Lyondellbasell Icorene 2550 Yew 2520 Polyethylene Linear Low Density

LyondellBasell Icorene 2550 YEW 2520 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 2550 YEW 2520 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 883231
    Productname LyondellBasell Icorene 2550 YEW 2520
    Manufacturer LyondellBasell
    Polymertype Polyethylene, Linear Low Density (LLDPE)
    Density 0.925 g/cm3
    Meltindex 0.8 g/10 min (190°C/2.16 kg)
    Meltingpoint 120 °C
    Vicatsofteningpoint 90 °C
    Tensilestrengthatyield 9 MPa
    Tensilestrengthatbreak 22 MPa
    Elongationatbreak 800%
    Flexuralmodulus 200 MPa
    Shoredhardness 50
    Dartdropimpact 200 g
    Elmendorftearstrengthmd 200 g
    Elmendorftearstrengthtd 300 g
    Haze 10%
    Gloss 80%
    Coefficientoffriction 0.2

    As an accredited LyondellBasell Icorene 2550 YEW 2520 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 2550 YEW 2520 Linear Low Density Polyethylene in 25 kg paper bags, 40 bags per pallet (1,000 kg).
    Container Loading (20′ FCL) 20′ FCL contains LyondellBasell Icorene 2550 YEW 2520 Linear Low Density Polyethylene, packed in 25 kg bags, palletized and stretch-wrapped.
    Shipping LyondellBasell Icorene 2550 YEW 2520 Polyethylene, Linear Low Density ships as non-hazardous LLDPE resin pellets. Typical packaging includes 25-kg bags, octabins, or bulk trucks/railcars. Transport in clean, dry containers, protecting from moisture, heat, and direct sunlight. No special UN hazard classification; follow standard handling and storage practices.
    Storage Store LyondellBasell Icorene 2550 YEW 2520 Polyethylene, Linear Low Density in original, closed packaging within a clean, dry, well-ventilated warehouse at ambient temperature. Keep away from direct sunlight, heat, flames, ignition sources, and strong oxidizers. Place on pallets off the floor. Prevent moisture, contamination, and dust; clean spills promptly due to slipping risk. Follow FIFO and local regulations.
    Shelf Life Typically 24 months when stored unopened in original packaging in a cool, dry place, away from direct sunlight.
    Application of LyondellBasell Icorene 2550 YEW 2520 Polyethylene, Linear Low Density

    On single-layer silage wrap extrusion lines running LyondellBasell Icorene 2550 YEW 2520, film thickness is typically set between 20 µm and 30 µm. The melt is conditioned through a barrier screw with L/D 30:1 and a screen pack staged at 250/180/150 mesh. A die gap of 1.8 mm to 2.4 mm and a blow-up ratio of 2.2:1 to 2.8:1 maintain bubble stability; blow-up ratios below 2.0:1 reduce dart impact in the transverse direction, while ratios above 3.0:1 generate bubble flutter on conventional air rings. The frost line height is positioned at 6 to 8 die diameters above the air ring; a frost line below 4 die diameters freezes orientation too early and reduces tear resistance. Dart impact resistance is measured according to ASTM D1709-16A; for a 25 µm film, commercial silage wrap of this density class is commonly specified above 400 g. Machine-direction Elmendorf tear is tested to ASTM D1922 and typically exceeds 1.5 N in the machine direction at this thickness. Cling performance depends on the controlled migration of a sorbitan oleate or polyisobutylene additive. The additive is compounded at 0.5 wt% to 2.0 wt%. Tack force greater than 0.5 N/cm is measured by ASTM D5458. Insufficient migration reduces tack; excessive migration causes blocking in film stored at temperatures above 30 °C for more than 48 h. The migration kinetics follow a diffusion-controlled process; equilibrium tack force is usually reached between 24 h and 72 h at 20 °C, although published data for this exact additive package is limited. Additive masterbatches are gravimetrically fed at 2 wt% to 5 wt%. Pellet exposure above 60% relative humidity without sealed hoppers can introduce surface moisture, causing bubble instability and gel formation. For this blown film application, the resin should not be processed above 230 °C for prolonged periods. When the silage film is repurposed for direct food contact, compliance is assessed under FDA 21 CFR 177.1520 and EU No 10/2011; specific migration testing is performed according to EN 1186-1.

