Lyondellbasell Icorene 2900 Uv Gry 7853 Polyethylene Linear Low Density

LyondellBasell Icorene 2900 UV+ GRY 7853 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 2900 UV+ GRY 7853 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 908278
    Materialtype Polyethylene, Linear Low Density (LLDPE)
    Polymerfamily Linear Low Density Polyethylene
    Color Gray
    Uvstabilization Yes
    Additive UV Stabilizer
    Form Powder
    Processingmethod Rotational Molding
    Density 0.939 g/cm³
    Bulkdensity 0.56 g/cm³
    Meltflowrate 3.0 g/10 min (190°C/2.16 kg)
    Tensilestrengthatyield 17.9 MPa
    Tensilestrengthatbreak 17.9 MPa
    Elongationatbreak 800%
    Flexuralmodulus 758 MPa
    Notchedizodimpact 0.53 kJ/m²
    Vicatsofteningtemperature 118°C
    Heatdeflectiontemperature 60°C at 0.45 MPa
    Environmentalstresscrackresistance >1000 h
    Hardnessshored 55
    Melttemperature 190-230°C
    Moldtemperature 230-300°C

    As an accredited LyondellBasell Icorene 2900 UV+ GRY 7853 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 2900 UV+ GRY 7853 is supplied in 25 kg polyethylene bags, with 40 bags per pallet (1,000 kg).
    Container Loading (20′ FCL) 20′ FCL loaded with palletized 25 kg bags of LyondellBasell Icorene 2900 UV+ GRY 7853 LLDPE, shrink-wrapped and secured.
    Shipping LyondellBasell Icorene 2900 UV+ GRY 7853 Polyethylene, Linear Low Density is non-hazardous and not regulated for transport by DOT, IMDG, IATA, or ADR. Ship in sealed bags, boxes, or octabins. Store dry, away from ignition sources and incompatible materials. No UN number, packing group, or marine pollutant designation applies.
    Storage Store this LLDPE resin in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and strong oxidizers. Keep original packaging closed and off the floor to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and static buildup. Use first-in, first-out stock rotation. Maintain appropriate ventilation and temperature control. Inspect containers regularly for damage or leaks. Follow local regulations.
    Shelf Life Shelf life is 24 months when stored in original unopened packaging under cool, dry conditions, away from direct sunlight.
    Application of LyondellBasell Icorene 2900 UV+ GRY 7853 Polyethylene, Linear Low Density
    `

    Specifying LyondellBasell Icorene 2900 UV+ GRY 7853 for rotationally moulded chemical storage vessels begins with a powder characterisation check rather than pellet melt-flow assumptions. A representative incoming lot is assessed for melt mass-flow rate under ISO 1133-1:2022 at 190°C and 2.16 kg, density under ISO 1183-1:2019, and bulk density and dry flow under ASTM D1895-96(2010)ε1. In the carousel process, the powder is charged into a fabricated steel or cast aluminium mould that is heated in an oven at 280–310°C while the arm rotates biaxially at 6–12 rpm on the primary axis and 1–3 rpm on the secondary axis. The internal air temperature measured with a wireless thermocouple logging system is raised to 190–205°C and held for 10–18 min to sinter the LLDPE fully at the inner wall and eliminate microvoids. Cooling is staged; forced ambient air lowers internal air temperature to 95–110°C before mist cooling reduces distortion, and demoulding occurs at 45–60°C. A chemical tank shell of 4.0–6.5 mm nominal wall thickness is produced with a shot weight calculated from surface area, target thickness, and polymer melt density plus 5–8% allowance for powder loss through venting. The design of rotationally moulded tanks uses kiss-off ribs and rotationally moulded-in fittings to avoid secondary welds. For chemical service, environmental stress-crack resistance is evaluated on the moulded wall under ASTM D1693-15; the exact F50 failure criterion is taken from the finished article specification. Chemical compatibility testing is run with representative immersion liquids under ASTM D543-21 at 23°C and 60°C for 7 d, with tensile property retention and mass uptake recorded. When the tank is intended for dangerous goods transport, the finished article is qualified as an UN packaging under 49 CFR 178.603 or ADR/RID equivalent, including drop, leakproofness, and stacking tests; the drop height is determined by the packing group and liquid specific gravity, not by the resin alone.

    Method / standardApplication-specific checkTest condition
    ISO 1133-1:2022Melt mass-flow rate190°C, 2.16 kg
    ISO 1183-1:2019Density23°C immersion
    ASTM D1895-96(2010)ε1Bulk density and dry flowSpecified funnel orifice
    ASTM D1693-15Environmental stress-crack resistance10% or 100% Igepal CO-630, 50°C or 23°C
    ASTM D543-21Chemical compatibilityRepresentative immersion fluid
    ISO 11357-6:2018Oxidation induction time210°C, 35 mL/min O₂

    Which Ageing Mechanisms Govern Grey LLDPE Sprayer Tank Shell Service Life?

