Lyondellbasell Icorene 2551 Blk 9001 Polyethylene Linear Low Density

LyondellBasell Icorene 2551 BLK 9001 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 2551 BLK 9001 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 255939
    Density 0.924 g/cm3
    Melt Flow Rate 0.70 g/10 min at 190°C/2.16 kg
    Tensile Strength At Yield 17.0 MPa
    Tensile Strength At Break 24.0 MPa
    Elongation At Break 700%
    Flexural Modulus 0.600 GPa
    Vicat Softening Point 100°C
    Brittleness Temperature < -70°C
    Environmental Stress Crack Resistance > 1000 hr
    Carbon Black Content 2.0%
    Uv Stabilization Yes

    As an accredited LyondellBasell Icorene 2551 BLK 9001 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 2551 BLK 9001 is packaged in 25 kg polyethylene bags, securely sealed and palletized for industrial shipment.
    Container Loading (20′ FCL) 20′ FCL loaded with 25 kg bags of LyondellBasell Icorene 2551 BLK 9001 Linear Low Density Polyethylene, palletized and stretch-wrapped.
    Shipping LyondellBasell Icorene 2551 BLK 9001 Polyethylene, Linear Low Density, is shipped as a non-hazardous resin in 25 kg bags, palletized and stretch-wrapped, or in bulk lined trucks/railcars. Keep dry, cool, and out of direct sunlight; avoid contamination. Handle with clean equipment. Standard freight handling applies; no hazardous placards required.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep containers tightly closed, labeled, and protected from moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Use appropriate secondary containment where required. Maintain good housekeeping to prevent slipping on spilled pellets. Follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf life: 24 months when stored in original unopened packaging in a cool, dry, well-ventilated area away from direct sunlight.
    Application of LyondellBasell Icorene 2551 BLK 9001 Polyethylene, Linear Low Density

    Rotational molding of carbon-black-stabilized linear low density polyethylene into vertical chemical storage vessels uses LyondellBasell Icorene 2551 BLK 9001 as the sole matrix resin. The normal charge is 100 parts per hundred resin; in-plant rotomolding regrind is reintroduced at a maximum 20 wt% only after the regrind is screened to the original lot’s certified melt flow rate range per ISO 1133-1:2022. Exceeding the 20 wt% regrind fraction reduces spiral-flow continuity during powder densification and widens the batch-to-batch variation in Charpy notched impact per ISO 179-1:2010. Additional carbon black masterbatch is not required because the grade is delivered with the 9001 black package; a fluoropolymer process aid is added at 0.1–0.3 phr only when venting pin clogging is recorded on the molding line. The relevant compliance framework for single-wall stationary tanks includes ASTM D1998-21 for design stress and fitting integrity, ISO 22088-3:2006 for environmental stress cracking under constant strain, and REACH (EC) No 1907/2006 for EU market obligations. Downstream production is performed in biaxial rotational molding machines with oven set points of 290–310°C and a peak internal air temperature of 200–210°C; mold rotation ratios are set at 4:1 primary-to-secondary for horizontal cylindrical vessels and 1:4 for vertical tanks with conical bases. The carbon black surface layer accelerates radiant heat absorption, so the external mold surface is monitored with an infrared pyrometer to avoid early outer-wall solidification that traps gas beneath the inner skin. Published data for full-thickness crystallinity gradients in this specific configuration is limited; preproduction samples at the tank base corner and top fitting boss are sectioned to verify a minimum wall thickness of 6.0 mm. Terminal parts include 2,500–10,000 L above-ground storage tanks for dilute fertilizer solutions, agricultural adjuvants, and secondary containment basins.

    Why Is Shore D Hardness Insufficient for Specifying Rotomolded Navigation Buoy Skins?