    What Limits Line Speed in Cast Pallet Stretch Film Extrusion?

    Cast film lines running Icorene 2550 YEW 2520 use slot dies with a nominal die gap from 0.5 mm to 0.9 mm. Melt temperature at the die is maintained between 220 °C and 250 °C. Below 220 °C, the melt web fails to adhere evenly to the chill roll; above 250 °C, oxidative gel formation in the die lips increases and reduces film clarity. The melt curtain is drawn over a chill roll with a surface finish of 0.05 µm Ra and a temperature setpoint from 15 °C to 30 °C. Edge pinning is achieved through vacuum boxes operating at −0.2 kPa to −0.8 kPa or air knives supplied with compressed air at 0.6 MPa to 1.0 MPa. The cling layer receives 1.0 wt% to 3.0 wt% polyisobutylene masterbatch to produce a tack force above 0.4 N/cm measured by ASTM D5458.

    Industrial pallet wrap is produced at 12 µm to 23 µm. Draw resonance limits line speed. For a linear low-density polyethylene of this class, draw resonance appears when the draw ratio exceeds 8:1 on a conventional single-chill-roll line. An air knife or vacuum box shifts the onset to higher draw ratios by stabilising the melt web. Pre-stretch at the converter is typically 150% to 300%, with machine-direction stretch force controlled below 80 N/cm at 200% pre-stretch. Puncture resistance is tested to ASTM D5748; for a 20 µm cast stretch film, commercial specifications often require greater than 20 J/cm³, but the value for this exact grade must be verified. The film is wound at 500 m/min to 900 m/min. Winding tension must be held at 0.2 N/mm to 0.4 N/mm to prevent blocking and telescoping. Excess tension above 0.4 N/mm causes pressure-induced blocking of the cling layer.

    ParameterTypical setpointMeasurement method / equipment
    Melt temperature at die220 °C to 250 °CIR thermometer, emissivity 0.95
    Die gap0.5 mm to 0.9 mmDial gauge
    Chill roll temperature15 °C to 30 °CEmbedded surface thermocouple
    Edge pinning vacuum−0.2 kPa to −0.8 kPaDigital manometer
    Line speed500 m/min to 900 m/minEncoder
    Converter pre-stretch150% to 300%Powered pre-stretch rollers

    Published data for this specific grade on high-speed cast stretch lines is limited. Processors should map draw-resonance onset and cling tack force against line speed for their own roll geometry.

    Extrusion of Heavy-Duty Form-Fill-Seal Film at Seal-Initiation Boundaries

    Vertical form-fill-seal machines convert Icorene 2550 YEW 2520 film into 25 kg industrial sacks at 80 to 120 bags per hour. The film is produced on a three-layer blown film line with die diameter 250 mm, die gap 2.0 mm, and melt temperature 195 °C to 215 °C. The inner sealant layer contains 10 wt% to 20 wt% of a lower-melting LLDPE or metallocene plastomer to achieve seal initiation below 95 °C. A sealant-layer plastomer level above 20 wt% reduces heat-seal strength and can cause pellet bridging in the hopper.

    Heat-seal strength is tested according to ASTM F88/F88M. A minimum seal strength of 1.8 N/15 mm is targeted after 0.3 s dwell at 115 °C. Hot-tack performance follows ASTM F1921 and requires holding force above 1.0 N/25 mm at the machine fill point. The film must maintain dart impact resistance above 350 g per ASTM D1709-16A and machine-direction Elmendorf tear above 2.0 N per ASTM D1922. Multilayer coextrusion is required when high dart impact and low seal initiation must be combined; the outer layers carry the load-bearing linear low-density polyethylene, while the sealant layer provides thermal response.

    The resin is extruded with a process aid to suppress sharkskin melt fracture. Without the additive, visible melt fracture occurs at apparent shear rates above 400 s⁻¹. The frost line height is kept at 5 to 7 die diameters to balance orientation. The bubble is collapsed and gusseted before winding; winding tension remains below 0.3 N/mm. Corona treatment at 38 mN/m to 42 mN/m is measured by ISO 8296. Published data for this specific grade on vertical FFS lines is limited; manufacturers should run seal-parameter dials for each laminate structure.

