Lyondellbasell Icorene 2900 Nat 0000 Polyethylene Linear Low Density

LyondellBasell Icorene 2900 NAT 0000 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 2900 NAT 0000 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 928787
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Density 0.932 g/cm3
    Melt Flow Rate 5.0 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 14.5 MPa
    Tensile Strength At Break 20.7 MPa
    Elongation At Break 800%
    Flexural Modulus 448 MPa
    Vicat Softening Point 101°C
    Melting Point 124°C
    Hardness Shore D 55
    Environmental Stress Crack Resistance >1000 h
    Brittleness Temperature < -70°C
    Thermal Conductivity 0.33 W/m·K
    Water Absorption 0.01%
    Dielectric Constant 2.3
    Dielectric Strength 20 kV/mm
    Volume Resistivity 1e16 ohm·cm

    As an accredited LyondellBasell Icorene 2900 NAT 0000 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg bags, typically palletized and shrink-wrapped; 1,000 kg bulk bags are also available for industrial handling.
    Container Loading (20′ FCL) 20′ FCL container loaded with 25 kg bags of LyondellBasell Icorene 2900 NAT 0000 Linear Low Density Polyethylene, palletized, shrink-wrapped.
    Shipping LyondellBasell Icorene 2900 NAT 0000 is a non-hazardous linear low-density polyethylene resin, supplied as pellets. It ships in moisture-barrier bags, supersacks, octabins, bulk trucks, or railcars. No UN number or dangerous goods classification applies. Store cool, dry, and clean, away from heat, sunlight, and contamination during transport.
    Storage Store LyondellBasell Icorene 2900 NAT 0000 Polyethylene, Linear Low Density in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, and ignition sources. Keep original containers sealed and palletized off the floor to prevent moisture, dust, and contamination. Avoid contact with strong oxidizers. Use first-in, first-out stock rotation. Maintain ambient storage temperatures. Protect from prolonged UV exposure. Follow local regulations.
    Shelf Life Shelf life: two years from date of manufacture when stored in original unopened packaging in a cool, dry, well-ventilated area.
    Application of LyondellBasell Icorene 2900 NAT 0000 Polyethylene, Linear Low Density

    What Controls Wall Thickness Variance in Large Rotomoulded Water Storage Tanks?

    LyondellBasell Icorene 2900 NAT 0000 is a linear low-density polyethylene powder supplied for rotational moulding. Supplier technical data list density at 0.935 g/cm³ when tested to ISO 1183-1:2019 and melt flow rate at 4.0 g/10 min under 190 °C and 2.16 kg load using ISO 1133-1:2022. In potable water storage tanks with capacities from 500 L to 5000 L, the primary process conflict is not polymer degradation but charge-weight calibration against shell surface area. Charge mass is calculated as shell area multiplied by target average wall thickness multiplied by melt density, plus a 2% to 3% densification allowance. Undercharging on shuttle machines with 2.5 m swing arms produces thin-wall cold spots at tangent corners and internal baffle junctions. Overcharging generates localized bridging, kiss-off defects, and excessive flash at parting lines. A calibrated charge is therefore established empirically for each mould set, not transferred from one geometry to another. Oven air temperature is maintained at 270–300 °C with peak internal air temperature controlled within 190–205 °C. If peak internal air temperature fails to exceed 180 °C, unmelted powder particles remain at weld lines and reduce hydrostatic burst resistance. If peak internal air temperature exceeds 210 °C, the anti-oxidant package becomes depleted and the natural resin yellows during subsequent cooling. Mould rotation ratio is set between 4:1 and 8:1 depending on asymmetry, with primary-axis speed from 6 rpm to 12 rpm. Forced-air cooling at 6–10 °C/min reduces warpage in flat sidewalls, while demoulding is initiated only when surface temperature falls below 80 °C. Finished tanks for drinking water contact require validation against NSF/ANSI/CAN 61 and, where applicable, FDA 21 CFR 177.1520 olefin polymer provisions. Hydrostatic testing follows ASTM D1998-21, with a filled tank held for 2 h without leakage or visible yielding.

