Lyondellbasell Icorene 2550 Yew 2227 Polyethylene Linear Low Density

LyondellBasell Icorene 2550 YEW 2227 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 2550 YEW 2227 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 375741
    Density 0.925 g/cm³
    Melt Index 190 C 2 16 Kg 20 g/10 min
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 13 MPa
    Elongation At Break 800%
    Flexural Modulus 300 MPa
    Vicat Softening Point 90 °C
    Melting Point 120 °C
    Hardness Shore D 50
    Mold Shrinkage 0.015 cm/cm
    Thermal Expansion Coefficient 1.5E-4 cm/cm/°C
    Color Yellow
    Form Pellets
    Processing Method Injection Molding

    As an accredited LyondellBasell Icorene 2550 YEW 2227 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 2550 YEW 2227 is typically supplied in 25 kg bags, palletized and stretch-wrapped for secure industrial transport and storage.
    Container Loading (20′ FCL) LyondellBasell Icorene 2550 YEW 2227 LLDPE loaded in 20′ FCL: 25 kg bags on pallets, shrink-wrapped, secured in dry container.
    Shipping LyondellBasell Icorene 2550 YEW 2227 is a non-hazardous linear low-density polyethylene resin. It is typically shipped in 25-kg bags, bulk bags, or octabins, palletized and stretch-wrapped in dry containers or trucks. Store cool, dry, away from direct sunlight; no special transport placards required.
    Storage Store LyondellBasell Icorene 2550 YEW 2227 Polyethylene, Linear Low Density indoors in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep original containers or bags closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure. Stack securely to prevent package distortion. Use first-in, first-out stock rotation and follow the manufacturer’s SDS.
    Shelf Life Shelf life is typically 12–24 months when stored unopened in a cool, dry area away from direct sunlight and heat.
    Application of LyondellBasell Icorene 2550 YEW 2227 Polyethylene, Linear Low Density

    In potable water tank production, Icorene 2550 YEW 2227 is charged into a fabricated aluminium tool mounted on a carousel-type rotational moulding machine. The charge weight is calculated from the target nominal wall thickness of 8–10 mm and the projected internal surface area. Shot-to-shot variation greater than ±0.5 kg produces measurable wall-thickness divergence at the tool parting line. Oven air is maintained at 280–300 °C, and the biaxial rotation ratio is set at 4:1 minor-to-major axis until the internal air temperature reaches 190–205 °C. The inner surface is the last to fuse. Termination before that point leaves a granular, porous boundary that fails the NSF/ANSI 61 leaching protocol because surface area and low-molecular-weight extractables increase. For potable water service, the rotomoulded wall must meet NSF/ANSI 61 and AS/NZS 4020. Where EU food-contact status is required, compliance is verified against Regulation (EU) No 10/2011 with overall migration measured by EN 1186-1. The powder is processed as supplied without post-blending of unlisted additives. If a colour concentrate is specified, the addition level is capped at 1.0–2.0 wt% of a potable-water-certified masterbatch to avoid exceeding 10 mg/dm² overall migration on thin walls. The terminal part is a 500–5,000 L cylindrical vertical tank with integrally moulded lugs, baffles, and threaded metal fasteners isolated from the fluid by a polyethylene boss. Post-mould cooling is controlled at 4–8 °C/min in the mould until the part reaches 85 °C. Forced demoulding at higher temperatures distorts the neck flange and causes local stress whitening at the insert bosses.

    Does Liquid Fertiliser Service Require a Linear-Low-Density Shell or a Crosslinked Alternative?