    When Extrusion Coating Replaces Adhesive Lamination on Board

    Extrusion coating of paper and board with Icorene 2550 YEW 2520 uses a 90 mm single-screw extruder with L/D 28:1. The melt is held at 285 °C to 315 °C to lower viscosity and promote adhesion to the substrate. Below 285 °C, adhesion to unprimed board drops sharply; above 315 °C, the melt degrades into visible gels. The die is a T-slot geometry with internal deckles set to minimise edge bead. The melt curtain is drawn down onto the paper web at 250 m/min to 450 m/min. Coating weight is controlled at 15 g/m² to 30 g/m².

    Adhesion develops through oxidation of the melt surface. Air gap is set at 150 mm to 250 mm. Melt web neck-in for linear low-density polyethylene is greater than that for low-density polyethylene and typically falls between 10 mm and 20 mm per side under these conditions. Surface treatment of the board is not required when the board temperature is above 25 °C. The coated substrate is tested for seal strength per ASTM F88 and for hot-water resistance at 80 °C by peel adhesion after immersion. The melt is stabilised for high-temperature hold-up; residence time above 300 °C should remain below 15 minutes to avoid gel formation.

    To reduce draw instability, the grade is diluted with low-density polyethylene in ratios from 30 wt% LLDPE to 70 wt% LDPE. Higher LLDPE content improves hot-tack and tear but increases neck-in. When food-contact board is produced, compliance is assessed under FDA 21 CFR 177.1520 and EU No 10/2011. Specific extraction tests are performed according to EN 1186-1.

    Rotational moulding of Icorene 2550 YEW 2520 is performed on biaxial machines with a 4:1 arm ratio and oven air temperatures from 250 °C to 290 °C. The powder is ground to a particle size distribution with 95% passing 35 mesh and not more than 10% below 200 mesh. Peak internal air temperature is held between 190 °C and 205 °C. The mould rotates at 6 rpm to 10 rpm on the primary axis and 1.2 rpm to 2.0 rpm on the secondary axis.

    Cycle time for a 3 mm wall is 18 min to 25 min. Under-cured parts show pitting and reduced impact strength; over-cured parts show yellowing and embrittlement. The tensile yield strength is tested per ISO 527-2 and typically exceeds 17 MPa for a 3 mm plaque. Notched Charpy impact at −40 °C is measured per ISO 179-1 and should exceed 6 kJ/m². The part is force-cooled with 0.3 m³/min to 0.6 m³/min air per kg of part weight. Warpage occurs when cooling is uneven; mould release is applied at 0.5 g/m² to 1.0 g/m². For agro-chemical tank applications, the resin is compounded with 2 wt% to 4 wt% carbon black masterbatch to achieve a UV-stabilised outer layer; dispersion is checked by particle analysis on 100 µm microtome sections.

    Published data for this rotomoulding configuration is limited. Processors should generate peak internal air temperature and part property curves for each mould geometry. Contact with strong oxidising acids above 50 °C is not recommended.

    Welding a geomembrane liner made from Icorene 2550 YEW 2520 requires a dual-track wedge welder with a 900 W to 1600 W heating element. Sheet thickness is 1.0 mm to 2.5 mm. Welder travel speed is set at 1.8 m/min to 2.5 m/min with wedge temperature 350 °C to 420 °C. Peel adhesion per ASTM D6392 requires at least 80% of parent sheet strength. Shear strength per ASTM D6392 is tested in the weld zone. A weld speed above 2.5 m/min produces a narrow heat-affected zone and intermittent unbonded spots on textured surfaces.

    Oxidative induction time is determined by ASTM D3895 at 200 °C. A minimum OIT of 100 min is typical for long-term landfill service, but specific values for this grade must be confirmed. Environmental stress cracking is tested per ASTM D5397 with a 30% yield stress load and 10% Igepal CO-630 solution at 50 °C; failure time should exceed 400 h. Seams are tested with air lance per ASTM D4437 and vacuum box per ASTM D5641. The liner is welded only in dry conditions; dew point must be below 15 °C. Surface oxidation from storage longer than 6 months must be removed by light abrasion before welding.

