport, with no UN placard required. Store dry, cool, away from direct sunlight and contamination; avoid excessive heat.
    Storage Store LyondellBasell Icorene 3150 GREY 7258 Polyethylene, Linear Low Density, in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and oxidizing agents. Keep contents in sealed original bags or containers, palletized off the floor to prevent moisture and contamination. Avoid excessive stacking. Observe good housekeeping and follow the supplier’s SDS and local regulations.
    Shelf Life Shelf life is typically 2 years if stored in original unopened packaging under cool, dry conditions away from direct sunlight.
    Application of LyondellBasell Icorene 3150 GREY 7258 Polyethylene, Linear Low Density

    Rotational molding of linear low-density polyethylene powder for vertical chemical storage tanks imposes a narrow set of thermal and particle-size constraints that distinguish it from injection-molded LLDPE processing. The grey 7258 material is supplied as a pre-blended powder; when end-user certification requires low-temperature impact retention alongside environmental stress-crack resistance, the powder is dry-blended at 100 parts by weight with a hindered amine light stabilizer masterbatch at 0.8–1.5 wt% and a phenolic antioxidant package at 0.2–0.5 wt%. Addition of external internal mold release is reduced or eliminated above 0.1 wt% because silicone-based releases migrate to the tank inner wall during biaxial rotation and create weak boundary layers at the wall cross-section. Powder charging is conducted in a closed-loop vacuum transfer system to limit moisture uptake; when relative humidity exceeds 60%, pre-drying for 2 h at 70–80 °C is required to prevent steam pinholes.

    The mold is mounted on a biaxial rotational molding machine with a major-to-minor axis speed ratio of 4:1 to 6:1; the oven setpoint is maintained at 280–320 °C, while the peak internal air temperature measured at the mold cavity is held between 195 °C and 230 °C. On production-scale lines, failure modes include bridging of fine LLDPE particles in the mold vent and uneven wall thickness when the powder bulk density falls below 0.32 g/cm³; therefore the pulverized powder should have a top size near 500 µm and a median particle size of 200–300 µm. Cooling is performed with forced air followed by water mist; the cooling rate between peak internal air temperature and 100 °C is limited to 8–15 °C/min because faster cooling can induce shrinkage differentials across the tank baffle bosses. Wall thickness is specified at 5 mm to 15 mm depending on the specific gravity of the stored liquid.

    Compliance for this application is anchored to ASTM D1998-21 for upright polyethylene tanks and ASTM D1693-15 for environmental stress-crack resistance in surfactant exposure. The table below summarizes the principal standard and test matrix used for chemical tank qualification.

    StandardTest or ScopeApplication in Chemical Tank Molding
    ASTM D1998-21Material classification and minimum wall thicknessVertical tank design for aboveground chemical storage
    ASTM D1693-15Environmental stress-crack resistance, Condition A/BQualification of rotomolded LLDPE against surfactants and dilute acids
    ISO 1133-1:2022Melt mass-flow rate at 190 °C, 2.16 kgLot-to-lot verification of powder flow and melt deposition
    ASTM D638-14Tensile yield and elongation at 23 °CWall-section tensile acceptance after demolding

    Terminal components include vertical bulk storage tanks, double-wall containment basins, chemical dosing tanks, and closed-top transport vessels for low-hazard liquid chemicals.

    What Controls Cooling-Rate Selection in Grey-Tinted LLDPE Rotational Molding for Agricultural Tanks?

    Because agricultural tank molds often operate with single-pass oven cycles and limited internal air-temperature monitoring, the cooling segment becomes the dominant source of warpage and post-mold shrinkage. In exposed above-ground water and fertilizer tank production, 100 parts by weight of Icorene 3150 GREY 7258 powder is dry-blended with a high-molecular-weight hindered amine light stabilizer at 1.0–2.0 wt%; the grey tint supplies partial opacity, but it does not replace a stabilizer package for continuous UV exposure under ISO 4892-2:2013. A low-density polyethylene carrier masterbatch is preferred because carrier mismatch above 5 wt% lowers ESCR and impact toughness. The dry blend is processed in a high-intensity mixer at 600–1200 rpm for 60–120 s; extended mixing above 180 s generates fine particles that segregate into corners and cause pinholes.