    The decision is resolved by the escape of small-molecule carriers through the wall and by environmental stress cracking at integrally moulded fittings. For Icorene 2550 YEW 2227, rotational moulding of a single-shell induction tank intended for 28–32 wt% urea ammonium nitrate solution typically involves a wall section of 6–12 mm with a minimum inner corner radius of 12.5 mm at outlet sumps to avoid stress concentration. The powder is charged into a fabricated stainless steel or cast aluminium tool. Steam tracing lines are not applied directly to the mould surface because local hot spots above 210 °C internal air oxidise the inner wall. The biaxial rotation ratio is held at 4:1 for cylindrical induction tanks. The specified stress-crack test is ASTM D1693, Condition B, in 100% Igepal CO-630 at 50 °C, with failure defined as F50 below 1,000 h for the unfilled shell. Published data for this specific grade in concentrated pesticide carriers is limited, so tank fabricators run immersion coupons in the actual formulated product per ASTM D543 for 28 days at 40 °C before approving the material. The full shell is also verified against EN 13575 for above-ground chemical storage tanks, including hydrostatic pressure and low-temperature drop tests. The outer surface is dry-blended or compounded with 2.0–3.0 wt% carbon black masterbatch where tropical ultraviolet exposure is expected. Carbon black above 3.5 wt% reduces impact strength and increases surface conductivity. End products are 1,000–20,000 L conical-bottom induction tanks with integrally moulded fill ports, drain sumps, and secondary containment bunds. The tank wall is checked for drop impact at -20 °C using ASTM D5276. Brittle failure at the sump radius indicates excessive cooling rate or premature demoulding rather than base resin failure. Crosslinked tanks are not automatically superior; they exhibit lower impact strength after prolonged thermo-oxidative ageing and cannot be reprocessed, so the linear-low-density shell is retained for standard UAN and pesticide formulations.

    Marine Buoy Shells, Foam-Filled Ballast Cavities and UV Stabiliser Migration Limits

    Marine buoy shells made from this linear-low-density powder are rotationally moulded as a closed outer skin, then filled with a two-component closed-cell polyurethane foam at a free-rise density of 32–48 kg/m³. The shell itself is charged to a rock-and-roll machine for cylindrical channel buoys because the long axis requires a 2:1 ratio and a slow sweep over the lower internal surface. Oven air is set at 300–320 °C for yellow or international-orange pigmented shells to compensate for the lower heat transfer through oxide colourants. Internal air is held at 200–210 °C for 6–9 mm walls. The critical failure mode is not beach impact but ultraviolet embrittlement at the waterline. Laboratory qualification uses ISO 4892-2 xenon-arc exposure with 0.35 W/m² irradiance at 340 nm, 102 min dry and 18 min water spray cycles. Retention of elongation at break is measured by ISO 527-2. A drop below 50% of the original value after 3,000 h is treated as unacceptable for 5-year marine service. The outer skin is dry-blended with 1.0–2.0 wt% high-lightfastness pigment concentrate and 0.1–0.3 wt% of a hindered amine light stabiliser masterbatch. Additional stabiliser loading beyond this range widens the melt flow window and produces pinholing at the foam fill port. Terminal parts are 0.5–3 m navigation buoys, mooring floats, and flotation collars fitted with galvanised steel hardware. Salt spray exposure per ASTM B117 for 1,000 h is used only for the metallic inserts because the polyethylene wall itself is not degraded by sodium chloride.

    Service exposureStandard designation or regulationTypical conditioning or exposureMeasured parameter
    Potable waterNSF/ANSI 61, AS/NZS 4020, EN 1186-1Extraction at 23 °C and 60 °CSpecific migration, turbidity, total organic carbon
    Liquid fertiliser and pesticideEN 13575, ASTM D1693, ASTM D543Igepal CO-630 at 50 °C; product immersion at 40 °C for 28 daysEnvironmental stress crack F50, mass change, tensile retention
    Marine ultravioletISO 4892-2, ISO 527-20.35 W/m² at 340 nm, 102 min dry/18 min sprayElongation at break retention
    Diesel exhaust fluidISO 22241-3, ASTM D54332.5 wt% urea solution at 40 °CTotal organic carbon, pH drift, metal ion migration
    Dry food and pharmaceutical contactFDA 21 CFR 177.1520, USP <661.1>Extraction by method-specific solventsOverall migration, heavy metals

    Where bulk ingredient bins are produced for dry food and pharmaceutical intermediates, the primary process limitation is not fusion but dimensional stability during forced cooling. Icorene 2550 YEW 2227 is moulded on a shuttle machine into 30–100 L nestable containers with wall thickness 3–5 mm. The charge weight per cavity is held within ±0.2 kg. A 3:1 minor-to-major rotation ratio and oven air at 270–290 °C are used for flat-wall boxes, but the internal air is terminated at 185–195 °C to reduce warpage. Pre-drying at 60 °C for 2 h is applied only when storage relative humidity exceeds 60%, because moisture absorbed on the powder surface increases pinholing at intersections. These bins are usually supplied in natural or food-contact-approved colours. Any reprocessing material is limited to 20 wt% of the same lot to maintain FDA 21 CFR 177.1520 compliance. The terminal part includes a moulded-in lip and fork pockets, and it is stack-tested for 24 h under a 3:1 load at 40 °C using an internal gauge block.