    TestStandardTypical requirement
    Peel adhesionASTM D6392≥ 80% of parent sheet strength
    Shear strengthASTM D6392≥ 80% of parent shear strength
    Oxidative induction timeASTM D3895100 min at 200 °C
    SP-NCTLASTM D5397≥ 400 h in 10% Igepal CO-630 at 50 °C
    Air lance seam testASTM D4437No leakage under test pressure specified in ASTM D4437
    Free Quote

    Competitive LyondellBasell Icorene 2550 YEW 2520 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 2550 YEW 2520 Polyethylene, Linear Low Density is supplied as a pulverised polyolefin intended for rotational moulding. The YEW 2520 suffix denotes a supplier-specific yellow pigmentation and UV-stabilisation package, while Icorene 2550 identifies the base linear low density polyethylene. The base polymer is a butene-copolymer LLDPE with a nominal melt flow rate of 5.0 g/10 min at 190 °C under 2.16 kg load when tested to ISO 1133-1:2022 or ASTM D1238, and a nominal density of 0.925 g/cm³ determined by ISO 1183-1 or ASTM D1505. The material is used for single-layer thick-walled hollow parts such as agricultural saddle tanks, fuel storage tanks, playground equipment, and industrial housings. Because the product is a powder, its handling characteristics, feed consistency, and sintering behaviour depend on particle size distribution, bulk density, and stabiliser content. Certificates of analysis should be consulted for lot-specific melt flow rate, density, colour attributes, and additive loading. Published data for the pre-coloured YEW 2520 configuration is limited relative to the natural base grade; therefore the values cited below are representative of the uncoloured Icorene 2550 resin and must be verified for each coloured batch.

    How does the designation relate to the base resin and colourant package?

    The designation carries two distinct pieces of information. The Icorene 2550 portion refers to the polymer backbone and its molecular architecture. The YEW 2520 suffix identifies the colourant and additive package incorporated during compounding. In rotational moulding, pigmentation is not a cosmetic aftertreatment; pigment particle size, carrier resin, and additive dispersion influence powder melt-out and pinholing. A pre-coloured package reduces the need for dry-blending pigment masterbatch at the machine, but it may shift the melt flow rate by approximately ±0.5 g/10 min and the density by approximately 0.001–0.002 g/cm³ relative to natural powder. The UV stabiliser package in YEW 2520 is intended for outdoor exposure. Documentation should be checked to confirm the stabilisation level against ISO 4892-2, ISO 4892-3, or ASTM G154 conditions before long-term exterior use.

    Typical property profile of the base resin

    The property profile of the Icorene 2550 base resin is summarised in Table 1. Values are generated from compression-moulded specimens according to the listed methods and are not to be interpreted as specification limits.

    Property Test method Typical value
    Density ISO 1183-1 / ASTM D1505 0.925 g/cm³
    Melt flow rate, 190 °C, 2.16 kg ISO 1133-1:2022 / ASTM D1238 5.0 g/10 min
    Tensile yield strength ISO 527-2 / ASTM D638-14 14 MPa
    Tensile elongation at break ISO 527-2 / ASTM D638-14 800%
    Flexural modulus ISO 178 / ASTM D790-17 450 MPa
    Vicat softening temperature, A50 ISO 306 95 °C
    Low-temperature brittleness ISO 974 / ASTM D746-20 -70 °C
    Environmental stress crack resistance, 100% Igepal CO-630 ASTM D1693-15 Condition B >1000 h

    In dry-flow handling, bulk powder properties influence shot-to-shot consistency. The powder is typically transported by vacuum loaders or screw augers into the mould. Bulk density measured by ASTM D1895-17 generally falls between 0.34 g/cm³ and 0.42 g/cm³. A bulk-density variation of more than 0.02 g/cm³ can produce a charge-weight shift of approximately 5–8% in fixed-volume metering equipment. Moisture content should remain below 0.05 wt% by Karl Fischer titration according to ISO 15512. If the powder is exposed to relative humidity above 60% for more than 24 h, pre-drying at 70–80 °C for 2–4 h in a dehumidified oven is recommended before charging. At the machine, uniaxial or biaxial rotational ratios between 4:1 and 10:1 are typical; the exact ratio is set by part geometry and wall thickness. Oven air temperature for LLDPE powders of this density class is commonly set between 260 °C and 320 °C. Peak internal air temperature during gelation typically reaches 190–220 °C, and the mould surface temperature should be held above 180 °C for sufficient densification. Incomplete gelation below 170 °C produces bubble retention and weld-line porosity.