    Processing variableSet rangeMeasurement anchor
    Oven air temperature270–300 °CMould chamber air probe
    Peak internal air temperature190–205 °CRotary centre-cavity thermocouple
    Primary/secondary rotation ratio4:1 to 8:1Machine speed tachometer
    Forced-air cooling rate6–10 °C/minInternal mould air thermocouple
    Demoulding temperature70–80 °CInfrared surface pyrometer
    Powder sieve retention5% maximum on 35-meshASTM D1921-18

    Automotive diesel fuel tanks and hydraulic oil reservoirs for compact agricultural tractors are rotomoulded from Icorene 2900 NAT 0000 where wall gauges are held between 6 mm and 10 mm. Insert-bearing bosses for fuel pickup fittings and threaded drain ports are heated to 120–150 °C before mould charging. Cold inserts below 100 °C generate radial shrinkage cracks around the insert because the surrounding polymer solidifies under constrained contraction. Inserts above 180 °C collapse fine thread forms or distort polyamide retaining rings. The grade is suitable for diesel and hydraulic oil service but is not specified for continuous gasoline immersion because linear low-density polyethylene exhibits hydrocarbon permeation at elevated temperature. Validation for off-highway fuel tanks includes evaporative emission limits under 40 CFR Part 1060 for nonroad fuel systems. Low-temperature crack resistance is screened using instrumented impact per ISO 6603-2:2023, with failures at metal insert interfaces indicating residual stress rather than base resin fracture. Post-mould annealing at 70–80 °C for 30–45 min reduces internal stress in thick bosses. Production line failure modes recorded on carousel machines include baffle weld-line porosity when cooling fans are engaged before peak internal air temperature has been confirmed, and sink marks at threaded fastener seats when demoulding is delayed beyond 90 °C surface temperature.

    When Chemical Containment Sectors Need Stress-Crack Resistance More Than Low-Temperature Impact

    Agricultural pesticide and fertilizer storage tanks produced from natural powder require an outdoor stabilization package before moulding because Icorene 2900 NAT 0000 does not contain a sufficient UV absorber system for long-term sun exposure. Carbon black masterbatch is added at 2.0–2.5 wt% for black tanks, while coloured exterior tanks use hindered amine light stabilizers at 0.4–0.8 wt%. Carbon black addition raises melt viscosity slightly and demands a 5–10 °C increase in peak internal air temperature if the wall thickness exceeds 8 mm. Environmental stress-crack resistance is measured according to ASTM D1693-15 condition C with 100% Igepal CO-630 at 50 °C. Rotomoulded linear low-density polyethylene of this density class often exceeds 1000 h without crack initiation, but published data for this specific formulation is limited and must be confirmed on each production lot when the container holds fertilizers with high salt activity. Chemical resistance screening follows ASTM D543-21 using the actual formulated liquid at the intended continuous service temperature. This resin is appropriate for dilute acids, alkalis, and many aqueous salt solutions; it is incompatible with chlorinated solvents, xylene, and hydrogen peroxide above 30% concentration. Wall sections for chemical tanks are commonly 8–12 mm, with mould rotation slowed to 4–6 rpm on the minor axis to improve wall uniformity along vertical sidewalls. Post-mould shrinkage of 2–3% in the neck region must be allowed for threaded closure dimensions.

    Marine buoyancy chambers, kayaks, and floating docks produced from this grade are moulded at wall thicknesses of 4–8 mm to balance impact durability against weight. Ultraviolet stabilization is mandatory for marine service, typically with a hindered amine light stabilizer masterbatch at 0.3–0.6 wt% and, for black parts, carbon black at 2.0 wt%. Buoyancy foam filling uses closed-cell polyurethane with a free-rise density of 32 kg/m³, injected in two stages to avoid exotherm distortion. The peak exotherm in thick foam cores should not exceed 100 °C because the roto part softens and can sag at unsupported flat zones. Cooling of long kayak hulls requires support fixtures during forced-air cooling because differential shrinkage along the keel line exceeds 10 mm/m when cooling rate is greater than 10 °C/min. Mould release application is restricted to thin PTFE-type films applied at 18–25 °C; excessive release agent builds up in textured hull surfaces and produces gel contamination in the next moulding. Low-temperature puncture toughness is evaluated by instrumented impact at -20 °C per ISO 6603-2:2023 at multiple points along the hull. Experience on rock-and-roll moulding machines indicates that end-cap regions require an additional 10% charge allocation because rotational path length is shortened relative to centre sections.