    When Diesel Exhaust Fluid Tanks Are Rotomoulded as Drop-In Replacements for Welded HDPE

    Welded high-density polyethylene tanks for 32.5 wt% urea solution have failed at extrusion weld lines because of slow crack growth promoted by thermal cycling and urea crystallisation. A single-piece rotationally moulded shell in Icorene 2550 YEW 2227 removes the longitudinal weld. The mould is a fabricated aluminium two-piece tool with an integrally moulded sump and level gauge boss. The tool is charged to achieve 8–12 mm sidewall thickness on a 4:1 rotating arm. Processing differs from water tanks: the demoulding temperature is lowered to 70 °C because the large flat roof panel shrinks unevenly and forms a residual internal stress field. Brittle failure in ASTM D1693 Condition A coupons is observed after 48 h immersion in 10% Igepal CO-630 when demoulding is too hot. For DEF service, the material must avoid copper-based antioxidants and unbound zinc stearate, because leached ions accelerate urea decomposition. The moulded part is tested for 28 days at 40 °C in concentrated urea solution per ASTM D543, with total organic carbon and pH drift measured against ISO 22241-3. The upper addition limit for regrind from the same production lot is 15 wt%, and no post-consumer polyethylene is permitted. The terminal product is a 500–5,000 L vertical or horizontal DEF storage tank with an integrally moulded secondary containment. The tank is hydrostatically tested at 1.5× rated pressure for 30 min and inspected for stress whitening at the sump knuckle.

    Underground Attenuation Chambers Demand Creep Rupture Data Not Shown on Standard Datasheets

    Rotational moulding of stormwater attenuation chambers from linear-low-density polyethylene requires a different acceptance logic than above-ground tanks because the buried structure carries live loads for decades without visible inspection. Icorene 2550 YEW 2227 is processed into arched double-walled chambers with a wall thickness of 10–15 mm and a corrugated profile to resist ring deflection. The tool is rotated at 4:1 in a carousel oven at 290–310 °C. The shot weight is calculated from the total part surface area and the density shown on the manufacturer’s lot certificate; a density outside the specified lot range shifts the shot weight calculation and alters wall uniformity. Long-term design uses creep modulus derived from ISO 899-2 or ASTM D2990 at 40 °C in air. Published data for this specific material in buried soil environments is limited, so a minimum creep rupture factor of 4.0 on the initial flexural modulus is usually required by civil engineers before specifying a burial depth. The moulded chamber is filled with water and loaded in a hydraulic compression frame to 25% vertical deflection to verify elastic recovery. This test does not replace long-term creep data. A typical formulation uses no mineral filler because mineral fillers reduce low-temperature impact after soil settlement. If biofilm growth is a concern, the moulder adds 0.5–1.0 wt% of a non-leaching antimicrobial masterbatch that does not affect weldability. The terminal part is a modular stormwater soakaway chamber 2,000–5,000 mm in length, buried at 600–1,200 mm cover depth and connected to inspection ports and geotextile wrap.

    Free Quote

    Competitive LyondellBasell Icorene 2550 YEW 2227 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 2550 YEW 2227 is a linear low density polyethylene (LLDPE) supplied as a free-flowing rotomoulding powder. The base resin is produced by copolymerization of ethylene with a short-chain alpha-olefin, yielding a molecular architecture that contains short-chain branches but lacks the long-chain branching characteristic of conventional high-pressure LDPE. The 2550 designation places the grade within the intermediate stiffness and high-toughness segment of the Icorene rotomoulding portfolio; the YEW 2227 suffix identifies the colour, stabilizer, or packaging configuration and should be specified at order entry. The powder is intended for processing on biaxial rotational moulding equipment, where it is charged into a cold mould, heated in a forced-air or gas-fired oven, and cooled under continuous rotation. Typical release testing for the grade includes melt mass-flow rate, density, tensile properties, flexural modulus, environmental stress-crack resistance, low-temperature impact, and dry flow. The grade is used in thick-walled parts such as storage tanks, agricultural chemical containers, playground components, and marine buoys, where low-temperature ductility and stress-crack resistance are more important than maximum rigidity.

