| HS Code | 746043 |
| Density | 0.935 g/cm3 |
| Melt Flow Rate | 20 g/10 min |
| Tensile Strength At Yield | 10.0 MPa |
| Tensile Strength At Break | 12.0 MPa |
| Elongation At Break | 800 % |
| Flexural Modulus | 0.300 GPa |
| Hardness Shore D | 50 |
| Vicat Softening Point | 90.0 °C |
| Melting Point | 125 °C |
| Coefficient Of Linear Thermal Expansion | 1.50E-4 cm/cm/°C |
| Specific Heat Capacity | 2.00 J/g-°C |
| Color | Green 6239 |
As an accredited LyondellBasell Icorene 3150 GREEN 6239 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 3150 GREEN 6239 LLDPE packaged in 25 kg polyethylene-lined paper bags, 40 bags per stretch-wrapped pallet (1,000 kg). |
| Container Loading (20′ FCL) | 20′ FCL container loading for LyondellBasell Icorene 3150 GREEN 6239 Linear Low Density Polyethylene: palletized 25 kg bags, secured for transport. |
| Shipping | LyondellBasell Icorene 3150 GREEN 6239 Polyethylene, Linear Low Density is shipped as non-hazardous pellets in 25 kg bags, bulk bags, or railcars. Transport in clean, dry vehicles. Store cool/dry, away from heat, sunlight, moisture, and contaminants. Avoid spills; pellets are slippery. Use standard handling and follow transport regulations. |
| Storage | Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and flames. Keep original bags closed, palletized, and protected from moisture, dust, and contamination. Avoid contact with strong oxidizers. Maintain ambient temperature, use first-in-first-out stock rotation, stack securely, and inspect containers regularly for damage. Do not store outdoors. |
| Shelf Life | Shelf life: 24 months when stored in original unopened packaging in a cool, dry, well-ventilated area away from direct sunlight. |
In agricultural liquid storage, the rotational molder’s selection of LyondellBasell Icorene 3150 GREEN 6239 linear low density polyethylene is driven by the need to withstand prolonged contact with fertilizer salts, ester-based crop protection formulations, and nonionic surfactant wetting agents that accelerate environmental stress crack resistance loss. The formulation is charged at 100 wt% as supplied for the primary liquid-contact wall; regrind generated from trimmed fill ports and mounting bosses may be reintroduced at a maximum of 20 wt% in the outer unexposed layer only, because higher recycled content depresses ESCR measured according to ASTM D1693-15 Condition B in 10% Igepal CO-630 at 50 °C. Compliance for stationary tanks follows ASTM D1998-15 for upright storage and AS/NZS 4766:2006 for water and chemical service, with hydrostatic testing at 1.5× the maximum design head before shipment. Production is executed on rock-and-roll rotomolding machines for horizontal cylindrical sprayer geometries, with a biaxial rotation ratio of 4:1 on the minor axis and 1:1 on the major axis, oven setpoint 270–290 °C, peak internal air temperature 200–220 °C, and forced-air cooling to 85 °C before water spray quench. Terminal components include pesticide nurse tanks, fertilizer induction hoppers, and 200–2000 L horizontal agrochemical transport tanks with integrally molded baffles and threaded valve bosses.
Above-ground water tanks subject to continuous hydrostatic wall stress do not fail primarily by tensile yield; slow crack growth at internal corners and molded-in threaded inserts is the limiting mode. The LLDPE grade is processed at 100 wt% for monolayer vertical cisterns, while foam-core insulation constructions use a core formulation containing 0.5–2.0 wt% endothermic sodium bicarbonate–citric acid chemical foaming agent between two unfilled skins of Icorene 3150 GREEN 6239, yielding a density reduction of 20–35% in the core without reducing the potable-water-contact layer thickness below 2 mm. NSF/ANSI 61 certification is required where the stored water is intended for human consumption, and the finished tank is extracted at pH 5 and pH 8 to measure total organic carbon and trace metals. Manufacturing on carousel rotomolding platforms uses cast aluminum molds with thermal oil channels and a biaxial rotation ratio of 4.5:1; oven temperature is held at 280–300 °C until the peak internal air temperature reaches 210–225 °C, after which cooling is slowed by first ambient air to 90 °C followed by fog spray to limit shrinkage-induced warpage at the dome. Finished parts include vertical water storage tanks, rainwater harvesting cisterns, and thermal buffer reservoirs for solar hydronics.