    When the powder reaches gelation inside a closed forced-air rotational moulding machine

    During rotation, the powder passes through tackifying, sintering, and densification stages. With Icorene 2550, these stages occur within a relatively narrow thermal window. The low-density butene-copolymer backbone gives a lower melting range than medium-density hexene copolymers; the peak melting temperature of the base resin typically lies between 122 °C and 128 °C by differential scanning calorimetry according to ISO 11357-3. On a production line equipped with internal air-temperature probes, the gelation plateau is observed as a flattening of the internal air temperature at around 150–170 °C for thick sections, followed by a rise to the final peak. If the mould surface drops below 170 °C before complete densification, residual bubbles remain entrapped. If the material is held above 220 °C internal air temperature for prolonged periods, yellowing of the pre-coloured product and additive consumption may occur. The recommended target peak internal air temperature is therefore 200–210 °C for sections between 6 mm and 10 mm. For larger parts above 15 mm nominal wall, longer dwell times and lower oven air temperatures of 260–280 °C are used to avoid surface degradation while allowing thermal penetration.

    Comparison against general-purpose LDPE and medium-density rotomoulding powders

    The closest commercial comparisons are general-purpose high-pressure LDPE rotomoulding powders and medium-density polyethylene rotomoulding grades. The material differs from conventional high-pressure LDPE rotomoulding powders in its comonomer distribution and mechanical profile. Butene-copolymer LLDPE provides higher environmental stress crack resistance and higher stiffness at comparable density because of its controlled short-chain branching. Against a medium-density rotomoulding grade, Icorene 2550 trades flexural modulus and upper-temperature resistance for lower-temperature ductility. The comparative values in Table 2 are drawn from representative rotomoulding data for the base resin class; they are not direct specification values for the exact coloured batch.

    Material class Nominal density Melt flow rate Flexural modulus ESCR trend Low-temperature behaviour
    Icorene 2550 YEW 2520 LLDPE 0.925 g/cm³ 5.0 g/10 min 450 MPa >1000 h Ductile below -20 °C
    General-purpose LDPE rotomoulding powder 0.920–0.925 g/cm³ 5.0–9.0 g/10 min 250–350 MPa 100–300 h May become brittle below -10 °C
    Medium-density polyethylene rotomoulding powder 0.935 g/cm³ 2.0–5.0 g/10 min 600–700 MPa >1000 h Reduced impact at low temperature

    The difference in low-temperature ductility is most significant in applications where the moulded part is subjected to impact below -20 °C. Icorene 2550 YEW 2520 retains deformation without crack propagation under such conditions, whereas medium-density rotomoulding powders of equivalent wall thickness may exhibit brittle fracture. For applications requiring greater stiffness at elevated temperature, a medium-density or high-density rotomoulding grade should be evaluated instead. The butene-copolymer architecture of Icorene 2550 also gives a broader sintering window than many high-density rotomoulding powders, but it does not provide the same upper service temperature as crosslinked or higher-density systems.

    Regrind reuse is constrained by additive package dilution

    Regrind reuse of this material requires control of additive package dilution and particle size distribution. A grind from rejected parts may contain particles larger than 500 µm and irregular shapes; the powder should be screened through a 500 µm sieve and blended with virgin powder at a maximum of 20 wt% regrind unless full lot qualification is repeated. Because the YEW 2520 UV stabiliser is present at a calibrated concentration, blending with natural uncoloured powder or non-UV LLDPE lowers the stabiliser concentration and may cause accelerated weathering failure under ISO 4892-3 or ASTM G154. The pigment and stabiliser package can also interact with metal stearate mould release agents; excess release agent above 0.1 wt% may produce surface pitting and reduce print adhesion. Lot-to-lot colour variation should be monitored with a spectrophotometer using CIELAB coordinates if the part is visible in assembled products.