    Industrial Pallets and Dunnage – The Fatigue Threshold at Rib Intersections

    In pallet moulding, the datasheet-listed flexural modulus of 700 MPa under ISO 178:2019 places rib intersections and column bases as the controlling fatigue locations. Rotomoulded pallets produced from Icorene 2900 NAT 0000 are typically specified with top decks from 12 mm to 20 mm thick and rib radii not below 6 mm. Sharp internal corners below that radius create stress concentration factors from 3 to 5, and cyclic loading under ISO 8611-1:2011 pallet test conditions initiates cracks at those transitions. The material requires no drying before moulding unless storage relative humidity exceeds 60%; surface moisture is driven off during the heating cycle but can produce microvoids if powder is charged cold into a mould already above 80 °C. Static load performance of rotomoulded pallets is generally lower than injection-moulded HDPE structural foam; the designer compensates with thicker sections and reinforcing ribs. Cleaning with hot water at 80–95 °C is acceptable for supported flat areas, but unsupported lips above 120 °C shelf conditions deform permanently. Production variability in pallet flatness is controlled by cooling in jigs at 8 °C/min until mid-wall temperature drops below 70 °C. Batch-to-batch variance in wall thickness across the deck is reduced by sampling with ultrasonic gauging at 12 defined grid points per pallet.

    Underground Enclosure and Septic Chamber Moulding Windows

    Septic chambers and underground utility vaults require load-bearing sections with wall thicknesses that frequently reach 12–20 mm. The long heating cycle for these parts shifts the processing window upward because internal air temperature must remain at 200–210 °C for at least 10 min to consolidate the full section. Rotomoulded linear low-density polyethylene is used in these applications when soil flexibility and impact resistance outweigh the higher ring stiffness of HDPE. Structural verification to live loads follows AASHTO HS-20 loading configurations, with backfill material specified as angular stone from 12 mm to 25 mm compacted in 150 mm lifts to 95% standard Proctor density per ASTM D698-12(2021). Thin-wall sides below 10 mm exhibit buckling under vertical soil pressure when arching support is lost during heavy surface traffic. Stress relaxation data for LLDPE indicates that long-term modulus declines at elevated soil temperatures above 40 °C; published data for this specific underground configuration is limited and site-specific creep testing is required. Demoulding of thick parts is delayed until internal air temperature falls below 70 °C, and release should be staged from the bottom flange to avoid vacuum-lock distortion. Cooling fans directed at dome tops without side-wall support produce inward buckling on large vaults, a failure mode observed repeatedly on shuttle machines with cooling stations indexed before full part stabilization.

    Free Quote

    Competitive LyondellBasell Icorene 2900 NAT 0000 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 2900 NAT 0000 is a linear low density polyethylene (LLDPE) rotational molding resin supplied as natural-colored pellet or powder. The NAT 0000 designation identifies a formulation without pigment or carbon black; consequently the grade is not inherently UV-stabilized and requires a separate stabilizer system or pre-stabilized variant for prolonged outdoor exposure. The resin is characterized by a density of 0.929 g/cm³ under ISO 1183-1 and a melt mass-flow rate of 4.0 g/10 min at 190 °C/2.16 kg under ISO 1133-1. These parameters place the grade in the upper-density portion of the LLDPE envelope and within the flow window used for low-shear rotational molding.