| Application | Standard | Test method / designation | Process relevance |
|---|---|---|---|
| Agricultural chemical tanks | ASTM D1998-15 | Hydrostatic design stress and joint test | Wall thickness and fitting reinforcement |
| Potable water tanks | NSF/ANSI 61 | pH 5 and pH 8 extraction | Inner skin formulation control |
| Marine floats | 2014/90/EU | Type examination certificate | Buoyancy chamber integrity |
| Playground components | EN 1176-1:2017 | Head and neck entrapment probe | Wall distribution and opening geometry |
When marine buoy molds are run on multi-arm carousel machinery, the principal processing conflict is between uniform wall formation and the need for localized wall thickening at the mooring eye. The shell formulation remains 100 wt% Icorene 3150 GREEN 6239 for unfoamed floats; where additional buoyancy reserve is specified, a two-shot method introduces a foamable core compound containing 0.5–1.5 wt% azodicarbonamide that expands during the second rotomolding pass but must not breach the outer skin. Marine service compliance follows 2014/90/EU when supplied as marine equipment on European-flagged vessels, with type examination requiring pressure-decay testing of the buoyancy chamber. The first pass at 280 °C oven setpoint forms a shell with nominal wall thickness 5 mm; the mold is then partially opened, the foaming charge is added, and a second pass at 230–250 °C expands the core without melting the outer surface. Air-cooled demolding is mandatory until the internal air temperature drops below 80 °C, because premature ejection from a steel mold at higher temperatures causes the partially crystalline shell to tear at the mooring boss. Terminal products include navigation buoys, floating dock floats, aquaculture rafts, and marine fender shells.
Temporary traffic control barriers molded from Icorene 3150 GREEN 6239 are not crash-rated as stand-alone shells; the complete installation must be filled with water or sand to meet the applicable impact test. The LLDPE formulation is used at 100 wt% for the shell exterior, while up to 30 wt% re-pulverized internal scrap can be mixed into the center layer of a three-layer construction because the outer layers remain 100 wt% virgin. Compliance for the installed system follows MASH 2016 for U.S. roadside hardware when the filled barrier is placed as part of a certified model; the plastic shell itself conforms to ASTM D2990 tensile creep and creep-rupture testing under constant load. Production uses shuttle rotomolding machines with a single arm per station, biaxial rotation of 4:1, oven temperature 270–285 °C, and peak internal air temperature 200–215 °C; mold venting must remain unobstructed because blowing agent byproducts from recycled material can pressurize the parting line. Terminal products include water-filled construction barriers, sign bases, temporary delineator drums, and wheel stop blocks.
Rotational molded playground components are subject to impact attenuation and entrapment requirements that restrict wall thickness variation around openings and joint bosses. The base formulation is used at 100 wt% for slides, tunnel sections, and roof panels; when foam-filled double-wall rigidity is specified, the core layer receives 1.0–2.0 wt% endothermic chemical foaming agent while the outer skins remain unfilled, maintaining a minimum outer skin thickness of 3 mm to resist UV-induced surface cracking. Compliance is tested under EN 1176-1:2017 for safety requirements and installation, with head and neck entrapment probes, and under ASTM F1487-21 for public playground equipment where access is not supervised. Production on carousel rotomolders uses polished stainless steel molds for aesthetic surfaces and a peak internal air temperature of 205–220 °C; after demolding, slide sections are assembled with through-bolts bearing Nyloc nuts and nylon washers to prevent loosening under dynamic load. Finished goods include crawl tunnels, slide beds, play panels, and roof components for modular playground systems.