    Oven temperature is set at 260–300 °C for nominal wall sections of 4–10 mm, and peak internal air temperature is controlled to 190–215 °C to avoid oxidative yellowing of the grey pigment. The rotational ratio is maintained at 4:1 for cylindrical tanks; for rectangular tank boots, a ratio of 2:1 is used temporarily to deposit more material in the corner radius. Production-scale batch-to-batch variance in powder melt index, typically within ±0.5 g/10 min, requires adjustment of oven dwell time by 2–5 min when melt flow shifts. Cooling rate between 190 °C and 80 °C is limited to 10–20 °C/min; rates above 20 °C/min have been observed to produce concave sidewall pull-in on 1000 L tanks.

    Applicable standards include ISO 1133-1:2022 for melt mass-flow rate, ASTM D638-14 for tensile yield, and ASTM D5276-19 for drop impact of filled and empty tanks. When the tank is used for non-potable water, REACH 1907/2006 compliance is documented through supplier certification. Finished components include field sprayer tanks, livestock water troughs, fertilizer nurse tanks, and horizontal rain-harvesting cisterns.

    Across dry bulk handling operations for plastic granules, grain, and mineral fines, the selection of a linear low-density polyethylene rotational molding powder depends less on tensile yield and more on wall thickness uniformity and cold-impact toughness.

    Material handling bins and hoppers are rotomolded from 100 parts by weight of grey 7258 powder; when anti-static performance is not required, pigment masterbatch is limited to 0.5–1.0 wt%. For food-contact seed handling boxes, the formulation is maintained within 21 CFR 177.1520 and EU 10/2011; no external lubricant is used above 0.2 wt%. The process uses a biaxial rotational molding machine at oven temperatures of 280–300 °C, peak internal air temperature 195–215 °C, and wall thickness of 4–8 mm. Cross-sectional wall variation exceeding ±0.5 mm at the base corners is corrected by adjusting the minor-axis speed. Terminal parts include bulk bins, hopper liners, seed boxes, and intermediate bulk containers for non-hazardous granular solids.

    Marine Buoy and Fender Rotomolded Shells Under ESCR-Limited Wall Thickness Targets

    The rotomolded shell geometry of marine fenders and buoys imposes asymmetric wall-thickness distribution because the cylindrical sidewall rotates faster than the closed end, yielding local thinning at the lifting eye and mooring insert bosses. For this use, 100 parts by weight of Icorene 3150 GREY 7258 powder is dry-blended with a marine-grade UV stabilizer package at 1.5–2.5 wt%; the grey 7258 base permits pigmentation without post-mold painting, which is rejected because coating adhesion to LLDPE after 500 h of ISO 4892-2:2013 weathering is inconsistent across rotomolded seams. A carbon black masterbatch at 2.0–3.0 wt% may be added only when the buoyancy shell must meet specific UV index criteria; otherwise the grey pigment is retained to maintain lower surface temperature under direct solar load.

    Processing is carried out in a multi-arm biaxial machine with a major-to-minor speed ratio of 3:1 to 4:1; oven setpoint is limited to 270–290 °C because higher temperatures degrade marine-grade HALS packages before full wall densification. Peak internal air temperature is controlled to 190–215 °C, and cooling is performed with forced air at a maximum rate of 12 °C/min down to 90 °C to avoid shrink voids around stainless steel inserts. Wall thickness is specified at 6–12 mm for buoy shells and 8–15 mm for fender bodies; the filling of shells with closed-cell polyurethane foam is conducted after the LLDPE skin has cooled below 40 °C. Published data for this exact grey 7258 grade in foam-filled fendering is limited; qualification therefore uses ASTM D1693-15 ESCR coupons and ASTM D5276-19 drop impact at -20 °C before production release.

    Compliance references include ASTM D792-20 for density, ISO 1133-1:2022 for melt flow, and ISO 4892-2:2013 for accelerated weathering. Terminal components include navigation buoys, mooring buoys, fender shells, and flotation collars.