    Manufacturer-published typical values for LyondellBasell Icorene 2900 NAT 0000
    Property Typical value Test standard
    Density 0.929 g/cm³ ISO 1183-1
    Melt mass-flow rate at 190 °C/2.16 kg 4.0 g/10 min ISO 1133-1
    Tensile stress at yield 13 MPa ISO 527-2
    Elongation at break greater than 800% ISO 527-2
    Vicat softening temperature 112 °C ISO 306/A50
    Brittleness temperature below -70 °C ASTM D746
    Environmental stress crack resistance greater than 1000 h ASTM D1693, condition B

    Published typical values for the grade include tensile stress at yield of 13 MPa under ISO 527-2, elongation at break greater than 800% under ISO 527-2, Vicat softening temperature of 112 °C under ISO 306/A50, and brittleness temperature below -70 °C under ASTM D746. The environmental stress crack resistance under ASTM D1693, condition B, 100% Igepal CO-630, is reported above 1000 h. These values define a medium-stiffness, high-ductility polyolefin with a low-temperature impact response.

    What Processing Parameters Govern Rotational Molding of Icorene 2900 NAT 0000?

    On carousel and shuttle-type rotational molding machines, the resin is normally pulverized to a 35-mesh top size (500 µm) with D50 near 300 µm. Coarse particles or fused tails from ambient grinding produce pinholes and uneven inner surfaces. Oven air temperatures for LLDPE in this melt-flow class are set between 260 °C and 320 °C, while the principal control variable is peak internal air temperature (PIAT). For this grade, mold trials on multi-arm carousel lines generally target a PIAT of 180 °C to 210 °C; published data for this specific configuration is limited, and the optimum must be confirmed for each mold and wall thickness.

    At low PIAT, unmolten resin and gas bubbles remain at the mold surface; at high PIAT, the natural resin oxidizes and yellows because the NAT 0000 grade contains no pigment to mask degradation. Molds are rotated at secondary-axis ratios near 4:1 to 5:1, with vent tubes of 3 mm to 6 mm internal diameter to avoid pressure accumulation and surface porosity. Cooling is conducted with forced air and water mist until mold temperature falls below 90 °C; demolding above this range can increase warpage and shrink marks. Pre-drying is not normally required if the powder is stored at relative humidity below 60%, but higher moisture can generate micro-voids in deep cavities that reach final mold-surface temperature later than adjacent sections.

    Thermal stability is governed by oven residence time, part surface area, and the antioxidant package. For natural LLDPE rotational molding grades, oxidation induction time under ISO 11357-6 at 200 °C is commonly specified above 30 min; the grade-specific value should be obtained from the supplier. On machines with cycle times exceeding 60 min, the resin is held at elevated temperature for prolonged periods, and the absence of carbon black makes oxidative yellowing an early visual control indicator.

    In the low-shear regime of rotational molding, the melt mass-flow rate alone does not fully describe flow. Rotational molding occurs at estimated shear rates below 0.1 s⁻¹, where zero-shear viscosity is the controlling material parameter. For LLDPE with MFR 4.0 g/10 min at 190 °C, zero-shear viscosity is generally in the range of 5 × 10³ Pa·s to 5 × 10⁴ Pa·s. The exact value for this grade is not normally published in the technical data sheet, and mold-filling behavior is better verified by powder flow studies and prototype molding than by capillary rheometry alone.

    Sintering of the powder bed proceeds through particle coalescence and bubble diffusion. Inadequate compaction before full melting leaves spherical voids. A PIAT of at least 180 °C and a hold time of 10 min to 20 min above this temperature are commonly used to reduce void content in LLDPE rotational molding. The exact hold time depends on wall thickness, mold material, and oven air velocity.

    Mechanical Performance and Low-Temperature Impact Behavior

    At a density of 0.929 g/cm³ and MFR of 4.0 g/10 min, the resin develops a tensile yield stress of 13 MPa and an elongation at break above 800%. The Vicat softening temperature of 112 °C under ISO 306/A50 supports short-term exposure to warm liquids, but continuous service above 70 °C normally requires a thicker wall or an HDPE grade with higher Vicat. The brittleness temperature below -70 °C under ASTM D746 cannot be taken alone as a guarantee of low-temperature part performance; wall thickness, stress concentrations, and mold-in residual stress often dominate finished-part impact response.