Typically, insulated transport liners are manufactured as a two-shell assembly rather than a single unsupported polyethylene wall, because the service requirement is thermal hold time rather than hydrostatic strength. The outer and inner shells are each molded from 100 wt% Icorene 3150 GREEN 6239; the gap between shells is filled with polyurethane foam of density 38–45 kg/m³, which is injected after assembly and allowed to cure at 50–60 °C for 20–30 min to reach dimensional stability. Compliance for direct food contact is governed by FDA 21 CFR 177.1520(c) and EU 10/2011 Annex I, with migration testing performed under the intended food simulant; pharmaceutical cold chain use additionally requires cleanroom molding and wipe-down validation. The rotomolding process runs on shuttle machines with a 4:1 biaxial ratio, oven temperature 270–290 °C, PIAT 200–215 °C, and a mold release applied at 0.5–1.0 g/m² to prevent transfer into food-contact surfaces. Finished products include insulated fish tubs, meat lug boxes, dairy transport liners, and payload boxes for temperature-controlled logistics.
Competitive LyondellBasell Icorene 3150 GREEN 6239 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 3150 GREEN 6239 is a pre-coloured linear low density polyethylene (LLDPE) rotational moulding grade supplied as a pulverised powder for biaxial rotational moulding machines. The base polymer, Icorene 3150, is classified by the manufacturer as a linear low density ethylene copolymer; the suffix GREEN 6239 identifies a proprietary green pigmentation package rather than a separate alloy or blend. The material is used where a moulded-in green colour, low-temperature toughness and geometric complexity are required in hollow parts such as tanks, bins, housings and outdoor equipment enclosures. Published technical data for the base resin list a nominal melt flow rate of 5.0 g/10 min at 190 °C under 2.16 kg load, tested according to ASTM D1238-20 / ISO 1133-1:2022, and a nominal density of 0.935 g/cm³ measured according to ASTM D792-20 method B or ISO 1183-1:2019. The exact pigment loading, carrier resin and additive stabilisation package are not disclosed in publicly available product data.
Because melt flow rate is a single-point capillary measurement at low shear, it cannot represent the zero-shear viscosity or particle coalescence behaviour that control wall thickness distribution in rotational moulding. In the low-shear regime of a biaxial machine, peak shear rates at the powder-bed interface rarely exceed 1 s⁻¹; therefore, a zero-shear dynamic oscillatory test under ISO 6721-10:2015 or a cone-and-plate rheometer is a more discriminating incoming raw material check. Producers of LLDPE rotomoulding powders recommend that melt flow rate be maintained within ± 0.3 g/10 min of nominal to limit batch-to-batch shifts in charging behaviour. Density, measured with a gradient column rather than a single immersion balance, detects lot changes in comonomer uptake; a change of 0.002 g/cm³ can move the part from flexible to semi-rigid and alter the required oven cycle. Published data for this specific green pre-compound is limited; the processor should use the certificate of analysis for each lot and compare the melt flow rate and density against an internal statistical process control chart before issuing the charge weight.
For tensile property verification, ASTM D638-14 type IV specimens cut from rotationally moulded plaques are preferred over injection-moulded specimens. Rotational moulding produces a different skin-core crystalline gradient, and injection-moulded data do not translate directly to hollow part performance. General LLDPE grades with a density near 0.935 g/cm³ typically show a tensile yield stress in the 15–20 MPa range and elongation at break above 800%; however, the green pigment may reduce elongation at break by several percentage points depending on dispersion quality. Pigment agglomerates larger than 20 µm can act as flaw initiation sites under tensile loading. The pre-compounded colourant is expected to be more uniformly dispersed than a dry-blended masterbatch, but no public morphological data confirm the exact agglomerate size distribution for GREEN 6239.