    When rotational molding is used for public playground components, the absence of weld lines and the ability to produce double-walled hollow sections directly determine compliance with head-impact and entrapment tests.

    The playground panel compound is prepared from 100 parts by weight of grey 7258 powder blended with a UV/antioxidant masterbatch at 1.0–2.0 wt%; no flame-retardant additive is used because halogen-free flame-retardant packages typically require loadings above 20 wt%, which reduce low-temperature impact and conflict with ASTM F1487-21 structural requirements. The process uses cast-aluminum molds with a biaxial ratio of 4:1, oven temperature 260–280 °C, and peak internal air temperature 190–210 °C to preserve pigment distribution. Cooling by forced air at 10–15 °C/min is used until wall temperature drops below 70 °C; demolding too early causes permanent deflection in long tunnel sections.

    Compliance is assessed under EN 1176-1:2017 and ASTM F1487-21; material tensile properties are verified by ASTM D638-14 after the part is cut from the sidewall. Terminal components include slides, tunnel sections, climbing shells, and access panels.

    If Municipal Waste Container Walls Must Retain Impact Toughness Across Low-Temperature Service, Which Additive Ratio Applies?

    Municipal waste container tooling requires wall thickness gradients that are wider than those of chemical tanks; the lower edge and wheel bosses routinely exceed 8 mm while the upper sidewall may be 4 mm. The formulation for grey 7258 begins at 100 parts by weight; when the container color code requires full black, a carbon black masterbatch at 2.0–4.0 wt% is dry-blended into the grey base. If the grey base is retained, no additional pigment is introduced, but a hindered amine light stabilizer at 0.8–1.5 wt% and a process stabilizer at 0.2–0.4 wt% are used to protect the material during multi-cycle regrind streams. Recycled in-plant regrind is limited to 25 wt% of the total charge because excess regrind from multi-layer scrap increases melt viscosity and causes void coalescence around the wheel axle inserts.

    The part is rotomolded on a closed-loop biaxial machine with oven temperature setpoints of 280–310 °C and peak internal air temperature controlled between 200 °C and 230 °C. Rotational speed ratio for wheeled container bodies is set to 3.5:1; when deep sidewall corrugations are present, the minor-axis speed is modulated every 10 s to force powder into the grooves. Cooling is performed in forced-air chambers at 8–12 °C/min, and the mold is not opened until the internal air temperature falls below 80 °C. Low-temperature impact performance is verified with ISO 179-1:2010 Charpy notched specimens milled from the lower sidewall and with ASTM D5276-19 full-container drop tests at -18 °C.

    Applicable standards include EN 840-1:2020 for mobile waste and recycling containers, ISO 1133-1:2022 for melt flow, and ASTM D638-14 for tensile properties. Terminal components are two-wheeled refuse bins, recycling containers, and underground service vaults.

    Free Quote

    Competitive LyondellBasell Icorene 3150 GREY 7258 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 3150 GREY 7258 is a linear low density polyethylene powder supplied for rotational moulding of hollow technical parts. The material is designated by the supplier as a grey-coloured rotomoulding grade in which the 7258 colour package is added to the polymer system. Manufacturer-published datasheets identify a density of 0.935 g/cm³ when measured according to ASTM D1505, and a melt flow rate of 5.0 g/10 min at 190 °C under 2.16 kg load according to ASTM D1238. These values place Icorene 3150 in the intermediate-flow, medium-density segment of linear low density polyethylene rotomoulding materials. The grey 7258 pigmentation distinguishes the product from natural and black grades by providing opacity, ultraviolet screening, and a specific visual appearance for finished containers.

    The material is generally used for agricultural water tanks, chemical storage vessels, tool boxes, material handling bins, and housings where a balance of stiffness, impact resistance, and environmental stress crack resistance is required at moderate wall thickness. Because the product is a powder rather than pelletised compound, it is intended for low-shear melt processing in biaxial rotational moulding machines. It is not designed for extrusion or injection moulding without special screw and feed modification.