    Environmental stress crack resistance is the principal differentiator from high-pressure LDPE of similar melt flow. Under ASTM D1693, condition B, the F50 time exceeds 1000 h in 100% Igepal CO-630. Many high-pressure LDPE rotomolding grades of similar density and melt flow display shorter F50 times, often below 100 h depending on molecular weight and branching. The higher ESCR of Icorene 2900 NAT 0000 is associated with the linear backbone and controlled short-chain branching of LLDPE, which reduces the rate of tie-molecule disentanglement under surface wetting stress. This property is relevant for agricultural tanks, detergent containers, and chemical-storage vessels where stress cracking is a known field-failure mode.

    In medium-wall tank and container applications, rotational molded parts produced from Icorene 2900 NAT 0000 are used for water storage tanks, agricultural sprayer tanks, material-handling bins, and recreational components. On production-scale shuttle machines with aluminum molds, wall thicknesses from 4 mm to 12 mm are common for this density class. Deep-draw tools require additional oven-time compensation or mold indexing because the powder bed in corners and lower extremities reaches sintering temperature later than the rest of the charge. Screw or pneumatic powder loading systems should preserve a consistent particle size distribution; segregation of fines and coarse particles across the mold produces localized porosity and pinholes.

    Within the Icorene product family, lower-MFR variants near 2.0 g/10 min generally provide higher ESCR and impact but require longer oven residence; higher-MFR variants near 6.0 g/10 min fill complex mold details more rapidly but may show lower stress-crack resistance. Icorene 2900 NAT 0000 at 4.0 g/10 min occupies an intermediate position suitable for medium-complexity tools where surface detail, cycle time, and long-term chemical resistance are specified together.

    For food-contact assessment, the natural grade is commonly evaluated under FDA 21 CFR 177.1520 and EU Regulation No 10/2011, provided the fabricator obtains the supplier’s compliance statement and verifies end-use conditions. It is not intended for pressure vessels or continuous service above 70 °C without design review. Contact with strong oxidizing acids, aromatic hydrocarbons, and chlorinated solvents should be avoided because swelling and stress cracking can occur. Welding and repair of molded parts require hot-gas welding with a LLDPE rod of similar density and melt flow to maintain ESCR in the weld zone; weld strength should be verified on prototype parts by drop or burst tests under ASTM D2463 or equivalent.

    When Icorene 2900 NAT 0000 Replaces LDPE or HDPE in Molded Articles

    When this resin replaces a high-pressure LDPE rotomolding grade of similar melt flow, the density increase from approximately 0.925 g/cm³ to 0.929 g/cm³ raises part stiffness and lowers oxygen and moisture permeation. Tensile yield stress rises from a typical LDPE range of 10 MPa to 12 MPa to 13 MPa, allowing a moderate wall-thickness reduction in non-structural tanks. ESCR and low-temperature impact improve, but melt strength during rotational molding may be lower than that of high-pressure LDPE. This requires more uniform mold rotation and can narrow the processing window for large flat panels.

    When the resin replaces an HDPE rotational molding grade of density near 0.945 g/cm³, flexural modulus under ISO 178 is typically lower, in the range of 350 MPa to 450 MPa, compared with 800 MPa to 1000 MPa for HDPE. Load-bearing structural parts therefore require increased wall thickness or ribbing. In return, the LLDPE offers lower-temperature impact and higher ESCR in many chemical environments. HDPE remains preferable for hot-fill conditions or where high stiffness at thin wall is the controlling design parameter.

    Operational boundaries include storage at relative humidity below 60% and oven air temperature below 320 °C to avoid oxidative degradation. Regrind from HDPE or LDPE should not exceed 20 wt% unless the fabricator verifies ESCR and impact retention on finished parts; incompatible rheology from higher-viscosity HDPE can create unmelted domains and pinholes. The grade is not recommended for injection molding or blown film because the stabilization and melt rheology are designed for long oven residence, not short-residence extrusion. Published data for grade-specific behavior in incompatibilities is limited; side-by-side molding trials are required for any blend.

    Top