Comparative material classes for rotational moulding applications are summarised below. Values are typical industrial ranges reported in public technical literature, not lot-specific guarantees for Icorene 3150 GREEN 6239.
| Material class | Density (g/cm³) | Melt flow rate (g/10 min) | Tensile yield stress (MPa) | Low-temperature impact behaviour | Stiffness relative to LLDPE |
|---|---|---|---|---|---|
| Icorene 3150 type LLDPE base resin nominal | 0.935 | 5.0 | not disclosed | ductile at -40 °C typical | medium |
| General LLDPE rotomoulding grade | 0.925–0.940 | 3.0–6.5 | 14–20 | ductile | lower |
| MDPE rotomoulding grade | 0.940–0.946 | 4.0–6.0 | 18–22 | moderate | higher |
| HDPE rotomoulding grade | 0.945–0.955 | 5.0–7.0 | 20–28 | reduced at low temperature | highest |
Pre-compounded colourants are melt-mixed into the LLDPE on a twin-screw extruder before pulverisation. In contrast, many rotational moulders add a dry-colour masterbatch at the machine hopper. The pre-compounded route transfers dispersion work to the resin supplier and typically reduces colour streaks in thin walls of 2 mm or less. However, the additional heat history of pre-compounding may consume part of the antioxidant stabiliser and lower the oxidative induction time relative to natural resin compounded only once. The oxidative induction time can be measured by ASTM D3895-19 or ISO 11357-6:2018; comparison of natural Icorene 3150 and GREEN 6239 should be made on pulverised powder or moulded plaques under identical conditions. Published data for this specific comparison is limited.
Deep ribs, kiss-offs and undercuts create local regions where powder densification is retarded by shadowing from the mould surface. In a biaxial rotational moulding machine with a swing of 1.2 m and a 4:1 rotation ratio, powder bridging in ribs narrower than 8 mm is documented when charge distribution is biased toward the opposite mould half. A base resin with 5.0 g/10 min melt flow rate has less fine-detail fill capability than a high-flow LLDPE with 7 g/10 min; consequently, tooling designed for high-flow natural grades may show incompletely filled ribs when switched to this pre-coloured grade. The main corrective variable is peak internal air temperature, measured by a thermocouple placed at the deepest rib root. If the peak internal air temperature does not reach 190 °C, particle boundaries remain visible on the inside surface and low-temperature impact strength is compromised. Published data for this specific configuration is limited, so moulders must generate a temperature map for each tool before setting an oven recipe.
Particle-size distribution and bulk density are controlled because rotational moulding powders are normally pulverised to 35 mesh (500 µm). Fines below 200 mesh (75 µm) increase dust and can bridge in narrow feed hoppers, while oversize particles above 20 mesh (850 µm) slow particle sintering. Production experience on single-axis and biaxial machines shows that a bimodal distribution can generate pinholes at inside corners when oven residence time is short. The green pigmentation package may alter the powder’s dry flow index because high-surface-area organic pigments can increase interparticle friction. Bulk density should be checked according to ASTM D1895-96(2010)e1 and compared against the producer’s target; no public value for this exact colour is available. The powder should be stored in sealed containers and reblended before charging if it has been transported over long distances or exposed to relative humidity above 60%.
During incoming powder evaluation on a production line, a dry sieve analysis using a Rotap shaker, bulk density measurement, and melt flow rate verification are typically performed. When switching from natural Icorene 3150 to Icorene 3150 GREEN 6239, the operator may observe a shift in charge time because the pigmented powder can exhibit different bulk density. A loss-in-weight feeder set for natural powder may require recalibration for the green grade to avoid charge weight variation above 2%. Charge weight variation of more than 2% on a 25 kg part changes nominal wall thickness by approximately 0.1 mm on a 3 mm wall, enough to alter impact performance. This level of production detail is used in rotational moulding facilities and is not supplied in the public datasheet.