    What limits processing latitude in rotational moulding with this LLDPE powder?

    Processing latitude is limited by the interplay between peak internal air temperature, oven residence time, powder particle size distribution, and cooling rate. On production-scale carousel and shuttle machines, oven setpoints between 260 °C and 320 °C are used, but the controlling parameter is the internal air temperature inside the mould, typically reaching 190 °C to 220 °C for complete densification. Internal air temperatures below 180 °C can leave porosity at the inner surface and reduce wall-thickness uniformity; temperatures above 230 °C for extended periods accelerate thermo-oxidative degradation, shift melt index, and cause yellowing in unpigmented parts. A rotation ratio of 4:1 or 5:1 is common for symmetrical moulds, while highly asymmetric parts require variable-speed direct-drive arms to prevent thin sections at corners. Baffle-mounted moulds and air-assisted powder charging are used to manage powder fines. Cycle time is adjusted by monitoring the internal air temperature trace; cooling with forced air followed by water spray is used to reduce warpage, but rapid cooling can increase residual stress and reduce low-temperature impact. No solvent is required; the powder is charged directly into the mould.

    For engineering design of thick-walled containers, tensile yield, flexural modulus, falling-weight impact, and environmental stress-crack resistance are the controlling properties. In LLDPE rotomoulding class materials with density near 0.935 g/cm³, tensile yield strength determined according to ASTM D638-14 is typically 14 MPa to 18 MPa, while flexural modulus under ISO 178:2019 is generally 450 MPa to 700 MPa. Elongation at break in unfilled formulations exceeds 800%, and the Vicat softening point under ISO 306/A50 is above 110 °C. Low-temperature brittleness under ASTM D746-20 is below -40 °C. Environmental stress-crack resistance under ASTM D1693-15e1 Condition B in 100% Igepal is typically greater than 1 000 h for this density class. Published data for the specific YEW 2227 configuration is limited; therefore these figures are presented as class-typical benchmarks and should be confirmed against the current LyondellBasell technical data sheet before design release.

    Comparative behaviour against LDPE, MDPE, and HDPE in thick-walled mouldings

    The product differs from LDPE mainly in molecular architecture and solid-state properties. Because the LLDPE backbone is linear with controlled short-chain branches, it exhibits higher tensile yield, higher flexural modulus, better puncture resistance, and better environmental stress-crack resistance than LDPE of equivalent melt index. Compared with HDPE, the lower density and lower crystallinity of Icorene 2550 YEW 2227 reduce stiffness and chemical resistance but improve low-temperature impact and ESCR. The grade sits near the upper density end of LLDPE and is therefore comparable to some MDPE rotomoulding grades; however, its melt-flow and stabilization package are optimized for rotomoulding rather than extrusion blow moulding. In comparison with lower-density Icorene grades near 0.920 g/cm³, the 2550 class provides higher flexural modulus and better dimensional stability at elevated temperatures, while sacrificing some low-temperature impact and ease of flow into complex ribs. Against higher-density rotomoulding grades near 0.940 g/cm³, the product offers a tougher crack-arrest response in thick-walled sections and is less prone to brittle failure at sub-zero temperatures. The choice between these classes is driven by the required balance between stiffness under load and impact at the minimum service temperature.

    PropertyLLDPE class, Icorene 2550 YEW 2227LDPEMDPEHDPE
    Density (g/cm³)0.935 supplier nominal0.915–0.9300.926–0.9400.940–0.970
    Flexural modulus (MPa)450–700200–400400–700800–1 500
    ESCR, 100% Igepal (h)Class-typical >1 0001–1050–50010–100
    Low-temperature impactHighModerateModerateLower in thick-walled sections

    Regulatory assessment is performed on the finished rotomoulded article rather than on the powder alone. For food-contact use, the base olefin polymer can be evaluated against 21 CFR 177.1520; compliance depends on the end-use conditions described in 21 CFR 177.1520(c) and on any colourants, processing aids, or additives introduced before moulding. In the European Union, overall migration and specific migration limits for finished articles are established under Regulation (EU) 10/2011; testing is completed on the moulded part because oven temperature and residence time can influence degradation products. The product is subject to REACH registration obligations under Regulation (EC) No 1907/2006. For electronics or electrical applications, the RoHS Directive 2011/65/EU applies to the finished component; unfilled, unpigmented LLDPE that is not intentionally doped with restricted substances is generally below the homogeneous-material maximum concentration values.