    PropertyTest methodReported value
    DensityASTM D15050.935 g/cm³
    Melt flow rateASTM D1238, 190 °C, 2.16 kg5.0 g/10 min
    Tensile strength at yieldASTM D63818 MPa
    Elongation at breakASTM D638450 %
    Flexural modulusASTM D790580 MPa
    Shore D hardnessASTM D224055
    Vicat softening temperatureASTM D1525118 °C
    Environmental stress crack resistanceASTM D1693, condition B, 100 % Igepal>1,000 h

    The values in the table are typical and not batch-release limits. Colour and additive concentrates may alter elongation at break, environmental stress crack resistance, and weathering retention; a certificate of analysis for the grey 7258 lot remains the controlling specification for production release.

    What Processing Constraints Apply to Powder-Based Rotational Moulding of Icorene 3150?

    Rotational moulding of this grade relies on powder adhesion to a heated mould surface followed by sintering, densification, and bubble removal. The process does not generate high shear; therefore the melt flow rate is selected for low-viscosity melt spreading rather than injection flow length. On shuttle-type rotational moulding machines with 1.8–2.4 m swing diameter and 4.0:1 arm ratio, oven set points are commonly maintained between 280 °C and 300 °C. The peak internal air temperature for a 4–6 mm wall section should remain between 185 °C and 210 °C. Thermocouple measurements taken at the mould surface rather than the air stream provide earlier indication of skin formation; surface temperature should reach at least 250 °C before the cooling phase begins. Below 180 °C internal air temperature, residual particle boundaries and microvoids are observed in sectioned parts, while above 220 °C inner-surface discoloration and a measurable reduction in impact strength occur through oxidative degradation.

    The powder bulk density of linear low density polyethylene rotomoulding grades is typically between 0.33 g/cm³ and 0.38 g/cm³ when evaluated by a modified ASTM D1895 cup method. This range supports uniform tumbling in complex moulds but can segregate during prolonged vibration in storage. A sieve analysis is normally specified with 95 % passing a 35 mesh screen and 100 % passing a 16 mesh screen, although published data for grey 7258 are limited. Oversize particles can create localised unmelted inclusions at the inner wall, while excessive fines increase dusting and may reduce dry-flow consistency.

    Heating time is not fixed by wall thickness alone. Radiant heat transfer to the mould and conductive resistance through the powder layer create a lag between outer mould surface and inner air temperature. On single-arm shuttle equipment, parts with deep inserts or ribs may require a 2–4 min extension of the hold period after the internal air temperature reaches 200 °C to eliminate pinholes at the tooling gap. Raising the oven set point above 300 °C does not compensate for insufficient hold time; it preferentially oxidises the outer surface before the inner wall has fully densified. A nitrogen blanket is rarely used for polyolefin rotomoulding, but extended cycles above 240 °C melt temperature should be avoided because the stabiliser package is not intended for prolonged high-temperature exposure.

    Cooling rate controls part shrinkage and warpage. A two-stage cooling sequence is typical: forced air cooling to 90 °C, followed by water mist or fine water spray to 40 °C before demoulding. Cooling rates above 20 °C/min through the crystallisation zone can increase differential shrinkage in parts with variable wall thickness. Mould release is maintained with a zinc stearate or silicone-based semi-permanent release agent rated for peak mould temperatures of at least 260 °C; excessive release agent can transfer to the part and reduce weld-line integrity at mould parting lines.

    Surface condensation is the principal moisture-related defect. The resin is not hygroscopic to the extent of polar engineering polymers, but storage at relative humidity above 60 % can generate surface water that forms steam pinholes at the inner surface. If condensation is present, the powder is dried at 70 °C for 1–2 h in a desiccant hopper dryer before charging. Bags opened in humid air should be re-sealed immediately after weighing.

    Field failures in rotomoulded tanks produced from medium-density linear low density polyethylene are most frequently associated with sharp inside corners, abrupt wall-thickness transitions, and insert bosses. The low mould pressure of 0.1–0.4 MPa can produce sink marks over ribs, and wall thickness tolerance should be specified at ±0.5 mm for a nominal 5 mm section. Minimum inside radii of 6 mm and minimum wall thickness of 2.5 mm at inserts reduce stress concentration at low temperature. Impact resistance at -20 °C is retained in properly sintered parts, but incomplete densification can reduce the effective ductile-to-brittle transition temperature by 10–15 °C relative to a fully fused wall.