    Shore D hardness per ISO 868 measures only near-surface indentation and does not capture the microcrack tolerance that governs a black LLDPE navigation buoy shell after multi-season UV exposure. The molding charge for the outer shell is 100 parts per hundred resin of Icorene 2551 BLK 9001; regrind from harbor-retired shells is capped at 15 wt% because the spent shell carries depleted stabilizer packages that reduce retention of tensile elongation after ISO 4892-3:2016 cyclic UV exposure. Material qualification for buoy suppliers is screened using ASTM D1693-15b environmental stress crack resistance in 10 wt% Igepal CO-630 at 50°C, ISO 527-2:2012 tensile yield stress, and ISO 179-1:2010 Charpy notched impact at -30°C. The downstream conversion uses clam-shell rotational molding with a 4:1 primary-to-secondary rotation ratio and a peak internal air temperature of 198–208°C; the molded shell wall is held at 5.0–6.5 mm to prevent sink marks at the lifting padeye bosses. After shell demolding, the cavity is filled through an inserted port with closed-cell polyurethane foam at a density of 42–55 kg/m³, which provides reserve buoyancy in case of outer-skin puncture. Terminal parts include 1.2–2.4 m diameter channel marker buoys, cardinal mark floats, and radar-reflector mounting shells.

    Rotomolded black LLDPE road barrier shells are produced as hollow bodies that receive sand or water ballast after site placement; the molding formulation uses Icorene 2551 BLK 9001 undiluted at 100 parts per hundred resin and permits up to 10 wt% in-house regrind only when the regrind fraction falls within the original lot’s certified melt flow rate range per ISO 1133-1:2022. Compliance for temporary traffic control devices is screened against ASTM D638-14 for tensile yield and ISO 179-1:2010 for cold-weather impact; photostability of the black shell is evaluated by ISO 4892-2:2013 method A with surface-crack inspection at 500 h intervals. The production line uses shuttle-type rotational molding machines with aluminum cast molds; peak internal air temperature is controlled at 195–205°C and oven residence is adjusted for 8.0–9.5 mm wall thickness at the base rib. Mold release is applied at 0.2–0.4 g/m² of mold surface to reduce demolding deformation without attacking the carbon black-rich surface. Terminal products include 1.0–2.5 m water-filled barricade shells, lane delineator bases, and parking stop bodies.

    Typical black LLDPE rotomolding processing envelope by downstream sector; values represent industry practice unless supplier documentation states otherwise.
    Application sectorMaximum in-plant regrindPeak internal air temperatureNominal wall thicknessRepresentative terminal part
    Chemical storage vessels20 wt%200–210°C6.0 mm minimum2,500–10,000 L vertical tank
    Navigation buoy shells15 wt%198–208°C5.0–6.5 mm1.2–2.4 m channel buoy
    Traffic barrier shells10 wt%195–205°C8.0–9.5 mm1.0–2.5 m barricade
    Insulated seafood tubs20 wt%200–210°C3.8–5.0 mm600–1,200 L fish tub
    Underground utility bodies15 wt%190–200°C7.0–9.0 mm600–1,200 mm riser section
    Playground structural shells10 wt%195–205°C4.0–5.5 mmSlide hood and entry ring

    Cold-Chain Seafood Tubs and Washdown Resistance in Black LLDPE

    Black LLDPE rotomolded tubs for chilled seafood distribution are specified when the outer shell must withstand repeated high-pressure washdown, UV exposure during deck haul-back, and subzero holding-room storage. The charge formulation is 100 parts per hundred resin of Icorene 2551 BLK 9001; mixed-color regrind from returned tubs is limited to 20 wt% because moisture entrained in post-wash regrind produces steam pocks unless the flake is pre-dried at 70°C for 2 h at a dew point below -20°C. The relevant compliance framework includes FDA 21 CFR 177.1520 for olefin polymers used in repeat-contact food-handling articles, with migration testing conducted by the finished-article producer; ISO 8611-1:2011 covers flat pallet stacking tests adapted for lug-base deflection; ASTM D638-14 is used for sidewall tensile yield. Downstream processing is single-station biaxial rotational molding with steel tooling; the peak internal air temperature of the molded tub is held at 200–210°C, and the mold rotation ratio is maintained at 4:1 primary to secondary. After demolding the tubs are forced-air cooled at 15–20°C/min through the 120–80°C crystallization interval to minimize base warpage. Terminal parts include 600–1,200 L insulated fish tubs, shellfish transport boxes, and dairy lug carts.