    When outdoor exposure governs stabilizer selection in LLDPE tanks

    When outdoor exposure governs stabilizer selection, the polymer must resist ultraviolet-induced chain scission, embrittlement, and surface chalking. Weather-resistant rotomoulding grades typically contain a hindered amine light stabilizer package and a UV absorber. Accelerated weathering under ASTM G154-23 Cycle 1 with UVA-340 lamps or ISO 4892-3:2024 is used for screening, while xenon-arc testing under ASTM D2565-23 or ISO 4892-2:2013 provides a broader spectral match for specification purposes. In class-typical LLDPE rotomoulding grades, unpigmented natural material can show chalking and microcracking after 1 000 h to 2 000 h of QUV exposure; UV-stabilized grades are often specified to retain at least 50% of original falling-weight impact after 3 000 h to 5 000 h. The YEW 2227 suffix may identify a specific UV-stabilized or custom colour package; if weather resistance is required, the supplier should confirm the exact stabilization package and any expected colour shift under ASTM G154 testing. Outdoor parts in high-UV climates should be evaluated with natural weathering correlation data, because accelerated tests do not fully capture the effect of thermal cycling and wet-dry stress.

    Powder-flow characteristics and the effect of 35-mesh versus 60-mesh fractions

    Powder flow and bulk density are determined by particle size distribution, particle shape, and surface moisture. Rotomoulding powders are typically ground to a top size of 500 µm (35 mesh); the fraction passing 250 µm (60 mesh) commonly falls between 20% and 40%. Excessive fines below 100 µm increase electrostatic adhesion, reduce bulk density, and can produce surface defects on the inner mould surface. Dry flow through a standard funnel under ASTM D1895 Method A is generally 25 s/100 g to 40 s/100 g for usable LLDPE rotomoulding powder; higher values indicate bridging in hoppers and uneven charging. Bulk density is usually 0.30 g/cm³ to 0.40 g/cm³. On production-scale shuttle machines, moulders observe that powders with a high fines fraction tend to stick to feed lines and produce corner thinning in deep-draw parts; vibratory feeders, air-assisted conveying, and ground straps on hoppers are used to reduce static charge. The powder should be stored in closed containers at ambient temperature and protected from moisture, because surface water can cause bubble defects during the early heating phase.

    RequirementStandardCondition or matrix
    Melt mass-flow rateISO 1133-1:2022 / ASTM D1238-20190 °C, 2.16 kg
    DensityISO 1183-1:2019 / ASTM D792-2023 °C
    Tensile yieldISO 527-2:2012 / ASTM D638-14Type IV specimen, 50 mm/min
    Flexural modulusISO 178:2019 / ASTM D790-172 mm/min
    Environmental stress-crack resistanceASTM D1693-15e1Condition B, 100% Igepal
    Brittleness temperatureASTM D746-20Low-temperature impact exposure
    Food contact21 CFR 177.1520 / (EU) 10/2011Finished article
    Accelerated weatheringASTM G154-23 / ISO 4892-3:2024QUV or condensation exposure

    Typical uses include agricultural chemical storage tanks, water tanks, road barriers, playground equipment, marine buoys, and corrosion-resistant liners. The material is selected where the part must withstand impact at temperatures below -20 °C and where contact with aqueous surfactants, weak acids, or alkalis requires resistance to environmental stress cracking. The upper continuous service temperature under low mechanical load is generally below 60 °C for this class; high loads at elevated temperatures can cause creep and stress relaxation. The material is not recommended for continuous contact with strong oxidizing acids, aromatic hydrocarbons, chlorinated solvents, or low-molecular-weight polar solvents at elevated temperatures, because these agents can cause swelling, stress cracking, or degradation. Processing should avoid prolonged exposure above 250 °C internal air temperature, and regrind levels should be controlled to maintain lot-to-lot impact consistency. If moisture absorption is suspected after storage at high relative humidity, drying at 60 °C to 70 °C for 1 h to 2 h may be used, although LLDPE is not hygroscopic.

    Top