    In field crop spraying, agricultural sprayer tanks made from Icorene 2900 UV+ GRY 7853 fail in service through a combination of UV embrittlement, chemical attack by surfactants and organic solvents, and cyclic pressure fluctuations from tractor-mounted motion. The grey UV-stabilised compound slows the first mechanism; retention of oxidative stabiliser is verified by isothermal oxidation induction time under ISO 11357-6:2018 at 210°C with an oxygen flow of 35 mL/min. A lot that has been overground or stored at high temperature may show reduced OIT before moulding, and this is treated as a release criterion when the tank is intended for multi-season use. The moulded wall is exposed to a representative tank-mix of 1–5% active ingredient in water plus 0.1–0.5% non-ionic surfactant under ASTM D543-21 at 23°C and 60°C for 7 d, then tested for tensile property retention and mass uptake. A practical external tank shell of 1,500–3,500 L is rotationally moulded with a nominal wall thickness of 5.0–8.0 mm at the bottom sump and 4.0–5.0 mm in the upper sidewall. The design uses rotational moulding in of threaded inserts, baffle kiss-off ribs, and a large access lid with a gasket seat. Because the process is low shear, any manually added antifoam or colour concentrate must be pre-blended with the powder at a dosage not exceeding 1–2 wt%, and dry blended formulations are checked for segregation under ASTM D1895-96(2010)ε1 after tumbling. The finished tank after moulding is subjected to a 24 h hydrostatic fill test at 1.1 times service volume to detect pin-holes in the rib intersections. The terminal article is a tractor-mounted or trailed sprayer tank, with field replacement thresholds tied to ΔE colour shift and surface microcracking observed after accelerated weathering under ISO 4892-3:2016 cycle 2, not by loss of leakage alone.

    Park benches, picnic table tops, modular outdoor seating shells, and refuse-bin liners are rotationally moulded from the same powder because the grey UV-stabilised system removes the need for post-mould painting and provides a low-gloss commercial surface. In this application the moulded wall thickness is normally 3.0–5.0 mm, with internal steel stiffeners inserted before powder filling or retained by rotationally moulded-in bosses. The shot weight is calculated to produce a nominal 4.0 mm wall on vertical faces, while horizontal seating surfaces are designed with a 2.5–4.0% draft angle and a minimum radius of 5.0 mm to prevent powder bridging and corner thinning. The mould is heated to an oven temperature of 280–300°C, and the part is removed from the oven after the internal air temperature has remained at 190–200°C for 8–12 min. For outdoor furniture exposed to direct sunlight, colour retention is assessed by ISO 4892-3:2016 cycle 2 with a defined ΔE limit under ISO 11664-4:2008; the grey colour system is specified to avoid the high heat buildup of darker colours and the yellowing of white parts. The terminal products are municipal benches and street-side seating, where the primary acceptance criteria are impact after UV ageing under ISO 6603-2:2000 at −20°C, not high-temperature creep. Published data for this specific grade's furniture-specific accelerated weathering index is limited, so moulders run a pre-production 500 h UV exposure panel against a retained physical property matrix.

    When the Powder Is Specified for Foam-Filled Marine Buoy Shells

    A moulder entering buoy production with this powder first validates powder flow behaviour on the intended shuttle machine, because narrow shell cavities and complex lifting lugs require consistent biaxial distribution. Marine buoy shells produced from Icorene 2900 UV+ GRY 7853 are typically moulded in two rotational halves with a tongue-and-groove seam, each half having a wall thickness of 5.0–8.0 mm. The oven set point is held at 280–310°C, and the internal air temperature reaches 195–205°C for 12–20 min to compensate for the thicker seams around moulded-in flanges. After moulding and cooling to 50–60°C, the halves are assembled and filled with a closed-cell polyurethane pour-in-place foam with a moulded density of 40–80 kg/m³. The foam exotherm is controlled below the LLDPE softening limit, normally 80–100°C at the shell inner surface, by adjusting shot size and water blowing agent. Low-temperature puncture impact of the rotomoulded shell is evaluated under ISO 6603-2:2000 at −20°C and −30°C; the foam backing changes the puncture response, so the assembled buoy is tested as a system rather than as an isolated shell. Salt fog exposure is evaluated under ISO 9227:2022 for 500 h, with the grey colour providing a stable surface that does not require antifouling paint for non-immersed sections. For sealed hollow floats produced without foam, a pressure relief vent of 10–15 mm diameter is inserted or rotomoulded into the wall to prevent seam rupture from diurnal thermal expansion. The terminal products are navigation buoys, aquaculture floats, and subsea marker buoys, where the governing failure modes are cold-water impact, seam fatigue, and UV embrittlement at the waterline.