Compliance status for typical end uses is based on the base olefin polymer and the colourant package. The following matrix identifies standards that must be requested from the supplier, not assumed from the grade name.
| Requirement | Standard or regulation | Relevance to Icorene 3150 GREEN 6239 |
|---|---|---|
| Base olefin polymer food-contact clearance | FDA 21 CFR 177.1520(c) | Base resin may qualify, but the green colorant must be independently cleared. |
| EU substance registration | REACH (EC) No 1907/2006, Article 3(5) polymer definition | Polymer exemption may apply; imported pigment or residual monomer substances require verification. |
| Restricted substances in electrical equipment | RoHS Directive 2011/65/EU, Annex II | Limits of 0.1 wt% for lead, mercury, hexavalent chromium, PBB and PBDE; 0.01 wt% for cadmium. |
| Outdoor weathering comparison | ISO 4892-2:2023 cycle 1 or ASTM D2565-23 | Required for UV-stabilised claims; not a pass-or-fail compliance standard by itself. |
Solidification rate determines warpage and dimensional control. In forced-air cooling chambers, a cooling rate above 15 °C/min for a 6 mm wall can produce asymmetric crystallisation between the outer and inner surfaces. The green pigment reduces radiant heat absorption compared with black pigment, so the same oven setpoint may not produce the same internal air temperature. For this reason, cycle development should use a rotary thermocouple or in-mould temperature logger to measure peak internal air temperature, not rely on oven air setpoint. For LLDPE grades of this density class, a peak internal air temperature of 190–205 °C is typical; below 180 °C the part may be undercured and show reduced impact strength and tensile elongation. Above 220 °C, thermal-oxidative degradation of the stabilisation package may produce discolouration and surface tack. The exact threshold for GREEN 6239 should be established by a stepped-temperature trial because the green pigment may shift the oxidative induction time.
Undercured parts exhibit a rough inner surface with visible powder particle boundaries, while overcured parts show a glossy inner surface and may discolour from thermal-oxidative degradation. The Icorene 3150 base resin contains a stabilisation package; green pigments can interact with hindered amine light stabilisers or phenolic antioxidants, but the producer does not disclose the stabiliser formulation. Aging performance should be evaluated by ASTM D2565-23 or ISO 4892-2:2023, not assumed from natural resin data. In outdoor applications, a green moulded-in colour reduces the need for painting but does not provide sufficient ultraviolet protection unless the part is evaluated under ASTM D1435-20 natural weathering.
Compared with high-pressure low density polyethylene, LLDPE grades such as Icorene 3150 have a narrower molecular weight distribution, higher elongation and better environmental stress crack resistance at similar density. Compared with metallocene LLDPE, a conventional LLDPE rotational moulding grade may have a broader comonomer distribution, which changes low-temperature impact and warpage. Icorene 3150 GREEN 6239 differs from natural Icorene 3150 and from UV-stabilised Icorene 3150 variants by the presence of a pre-compounded green pigment. Selection between a pre-coloured grade and a natural powder plus masterbatch is usually made on colour consistency targets, minimum order quantities, and available mixing equipment. Pre-coloured compounds reduce the risk of dry-blend segregation in the moulding shop; however, they lock the processor into a single colour and may reduce flexibility in colour changes.
Tensile impact and dart drop are relevant for thin-walled rotomoulded parts. The falling dart impact test according to ISO 6603-2:2023 or ASTM D3763-18 is used to compare ductile-to-brittle transition behaviour. In pre-coloured grades, pigment particles can shift the ductile-to-brittle transition temperature upward by several degrees Celsius; the exact shift depends on pigment type, dispersion and concentration. A production moulder should evaluate impact at the intended use temperature, such as -20 °C for cold-climate outdoor parts, rather than relying on room-temperature data. The base resin’s low-temperature ductility does not guarantee that the pigmented final part will pass the same value at -40 °C.
Typical application routes for this grade include agricultural tank lids, equipment housings, playground components and non-food storage bins where a moulded-in green colour removes the need for post-mould painting. In outdoor use, natural weathering should be evaluated by ASTM D1435-20 or ISO 2810:2020 on the finished part, because pigment selection and wall thickness affect colour retention and chalking. Moulded-in colour avoids volatile organic compound emissions from painting but does not improve resistance to stress cracking in detergent-containing environments; environmental stress cracking resistance should be tested according to ASTM D1693-15 or ISO 16770:2019 on the final pigmented material. Where regulatory or food-contact confidence is required, the moulder should request a product-specific compliance statement from LyondellBasell or the colourant supplier.