    Compliance and material qualification matrix for downstream rotomolded applications of Icorene 2551 BLK 9001.
    Application sectorStandard designationAssessment target
    Chemical storage vesselsASTM D1998-21Single-wall upright tank design stress and fitting integrity
    Chemical storage vesselsISO 22088-3:2006Environmental stress cracking under constant strain
    Navigation buoy shellsASTM D1693-15bStress-crack resistance in surfactant at 50°C
    Navigation buoy shellsISO 527-2:2012Tensile yield stress of molded shell
    Traffic barrier shellsASTM D638-14Tensile yield of barrier skin
    Traffic barrier shellsISO 4892-2:2013Xenon-arc weathering and surface cracking
    Insulated seafood tubsFDA 21 CFR 177.1520Olefin polymer specification for food-contact articles
    Insulated seafood tubsISO 8611-1:2011Lug-base deflection under pallet stacking
    Underground utility bodiesISO 17855-1:2014Polyethylene molding material classification
    Underground utility bodiesASTM D2412-11External loading characteristics of riser section
    Playground structural shellsEN 1176-1:2017Public play equipment safety requirements
    Playground structural shellsASTM F1487-21Consumer safety specification for public play equipment

    When Black LLDPE Replaces Glass-Reinforced Polyester in Underground Utility Manway Bodies

    Rotational molding of black LLDPE underground utility manway bodies and septic riser sections uses Icorene 2551 BLK 9001 as the sole matrix polymer. The formulation charge is 100 parts per hundred resin; regrind from rejected risers is capped at 15 wt% after density verification per ISO 1183-1:2019, because off-spec lower-density regrind reduces the circumferential stiffness of the riser lip and increases the probability of lid disengagement under soil load. Compliance for the material classification follows ISO 17855-1:2014, while tensile yield and low-temperature notch resistance are assessed per ASTM D638-14 and ISO 179-1:2010; finished riser sections are subjected to external parallel-plate loading per ASTM D2412-11. Downstream production uses biaxial rotational molding with fabricated steel tooling and a peak internal air temperature of 190–200°C; because the carbon black package raises radiant heat absorption at the outer mold surface, infrared pyrometer tracking of the mold surface is used to prevent premature skin formation. The demolded riser is slow-cooled in still air to limit rim ovality below the geometric tolerance band of the mating lid. Terminal parts include 600–1,200 mm diameter riser sections, effluent manway lids, and underground utility pull-box housings.

    Rotomolded playground hoods and entry rings are produced with the compound at 100 parts per hundred resin plus 10 wt% clean in-house regrind; structural compliance for public play equipment is verified against EN 1176-1:2017 and ASTM F1487-21, processing uses 4:1 rotational molding with peak internal air temperature 195–205°C, and terminal parts are slide hoods, tunnel connectors, and impact-absorbing entry rings.

    Free Quote

    Competitive LyondellBasell Icorene 2551 BLK 9001 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 2551 BLK 9001 is a black linear low density polyethylene powder formulated specifically for rotational moulding. The grade combines a nominal density of 0.925 g/cm³ when tested to ISO 1183-1 with a melt flow rate of 5.0 g/10 min at 190 °C/2.16 kg according to ISO 1133-1. It is supplied in a black colour package intended to provide ultraviolet screening and long-term outdoor weathering resistance. Typical application areas include chemical storage tanks, agricultural reservoirs, outdoor enclosures, and recreational structures where a non-natural, weather-stable rotomoulded part is specified. The grade is not a general-purpose injection moulding or film resin; its powder morphology, dry-flow behaviour, and stabilizer system are designed specifically for rotational moulding heat cycles on shuttle, carousel, and rock-and-roll equipment.

    What Are the Core Physical Property Boundaries for This Grade?