    Used for wheeled waste containers, stacking pallet boxes, and seed or salt spreader hoppers, the rotomoulded bin body is specified when the part must survive fork tine impacts and cold-weather handling without brittle fracture. The powder is processed on shuttle machines with a wall thickness of 4.0–7.0 mm at the base and 3.0–5.0 mm at the sidewall; moulded-in corner ribs and a thickened top lip prevent distortion during demoulding. Impact acceptance uses ISO 6603-2:2000 at −20°C, or a drop test from 0.5 m onto a concrete floor after conditioning at −20°C. The low-shear melt flow range of the rotomoulding grade, verified under ISO 1133-1:2022 at 190°C/2.16 kg, is judged against the certificate of analysis. The terminal products are 120–770 L wheeled bins and industrial pallet boxes, where dimensional stability under load is checked after a 7 d creep exposure at 40°C using the end user's specified loading protocol.

    Irrigation Control Enclosures and Low-Voltage Outdoor Cabinets

    In pump station and irrigation control construction, outdoor enclosures made from Icorene 2900 UV+ GRY 7853 are specified for chambers that must survive impact from grounds maintenance equipment and continuous exposure to wet soil. The rotomoulded enclosure wall is held to 3.0–5.0 mm, with a moulded-in gasket groove and stainless steel threaded bosses inserted after cooling. The closed cabinet is tested for ingress protection under IEC 60529:2013 at the required IP65 or IP66 rating, using the water spray and dust exposure methods defined in the standard. Polyethylene flammability class is normally UL 94 HB, and this limitation is stated in the end-use specification. Accelerated weathering under ISO 4892-3:2016 cycle 2 is run for 1,000 h before impact testing to confirm that the grey UV-stabilised skin does not embrittle at exposed corners. The terminal products are irrigation controller cabinets, cathodic protection junction boxes, and low-voltage distribution pedestals, where the acceptance protocol includes wall thickness uniformity, insert pull-out resistance, and gasket seat flatness after demoulding.

    Free Quote

    Competitive LyondellBasell Icorene 2900 UV+ GRY 7853 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 2900 UV+ GRY 7853 is a linear low-density polyethylene rotational moulding compound supplied as a precompounded grey powder. The base grade, Icorene 2900 UV+, belongs to an ethylene-alpha-olefin copolymer family produced in powder form for rotational moulding; the comonomer type, catalyst architecture, and full additive package are not disclosed in the public datasheet. The suffix GRY 7853 identifies the grey colour concentrate incorporated at a controlled let-down, while the UV+ designation indicates an ultraviolet stabilisation package intended for outdoor exposure. As a powder grade, the material is processed primarily by rotational moulding rather than injection moulding or extrusion, and its particle-size distribution, bulk density, and dry-flow behaviour are controlled for mould cavity filling.

    Representative property values for the unfilled Icorene 2900 UV+ base resin
    PropertyTest methodUnitRepresentative range
    DensityISO 1183-1:2019g/cm³0.937–0.941
    Melt flow rate 190 °C/2.16 kgISO 1133-1:2022g/10 min3.5–4.5
    Tensile stress at yieldISO 527-2:2012MPa18–20
    Tensile elongation at breakISO 527-2:2012%800–900
    Flexural modulusISO 178:2019MPa650–750
    Vicat softening temperatureISO 306:2022 method A50°C120–124
    Shore D hardnessISO 868:2003—62–65

    These values are not specification limits and are drawn from typical published data for the unfilled UV-stabilized base resin; the grey precompound GRY 7853 may shift melt rheology, density, and shrinkage by 1–3%. Lot-specific values should be verified against the certificate of analysis before tooling compensation or compliance decisions.

    How does the UV+ package alter weatherability in thin-walled rotomolded parts?

    The UV+ additive system is formulated to retard photo-oxidative degradation in outdoor applications. Hindered amine light stabilizers and UV absorbers are the usual functional classes for polyethylene rotational moulding grades; the supplier does not disclose the precise chemistry in the public datasheet. For accelerated weathering verification, test specimens should be exposed according to ISO 4892-2:2013 cycle 1 or ASTM G154-23 using UVA-340 lamps, and retained tensile elongation at break should be monitored under ISO 527-2:2012. Grey pigments may include carbon black, titanium dioxide, or inorganic colourants; if carbon black is present, it can provide supplementary UV screening, but its particle size and dispersion influence surface appearance and impact retention. Published data for this specific grey compound under long-term outdoor exposure is limited; therefore field trials at the intended wall thickness are required for service-life claims.