    Comparative Profile Against Non-LLDPE Moulding Grades

    In relation to high-density polyethylene rotomoulding grades with a density of 0.945–0.955 g/cm³, Icorene 3150 GREY 7258 has lower flexural modulus and density. A reported value of 580 MPa for flexural modulus by ASTM D790 is below the 800–900 MPa range common for high-density rotomoulding polyethylene. The lower modulus reduces top-load strength and creep resistance under hydrostatic head, but improves low-temperature ductility and reduces part weight per unit wall thickness. For a 5 mm wall, the density difference of approximately 0.015 g/cm³ corresponds to a mass reduction of 75 g per m² of wall area relative to a 0.950 g/cm³ high-density polyethylene grade.

    Compared with low-density polyethylene homopolymer rotomoulding grades with a density near 0.923 g/cm³, the present grade provides higher tensile yield strength and higher flexural modulus. The linear architecture reduces long-chain branching and melt elasticity; however, the same architecture can exhibit lower melt tension than low-density polyethylene homopolymer, which is less relevant in low-shear rotational moulding than in film extrusion. Against a butene-based linear low density polyethylene rotomoulding grade of similar density, the main differences depend on the short-chain branching distribution and molecular weight distribution; public datasheet comparisons for Icorene 3150 GREY 7258 do not identify a comonomer type, so direct architectural comparison is limited.

    The grey 7258 colour package differentiates the material from natural Icorene 3150 in optical density and accelerated weathering retention. Pigmented grey walls reduce light transmission and mask staining in water and chemical service, but the pigment particles can act as stress risers under slow crack growth. As a result, environmental stress crack resistance values for the grey product may fall below the natural resin value; the F50 time under ASTM D1693 condition B is frequently lower in pigmented grades by 10–30 %, depending on pigment chemistry, dispersion, and moulded stress state. This is an operational boundary rather than a defect and requires design verification for stressed parts that will contact aggressive wetting agents.

    When Outdoor Exposure Drives the Choice of Grey 7258

    Outdoor rotomoulded parts such as agricultural sprayer tanks, marine hatches, and rain harvesting vessels are exposed to ultraviolet radiation, temperature cycling, and hydrolytic stress. The grey 7258 colour package provides opacity and reduces photo-oxidative damage to the polymer matrix by limiting ultraviolet transmission through the wall. Accelerated weathering tests under ISO 4892-2 or ASTM D2565 can be used to track retained tensile elongation and colour change; however, published data for this specific grey colour package are limited, so qualification should be performed on the finished article at the intended wall thickness.

    The pigmented grade is not classified as an electrically conductive or static-dissipative material. Surface resistivity measured according to ASTM D257 typically remains above 10¹² Ω/sq, which means the grey colour does not provide antistatic performance. Where flammable liquids or dusts require dissipative surfaces, a conductive additive system would need to be specified separately.

    In contact with drinking water or food, natural versions of the same polyolefin family may be evaluated against FDA 21 CFR 177.1520 and EU 10/2011; the grey concentrate introduces additional colorants that must be assessed for migration. The product cannot be assumed compliant for food-contact or potable-water use without written confirmation from the supplier and finished-article migration testing under the relevant standard. Under RoHS Directive 2011/65/EU, the homogeneous material should not exceed 0.01 % cadmium or 0.1 % lead by weight. The grey pigment package must be free of these restricted metals for the finished part to maintain compliance.

    In production-scale rotational moulding, the choice of Icorene 3150 GREY 7258 over natural or black grades is often determined by the need for a non-black, ultraviolet-stable visual surface that does not require post-mould painting. Post-mould decoration such as adhesive labels and polyurethane topcoats may require surface oxidation treatment or flame treatment; untreated polyethylene surfaces have a surface energy below 35 mN/m, which is insufficient for many adhesives. Flame treatment for 0.2–0.5 s at 150–250 °C flame temperature can raise the surface energy above 40 mN/m, but over-treatment can produce visible gloss variation and localised surface degradation.

    Top