    The table below summarizes representative physical properties published for this grade. These values are not batch certificates and should be confirmed against the producer’s current technical data sheet and certificate of analysis. Mechanical data are generated on compression-moulded plaques because the slow, low-shear nature of rotational moulding inhibits the molecular orientation that can occur in injection moulding.

    Representative physical property profile for LyondellBasell Icorene 2551 BLK 9001
    PropertyTest methodTypical value
    DensityISO 1183-10.925 g/cm³
    Melt flow rateISO 1133-1, 190 °C/2.16 kg5.0 g/10 min
    Melting temperatureISO 3146124 °C
    Vicat softening temperatureISO 306, A50110 °C
    Tensile modulusISO 527-2, 1 mm/min260 MPa
    Tensile stress at yieldISO 527-2, 50 mm/min11 MPa
    Tensile strain at breakISO 527-2>800%
    Flexural modulusISO 178300 MPa
    Charpy notched impact, 23 °CISO 179-1/1eAno break
    Environmental stress-crack resistanceASTM D1693>1000 h
    Shore hardnessISO 868, D scale56

    For mechanical design, the combination of a tensile strain at break above 800% and a flexural modulus of 300 MPa places the material in the low-stiffness, high-elongation region of the polyethylene family. The high environmental stress-crack resistance value indicates suitability for parts exposed to detergents, surface wetting agents, and slow mechanical loading. The Shore D hardness of 56 is lower than typical medium-density grades, which should be considered when specifying abrasion resistance or dynamic loading on external surfaces.

    When the powder is processed on carousel and shuttle rotational moulding lines

    The powder is charged into preheated steel or aluminium tools. Oven air temperatures between 280 °C and 310 °C are normally required; the governing variable is not oven temperature alone but the peak internal air temperature, which should reach 190 °C to 205 °C for this LLDPE grade. At a peak internal air temperature below 180 °C, powder particles at the inner wall may fail to fully coalesce, leaving a rough inner surface and reducing tensile strain at break. Above 210 °C, thermo-oxidative degradation accelerates; the practical indicators are a visible yellowing of the inner surface, a marked decrease in notched impact, and a rise in carbonyl index measured by infrared spectroscopy. The recommended processing window is therefore narrower than that of some MDPE rotomoulding grades and requires continuous temperature logging rather than manual judgement.

    Cooling should be conducted in forced air at a rate of 0.5 °C/min to 1.5 °C/min until the mould surface temperature falls below 70 °C. Rapid water quenching of thick sections is associated with differential shrinkage, warpage, and reduced impact at the inner weld line. The grade is not hygroscopic in the conventional sense, but condensation on powder stored in a cold room can create pinholes during sintering; storage below 60% relative humidity and above 10 °C is recommended. If moisture exposure occurs, forced-air drying at 60 °C for a short period may be used, but the powder should not be exposed to temperatures above 70 °C for extended periods because additive migration and agglomeration can occur.

    Repetitive processing of regrind is possible but should be validated for each part. Rotomoulding scrap from this grade can often be reintroduced at up to 20 wt% if particle size distribution and dry flow remain within the original powder specification. Higher regrind levels reduce dry-flow and increase the fraction of fines, leading to uneven wall thickness and surface porosity. Regrind should be sieved through a 35 mesh screen and blended before charging. More than two regrind cycles are not recommended for outdoor parts because the carbon black dispersion is progressively degraded and the UV protection may become non-uniform.

    Mould release chemistry influences demoulding and post-mould finishing. Fluoropolymer dispersions are preferred when the finished article is to be painted, bonded, or lined; silicone-based release agents can leave a low-surface-energy layer that interferes with adhesion. Steel tools benefit from surface preparation to minimize backside rust during alternating heating and cooling. Aluminium tools with average grain roughness below Ra 0.8 µm can improve part release, but polished surfaces may also reduce powder adherence during the early heating phase and should be qualified prior to production.