    Peak internal air temperature, not oven set point, governs the consolidation of the LLDPE powder. In rotational moulding, heat transfer proceeds through the steel or aluminium mould wall into the tumbling powder bed. Oven air temperatures for medium-walled parts typically range from 280 °C to 320 °C, with forced-air velocities of 2–4 m/s measured at the mould surface. The peak internal air temperature should remain between 200 °C and 220 °C for full particle densification; exceeding 245 °C leads to carbonyl index increase, discolouration, and blister formation. Insufficient heating below 190 °C leaves unmelted powder agglomerates, pinholes, and reduced tensile impact strength. Cooling should be forced-air rather than water quench when dimensional stability is critical, because rapid cooling increases moulded-in stress and warpage in flat panels. Typical rotomoulding machines with biaxial speed ratios of 4:1 to 5:1 and minor-axis speeds of 6–12 min⁻¹ provide adequate powder flow. The material does not require pre-drying under normal ambient humidity, but condensation on cold powder should be avoided when relative humidity exceeds 80%. In multi-cavity aluminium moulds, wall-thickness variations greater than ±10% can produce non-uniform part wall thickness because of differences in heat capacity.

    Material differentiation against LDPE and HDPE rotational molding powders

    Icorene 2900 UV+ GRY 7853 occupies an intermediate stiffness region. Compared with low-density polyethylene rotomoulding grades, the LLDPE backbone provides higher tensile strength, puncture resistance, and environmental stress crack resistance; compared with high-density polyethylene rotomoulding powders, it provides lower flexural modulus and greater low-temperature ductility. The melt flow rate near 4 g/10 min is lower than many general-purpose LDPE rotomoulding powders, which can complicate filling of very thin ribs but improves bubble release and impact retention in thick sections. The grey colour concentrate differentiates it from natural UV+ grades by eliminating dry-blend colour addition; however pigment particles can act as nucleation sites, producing higher crystallinity and different linear shrinkage than the natural base resin. Shrinkage should be measured under ASTM D955-21 on a flat plaque of the same nominal wall thickness, and the measured value used for tooling compensation rather than generic tabulated data.

    Where dimensional stability is specified for large flat grey panels or tank lids, the precompounded grey compound requires tooling trials at the production wall thickness because published shrinkage data for this specific colour is limited. Environmental stress crack resistance should be evaluated by ASTM D1693-21, method B, in 10% nonylphenoxy poly(ethyleneoxy)ethanol solution. Outdoor load-bearing parts should not be designed at stresses above the published flexural creep modulus without testing at 40–60 °C, because creep accelerates with temperature in polyethylene. The compound is intended for outdoor panels, storage tanks, agricultural hoppers, playground components, and utility enclosures where UV resistance and colour-matched grey are specified.

    Clean in-plant regrind of unfilled natural UV+ parts may be mixed with virgin powder at levels up to 20% by weight in non-appearance parts, but the grey precompound GRY 7853 requires colour adjustment if regrind from mixed colours is introduced. Regrind particle size below 300 µm and control of fines content are necessary to maintain dry-flow behaviour. Do not combine with amine-based flame retardants or certain hindered phenols without compatibility testing due to potential additive antagonism with the UV stabiliser package. Published data for this specific grey-compounded configuration is limited; consequently, differential scanning calorimetry under ISO 11357-3:2018 and Fourier-transform infrared spectroscopy should be used for incoming lot verification when the part is exposed to long-term heat or ultraviolet load.

    When the grey 7853 precompounded color concentrate modifies shrinkage behaviour

    Colourants and filler particles at low loading can nucleate polyethylene and narrow the crystallisation exotherm. This effect is particularly visible in rotomoulding because slow cooling from the melt exposes differential crystallinity between natural and pigmented layers. For GRY 7853, the use of a precompounded concentrate reduces dry-colour dusting and improves colour consistency, but the crystal nucleation effect may increase linear shrinkage toward the upper end of the LLDPE range. Tooling cut for a natural UV+ grade may therefore produce under-dimensioned grey parts. The processor should conduct differential scanning calorimetry under ISO 11357-3:2018 to compare recrystallisation enthalpy and cooling-rate sensitivity, and should verify wall-thickness distribution with ultrasonic thickness gauges calibrated for polyethylene. Bulk density and dry-flow consistency can be checked by ASTM D1895-96:2017 method A; values falling outside the supplier lot-control range can indicate fines accumulation or moisture uptake.

    Regulatory status and documented standard designations

    Compliance declarations for the compound should be obtained from the supplier for each production lot. The base polyolefin is generally subject to REACH registration obligations as a polymer, and the UV stabilizers and grey colourants must be assessed under EU No 10/2011 if food-contact use is claimed; no food-contact status is implied by the public datasheet for this grey compound. Heavy-metal and hazardous-substance screening can be performed according to the IEC 62321 series for RoHS, but RoHS applies only to electrical and electronic equipment. For potable water or toy applications, the processor must verify migration and heavy-metal release under the relevant national or international standard, because published data for this specific configuration is limited.