    Accelerated weathering, carbon black dispersion, and retention of mechanical properties

    The BLK 9001 designation indicates a black ultraviolet-stabilised formulation. Carbon black functions as a UV absorber and a free-radical scavenger; its effectiveness depends on dispersion quality and particle size. For rotomoulded polyolefins, carbon black agglomerates larger than 20 µm can act as stress concentrators and reduce weld-line toughness. Dispersion quality can be evaluated by ISO 18553; a rating of ≤2 is typically targeted for outdoor tank and pipe grade compounds. Accelerated weathering to ASTM G154 with UVA-340 lamps at a black panel temperature of 60 °C and an irradiance of 0.89 W/m²/nm is used to screen retention of elongation. Well-dispersed black LLDPE grades generally retain more than 70% of tensile strain at break after 2000 h, whereas equivalent natural resins may fall below 50%. Published data for this specific grade under all alternate weathering cycles is limited; end-users should commission xenon-arc testing to ISO 4892-2 for applications where the article will be exposed to high ultraviolet irradiance or acidic rainfall.

    The weathering package does not prevent loss of surface gloss. Chalking may occur on exposed surfaces; the mechanical consequence is usually a reduction in outer-surface hardness before a significant loss in bulk tensile properties. For black rotomoulded tanks, post-mould lining or painting is not required for aqueous service, but solvent-based linings should be tested for adhesion because low-molecular-weight oxidized species can migrate to the surface during outdoor exposure.

    Compared with natural LLDPE rotomoulding powder, the black grade has a narrower processing appearance window because degradation discoloration is less visible on black inner surfaces. The use of thermocouple loggers and infrared surface readings is therefore more important than visual observation. Compared with MDPE grades in the 0.934–0.940 g/cm³ density range, Icorene 2551 BLK 9001 exhibits lower flexural modulus and higher environmental stress-crack resistance, making it more suitable for parts that undergo repeated flexure rather than high top-load. Compared with HDPE rotomoulding grades, it should not be used as a direct substitute in applications where sidewall stiffness or compression strength at elevated temperature is the controlling requirement.

    Regulatory Status Is Determined on the Fabricated Article

    The base olefin polymer is covered by EU Regulation 1907/2006 as a polymer, and the grade is not formulated with phthalate plasticizers. RoHS Directive 2011/65/EU compliance for the homogeneous material depends on the finished article because bulk polyethylene powders do not carry a stand-alone RoHS certification. Food-contact evaluations must be performed on the final moulded part; the polyethylene base falls under 21 CFR 177.1520, but the carbon black package and any processing aids require migration testing under 21 CFR 178.3297 or the applicable national standard before a food-contact declaration is issued. Potable water contact approvals such as NSF/ANSI 61, WRAS, and KTW are end-use article approvals and are not granted to the raw powder alone.

    The material is not recommended for continuous service with strong oxidizing acids, aromatic hydrocarbons, or multicomponent fuel blends. Polyethylene can exhibit stress cracking in the presence of polar surfactants and detergents, but the LLDPE structure of this grade provides a higher threshold than many HDPE grades. When chemical resistance is critical, immersion testing under ASTM D543 for the specific fluid, stress, and temperature combination is required. Published data for this specific black compound under aggressive solvent immersion is limited; the ESCR value should not be extrapolated to oxidizing or aromatic environments.

    Rotational moulding powders of this type are combustible dusts. Under NFPA 654 and ATEX Directive 1999/92/EC, charging stations should be bonded and grounded, and dust extraction should be designed to prevent a suspended cloud above the lower explosion limit. No specific minimum ignition energy or maximum explosion pressure for this grade is published in the public domain; users should perform dust explosivity screening to ASTM E1226 and ASTM E2019 before designing pneumatic transfer systems. Weld lines in rotomoulded parts are formed at the internal surface where molten polymer fronts meet; the strength of this region depends on the peak internal air temperature and the time spent above the melting point. For this grade, the inner surface should remain above 124 °C for at least 3 min to assure molecular interdiffusion across particle boundaries. Moving the part from oven to cooling too early creates a brittle inner surface despite acceptable outer-surface appearance. Infrared pyrometers aimed at the inner air space are more useful than visual inspection because the black pigment masks colour changes.